A study on coil temperature bariation in 75% hydrogen batch annealing furnace (75% 수소 BATCH 소둔시에서의 코일 온도변화에 관한 연구)

  • Jeon, Eon-Chan;Kim, Soon-Kyung
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.11 no.2
    • /
    • pp.173-181
    • /
    • 1994
  • A Cold spot temperature control system for the batch annealing furnace has been estabilished in order to reduce energy consumption to improve productivity and stabilize the propertics of products. Therefore we confirmed a relation between annealing cycle time and atmospheric gas, variation of coil cold spot temperature with time during heating and actual temperature measurements at mid-width of each coil during heating and actual temperature measurements at mid-width of each coil during soaking. The results of the tempaeature variation effect on the batch annealing are as follows. 1) Heating time is reduced to one half with increasing atmospheric gas flow rate and changing of atmospheric gas component from HNx to Ax gas, and annealing cycle time is reduced to 2.7 times. 2) In case of short time healing, the slowest heating part is the center of B coil, in case of long time heating, the low temperature point moves from the center of coil to inside coil. And the temperature in this part is higher than other parts when cooling. When finished heating, the cold spot is located 1/3 of coil inside in case of HNx atmospheric gas. But center of coil in case of Ax atmospheric gas. 3) The outside of top coil is the highest temperature point when heating, which becomes the lowest temperature point when cooling. So, this point becomes high temperature zone at heating and low temperature zone at cooling, It has relation according to atmospheric gas component and flow rate. 4) Soaking time at batch annealing cycle determination is made a decision by the input coil width, and soaking time for quality homogenization of 1214mm width coil must be 2.5 hours longer than that of 914mm width coil for the same ciol weight. 5) Annealing cycle time with Ax atmospheric gas is extended 1 hour in of slow cooling during 5 hours in order to avoid rapid cooling.

  • PDF

Effective Annealing and Crystallization of Si film for Advanced TFT System

  • Noguchi, Takashi
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2009.10a
    • /
    • pp.254-257
    • /
    • 2009
  • The crystallization and activated annealing effect of Si films using an excimer laser and a new CW blue laser are described comparing with furnace annealing (SPC) for the application of advanced TFTs and future applications. Currently, pulsed ELA is used extensively as a LTPS process on glass substrates as the efficiency is high in UV region for thin Si film of 40- 60 nm thickness. ELA enables extremely low resistivity for both n- and p-typed Si films. On the other hand, CW BLDA enables the smooth Si surface having arbitral grains from micro-grains to anisotropic huge grain structure only controlling its power density.

  • PDF

Furnace Annealing Effect on Ferroelectric Hf0.5Zr0.5O2 Thin Films (강유전체 Hf0.5Zr0.5O2 박막의 퍼니스 어닐링 효과 연구)

  • Min Kwan Cho;Jeong Gyu Yoo;Hye Ryeon Park;Jong Mook Kang;Taeho Gong;Yong Chan Jung;Jiyoung Kim;Si Joon Kim
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.36 no.1
    • /
    • pp.88-92
    • /
    • 2023
  • The ferroelectricity in Hf0.5Zr0.5O2 (HZO) thin films is one of the most interesting topics for next-generation nonvolatile memory applications. It is known that a crystallization process is required at a temperature of 400℃ or higher to form an orthorhombic phase that results in the ferroelectric properties of the HZO film. However, to realize the integration of ferroelectric HZO films in the back-end-of-line, it is necessary to reduce the annealing temperature below 400℃. This study aims to comprehensively analyze the ferroelectric properties according to the annealing temperature (350-500℃) and time (1-5 h) using a furnace as a crystallization method for HZO films. As a result, the ferroelectric behaviors of the HZO films were achieved at a temperature of 400℃ or higher regardless of the annealing time. At the annealing temperature of 350℃, the ferroelectric properties appeared only when the annealing time was sufficiently increased (4 h or more). Based on these results, it was experimentally confirmed that the optimization of the annealing temperature and time is very important for the ferroelectric phase crystallization of HZO films and the improvement of their ferroelectric properties.

