Effect of Al and Nb Doping on the Electrochemical Characteristics of Garnet-type Li7La3Zr2O12 Solid Electrolytes

  • Ahmed Tarif;Chan-Jin Park
    • Corrosion Science and Technology
    • /
    • v.22 no.6
    • /
    • pp.408-418
    • /
    • 2023
  • In this study, we synthesized and characterized garnet-type Li7-xAlxLa3Zr2-(5/4)yNbyO12 (LALZN) solid electrolytes for all-solid-state battery applications. Our novel approach focused on enhancing ionic conductivity, which is crucial for battery efficiency. A systematic examination found that co-doping with Al and Nb significantly improved this conductivity. Al3+ and Nb5+ ions were incorporated at Li+ and Zr4+ sites, respectively. This doping resulted in LALZN electrolytes with optimized properties, most notably enhanced ionic conductivity. An optimized mixture with 0.25 mol each of Al and Nb dopants achieved a peak conductivity of 1.32 × 10-4 S cm-1. We fabricated symmetric cells using these electrolytes and observed excellent charge-discharge profiles and remarkable cycling longevity, demonstrating the potential for long-term application in battery systems. The garnet-type LALZN solid electrolytes, with their high ionic conductivity and stability, show great potential for enhancing the performance of all-solid-state batteries. This study not only advances the understanding of effective doping strategies but also underscores the practical applicability of the LALZN system in modern energy storage solutions.

INVESTIGATION ON THE CORROSION BEHAVIOR OF HAHA-4 CLADDING BY OXIDE CHARACTERIZATION

  • Park, Jeong-Yong;Choi, Byung-Kwon;Jeong, Yong-Hwan
    • Nuclear Engineering and Technology
    • /
    • v.41 no.2
    • /
    • pp.149-154
    • /
    • 2009
  • The microstructure, the corrosion behavior and the oxide properties were examined for Zr-1.5Nb-0.4Sn-0.2Fe-0.1Cr (HANA-4) alloys which were subjected to two different final annealing temperatures: $470^{\circ}C$ and $570^{\circ}C$. HANA-4 was shown to have $\ss$-enriched phase with a bcc crystal structure and Zr(Nb,Fe,Cr)$_2$ with a hcp crystal structure with $\ss$-enriched phase being more frequently observed compared with Zr(Nb,Fe,Cr)$_2$. The corrosion rate of HANA-4 was increased with an increase of the final annealing temperature in the PWR-simulating loop, $360^{\circ}C$ pure water and $400^{\circ}C$ steam conditions, which was correlated well with a reduction in the size of the columnar grains in the oxide/metal interface region. The oxide growth rate of HANA-4 was considerably affected by the alloy microstructure determined by the final annealing temperature.

Dielectric and Piezoelectric Characteristics of Ceramics in the $Pb(Mg_{1/2}W_{1/2})O_3-Pb(Ni_{1/3}Nb_{2/3})O_3-PbTiO_3-PbZrO_3$ system ($Pb(Mg_{1/2}W_{1/2})O_3-Pb(Ni_{1/3}Nb_{2/3})O_3-PbTiO_3-PbZrO_3$계 세라믹스의 유전 및 압전 특성)

  • Kim, Woo-Hyun;Yoon, Kwang-Hee;Yoon, Hyun-Sang;Park, Yong-Wook;Park, Chang-Yeop
    • Proceedings of the KIEE Conference
    • /
    • 1994.11a
    • /
    • pp.193-195
    • /
    • 1994
  • In this study, the structural, dielectric and piezoelectrical properties of $xPb(Mg_{1/2}W_{1/2})O_3-(1-x)[0.41Pb(Ni_{1/3}Nb_{2/3})O_3-0.36PbTiO_3-0.23P Zr)_3]$ (x=0, 0.01, 0.02, 0.03, 0.04, 0.05) system ceramics were investigated. The dielectric constant ${\varepsilon_{33}}^{\tau}$ at loon temperature increased up to 3mol% PMW and decreased with further PMW content. The specimen with 1mol% $Pb(Mg_{1/2}W_{1/2})O_3$, which has the ${\varepsilon_{33}}^{\tau}=5509$, kp=59[%] and $d_{33}=758{\times}10^{-12}[C/N]$, exhibits good characteristics.

