• Title/Summary/Keyword: alkali perspiration

Search Result 16, Processing Time 0.017 seconds

Dyeing of Silk Fabric with Amur Cork Tree (황백에 의한 견직물의 염색)

  • Kim, Byung Hee;Cho, Seung Sik
    • Textile Coloration and Finishing
    • /
    • v.8 no.1
    • /
    • pp.26-33
    • /
    • 1996
  • The berberine from Amur cork tree is natural yellow dye and can be extracted more easily by water. The berberine is basic dye and was extracted at 90-95$^{\circ}C$. We have obtained the following results; 1. K/S value in the abstract of dye was increased by time-elapsing, but the reasonable time was between 90-120min. 2. The reasonable weight of Amur cork tree in the abstract of dye was between 10-20 g/L. 3. We obtained various colors in case of using mordants. ―In case of 10g/L and 20g/l, the reasonable value of mordant was 5-10%(owf). and in case of using tannic acid and $FeSO_{4}$ we could obtain high K/S value. 4. &{\lambda}_{max}& of UV spectra was shown 420nm. 5. Genarally fastness of drycleaning indicated more than grade 4. but it of perspiration was more stable in acid than alkali.

  • PDF

Dyeing of silk in green color used kudzu-vine leaves (칡잎을 이용한 견직물의 녹색염 연구)

  • 정영옥
    • Korean Journal of Rural Living Science
    • /
    • v.10 no.2
    • /
    • pp.28-36
    • /
    • 1999
  • The purpose of this study was to examine the best condition for dyeing silk in green color used kudzu-vine leaves which were available everywhere in our country except winter. Dyeing experiments were done under various dyeing conditions according to extracting method of dyebath from kudsu-vine leaves, pH of dyebath, dyeing time, concentration of dyebath and mordants which were treated after dyeing. Color difference ($\Delta$E) and Munsell's HV/C and color fastness to drycleaning, washing, perspiration and light were measured. The main results were as follows : 1. The color difference of dyed silk increased in dyebath B & C which were extracted in alkali water comparing with dyebath A which was extracted in distilled water. In dyebath B & C, the color difference was the highest in case of dyebath pH 5.0. 2. The colors of fabrics dyed in dyebath A were mainly yellow and the colors in dyebath B & C were yellow green. 3. The color differences of dyed silk increased according to dyeing time and concentration of dyebath. 4. The color were changed with the treatment of mordants. The most strong green color could get in Cu mordant treatment in dyebath C, pH 5.0, and concentration 4. 5. The peak of reflectance within the visible light of the fabric dyed in the most strong green color could be seen in $\lambda$500-520nm. 6. On the whole, the colorfastness of experimental fabrics dyed in dyebath B, C and Cu mordant treatment was good except the colorfastness to the light.

  • PDF

A Study on the Property of Hair Dyed with Fermented Indigo (천연염료 발효(天然染料 醱酵) 쪽으로 염색(染色)한 모발(毛髮)의 특성 연구(特性 硏究))

  • Kim, Kyung-Sun;Lee, In-Sook;Jeon, Dong-Won;Ha, Byung-Jo
    • Journal of Fashion Business
    • /
    • v.10 no.1
    • /
    • pp.120-131
    • /
    • 2006
  • Recently, it has been reported that chemical hair coloring can cause allergic reactions, the toxicity issue of chemical hair color was issued. Therefore, there is an increasing interest in the hair coloration technique using non-toxic and bio-compatible hair color gotten from natural resource. In this study, the possibility using fermented Indigo as natural hair coloring agent was investigated. Bleached hair samples were dyed using Indigo, and the effect of dyeing frequency, the physical change after dyeing, color, surface and cross-section characteristics, and tensile property were also studied. In addition, the protection property of cationic detergent finishing on damaged hair samples were also studied. The following conclusions are made; 1. While bleached hair samples with low value showed the negligible effect of repeated dyeing, bleached hair samples with high value showed the good effect of repeated dyeing. 2. Hair sample dyed with Indigo showed a high light-fastness, however, tensile strength and elongation showed very low values (high damage on hair sample). 3. Cationic detergent finishing did not affect on the colorfastness because of decoloration after dyeing, however, it increased the smoothness of hair sample, and therefore, can use as protectant of damaged hair. 4. Hair scale was damaged after dyeing. It seemed that the alkali, potassium carbonate, increased pH of dyeing bath to 11, as a result, the hair was swollen, weaken, and dissolved on the prolonged dyeing time. Dyed hair sample became stiff and fine. 5. The color difference was 4.62 (a high fastness value) in the test of sunlight exposure, shampoo, cationic detergent finishing, and acid perspiration fastness.

