Effect of Fiber Orientation on Failure Strength Properties of Natural Fiber Reinforced Composites including Adhesive Bonded Joints (접착제 접합된 자연섬유강화 복합재료의 파괴 강도특성에 미치는 섬유방향의 영향)

  • Im, Jae-Gyu;Yun, Ho-Cheol;Lee, Sang-Yong;Renliang, Wang
    • Proceedings of the KWS Conference
    • /
    • 2005.11a
    • /
    • pp.94-96
    • /
    • 2005
  • This paper is concerned with a fracture strength study of composite adhesive lap joints. The tensile and peel tests were carried out on specimen manufactured hybrid stacked composites such as the polyester and bamboo natural fiber layer. The main objective of the work was to test the failure strength of adhesive bonded joints using hybrid stacked composites with a polyester and bamboo natural fiber layer adjacent to the fiber orientation. From results, the load directional orientation, small amount and low thickness of bamboo natural fiber layer have a good effect on the tensile and peel strength of natural fiber reinforced composites. and these characters are have a great influence on fracture strength and failure shape of adhesive bonded joints using hybrid stacked composites in the difference of fiber orientation.

  • PDF

Thickness Assessment of Adhesive Layer in Inhomogeneous Layer by Guided Wave (유도초음파에 의한 비균질 적층의 접합층두께 평가)

  • Cho, Youn-Ho;Ham, Hyo-Sik;Choi, Heung-Ho
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.21 no.4
    • /
    • pp.391-397
    • /
    • 2001
  • The guided wave propagation in inhomogeneous multi-layered structures is experimentally explored based on theoretical dispersion curves. It turns out that proper selection of incident angel and frequency is critical for guided wave generation in multi-layered structures. Theoretical dispersion curves greatly depend on adhesive zone thickness, layer thickness and material properties. It was possible to determine the adhesive zone thickness of an inhomogeneous multi-layered structure by monitoring experimentally the change of dispersion curves.

  • PDF

Effect of stacking sequence of the bonded composite patch on repair performance

  • Beloufa, Hadja Imane;Ouinas, Djamel;Tarfaoui, Mostapha;Benderdouche, Noureddine
    • Structural Engineering and Mechanics
    • /
    • v.57 no.2
    • /
    • pp.295-313
    • /
    • 2016
  • In this study, the three-dimensional finite element method is used to determine the stress intensity factor in Mode I and Mixed mode of a centered crack in an aluminum specimen repaired by a composite patch using contour integral. Various mesh densities were used to achieve convergence of the results. The effect of adhesive joint thickness, patch thickness, patch-specimen interface and layer sequence on the SIF was highlighted. The results obtained show that the patch-specimen contact surface is the best indicator of the deceleration of crack propagation, and hence of SIF reduction. Thus, the reduction in rigidity of the patch especially at adhesive layer-patch interface, allows the lowering of shear and normal stresses in the adhesive joint. The choice of the orientation of the adhesive layer-patch contact is important in the evolution of the shear and peel stresses. The patch will be more beneficial and effective while using the cross-layer on the contact surface.

Adhesion of 10-MDP containing resin cements to dentin with and without the etch-and-rinse technique

  • Turp, Volkan;Sen, Deniz;Tuncelli, Betul;Ozcan, Mutlu
    • The Journal of Advanced Prosthodontics
    • /
    • v.5 no.3
    • /
    • pp.226-233
    • /
    • 2013
  • PURPOSE. This study evaluated the adhesion of 10-MDP containing self-etch and self-adhesive resin cements to dentin with and without the use of etch-and-rinse technique. MATERIALS AND METHODS. Human third molars (N=180) were randomly divided into 6 groups (n=30 per group). Conventional (Panavia F2.0, Kuraray-PAN) and self-adhesive resin cements (Clearfil SA, Kuraray-CSA) were bonded to dentin surfaces either after application of 3-step etch-and-rinse (35% $H_3PO_4$ + ED Primer) or two-step self-etch adhesive resin (Clearfil SE Bond). Specimens were subjected to shear bond strength test using the universal testing machine (0.5 mm/min). The failure types were analyzed using a stereomicroscope and quality of hybrid layer was observed under a scanning electron microscope. The data (MPa) were analyzed using two-way ANOVA and Tukey's tests (${\alpha}$=.05). RESULTS. Overall, PAN adhesive cement showed significantly higher mean bond strength ($12.5{\pm}2.3-14.1{\pm}2.4$ MPa) than CSA cement ($9.3{\pm}1.4-13.9{\pm}1.9$ MPa) (P<.001). Adhesive failures were more frequent in CSA cement groups when used in conjunction with two-step self-adhesive (68%) or no adhesive at all (66%). Hybrid layer quality was inferior in CSA compared to PAN cement in all conditions. CONCLUSION. In clinical situations where bonding to dentin substrate is crucial, both conventional and self-adhesive resin cements based on 10-MDP can benefit from etch-and-rinse technique to achieve better quality of adhesion in the early clinical period.