  • PDF

Electrical properties of sol-gel derived $ PbZrO_3$-$PbTiO_3$-$Pb(Ni_{1/3}Nb_{2/3})O_3$ thin film (Sol-Gel 법에 의한$ PbZrO_3$-$PbTiO_3$-$Pb(Ni_{1/3}Nb_{2/3})O_3$)

  • 임무열;구경완;한상옥
    • Electrical & Electronic Materials
    • /
    • v.10 no.2
    • /
    • pp.134-140
    • /
    • 1997
  • PbTiO$_{3}$-PbZrO$_{3}$-Pb(Ni$_{1}$3/Nb $_{2}$3/O$_{3}$)(PZT-PNN) thin films were prepared from corresponding metal organics partially stabilized with diethanolamine by the sol-gel spin coating method. Each mol rates of PT:PZ:PNN solutions were #1(50:40:10), #2(50:30:20), #3(45:35:20) and #4(40:40:20), respectively. The spin-coated PZT-PNN films were sintered at the temperature from 500.deg. C to 600.deg. C for crystallization. The P-E hysteresis curve was drawn by Sawyer-Tower circuit with PZT-PNN film. The coercive field and the remanent polarization of #4(40:40:20 mol%) PZT-PNN film were 28.8 kV/cm and 18.3 .mu.C/cm$^{2}$, respectively. Their dielectric constants were shown between 128 and 1120, and became maximum value in MPB(40:40:20 mol%). The leakage currents of PZT-PNN films were about 9.4x 10$^{-8}$ A/cm$^{2}$, and the breakdown voltages were about 0.14 and 1.1 MV/cm. The Curie point of #3(45:35:20 mol%, sintered at 600.deg. C) film was 330.deg. C.

  • PDF

Grain Shape and Grain Growth Behavior in the (K0.5Na0.5)NbO3-CaZrO3 System ((K0.5Na0.5)NbO3-CaZrO3 계에서 입자모양과 입자성장 거동)

  • Lee, Chul-Lee;Moon, Kyoung-Seok
    • Journal of Powder Materials
    • /
    • v.29 no.2
    • /
    • pp.110-117
    • /
    • 2022
  • The grain growth behavior in the (1-x)K0.5Na0.5NbO3-xCaZrO3 (KNNCZ-x) system is studied as a function of the amount of CZ and grain shape. The (1-x)K0.5Na0.5NbO3-xCaZrO3 (KNNCZ-x) powders are synthesized using a conventional solid-state reaction method. A single orthorhombic phase is observed at x = 0 - 0.03. However, rhombohedral and orthorhombic phases are observed at x = 0.05. The grain growth behavior changes from abnormal grain growth to the suppression of grain growth as the amount of CaZrO3 (CZ) increases. With increasing CZ content, grains become more faceted, and the step-free energy increases. Therefore, the critical growth driving force increases. The grain size distribution broadens with increasing sintering time in KNNCZ-0.05. As a result, some large grains with a driving force larger than the critical driving force for growth exhibit abnormal grain growth behavior during sintering. Therefore, CZ changes the grain growth behavior and microstructure of KNN. Grain growth at the faceted interface of the KNNCZ system occurs via two-dimensional nucleation and growth.

Effects of Deposition and Annealing Conditions on Structural and Magnetic Properties of CoNbZr Alloy Films (제조 조건 및 열처리 조건에 따르는 CoNbZr 합금 박막의 구조 및 자기적 성질에 관한 연구)

  • 양준석;이성래
    • Journal of the Korean Magnetics Society
    • /
    • v.10 no.2
    • /
    • pp.54-61
    • /
    • 2000
  • The structural and magnetic properties of sputtered CoNbZr alloy films were investigated. In the as-deposited $Co_{87.0}$N $b_{8.5}$Z $r_{4.5}$ film deposited at 2 mTorr and 130 W, we observed the minimum coercivity of 1.75 Oe, the maximum resistivity of 3000 $\mu$Ω.cm and permeability of 1095 at 100 MHz. As the Ar pressure or the RF input power increased, the permeability of films at 100 MHz decreased and the coercivity increased because of the development of columnar structure and the formation of unstable amorphous phase. Permeability lower than 100 and coercivity of 60 Oe were observed in film deposited at 1 mTorr or 190 W due to the formation of crystalline phase. Magnetic anisotropy field of as-deposited films could be reduced by rotating field annealing for 120 minutes at 30$0^{\circ}C$. After the annealing, the anisotropy field (Hk) decreased from 1.43 Oe to 0.3 Oe and the permeability increased from 1095 to 1345 because defects in as-deposited films were eliminated by the annealing.aling.

  • PDF

Physical properties of $PbZrO_3-PbTiO_3-Pb(Ni_{1/3}Nb_{2/3})O_3$ thin films by sol-gel method (Sol-gel법에 의한 $PbZrO_3-PbTiO_3-Pb(Ni_{1/3}Nb_{2/3})O_3$박막의 물리적 특성)

