• 제목/요약/키워드: adhesive thickness

검색결과 356건 처리시간 0.025초

적외선 램프 및 핫 플레이트 온도 제어를 통한 4 Bus Bar 결정질 실리콘 태양전지 솔더링 특성에 관한 연구 (A Study on the Soldering Characteristic of 4 Bus Bar Crystalline Silicon Solar Cell on Infrared Lamp and Hot Plate Temperature Control)

  • 이정진;손형진;김성현
    • Current Photovoltaic Research
    • /
    • 제5권3호
    • /
    • pp.83-88
    • /
    • 2017
  • The growth of intermetallic compounds is an important factor in the reliability of solar cells. Especially, the temperature change in the soldering process greatly affects the thickness of the intermetallic compound layer. In this study, we investigated the intermetallic compound growth by Sn-diffusion in solder joints of solar cells. The thickness of the intermetallic compound layer was analyzed by IR lamp power and hot plate temperature control, and the correlation between the intermetallic compound layer and the adhesive strength was confirmed by a $90^{\circ}$ peel test. In order to investigate the growth of the intermetallic compound layer during isothermal aging, the growth of the intermetallic compound layer was analyzed at $85^{\circ}C$ and 85% for 500 h. In addition, the activation energy of Sn was calculated. The diffusion coefficient of the intermetallic compound layer was simulated and compared with experimental results to predict the long-term reliability.

애크릴릭 및 실리콘 계열 연성 의치상 이장재의 결합력에 관한 연구 (A Study for Bond Strengths of Acrylic and Silicone Based Soft Lining Materials)

  • 남은주;임주환
    • 구강회복응용과학지
    • /
    • 제16권1호
    • /
    • pp.27-36
    • /
    • 2000
  • One of the methods to improve the softness and comfortness of denture base is the use of soft denture liners. In this study, specimens were made by 2 kinds of acrylic based soft lining materials and 2 kinds of silicone based soft lining materials, and bonded to acrylic resin(Lucitone $199^{(R)}$). Then they were tested the differences of tensile bond strengths according to the materials, thickness, surface treatment and failure mode. 1. Tensile bond strength according to soft lining materials was increased in order of Coe-$soft^{(R)}$, $Mollosil^{(R)}$, $Trusoft^{(R)}$, Ufi-Gel $C^{(R)}$. The differences between groups were statistically significant at level of 0.05. 2. Tensile bond strength according to thickness of soft lining materials was increased in order of 3mm, 2mm, 1mm. The differences between groups were not statistically significant. 3. Tensile bond strength of treated surface showed higher bond strength than nontreated surface. The difference between groups was not statistically significant. 4. The failure mode of Coe-$soft^{(R)}$, $Trusoft^{(R)}$, $Mollosil^{(R)}$ were mainly cohesive failure, and that of Ufi-Gel $C^{(R)}$ were mainly adhesive failure.

  • PDF

알루미나 세라믹(Alumina Ceramic) 코팅층의 기술적인 특성과 잔류응력의 해소에 관한 연구 (A Study on the Mechanical Properties and Residual Stresses of the Thermally Sprayed Alumina Ceramic Coating Layer)

  • 김영식
    • 한국해양공학회지
    • /
    • 제10권2호
    • /
    • pp.88-97
    • /
    • 1996
  • The pupose of this study is to improve the mechanical properies and to evaluate the residual stresses of flame-sprayed Alumina ceramic coating layer. The first work in this study is to investigate the effects of strengthening heat treatments on the mechanical properties of coating layer. Strengthening heat treatments for sprayed specimens were carried out in vaccum furnace. The mechanical properties such as microhardness, thermal shock resistance, adhesive strength and erosion resistance were tested for the sprayed specimens after strengthening heat treatments. And it was clear that the mechanical properties of coating layer were much improved by strengthening heat treatments. The second work in this study is to evalute the residual stresses in coating lsyer by numerical analysis. FDM and FEM were used to analyze temperature distribution and residul stresses in coating layer. It was proved that are tensile stresses in coating layer and that residual stresses can be controlled by the appropriate selection of the spraying parameters such as preheat temperature, coating thickness and bond coat thickness.

