• Title/Summary/Keyword: annealing ambient

Search Result 319, Processing Time 0.023 seconds

Dependence of RF power of ($Ba_{0.5}Sr_{0.5})TiO_3$ thin film using RF magnetron sputtering (RF magnetron sputtering을 이용한 ($Ba_{0.5}Sr_{0.5})TiO_3$ 박막의 RF power 의 존성)

  • 최형윤;이태일;정순원;박인철;최동한;김흥배
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.07a
    • /
    • pp.51-54
    • /
    • 2000
  • In this paper, $Ba_{0.5}$Sr$_{0.5}$TiO$_3$ thin films were prepared on Pt/Ti/SiO$_2$/Si substrate by RF magnetron sputtering method. We investigated effect of deposition conditions (especially RF input power) on structural properties of BST thin films. Deposit conditions of BST films were set working gas ratio, Ar:O$_2$= 70 : 30, working pressure 10mTorr, and RF input power 25W, 50W, 75W and 100W. Post-annealing using rapid thermal annealing(RTA) performed at 45$0^{\circ}C$, 55$0^{\circ}C$, $650^{\circ}C$, and 75$0^{\circ}C$ in oxigen ambient for 60 sec, respectively. The structural properties of BST films on Pt/Ti/SiO$_2$/Si substrate analysed by X-ray diffraction(XRD).).).

  • PDF

A properties of ZnO thin film deposited by magnetron sputtering and its resistivity and microstructure due to annealing (Magnetron sputtering으로 증착한 ZnO 박막의 특성과 열처리에 따른 비저항과 미세구조)

  • 이승환;성영권;김종관
    • Electrical & Electronic Materials
    • /
    • v.10 no.2
    • /
    • pp.126-133
    • /
    • 1997
  • In order to apply for the gas sensing layer and the piezoelectric thin film devices, we studied the effects of magnetron sputtering conditions and annealing temperature on the electrical and structual characteristics of the ZnO thin film. The optimal deposition conditions, in order to obtain a c axis of the ZnO (002) phase thin film which is perpendicular to SiO$_{2}$/Si substrate, were like these ; substrate temperature 150.deg. C, chamber pressure 2 mtorr, R.F. power 300 watts, gas flow ratio 0.4[O$_{2}$(Ar + $O_{2}$)]. When the ZnO thin film was annealed in 600.deg. C, $O_{2}$ gas ambient for 1 hr, the resistivity was 2.6 x 10$^{2}$.ohm.cm and the grain size of ZnO thin film was less than 1 .mu.m. So the ZnO thin film acquired from above conditions can apply for the gas sensing layer which require a c axis perpendicular to the substrate surface.

  • PDF

Annealing Temperature of Nickel Oxide Hole Transport Layer for p-i-n Inverted Perovskite Solar Cells (P-I-N 역구조 페로브스카이트 태양전지 응용을 위한 Nickel oxide 홀전달층의 열처리 온도 연구)

  • Gisung Kim;Mijoung Kim;Hyojung Kim;JungYup Yang
    • Current Photovoltaic Research
    • /
    • v.11 no.4
    • /
    • pp.103-107
    • /
    • 2023
  • A Nickel oxide (NiOx) thin films were prepared via sol-gel process on a transparent conductive oxide glass substrate. The NiOx thin films were spin-coated in ambient air and subsequently annealed for 30 minutes at temperatures ranging from 150℃ to 450℃. The structural and optical characteristics of the NiOx thin films annealed at various temperatures were measured using X-ray diffraction, field emission scanning electron microscopy, and ultraviolet-visible spectroscopy. After optimizing the NiOx coating conditions, perovskite solar cells were fabricated with p-i-n inverted structure, and its photovoltaic performance was evaluated. NiOx thin films annealed at 350℃ exhibited the most favorable characteristics as a hole transport layer, resulting in the highest power conversion efficiency of 17.88 % when fabricating inverted perovskite solar cells using this film.

