Park, Yong-Ha;Park, Yong-Ho;Cho, Kyung-Mox;Park, Ik-Min
Journal of Korea Foundry Society
/
v.28
no.6
/
pp.268-272
/
2008
Interfacial characteristics of aluminum borate whisker reinforced AS52 matrix composite was investigated. Peak hardness of AS52 composite was obtained aging at $170^{\circ}C$ for 15h and the aging process was accelerated by the presence of the aluminium borate whisker. The MgO layer, which was the interfacial reaction product between the reinforcement and the Mg matrix, was produced with 20 nm thickness in as-cast condition. As the aging time increased, the thickness of the interfacial reaction layer increased to 50 nm in peak aged condition. The nano-indentation test results indicated that the strength of interface was improved by the aging but over-aging degraded the reinforcement and decreased the interfacial strength which resulted in the decrease of overall composite strength.
Journal of the Korean Society of Industry Convergence
/
v.24
no.3
/
pp.261-269
/
2021
This study was evaluated the elastic wave properties according to tension of Incoloy 825 alloy with different solution treatment temperature and aging time. Solution treatment was carried out at 700, 800, 900, and 1000 ℃ for 1 hour, and aging was carried out at 700 ℃ for 1, 5, 10, and 30 hours. As the solution treatment temperature increased, the tensile strength decreased and the elongation increased. However, as the aging time increased, the tensile strength increased and the elongation decreased. The dominant frequency decreased as the solution treatment temperature increased, but increased as the aging time increased. The dominant frequency according to the solution treatment and aging time increased as the tensile strength increased, but increased despite the decrease in elongation.
The purpose of this study is to suggest an anti-aging health care plan through a literature analysis of the life activity system of Oriental Medicine. The source of normal maintenace, development, and change of the natural world and the human body's life activity process is the dynamical cooperative equilibrium of the internal Shen-Ji's discipline that creates, grows, changes, makes differences and stores(生长化收藏) and external Qi-Li's process of change from birth to growth, maturity to old age and ending of life(生長壯老已). Therefore, it was analyzed that the natural and human life activity processes are normally maintained, developed, and transformed. As a result, when the natural healing power of Genuine-Qi, the source of the human vitality, rises with the 'breathing massage' that combines a static breathing method which is anti-aging health care method applying the lifting entering movement of Qi and a dynamic abdominal massage, and it harmonizes the Shen-Ji which is the life process system and Qi-Li so that it is believed to be helpful in prolonging a healthy lifespan.
Transactions of the Korean Society of Automotive Engineers
/
v.13
no.3
/
pp.80-86
/
2005
In this study, we investigated the characteristics of the conversion efficiency and the effect of ageing Diesel Oxidation Catalyst (DOC). The DOC was composed of Warm-up Catalytic Converter (WCC) and Underbody Catalytic Converter (UCC). As the result, the conversion efficiency of THC was 10$\~$50$\%$ on WCC and 30$\~$40$\%$ on UCC .The conversion efficiency of CO was 80$\~$90$\%$ on WCC and remained 10$\~$20$\%$ of CO was purified on UCC. The WCC shows high conversion efficiency on CO. After 20 hours aging process of engine bench, conversion efficiencies of THC and CO were improved a little, because it was activated catalyst surface by 20 hours aging. In case of 80 hours aging, the conversion efficiencies of THC and CO were decreased on WCC. However, the UCC was not affected by aging process .
This study has investigated the effect of aging treatment on the microstructure and mechanical properties of Mg-6Al-xZn(x = 1.5, 2.5) alloys fabricated by the squeeze casting process. The microstructures of as-squeeze cast were composed of pro-eutectic ${\alpha}$, super saturated ${\alpha}$ and ${\beta}(Mg_{17}Al_{12})$ compound. Aged at both $200^{\circ}C$ and $240^{\circ}C$, Mg-6Al-xZn alloys showed the peak hardness due to the formation of ${\beta}(Mg_{17}Al_{12})$ precipitates. The discontinuous precipitates of the lamella type are predominant at $200^{\circ}C$ aging treatment, while the finely dispersed continuous precipitates were dominant at $240^{\circ}C$ aging treatment. Mg-6Al-xZn alloys fabricated by the squeeze casting process had the better combination of tensile strength and elongation compared to the conventionally cast alloys. As zinc contents increased, the tensile strength was increased by the solid solution strengthening effect of zinc.
The effect of humidity on crystallization and polymorphic transformation of hydrous aluminum oxide under various humidity at $37^{\circ}$ was examined by means of X-ray diffraction, scanning electron micrograph, IR spectra and DTA. The humidity was an important factor influencing crystallization of hydrous aluminum oxide. The growth or crystal was strongly accelerated by humidity. The aging process is assumed that it is composed of two seperate steps, an increase of the diffraction around $36{\sim}42^{\circ}$, and an appearance and its development of the peak at $18{\sim}20^{\circ}$ of $2{\theta}$ value. The former is considered to be nucleation and the latter correspond to the growth period on crystallization. The crystalline form of aging products was various depending on the degree of humidity, directly it leads to the eventual formation of bayerite in more than 72%, $b{\"{o}}hmite$ in 50% and resembled to Nordstandite in 0% relative humidity, respectively but once formed, it was mostly stable in each surroundings and does not transform to the other more stable form in solid state even after aging for five years. The mechanism responsible for aging is further polymerization process of six-membered rings by deprotonation-dehydration reaction in which positively charged polynuclear hydroxy aluminum complexes formed in the presence of moisture are joined at their edges by double hydroxide bridges.