Evaluation of Adhesive Characteristics of Mixed Cross Laminated Timber (CLT) Using Yellow Popular and Softwood Structural Lumbers

  • Keon-Ho KIM;Hyun-Mi LEE;Min LEE
    • Journal of the Korean Wood Science and Technology
    • /
    • v.52 no.1
    • /
    • pp.58-69
    • /
    • 2024
  • To evaluate the adhesive characteristics of mixed cross-laminated timber (CLT) using domestic softwoods structural lumber proposed by KS F 3020 and yellow poplar, penetration depth of adhesive and thickness of bonding line were analyzed based on the results of boiling water soaking delamination. 3 Types of adhesives and 2 types of major layer were divided into a 5 ply CLT using yellow popular as minor layer. The bonding performance of the mixed CLT as structural members was evaluated based on the KS F 2081. The thickness of bonding line between layers of the mixed CLT was measured with a scanning electron microscope, and the adhesive penetration depth in the layer members was measured with an optical microscope. As a result of boiling water soaking delamination test of mixed CLT, the CLT specimens using PRF and PUR adhesives met the requirements of KS F 2081. It was verified that the penetration path of the adhesive in the layes was mainly through the tracheid cell in the case of Japanese larch and Korean red pine layers, and through the vessel and radial tissue in yellow popular layers. The penetration depth of the adhesive was the highest for the PRF adhesive under the same pressing time conditions, and the thickness of the bonding line was in inverse proportion to the penetration depth in the case of the PUR adhesive.

Interface characteristics of RC beams strengthened with FRP plate

  • Peng, Minglan;Shi, Zhifei
    • Structural Engineering and Mechanics
    • /
    • v.18 no.3
    • /
    • pp.315-330
    • /
    • 2004
  • A four-point bending RC beam strengthened with FRP plate is investigated based on the theory of elasticity. Taking the adhesive layer into account but ignoring some secondary parameters, the analytical solutions of the normal stress and shear stress on concrete-adhesive interface are obtained and discussed. Besides, the pure bending region of the beam is analyzed and the ultimate load of the beam is predicted. The results obtained in the present paper agree very well with both the results of FEM and the experimental findings.

Influence of Manufacturing Environment on Delamination of Mixed Cross Laminated Timber Using Polyurethane Adhesive

  • SONG, Dabin;KIM, Keonho
    • Journal of the Korean Wood Science and Technology
    • /
    • v.50 no.3
    • /
    • pp.167-178
    • /
    • 2022
  • To investigate the influence of manufacturing environment on bonding performance of mixed cross laminated wood (CLT) using polyurethane (PUR) adhesive, a boiling water soak delamination test according to the temperature and relative humidity was conducted. The 5-ply mixed CLT consisted of Japanese Larch for external and middle layer and yellow poplar for internal layer. The PUR adhesives with different opening times of 10 and 30 minutes were used. The mixed CLT was manufactured according to pressing times of PUR and manufacturing environments of summer and winter. In case of summer environment, the delamination rate of the mixed CLT with pressing time of 4 hours using a PUR adhesive with open time of 10 minutes met the requirements of KS F 2081. In case of winter environment, the delamination rate of the mixed CLT didn't meet the requirements of KS standard. However, it was possible to confirm the effect of improving the adhesive performance by adjusting the pressing time according to the open time of the adhesive under the manufacturing conditions. The delamination rate of CLT with open time 30 minutes PUR, manufactured by indirect moisture supply methods was 11.2% better than direct moisture supply methods. As a result of delamination test in the same condition of relative humidity and adhesive, it was found that the temperature of manufacturing environment influences the adhesive performance.

