• Title/Summary/Keyword: Zone-casting

Search Result 63, Processing Time 0.03 seconds

The Effects of Centrifugal Casting Conditions on the Structure and Mechanical Properties in Fabrication Development of Super Heat-Resisting Steel Pipe of HP Alloy Modified with Nb (Nb을 첨가한 HP 초내열강관의 제조개발에 필요한 원심주조 조건이 조직과 기계적성질에 미치는 효과)

  • Choi, Sang-Ho
    • Journal of Korea Foundry Society
    • /
    • v.14 no.6
    • /
    • pp.566-575
    • /
    • 1994
  • The effects of varying the pouring temperature and the die preheating temperature in producing centrifugally cast HP alloy modified with Nb was evaluated on the basis of the resultant macrostructure, microstructure and hardness of these castings. Increased die preheating temperatures and pouring temperatures resulted in an increase in the thickness of the columnar dendritic zone, the primary and secondary dendrite arm spacing and the thickness of the zone of porosity at the casting I.D.(inner diameter). Lower die preheating temperature and pouring temperatures result in increased grain fineness and an increased zone of equiaxed grains. A higher hardness was achieved toward the casting O.D.(outer diameter) compared to the casting I.D., attributable to alloy segregation toward the casting I.D. and segregation differences resulting from reduced solidification cooling rates toward the casting I.D. Also, a higher hardness was realized at the cold end of the casting attributed to a more uniform distribution of carbides.

  • PDF

Evolution of Solidification Structures of Al-Si Alloys in a Vertical Centrifugal Casting (Al-Si합금의 수직원심주조시 응고조직의 형성)

  • Chang, Sung-Rak;Huh, Seung-Ho;Hong, Chun-Pyo
    • Journal of Korea Foundry Society
    • /
    • v.20 no.3
    • /
    • pp.197-207
    • /
    • 2000
  • Al-Si alloys were solidified in a rotating cylindrical mold by a vertical centrifugal casting process. Under a certain casting condition, there are four distinct zones such as the chill zone, the primary fine columnar zone, the equiaxed zone, and the secondary coarse columnar zone from the mold wall. The columnar-equiaxed transition (CET) and the equiaxed-columnar transition (ECT) were measured as functions of solute content, flow rate (mold velocity), pouring temperature and mold temperature. Within the critical value of solute content, as the flow rate increases, the columnar-equiaxed transition were found, but not the equiaxed-columnar transition. The aspect ratio of the primary columnar zone was more affected by the solute content than the flow rate. However the aspect ratio of the equiaxed zone was more affected by the flow rate than the solute content. The aspect ratio of the secondary columnar zone was affected by both the flow rate and the solute content.

  • PDF

Characterization of the Ni and Ni-Cr Porous Metal Reinforced AC4C Matrix Composites Fabricated by Squeeze Casting (용탕단조법에 의한 Ni, Ni-Cr 다공질 발포금속 강화 AC4C 합금기 복합재료에 관한 연구)

  • Kim, Eok-Soo
    • Journal of Korea Foundry Society
    • /
    • v.25 no.2
    • /
    • pp.80-87
    • /
    • 2005
  • The microstructure and mechanical property of the Ni and Ni-Cr porous metal reinforced AC4C matrix composites fabricated by squeeze casting were investigated. In this study Ni, Ni-Cr porous metals which are estimated to be easy to fabricate by squeeze casting are used as strengtheners for composite materials. As a matrix material, Al-7wt.%Si-0.3wt.%Mg(AC4C) has been used. In case of Ni/AC4C and Ni-Cr/AC4C composite, $750^{\circ}C$ melt temperature and minimum 25MPa squeezing pressure are needed to produce sound composite materials. The observation of interfacial reaction zone at various heat treatment condition shows that atsolutionizing temperature of above $520^{\circ}C$, the interfacial reaction zone increases proportionally with heat treatment time and the reaction products formed by interfacial reactions are mainly composed by $Al_{3}Ni$ and $Al_{3}Ni_{2}$ phases.

The Effect of Casting Conditions on the Fluidity during Lost Foam Casting of Al Alloy (알루미늄 합금의 소실모형주조 시 유동도에 미치는 주조 조건의 영향)

  • Shin, Seung-Ryoul;Han, Sang-Won;Lee, Kyong-Whoan;Lee, Zin-Hyoung
    • Journal of Korea Foundry Society
    • /
    • v.24 no.1
    • /
    • pp.34-39
    • /
    • 2004
  • The effects of casting condition and hot melt glue during Lost Foam Casting were investigated on the fluidity of Al alloy melt. The fluidity increased linearly with increasing pouring temperature in thick castings but non-linearly in thin casting due to the difference in main heat flow direction. The metal flow velocity was in range of $0.5{\sim}2.7$ cm/s in no evacuation condition and the minimum value of it was measured after the melt flow through the hot melt barrier. The mold evacuation improved the metal flow velocity by around $0.5{\sim}1$ cm/s. And the reaction zone layer thickness was about 1 cm in no-evacuation conditions but about 0.6 cm in mold evacuation condition of 710 torr due to the easier removal of pyrolsis product of EPS. And hot melt barrier thickness of 0.6 mm increased the reaction zone layer thickness up to about 2.5 cm. The fluidity decreased remarkably with an enlarged thickness of hot melt due to a lot of pyrolysis products.