Formation of Size-controllable Ag Nanoparticles on Si Substrate by Annealing (크기 조절이 가능한 은 나노입자 형성을 위한 박막의 열처리 효과)

  • Lee, Sang Hoon;Lee, Tae Il;Moon, Kyeong-Ju;Myoung, Jae Min
    • Korean Journal of Materials Research
    • /
    • v.23 no.7
    • /
    • pp.379-384
    • /
    • 2013
  • In order to produce size-controllable Ag nanoparticles and a nanomesh-patterned Si substrate, we introduce a rapid thermal annealing(RTA) method and a metal assisted chemical etching(MCE) process. Ag nanoparticles were self-organized from a thin Ag film on a Si substrate through the RTA process. The mean diameter of the nanoparticles was modulated by changing the thickness of the Ag film. Furthermore, we controlled the surface energy of the Si substrate by changing the Ar or $H_2$ ambient gas during the RTA process, and the modified surface energy was evaluated through water contact angle test. A smaller mean diameter of Ag nanoparticles was obtained under $H_2$ gas at RTA, compared to that under Ar, from the same thickness of Ag thin film. This result was observed by SEM and summarized by statistical analysis. The mechanism of this result was determined by the surface energy change caused by the chemical reaction between the Si substrate and $H_2$. The change of the surface energy affected on uniformity in the MCE process using Ag nanoparticles as catalyst. The nanoparticles formed under ambient Ar, having high surface energy, randomly moved in the lateral direction on the substrate even though the etching solution consisting of 10 % HF and 0.12 % $H_2O_2$ was cooled down to $-20^{\circ}C$ to minimize thermal energy, which could act as the driving force of movement. On the other hand, the nanoparticles thermally treated under ambient $H_2$ had low surface energy as the surface of the Si substrate reacted with $H_2$. That's why the Ag nanoparticles could keep their pattern and vertically etch the Si substrate during MCE.

A Study on Properites of PV Solar cell AZO thin films post-annealing by RTP technique (RTP 공정을 통한 태양전지용 AZO 박막의 후열처리 특성연구)

  • Yang, Hyeon-Hun;Kim, Han-Wool;Han, Chang-Jun;So, Soon-Youl;Park, Gye-Choon;Lee, Jin;Chung, Hea-Deok;Lee, Suk-Ho;Back, Su-Ung;Na, Kil-Ju;Jeong, Woon-Jo
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2011.05a
    • /
    • pp.127.1-127.1
    • /
    • 2011
  • In this paper, ZnO:Al thin films with c-axis preferred orientation were prepared on Soda lime glass substrates by RF magnetron sputtering technique. AZO thin film were prepared in order to clarify optimum conditions for growth of the thin film depending upon process, and then by changing a number of deposition conditions and substrate temperature conditions variously, structural and electrical characteristics were measured. For the manufacture of the AZO were vapor-deposited in the named order. It is well-known that post-annealing is an important method to improve crystal quality. For the annealing process, the dislocation nd other defects arise in the material and adsorption/decomposition occurs. The XRD patterns of the AZO films deposited with grey theory prediction design, annealed in a vacuum ambient($2.0{\times}10-3$Torr)at temperatures of 200, 300, 400 and $500^{\circ}C$ for a period of 30min. The diffraction patterns of all the films show the AZO films had a hexagonal wurtzite structure with a preferential orientation along the c-axis perpendicular to the substrate surface. As can be seen, the (002)peak intensities of the AZO films became more intense and sharper when the annealing temperature increased. On the other hand, When the annealing temperature was $500^{\circ}C$ the peak intensity decreased. The surface morphologies and surface toughness of films were examined by atomic force microscopy(AFM, XE-100, PSIA). Electrical resistivity, Gall mobility and carrier concentration were measured by Hall effect measuring system (HL5500PC, Accent optical Technology, USA). The optical absorption spectra of films in the ultraviolet-visibleinfrared( UV-Vis-IR) region were recorder by the UV spectrophotometer(U-3501, Hitachi, Japan). The resistivity, carrier concentration, and Hall mobility of ZnS deposited on glass substrate as a function of post-annealing.