Reverse annealing of $P^+/B^+$ ion shower doped poly-Si

  • Jin, Beop-Jong;Hong, Won-Eui;Ro, Jae-Sang
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2006.08a
    • /
    • pp.752-755
    • /
    • 2006
  • Reverse annealing was observed in $P^+/B^+$ ion shower doped poly-Si upon activation annealing. Phosphorous or boron was implanted by ion shower doping using a source gas mixture of $PH_3/H_2$ or $B_2H_6/H_2$. Activation annealing was conducted using a tube furnace in the temperature ranges from $350^{\circ}C$ to $650^{\circ}C$. Hall measurement revealed that reverse annealing begins at different annealing temperatures for poly-Si implanted with P and B, respectively. It was observed that reverse annealing starts at $550^{\circ}C$$ in $P^+$ ion shower doped poly-Si, while at $350^{\circ}C$ in the case of B-doping.

  • PDF

Reverse annealing of boron doped polycrystalline silicon

  • Hong, Won-Eui;Ro, Jae-Sang
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.02a
    • /
    • pp.140-140
    • /
    • 2010
  • Non-mass analyzed ion shower doping (ISD) technique with a bucket-type ion source or mass-analyzed ion implantation with a ribbon beam-type has been used for source/drain doping, for LDD (lightly-doped-drain) formation, and for channel doping in fabrication of low-temperature poly-Si thin-film transistors (LTPS-TFT's). We reported an abnormal activation behavior in boron doped poly-Si where reverse annealing, the loss of electrically active boron concentration, was found in the temperature ranges between $400^{\circ}C$ and $650^{\circ}C$ using isochronal furnace annealing. We also reported reverse annealing behavior of sequential lateral solidification (SLS) poly-Si using isothermal rapid thermal annealing (RTA). We report here the importance of implantation conditions on the dopant activation. Through-doping conditions with higher energies and doses were intentionally chosen to understand reverse annealing behavior. We observed that the implantation condition plays a critical role on dopant activation. We found a certain implantation condition with which the sheet resistance is not changed at all upon activation annealing.

  • PDF

Effective Annealing and Crystallization of Si Film for Advanced TFT System

  • Noguchi, Takashi
    • Journal of Information Display
    • /
    • v.11 no.1
    • /
    • pp.12-16
    • /
    • 2010
  • The effect of the crystallization and activated annealing of Si films using an excimer laser and the new CW blue laser are described and compared with furnace annealing for application in advanced TFTs and for future applications. Pulsed excimer laser annealing (ELA) is currently being used extensively as a low-temperature poly-silicon (LTPS) process on glass substrates as its efficiency is high in the ultra-violet (UV) region for thin Si films with thickness of 40-60 nm. ELA enables extremely low resistivity relating to high crystallinity for both the n- and p-type Si films. On the other hand, CW blue laser diode annealing (BLDA) enables the smooth Si surface to have arbitral crystal grains from micro-grains to an anisotropic huge grain structure only by controlling its power density. Both annealing techniques are expected to be applied in the future advanced TFT systems.

Effect of Galvanizing Furnace Temperature on Material Property and Galvanized Surface of Hot Rolled Galvanized Steel