Adhesive improvement of the Polyimide/Buffer layer/Cu at the COF(Chip On Film) (COF(Chip On Film)에서의 Polyimide/Buffer layer/Cu 접착력 향상)

  • 이재원;김상호;이지원;홍순성
    • Journal of the Semiconductor & Display Technology
    • /
    • v.3 no.3
    • /
    • pp.11-17
    • /
    • 2004
  • This research has been progressed for adhesive improvement of the Polyimide/Buffer layer/Cu at the COF(Chip On Film) which induced as the alternative plan about high concentration of a circuit or substrates according to demands of miniaturization and high efficiency of various electronic equipment. RF plasma equipment was applied to when plama pretreatment was performed for improvement of adhesive strength of PI and Cr as the buffer layer. Experimental fluents were a species of the buffer layer, depositied time and the ratio of $O_2$/Ar when performed to plasma pretreatment. The results are that Ni was superior to Cr at peel test according to a species of the buffer layer, peel strength and Cu THK were showed proportional relation to deposition structure of the same buffer layer and sample of the Cr depositied time(30 sec) and Cu depositied time(20 min) was showed good adhesion to peel test according to Cr's depositied time and Cu's depositied time. When perform PI's plasma pretreatment peel strength and $O_2$/Ar ratio were showed proportional relation. But $O_2$/Ar(2/5) was best condition since then decreased.

  • PDF

The effect of adhesive thickness on microtensile bond strength to the cavity wall (와동벽에서 접착제의 두께가 미세인장 결합강도에 미치는 영향)

  • Lee, Hwa-Eon;Kim, Hyeon-Cheol;Hur, Bock;Park, Jeong-Kil
    • Restorative Dentistry and Endodontics
    • /
    • v.32 no.1
    • /
    • pp.9-18
    • /
    • 2007
  • The purposes of this study were to examine the variability of adhesive thickness on the different site of the cavity wall when used total-etch system without filler and simplified self-etch system with filler and to evaluate the relationship between variable adhesive thickness and microtensile bond strength to the cavity wall. A class I cavity in six human molars was prepared to expose all dentinal walls. Three teeth were bonded with a filled adhesive, $Clearfil^{TM}$ SE bond ana the other three teeth were bonded with unfilled adhesives, $Scotchbond^{TM}$ Multi Purpose. Morphology and thickness of adhesive layer were examined using fluorescence microscope. Bonding agent thickness was measured at three points along the axial cavity wall edge of cavity margin (rim). halfway down each cavity wall (h1f), internal angle of the cavity (ang). After reproducing the adhesive thickness at rim, h1f and ang, micro-tensile bond strength were evaluated. For both bonding agents, adhesive thickness of ang was significantly thicker than that of rim and h1f (P <0.05). As reproduced the adhesive thickness, microtensile bond strength was increased as adhesive thickness was increased in two bonding agents. Adhesive thickness of internal angle of the cavity was significantly thicker than that of the cavity margin and the halfway cavity wall for both bonding agents. Microtensile bond strength of the thick adhesive layer at the internal angle of the cavity was higher than that of the thin adhesive layer at 1,he cavity margin and the halfway cavity in the two bonding systems.

Surface Modification of a Mild and Stainless Steel by Alumina Spraying (아루미나 용사에 의한 연강 및 스테인레스강의 표면개질)

  • 배종규;박승옥;정인상
    • Journal of the Korean institute of surface engineering
    • /
    • v.22 no.4
    • /
    • pp.185-196
    • /
    • 1989
  • The surface modification of a mild and stainless steel by alumina sprayed coating were studied. The effects of surface roughness and bond coating layer on the adhesive strengthy and durability of sprayed specimens were also investiated. The adhesive strength of ceramic coating was affected by surface roughness and bond coating layer thinkness. That showed excellent undergrit blast time and bond coating layer; 60 sec and 0.15-0.33mm, respectively. The adhesive strength and densification of sprayed coating with air pressure were superior to those of without and fracture was mainly occured at alumina-bond coating interface. Under ambient atmosphere at $800^{\circ}C$, the oxides existed within bond coating layer promote diffusion of oxygen to lower durability of sprayed specimens. In this case, fracure was occured at sudstrate-bond coating interface.

  • PDF