  • PDF

Large-Area Synthesis of High-Quality Graphene Films with Controllable Thickness by Rapid Thermal Annealing

  • Chu, Jae Hwan;Kwak, Jinsung;Kwon, Tae-Yang;Park, Soon-Dong;Go, Heungseok;Kim, Sung Youb;Park, Kibog;Kang, Seoktae;Kwon, Soon-Yong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.08a
    • /
    • pp.130.2-130.2
    • /
    • 2013
  • Today, chemical vapor deposition (CVD) of hydrocarbon gases has been demonstrated as an attractive method to synthesize large-area graphene layers. However, special care should be taken to precisely control the resulting graphene layers in CVD due to its sensitivity to various process parameters. Therefore, a facile synthesis to grow graphene layers with high controllability will have great advantages for scalable practical applications. In order to simplify and create efficiency in graphene synthesis, the graphene growth by thermal annealing process has been discussed by several groups. However, the study on growth mechanism and the detailed structural and optoelectronic properties in the resulting graphene films have not been reported yet, which will be of particular interest to explore for the practical application of graphene. In this study, we report the growth of few-layer, large-area graphene films using rapid thermal annealing (RTA) without the use of intentional carbon-containing precursor. The instability of nickel films in air facilitates the spontaneous formation of ultrathin (<2~3 nm) carbon- and oxygen-containing compounds on a nickel surface and high-temperature annealing of the nickel samples results in the formation of few-layer graphene films with high crystallinity. From annealing temperature and ambient studies during RTA, it was found that the evaporation of oxygen atoms from the surface is the dominant factor affecting the formation of graphene films. The thickness of the graphene layers is strongly dependent on the RTA temperature and time and the resulting films have a limited thickness less than 2 nm even for an extended RTA time. The transferred films have a low sheet resistance of ~380 ${\Omega}/sq$, with ~93% optical transparency. This simple and potentially inexpensive method of synthesizing novel 2-dimensional carbon films offers a wide choice of graphene films for various potential applications.

  • PDF

Effect of the Hydrogen Annealing on the Pb(Zr0.52Ti0.48)O3 Film using (Pb0.72La0.28)Ti0.94O3 Buffers ((Pb0.72La0.28)Ti0.94O3 Buffer를 사용한 Pb(Zr0.52Ti0.48)O3 박막의 수소 후열처리 효과)

  • Lee, Eun-Sun;Li, Dong-Hua;Chung, Hyun-Woo;Lim, Sung-Hoon;Lee, Sang-Yeol
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.18 no.4
    • /
    • pp.327-329
    • /
    • 2005
  • Pb(Zr/sub 0.52/Ti/sub 0.48/)O₃(PZT) thin films were deposited by using a pulsed laser deposition method on a Pt/Ti/SiO₂/Si substrate with (Pb/sub 0.72/La/sub 0.28/)Ti/sub 0.93/O₃ (PLT) buffer and on a Pt/Ti/SiO₂/Si substrate without buffer. These films were annealed in H₂-contained ambient for 30 minutes at the substrate temperature of 400。C to evaluate the forming gas annealing effects. The comparative studies on the ferroelectric properties of these two films were carried out, which are shown that ferroelectric properties, such as remanent polarization didn't change in the case of PLT buffered PZT film while remanent polarization value of PZT film degraded from 20.8 C/㎠ to 7.3 C/㎠. The leakage current became higher in both cases, but that of the more-oriented PZT film had the moderate value of the 10/sup -6/ order of A/㎠. This is mainly because the hydrogen atoms which make the degradation of PZT films cannot infiltrate into the more -oriented PZT film as well as the less-oriented PZT film.