  • Jong Chan Jeong;Jae Joong Kim;Seong Ho Han
    • Corrosion Science and Technology
    • /
    • v.23 no.4
    • /
    • pp.278-282
    • /
    • 2024
  • Recently, hot rolled galvanized steel is widely used in automotive parts. As the paradigm of the automotive market has changed from fossil fuel vehicle to electric vehicle, the automotive industry needs more high-strength steels to reduce weights of automobiles. However, because high-strength steel contains high solute carbon, it is expected to have a risk of stretcher-strain on the surface due to dislocation trapping by solute [C] and [N]. Generally, galvanized steel is supposed to pass through a furnace around the temperature of Zinc pot to increase material temperature. Otherwise, the inhibition layer could not be formed. However, solute carbon and nitrogen are volatile enough to move around the furnace temperature. Moreover, the ratio of ferrite phase and precipitated Fe3C can be variable, resulting in yield point elongation related to the stretcher strain. Furthermore, the quality of the galvanized surface can be affected by a high temperature of the furnace. Although a relatively hot rolled galvanizing line furnace has a lower temperature than an annealing line furnace, it can affect various quality aspects. In other words, this paper aims to determine how these phenomena appear concerning furnace temperature.

A Study on the Performance Evaluation of Heat Treatment Furnace Design for Copper Tube Bending (동관 벤딩을 위한 열처리로 설계 및 성능평가에 관한 연구)

  • Park, Dae-kwang;Kim, Jae-yeol;Gao, Jia-Chen
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.15 no.1
    • /
    • pp.136-144
    • /
    • 2016
  • The air-conditioning industry is closely related to types of lifestyles, climate, and products. With the improvement of national income, the pursuit of pleasant living and working environments, and South Korea's four seasons and distinct climatic conditions, demand for air conditioning has increased. In addition, the industry is becoming increasingly precise and cooperative, and the increase in the domestic production of sophisticated air conditioning and continued growth of future industrial cooperation are expected to rapidly rise. Accordingly, the study of air piping systems can improve the productivity and quality of products and cost savings and can achieve vibration reduction. Additionally, using a heat treatment furnace for copper tube annealing treatment reduces the risk of using an oxy-acetylene torch.

The Thermoelectric Properties of p-type SiGe Alloys Prepared by RF Induction Furnace (고주파 진공유도로로 제작한 p형 SiGe 합금의 열전변환물성)

  • 이용주;배철훈
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.5
    • /
    • pp.432-437
    • /
    • 2000
  • Thermoelectric properties of p-type SiGe alloys prepared by a RF inductive furnace were investigated. Non-doped Si80Ge20 alloys were fabricated by control of the quantity of volatile Ge. The carrier of p-type SiGe alloy was controlled by B-doping. B doped p-type SiGe alloys were synthesized by melting the mixture of Ge and Si containing B. The effects of sintering/annealing conditions and compaction pressure on thermoelectric properties (electrical conductivity and Seebeck coefficient) were investigated. For nondoped SiGe alloys, electrical conductivity increased with increasing temperatures and Seebeck coefficient was measured negative showing a typical n-type semiconductivity. On the other hand, B-doped SiGe alloys exhibited positive Seebeck coefficient and their electrical conductivity decreased with increasing temperatures. Thermoelectric properties were more sensitive to compaction pressure than annealing time. The highest power factor obtained in this work was 8.89${\times}$10-6J/cm$.$K2$.$s for 1 at% B-doped SiGe alloy.

  • PDF

Dopant-Activation and Damage-Recovery of Ion-Shower-Doped Poly-Si through $PH_3/H_2$ after Furnace Annealing

  • Kim, Dong-Min;Kim, Dae-Sup;Ro, Jae-Sang;Choi, Kyu-Hwan;Lee, Ki-Yong
    • Journal of Information Display
    • /
    • v.5 no.1
    • /
    • pp.1-6
    • /
    • 2004
  • Ion shower doping with a main ion source of $P_2H_x$ using a source gas mixture of $PH_3/H_2$ was conducted on excimer-laser- annealed (ELA) poly-Si. The crystallinity of the as-implanted samples was measured using a UV-transmittance. The measured value of as-implanted damage was found to correlate well with the one calculated through/obtained from TRIM-code simulation. The sheet resistance was found to decrease as the acceleration voltage increased from 1 kV to 15 kV at a doping time of 1 min. However, it increases as the acceleration voltage increases under severe doping conditions. Uncured damage after furnace annealing is responsible for the rise in sheet resistance.