• Title/Summary/Keyword: abnormal growth

Search Result 709, Processing Time 0.031 seconds

A Study of the mechanism for abnormal oxidation of WSi$_2$ (WSi$_2$이상산화 기구에 대한 조사)

  • 이재갑;김창렬;김우식;이정용;김차연
    • Journal of Surface Science and Engineering
    • /
    • v.27 no.2
    • /
    • pp.83-90
    • /
    • 1994
  • We have investigated the mechanism for the abnormal oxide growth occuring during oxidation of the crystalline tungsten silicide. TEM and XPS analysis reveal the abnormaly grown oxide layer consisting of crystalline $Wo_3$ and amorphous $SiO_2$. The presence of crystalline $Wo_3$ provides a rapid diffusion of oxygen through the oxide layer. The abnormal oxide growth is mainly due to the poor quality of initial oxide layer growth on tungsten silicide. Two species such as tungsten and silicon from decomposition fo tungsten silicide as well as silicon supplied from the underlying polysilicon are the main contributors sto abnormal oxide forma-tion. Consequently, the abnormal oxidation results in the disintegration of tungsten silicide and thinning of polysilicon as well.

  • PDF

Grain Shape and Grain Growth Behavior in the Na1/2Bi1/2TiO3-BaTiO3 System (Na1/2Bi1/2TiO3-BaTiO3 계에서 입자모양과 입자성장 거동)

  • Moon Kyoung-Seok;Kang Suk-Joong
    • Journal of Powder Materials
    • /
    • v.13 no.2 s.55
    • /
    • pp.119-123
    • /
    • 2006
  • The grain growth behavior of $0.95Na_{1/2}Bi_{1/2}TiO_{3}-0.05BaTiO_{3}$ (NBT-5BT) has been investigated with respect to the grain shape. The powder compacts of NBT-5BT were sintered at 1200 for various times. The corresponding equilibrium shape was a round-edged cube with flat {100}-faces. Abnormal grains were not observed in the specimens sintered for 1 to 12 h but abnormal grains appeared when sintered for 24 h. Before the formation of abnormal grains, a valley was observed in the measured grain size distribution of NBT-5BT, showing that the grain size distribution was a combination of two unimodal distributions. The present result suggests that the grain growth in NBT-5BT was governed by the growth of facet planes which would occur via 2-dimansional nucleation and growth.

Densification Behavior of $BaTiO_3$ Ceramics with Grain Growth ($BaTiO_3$ 요업체에서 입성장에 따른 치밀화 거동)

  • 이태헌;김정주;김남경;조상희
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.1
    • /
    • pp.51-56
    • /
    • 1995
  • Variation of sintered density of BaTiO3 powder calcined at 120$0^{\circ}C$ and 135$0^{\circ}C$ was investigated with respect to the grain growth behavior. It was found that BaTiO3 powder, which was calcined at 120$0^{\circ}C$, showed abnormal grain growth behavior during sintering process. At initial stage of sintering process, the densification rate of specimen was accelerated with rapid grain growth caused by the abnormal grain growth. But with the increase of sintering time, abnormally grown grain met each other and the density of specimen decreased drastically due to coalescence of pores located in triple junction. On the contrary, BaTiO3 powder calcined at 135$0^{\circ}C$ showed normal grain growth behavior and gradually densified with the increase of sintering time.

  • PDF

Effect of Excess PbO on Grain Growth and Densification of (65)Pb(${Mg_{1/3}}{Nb_{2/3}}$)$O_3$-(35)$PbTiO_3$ Ceramics ((65)Pb(${Mg_{1/3}}{Nb_{2/3}}$)$O_3$-(35)$PbTiO_3$의 입자성장과 치밀화에 미치는 과량 PbO의 영향)