The present paper describes the effects of pressure and post-mortem aging treatments on in situ proteasome activity in rabbit and bovine skeletal muscles. Synthetic peptide hydrolyzing activity of rabbit proteasomes remained in the muscle after exposure to pressures up to 100 MPa. However, when a pressure of 400 MPa or more was applied, proteasomes were markedly inactivated. The extraction of proteasomes from excessively pressurized muscle appeared to be difficult. Proteasomes in aged muscle remained relatively stable throughout the aging process, with activity after 168 h (7 days) being 35%, 48%, 53% and 31% of the 0 h post-mortem LLVY, LSTR, AAF and LLE total hydrolyzing activities, respectively. The synthetic peptide hydrolyzing activities of bovine muscle proteasomes were similar to those of rabbit skeletal muscle proteasomes. The results suggest that synthetic peptide hydrolyzing activity remains in muscle exposed to relatively low pressures. Furthermore, it is known that high-pressure treatment induces fragmentation of myofibrils, modification of actin-myosin interaction and activation of intramuscular proteinases, cathepsins and calpains. Thus, proteasomes are probably involved in the tenderization process in combination with other intramuscular proteinases under high-pressure conditions. Our findings confirmed that proteasomes play a role in meat tenderization induced by high-pressure treatment or aging.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2003.07a
/
pp.335-338
/
2003
Chemical mechanical polishing (CMP) process has been widely used to planarize dielectric layers, which can be applied to the integrated circuits for sub-micron technology. Despite the increased use of CMP process, it is difficult to accomplish the global planarization of in the defect-free inter-layer dielectrics (ILD). Especially, defects such as micro-scratch lead to severe circuit failure which affect yield. CMP slurries can contain particles exceeding $1\;{\mu}m$ in size, which could cause micro-scratch on the wafer surface. In this paper, we have studied aging effect the of CMP sin as a function of particle size. We prepared and compared the self-developed silica slurry by adding of abrasives before and after annealing. As our preliminary experiment results, we could be obtained the relatively stable slurry characteristics comparable to original silica slurry in the slurry aging effect.
Journal of the Korean institute of surface engineering
/
v.53
no.2
/
pp.43-52
/
2020
Various aging treatments were conducted on AISI 630 martensitic precipitation hardening stainless steel in order to optimize aging condition. Aging treatment was carried out in the vacuum chamber of Ar gas with changing aging temperature from 380℃ to 430℃ and aging time from 2h to 8h at 400℃. After obtaining the optimized aging condition, several nitrocarburizing treatments were done without and with the aging treatment. Nitrocarburizing was performed on the samples with a gas mixture of H2, N2 and CH4 for 15 h at vacuum pressure of 4.0 Torr and discharge voltage of 400V. The corrosion resistance was improved noticeably by combined process of aging and nitrocarburizing treatment, which is attributed to higher chromium and nitrogen content in the passive layer, as confirmed by XPS analysis. The optimized condition is finalized as, 4h aging at 400℃ and then subsequent nitrocarburizing at 400℃ with 25% nitrogen and 4% methane gas for 15h at vacuum pressure of 4.0 Torr and discharge voltage of 400V, resulting in the surface hardness of around 1300 HV0.05 and α'N layer thickness of around 11 ㎛ respectively.
Based on the actual operating environment of transformer, the aging tests of nitrile butadiene rubber (NBR) were conducted systematically under four conditions: in air, in transform oil, under compression in air and under compression in transform oil to studythe effect of high temperature, transform oil and compression stress simultaneously on the thermal aging behaviors of nitrile butadiene rubber and predict the lifetime. The effects of liquid media and compression stress simultaneously on the thermal aging behaviors of nitrile butadiene rubber were studied by using characterization methods such as IR spectrosc-opy, thermogravimetric measurements, Differential Scanning Calorimetry (DSC) measurements and mechanical property measurements. The changes in physical properties during the aging process were analyzed and compared. Different aging conditions yielded materials with different properties. Aging at $70^{\circ}C$ under compression stress in oil, the change in elongation at break was lower than that aging in oil, but larger than that aging under compression in air. The compression set or elongation at break as evaluation indexes, 50% as critical value, the lifetime of NBR at $25^{\circ}C$ was predicted and compared. When aging under compression in oil, the prediction lifetime was lower than in air and under compression in air, and in oil. It was clear that when predicting the service lifetime of NBR in oil sealing application, compression and media liquid should be involved simultaneously. Under compression in oil, compression set as the evaluation index, the prediction lifetime of NBR was shorter than that of elongation at break as the evaluation index. For the life prediction of NBR, we should take into account of the performance trends of NBR under actual operating conditions to select the appropriate evaluation index.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.