  • PDF

비대칭 마그네트론 스퍼터로 증착된 비정질 탄소박막의 트라이볼로지 특성에서 CrC 삽입층 효과에 대한 연구 (CrC Interlayer Effect on Tribological Properties of Amorphous Carbon Deposited by UBMS Method)

  • 김필중;박용섭
    • 한국전기전자재료학회논문지
    • /
    • 제31권7호
    • /
    • pp.475-480
    • /
    • 2018
  • We investigated the tribological properties of amorphous carbon (a-C) films deposited with CrC interlayers of various thicknesses as the adhesive layer. A-C and CrC thin films were deposited using the unbalanced magnetron (UBM) sputtering method with graphite and chromium as the targets. CrC films as the interlayer were fabricated under a-C films, and various structural, surface, and tribological properties of a-C films deposited with various CrC interlayer thicknesses were investigated. With various CrC interlayer thicknesses under a-C films, the tribological properties of CrC/a-C films were improved; the increased film thickness exhibited a maximum high hardness of over 27.5 GPa, high elastic modulus of over 242 GPa, critical load of 31 N, residual stress of 1.85 GPa, and a smooth surface below 0.09 nm at the condition of 30-nm CrC thickness.

연속 ECR-CVD 조업하에 RF-magnetron-sputter의 싸이클조업을 통해 PET위에 올려진 구리박막의 특성 (Characteristic of Copper Films on PET Substrate Deposited by Cyclic Operation of RF-magnetron-sputtering Coupled with Continuous Operation of ECR-CVD)

  • 명종윤;전법주;변동진;이중기
    • 한국재료학회지
    • /
    • 제15권7호
    • /
    • pp.465-472
    • /
    • 2005
  • Preparation of copper film on PET substrate was carried out by cyclic operation of RF-magnetron­sputtering under continuous operation of ECR-CVD. The purpose of this study is aimed to an increase in deposition rate with keeping excellent adhesion between copper film and PET. In order to optimize the sputtering time under continuous ECR-CVD, cyclic operation concept is employed. By changing parameters of cyclic operation such as split of e and cycle time of A, the characteristics and thickness of the deposited copper film are controlled. As $\theta$ value increase, film thickness could confirm to increase and its surface resistivity value decreases. The highest adhesive strength appears at $\theta=0.33$ and cycle time of 30 min. The uniformity of copper film shows $5\%$ in our experimental range.

이동형 핵종 분석 장치용 CZT 반도체 검출기의 완충전극에 대한 연구 (A Study of Interface Layer on CdZnTe Radiation Sensor for Potable Isotope Identifier)

  • 조윤호;박세환;김용균;하장호
    • 방사선산업학회지
    • /
    • 제5권1호
    • /
    • pp.95-99
    • /
    • 2011
  • The electrical and mechanical properties of electrode for radiation detection are very important. In general, Au electrode and CZT crystal are combined to form ohmic contacts, and the best energy resolution is shown at the Au electrode. The metal contacts are fabricated by electroless deposition method, sputtering deposition method and thermal evaporation method. The electrode fabrication is easy with use of the thermal evaporation method, while an adhesive strength is weak. Thus interface materials such as Ag, Al and Ni were investigated to overcome defects generated by the this method. The thickness of the interface material between the Au electrode and the CZT crystal was 100 Angstroms, the Au electrode with thickness of 400 Angstroms was deposited. The Al+Au electrode is shown that the results of current-voltage and radiation response are similar to results of Au electrode.