  • Lee, Jong-Bong;Hur, Tae-Moo;Lee, Ho-Yong;Choi, Kyun;Kim, Doe-Yeon
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.7
    • /
    • pp.673-680
    • /
    • 2000
  • The effect of excess PbO(0, 1, 2, 4, and 8 mol%) on grain growth and densification of (65)Pb(Mg1/3Nb2/3)O3-(35)PbTiO3 [mol%] ceramics has been investigaetd. With increasing the amount of excess PbO and sintering time, densities of sintered samples decreased gradually. The samples containing less than 1 mol% of PbO showed normal grain growth behavior, however abnormal grain growth was observed to occur in the samples with more than 2 mol% of PbO. In the samples with more than 2 mol% of PbO, the number of abnormal grains decreased and thus the average grain size became smaller with increasing the amount of excess PbO. These results demonstrated that the abnormal grain growth started to occur when a critical amount of excess PbO was added to a (65)Pb(Mg1/3Nb2/3)O3-(35)PbTiO3 sample. Since PMN-PT grains in a liquid matrix were angular, the observed abnormal grain growth was explained to proceed through the two dimensional nucleation process.

  • PDF

ABNORMAL GROWTH PATTERN OF HUMAN FETAL MAXILLA WITH CLEFT LIP AND PALATE (구순구개열 태아의 비정상적인 상악골 성장형태에 대한 연구)

  • Kim, Soung-Min;Kim, Jung-Hwan;Kim, Ji-Hyuck;Park, Young-Wook;Lee, Jong-Ho;Lee, Suk-Keun
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • v.33 no.3
    • /
    • pp.238-246
    • /
    • 2007
  • This study is aimed to elucidate the abnormal growth pattern of human fetal maxilla with cleft lip and palate (CLP). Total 71 fetal maxillae with CLP were obtained from aborted human fetuses. They were examined radiologically for the dimensional changes of maxillary trapezoid (MT) formed by maxillary primary growth centers (MxPGC)(Lee et al., 1992). In palatal radiogram of the CLP maxilla, the MT was traced by the anterior and posterior MxPGCs, and the dimensions of anterior and posterior maxillary widths, maxillary length, and MT length (MTL), and MT area were measured for evaluation of the basic growth pattern of the developing maxilla. The growth of anterior and posterior MxPGCs was severely retarded in the prenatal maxillae with CLPs, showing abnormal shape of MT. Cleft lip subjects without cleft palate also showed arrested growth of MT. Unilateral cleft lipalveolar cleft or cleft palate (UCL-AC/CP) and bilateral cleft lip-alveolar cleft or cleft palate (BCL-AC/CP) showed enhanced abnormal MT pattern. The abnormality of MT was most marked in BCL-AC/CP. It was also observed that the craniofacial malformations other than CLPs produced abnormal MT. In conclusion, the MT growth of prenatal CLP maxilla was severely arrested and resulting in abnormal MT shape on the palatal radiogram. BCL-AC/CP showed more protruded nasal septum than other types of CLPs, while UCL-AC/CP showed severe deviation of the protruded nasal septum towards the non-cleft side. Cleft lip only subjects also showed the abnormal growth of MT. These data suggest that the MT is primarily involved in CLPs, and MT shape could be utilized as a sensitive indicator for the analysis of maxillary malformation in different types of CLPs.

Effect of Debinding Conditions on the Microstructure of Sintered Pb(Mg1/3Nb2/3)O3-PbTiO3

  • Yun Jung-Yeul;Jeon Jae-Ho;L.Kang Suk-Joong
    • Journal of Powder Materials
    • /
    • v.12 no.4 s.51
    • /
    • pp.261-265
    • /
    • 2005
  • In order to fabricate complex-shaped polycrystalline ceramics by sintering, organic binders are usually pre-mixed with ceramic powders to enhance the formability during the shape forming process. These organic binders, however, must be eliminated before sintering so as to eliminate the possibilities of poor densification and unusual grain growth during sintering. The present work studies the effect of binder addition on grain growth behavior during sintering of $92(70Pb(Mg_{1/3}Nb_{2/3})O_3-30PbTiO_3))$-8PbO(mol%) piezoelectric ceramics. The microstructures of the sintered samples were examined for various heating profiles and debinding schedules of the binder removal process. Addition of Polyvinyl butyral(PVB) binder promoted abnormal grain growth especially in incompletely debinded regions. Residual carbon appears to change the grain shape from comer-rounded to faceted and enhance abnormal grain growth.