Synthesis of Azo based Disperse Dyes for Dyeing Polyester Fiber in Supercritical Carbon Dioxide (초임계 유체 염색용 아조계 분산염료 합성 및 PET 섬유에 대한 염색 특성 연구)

  • Shin, Seung-Rim;An, Kyoung-Lyong;Lee, Sunhye;Lee, Seung Eun;Ko, Eunhee;Kim, Changil;Jun, Kun
    • Textile Coloration and Finishing
    • /
    • v.31 no.3
    • /
    • pp.135-146
    • /
    • 2019
  • A series of azo based disperse dyes were synthesized and applied to polyester(PET) fiber in supercritical carbon dioxide($ScCO_2$). Various aniline derivatives were used as diazo component and coupled with glycine ethylester or carbonic acid ethylester derivatives to give azo based disperse dyes. Depending on the various diazo substituents, absorption maxima varied from 415 to 529nm in acetone. Dyeing in $ScCO_2$ was carried out at $120^{\circ}C$ and 250bar pressure for 2hrs with 0.5% o.w.f. of dye concentration. Dyed PET fiber had excellent brightness and good light, washing and perspiration(acid/alkali) fastness properties.

Synthesis of Azo Based Disperse Dyes for Dyeing Polyester Fiber in Supercritical Carbon Dioxide (초임계 유체 염색용 아조계 분산염료 합성 및 PET 섬유에 대한 염색 특성 연구)

  • Shin, Seung-Rim;An, Kyoung-Lyong;Lee, Sunhye;Ko, Eunhee;Lee, In-Yeol;Kim, Changil;Jun, Kun
    • Textile Coloration and Finishing
    • /
    • v.33 no.1
    • /
    • pp.10-23
    • /
    • 2021
  • In order to synthesize the dye suitable for supercritical carbon dioxide(ScCO2) dyeing, a series of azo based disperse dyes were prepared using various aniline derivatives as diazo components and indol derivatives as coupling components. Dyeing process in ScCO2 of the synthesized dyes was performed on PET fiber at 120℃ for 2 hrs under 250bar pressure with 0.5% o.w.f. of dye concentration. The absorption maxima varied from 400 to 580nm depending on the substituted groups in aniline derivatives and the indol derivatives. The dyes showed high molar extinction coefficients(ε) of 27,000~61,000M-1cm-1. Dyed PET fiber exhibited excellent brightness and good light, washing and perspiration(acid/alkali) fastness properties.

Eco-friendly, natural dyeing of linen, ramie, and hemp fabrics using Polygonum tinctoria (친환경을 위한 마직물(아마, 저마, 대마)의 쪽 천연염색에 관한 연구)

  • Mikyoung Kim
    • The Research Journal of the Costume Culture
    • /
    • v.31 no.2
    • /
    • pp.161-172
    • /
    • 2023
  • In this study, natural dyeing using Polygonum tinctoria was performed with linen, ramie, and hemp, which are biodegradable cellulose fibers, considering environmental aspects. In particular, the impacts of alkali NaOH and reducing agent Na2S2O4 were examined, and the possibilities of minimizing the use and reusing the dye were explored. The surface dye concentrations were found to be in the following order: hemp>linen>ramie. With the increase in all additives, the L* value decreased, and the ⊿E and K/S values increased gradually. When Na2S2O4 was 1g/L, the surface color of the dye appeared uniformly from the NaOH concentration of 0.4g/L (pH 10.84). When NaOH was 0.4g/L, the K/S values of linen and ramie increased rapidly after 0.4g/L of Na2S2O4, and hemp maintained a stable color from 0.6g/L of Na2S2O4. With the increase in the dye concentration from 1 to 6g/L, all the fibers were dyed uniformly. The K/S value increased or higher doubled upon repeated dyeing six times for 5 min than when dyed only once for 30 min. Therefore, the linen, ramie, and hemp fibers dyed repeatedly exhibited good washing, rubbing, and colorfastness to perspiration, which was rated between 4 and 4-5, and that to light was rated as 5. Moreover, no discoloration due to sunlight was observed. Finally, linen exhibited a bacterial reduction of 99.9%, thereby indicating its excellent antibacterial property.