  • 임무열;구경완;김성일;유영각
    • Electrical & Electronic Materials
    • /
    • v.9 no.10
    • /
    • pp.991-1000
    • /
    • 1996
  • PbTiO$_{3}$-PbZrO$_{3}$-Pb(Ni$_{1}$3/Nb$_{2}$3/O$_{3}$) (PZT-PNN) thin films were prepared from corresponding metal organics partially stabilized with diethanolamine by the sol-gel spin coating method. Each mol ratio of PT:PZ:PNN solutions were #1(50:40:10), #2(50:30:20), #3(45:35:20), #4(40:40:20), #5(40:50:10), #6(35:45:20) and #7(30:50:20) respectively. The spin-coated PZT-PNN films were heat-treated at 350.deg. C for decomposition of residual organics, and were sintered from 450.deg. C to 750.deg. C for crystallization. The substrates, such as Pt and Pt/TiN/Ti/TiN/Si were used for the spin coating of PZT PNN films. The perovskite phase was observed in the PZT-PNN films heat-treated at 500.deg. C. The crystalline of the PZT-PNN films was optimized at the sintering of 700.deg. C. By the result of AES analysis, It is confirmed that the films of TiN/Ti/TiN was a good diffusion barrier and that co-diffusion into the each films was not observed.

  • PDF

A Study on the Electrical properties of PSN-PMN-PZI system ceramics modified With $Y_2O_3$and $Fe_2O_3$ ($Y_2O_3$$Fe_2O_3$ 첨가에 따른 PSN-PMN-PZT 세라믹스의 전기적 특성에 따른 연구)

  • 민석규;황상모;이용우;류주현;김종선
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.269-272
    • /
    • 1999
  • In this study, electrical properties and TCFr of Pb(Sb$_{1}$2/Nb$_{1}$2/)O$_3$-Pb(Mn $_{1}$3/Nb$_{2}$3/)O$_3$-Pb(zr, Ti)O$_3$ composition ceramics were investigated wish the Zr/Ti ratio and the additions of Y2O3. and Fe$_2$O$_3$ Electromechanical coupling factor(Kp) showed the highest value of 0.555 in the Zr/Ti=0.50/0.50 ratio ,however, dielectric constant showed the highest value of 1,217 in the Zr/Ti = 0.49/0.51 ratio. Excellent TCFr vague of 421ppm/$^{\circ}C$] at-30~9O$^{\circ}C$ was appeared in the Zr/Ti=0.50/0.50 ratio and electro-mechanical coupling factor(Kp) , mechanical quility factor(Qm) and dielectric constant was 0.496, 1,286 and 1,085 ,respectively ,in the composition ceramics of lwt%Y$_2$O$_3$ and 0.3wt%Fe$_2$O$_3$.

  • PDF

Variation of Magnetic Properties of Fe/CoNbZr with Multilayer Structure and Annealing Condition (Fe/CoNbZr 다층박막의 구조 및 열처리 조건에 따른 자기적 특성)

  • 이성래;김은학;김영근
    • Journal of the Korean Magnetics Society
    • /
    • v.11 no.2
    • /
    • pp.45-49
    • /
    • 2001
  • Effects of multilayer structure and annealing condition on the soft magnetic properties of sputtered Fe/CoNbZr multilayers were investigated. We observed a minimum coercivity (1.1 Oe) at 5 nm thick Fe layer and the maximum permeability (2300) at 15 nm Fe layer and high saturation magnetization in the as-deposited state. As a result of increase of Fe grain size, coercivity increases with increasing Fe layer thickness. Degradation of ${\mu}$ at the thin Fe layer region may be due to the intermixed phase of high magnetostriction, such as CoFe. Optimum annealing condition was obtained through annealing at 300 $^{\circ}C$ for 40 min (${\mu}$=2500, H$\sub$c/=0.35 Oe). Enhancement of permeability was observed in the temperature range of 250∼300$^{\circ}C$. These results may closely be related with lowering the anisotropy energy by lattice deformation (0.4%) and enhanced uniaxial anisotropy.

  • PDF

X-Ray Spectrometric Determination of $Ta_2O_5,\;Nb_2O_5$ and $ZrO_2$in Tin-Slag Samples by Double Dilution Technique (주석-슬랙중 $Ta_2O_5,\;Nb_2O_5$$ZrO_2$의 이중희석법을 이용한 X-선 분광분석)

  • Young-Sang Kim;Kee-Chae Park
    • Journal of the Korean Chemical Society
    • /
    • v.28 no.5
    • /
    • pp.302-308
    • /
    • 1984
  • X-ray spectrometric determination of $Ta_2O_54, $Nb_2O_5$ and $ZrO_2$ in tin-slag samples using the double dilution technique was conducted. Tin-slag samples and one synthesized standard sample having similar composition to the samples were diluted with anhydrous $Li_2B_4O_7$ at the level of 1.00, 2.00 and 3.00% of the sample content, respectively. The diluted samples were fused at $1,150^{\circ}C$ for 30 minutes, and these glass beads were finely ground and pelletized. With the X-ray intensities measured, analytical results were calculated by the double dilution equation. The results agreed to the reference values obtained by the standard calibration method and the simple dilution technique within allowable error range and were reproducible.