The Growth and Development of Infants in Orphanage (일 지역 시설 영.유아의 신체 성장과 발달 평가)

  • Kim, Tae-Im
    • Korean Parent-Child Health Journal
    • /
    • v.5 no.2
    • /
    • pp.177-190
    • /
    • 2002
  • This study were conducted to assess the physical growth and developmental status of infants in orphanage in order to provide an empirical data. The subjects for this study were 104 infants and toddlers who were reared in an orphanage in D Metropolitan city. The instrument used for this study were anthropometric assessment and DDST for normative data of development. Data has been collected from September 1st, 1998 to August 31st, 2000 and were analyzed using SPSS/PC(Version 10.0) with frequency, mean, standard deviation, ANOVA and Chi-square test. The results of this study were as follows; 1. 30.8% of infants in orphanage had abnormal weight, 26.9% had abnormal length, and 22.1% had abnormal head circumference and most of them were distributed below 50 percentile of growth chart. 2. 53.8% of infants in orphanage had normal, 27.9% had qustionable, and 18.3% had abnormal developmental screening test results, especially, 31.5% of infants in orphanage ages 3 to 5 years had abnormal developmental screening test results, according to the Denver Developmental Screening Test(DDST). There was a significant developmental delay noted in the language and fine motor-adaptive sector. 3. It is anticipated that developmental delays would increase in severity by older the mean age of orphanage infants and longer the time being raised in orphanage. It would be concluded that the physical growth and developmental status of orphaned infants were very vulnerable and serious and it is suggested that there needed an effective intervention strategies to promote growth and development of infants in orphanage.

  • PDF

Suppression of Abnormal Grain Growth in Barium Titanate by Atmosphere Control

  • Lee, Byoung-Ki;Chung, Sung-Yoon;Jung, Yang-Il;Suk-Joong L. Kang
    • Journal of Powder Materials
    • /
    • v.8 no.2
    • /
    • pp.131-135
    • /
    • 2001
  • The ferroelectric properties of barium titanate strongly depend on its microstructure, in particular, grain size and distribution. During sintering, $BaTiO_3$ usually exhibits abnormal grain growth, which deteriorates considerably the ferroelectric properties. A typical technique to suppress the abnormal grain growth is the addition of dopants. Dopant addition, however, affects the ferroelectric properties and thus limits the application of $BaTiO_3$. Here, we report a simple but novel technique to prevent the abnormal grain growth of $BaTiO_3$ and to overcome the limitation of dopant use. The technique consists of stepwise sintering in a reducing atmosphere and in an oxidizing atmosphere. The materials prepared by the present technique exhibit uniform grain size and high dielectric properties. The technique should provide opportunities of having $BaTiO_3$-based materials with superior ferroelectric properties.

  • PDF

Effect of Aggregates on the Microstructure in Manganese Zinc Ferrite

  • Shin, Hyo-Soon;Lee, Dae-Hee;Kim, Chang-Bum;Kim, Nam-Kyung;Lee, Suk-Kee;Lee, Byung-Kyo
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.1
    • /
    • pp.1-4
    • /
    • 2003
  • To study the effect of aggregates on the microstructure of sintered bodies, Mn-Zn ferrite powders were prepared by an alcoholic dehydration method. Aggregate powders and reground powders were used as seeds and matrices, respectively. The mixing ratios for the aggregate and reground powders were varied with the sintering temperatures. Green densities were measured with changes in forming pressure and they were related to the microstructures of the sintered bodies. The aggregates proved to be capable of acting as seeds for abnormal grain growth. When the green density difference between the aggregate and the matrix was large, the aggregate could become the seed of abnormal grain growth. As the forming pressure increased, the more aggregates became seeds of abnormal grain growth.