Effects of Ti or Ti/TiN Underlayers on the Crystallographic Texture and Sheet Resistance of Aluminum Thin Films (Ti 또는 Ti/TiN underlayer가 Al 박막의 배향성 및 면저항에 미치는 영향)

  • Lee, Won-Jun;Rha, Sa-Kyun
    • Korean Journal of Materials Research
    • /
    • v.10 no.1
    • /
    • pp.90-96
    • /
    • 2000
  • The effects of the type and thickness of underlayers on the crystallographic texture and the sheet resistance of aluminum thin films were studied. Sputtered Ti and Ti/TiN were examined as the underlayer of the aluminum films. The texture and the sheet resistance of the metal thin film stacks were investigated at various thicknesses of Ti or TiN, and the sheet resistance was measured after annealing at $400^{\circ}C$ in an nitrogen ambient. For the Ti underlayer, the minimum thickness to obtain excellent texture of aluminum <111> was 10nm, and the sheet resistance of the metal stack was greatly increased after annealing due to the interdiffusion and reaction of Al and Ti. TiN between Ti and Al could suppress the Al-Ti reaction, while it deteriorated the texture of the aluminum film. For the Ti/TiN underlayer, the minimum Ti thickness to obtain excellent texture of aluminum <111> was 20nm, and the minimum thickness of TiN to function as a diffusion barrier between Ti and Al was 20nm.

  • PDF

Fabrications and Properties of Al/$VF_2$/$n^+$-Si(100) Structures by Dip Coating Methode (Dip Coating 법에 의한 Al/$VF_2$-TrFE/Si(100) 구조의 제작 특성)

  • Kim, Ka-Lam;Jeong, Sang-Hyun;Yun, Hyeong-Seon;Lee, Woo-Seok;Kwak, No-Won;Kim, Kwang-Ho
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.20-21
    • /
    • 2008
  • Ferroelectric vinylidene fluoride-trifluoroethylene ($VF_2$-TrFE) copolymer films were directly deposited on degenerated Si ($n^+$, 0.002 $\Omega{\cdot}cm$) using by dip coating method. A 1 ~ 3 wt% diluted solution of purified vinylidene fluoride-trifluoroethylene ($VF_2$:TrFE=70:30) in a dimethylformamide (DMF) solvent were prepared and deposited on silicon wafers using dip coating method for 10 seconds. After Post-Annealing in a vacuum ambient at 100~200 $^{\circ}C$ for 60 min, upper aluminum electrodes were deposited by thermal evaporation through the shadow mask to complete the MFS structure. The ferroelectric $\beta$-phase peak of films, depending on the annealing temperature, started to show up around $125^{\circ}C$, and the intensity of the peak increased with increasing annealing temperature. Above $175^{\circ}C$, the peak started to decrease. The C-V characteristics were measured using a Precision LCR meter (HP 4284A) with frequency of 1MHz and a signal amplitude of 20 mV. The leakage-current versus electric-field characteristics was measured by mean of a pA meter/DC voltage source (HP 4140B).

  • PDF

Study on Characteristics of 4H-SiC MOS Device with PECVD SiON Insulator (PECVD SiON 절연막을 이용한 4H-SiC MOS 소자 특성 연구)

  • Kim, Hyun-Seop;Lee, Jae-Gil;Lim, Jongtae;Cha, Ho-Young
    • Journal of IKEEE
    • /
    • v.22 no.3
    • /
    • pp.706-711
    • /
    • 2018
  • In this work, we have investigated the characteristics of 4H-SiC metal-oxide-semiconductor (MOS) devices with silicon oxynitride (SiON) insulator using plasma enhanced chemical vapor deposition (PECVD). After post metallization annealing, the trap densities of the fabricated devices decreased significantly. In particular, the device annealed at $500^{\circ}C$ in forming gas ambient exhibited excellent MOS characteristics along with negligible hysteresis, which proved the potential of PECVD SiON as an alternative gate insulator for use in 4H-SiC MOS device.