Numerical investigation of continuous composite girders strengthened with CFRP

  • Samaaneh, Mohammad A.;Sharif, Alfarabi M.;Baluch, Mohammed H.;Azad, Abul K.
    • Steel and Composite Structures
    • /
    • 제21권6호
    • /
    • pp.1307-1325
    • /
    • 2016
  • Nonlinear behavior of two-span, continuous composite steel-concrete girders strengthened with Carbon Fiber Reinforced Polymers (CFRP) bonded to the top of concrete slab over the negative moment region was evaluated using a non-linear Finite Element (FE) model in this paper. A three-dimensional FE model of continuous composite girder using commercial software ABAQUS simulated and validated with experimental results. The interfacial regions of the composite girder components were modeled using suitable interface elements. Validation of the proposed numerical model with experimental data confirmed the applicability of this model to predict the loading history, strain level for the different components and concrete-steel relative slip. The FE model captured the different modes of failure for the continuous composite girder either in the concrete slab or at the interfacial region between CFRP sheet and concrete slab. Through a parametric study, the thickness of CFRP sheet and shear connection required to develop full capacity of the continuous composite girder at negative moment zone have been investigated. The FE results showed that the proper thickness of CFRP sheet at negative moment region is a function of the adhesive strength and the positive moment capacity of the composite section. The shear connection required at the negative moment zone depends on CFRP sheet's tensile stress level at ultimate load.

프라이머 코팅과 열융착 필름 라미네이팅을 통해 제조한 충격 완화용 고강력 에어쿠션 직물에 관한 연구 (Study on the High-Strength Air-Cushion Fabrics for Impact-Relief Application Prepared through Primer Coating and Thermal Film Laminating)

  • 김지연;김훈민;민문홍
    • 한국염색가공학회지
    • /
    • 제33권4호
    • /
    • pp.269-279
    • /
    • 2021
  • In this study, the laminating of TPU film after coating of primer adhesive on the fabrics was applied in order to secure the strength to withstand a fall from a higher altitude by increasing the adhesion between the fabric and the film layer. It seems that the fineness of the yarn and the weave construction have a greater effect than the type of the laminating films. The order of superiority of the laminated fabrics by film type and thickness was the same for 1000 denier and 210 denier fabrics, and the tendency was consistent with the order of superiority in the film properties and peel strength tests. The tear strength of laminating fabrics increased three to four times for 1000 denier fabrics compared to the fabric alone, but it decreased by 2 times for the 210 denier fabrics. Summarizing the above results, it is most appropriate to combine 1000d fabric with three types of laminating films(100~200㎛ thickness) of A(0.2T) or B(0.15T) or D(0.1T) considering the air pressure resistance, the impact resistance during the fall, and the durability against damage during use.

전극 분할 적층형 압전변압기의 전기적 특성 (Electrical Properties of a Laminated Piezoelectric Transformer with the Divided Electrodes)

  • 이용국;이상철;허두오;한득영
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1995년도 하계학술대회 논문집 C
    • /
    • pp.1140-1142
    • /
    • 1995
  • The transformer is fabricated with two piezoelectric vibrator with the divided electrodes and adhesive insulator. We applied the electric input to the driving vibrator in parallel and connect the output voltage to the generating vibrator in series to the resistor load near its fundamental resonance frequency. Then we investigate output voltage in series twice as large as in parallal. Moreover we investigate the load characteristics at resonance frequencies under various resistor and the frequency characteristics near the resonance frequency under no load. Its equvalent circuit is derived from the Mason's model of a thickness-driven piezelectric vibrator. By its equevalent circuit, symbolic expressions for input impedances, voltage ratios, resonance frequencies, and bandwidths have been derived. The values calculated from those symbolic exprssions are shown to agree well with the measurement values.

  • PDF

Friction transition diagram considering the effects of oxide layer formed on contact parts of TiN coated steel ball

  • Cho, C.W.;Lim, J.S.;Lee, Y.Z.
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 proceedings of the second asia international conference on tribology
    • /
    • pp.179-180
    • /
    • 2002
  • In this study. the friction transition diagram based on the effect of oxide layer formation on contact surface between TiN coated steel ball and uncoated steel disk was constructed. From the diagram. it can be seen that as the contact load increases. the contact number of cycle at the beginning of oxide layer formation decreases linearly and as the coating thickness increases and the surface roughness of steel disk increases under same contact load. that increases. For the coated ball specimen, a AISI 52100 steel ball was used and AISI 1045 steel was used for the disk counter part.

  • PDF