The examination of the pores of casting bodies depending on the position of wax pattern in the ring for precious alloys (Ring 내 납형의 위치에 따른 귀금속합금 주조체의 수축공 관찰)

  • Park, Min-Ju;Noh, Hak;Ko, Dae-Jin;Jung, Jong-Hyun
    • Journal of Technologic Dentistry
    • /
    • v.30 no.1
    • /
    • pp.9-15
    • /
    • 2008
  • An investigation was carried out to examine the pores of casting bodies depending on the position of wax pattern in the ring for precious alloy by optical micrographs. From the result of optical micrographs, many pores were found in the Group C that wax pattern is placed in the center of the ring. However, any pores were scarcely found in the Group A, B, D and E that wax patterns are placed out of the center of thermal zone. In comparison with the pores of casting bodies of Group C, many pores were found at the cusp area rather than at the proximal surface. From these examination, it was concluded that wax pattern should be placed out of the center of thermal zone to prevent casting boies from occurring pores.

  • PDF

A Deformation Behavior Analysis of Dynamic Bulging in the Mini-Mill Continuous Casting System (Mini-Mill 연속주고기의 동적 Bulging해석 Model(I) -주편의 변형거동을 중심으로-)

  • 한성욱;정영진;강충길
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1998.03a
    • /
    • pp.138-143
    • /
    • 1998
  • The continuous casting process has been adopted increasingly in recent years to save both energy and labor. It has experienced a rapid development in the production of semi-finished steel products, replacing the conventional route of ingot casting plus rolling. To achieve this good merit, however, more studies about a heat transfer mechanism between roll and slab are needed. So this paper shows the results of the deformation behavior of steel cast slabs, which are about the solidification and heat transfer. This study is used to prevent internal cracks of a slab in a bending and unbending zone. The value of moving strand shell bulging between two supporting rollers under ferrostatic pressure and slab-self weight has been computed in terms of creep and elastic-plasticity. The high strand distributions in solidified shell undergoes a series of bulging are calculated with boundary condition a very closed to continuous steel cast slabs productions.

  • PDF

Effects of Cooling Method Followed by Casting on the Interfacial and Mechanical Properties of Dental CP-Ti Casts (치과용 티타늄 주조체의 냉각방법이 표면반응층 및 기계적 특성에 미치는 영향)

  • Moon, Soo;Jung, Jun-Young;Kim, Ki-Ju;Lee, Jin-Hyung
    • Journal of Biomedical Engineering Research
    • /
    • v.24 no.5
    • /
    • pp.375-380
    • /
    • 2003
  • In this study. we have intended to control the properties of surface reaction zone generated between pure titanium and oxide investment moulds. Commercially pure titanium was centrifugally casted and silica$.$alumina based phosphate bonded investment was used as the mould material. The effect of cooling methods after casting on the surface reaction zone and mechanical properties of casts were investigated. The resulting casts showed the multilayered surface reaction zone regardless of cooling method. Especially. water cooling method produced the titanium casts with thinner surface reaction zone. weaker strength. and higher elongation properties compared to air cooling. It can thus be known that the resulting casts had satisfactory mechanical properties as dental materials. From these results, the cooling rate dependence of interfacial and mechanical properties can be attributed to the diffusion of oxygen from casting environment, which control the reaction of titanium and mould.

A Study on the characteristics of the cast using forged insert (까단조형 인서트를 이용한 주물재의 특성연구)

  • Yim, H.S.;Park, H.K.;Lee, K.Y.;Kang, Y.K.;Moon, Y.H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.10a
    • /
    • pp.354-357
    • /
    • 2008
  • In this study, the casting process using forged insert was applied to manufacturing a knuckle, in order to prove that application of casting process using forged insert is likely to get the effect of light weight and superior mechanical characteristic compared with existing casting products. Firstly, in the forging experiment, it was confirmed that the optimal configuration of the forged insert could be predicted by FE analysis. And by using FVM (Finite Volume Method) software, it was verified that a proposed casting design was available. To identify the mechanical characteristic of the final casting product, the microstructual observation and hardness test were performed at the boundary zone between forging and casting part.

  • PDF

A study on the phase change in the cylindrical mold by the enthalpy method (엔탈피법을 이용한 원통형 몰드내에서의 상변화과정에 관한 연구)

  • 여문수;최상경;김문철
    • Korean Journal of Air-Conditioning and Refrigeration Engineering
    • /
    • v.11 no.6
    • /
    • pp.891-897
    • /
    • 1999
  • The heat transfer characteristics at the interface between the mold and the casting is one of the major factors for the solidification speed which determines the casting structures. The thermal resistance exists due to air gap formation at the mold/casting interface during the freezing process. In this study one dimensional Stefan problem with the air-gap resistance in the cylindrical mold is considered and the heat transfer characteristics is numerically examined by using the enthalpy method which is convenient in solving the Stefan problem with mushy zone. The present results agreed very well with those of previous papers. The effects of major parameters such as thermal conductivity, heat transfer coefficient of mold, on the thermal characteristics are investigated.

  • PDF

Process Simulation of Investment Casting for Large Gas Turbine Component (대형 가스터빈 부품의 정밀주조 응고해석)

  • Seo, Seong-Mun;Jo, Chang-Yong;Lee, Jae-Hyeon;Choe, Seung-Ju
    • 연구논문집
    • /
    • s.29
    • /
    • pp.173-183
    • /
    • 1999
  • The vacuum investment casting process for a large gas turbine component, Inner Preswirl Support (IPS), was simulated by using commercial FEM package ProCAST(TM) with view factor radiation method. The solid fraction in mushy zone was directly measured by Differential thermal analysis(DTA-DSC mode). Three types gating design. considering liquid flow and heat release through it. were proposed. Solidification had begun at the ribs or thin sections of the IPS casting and advanced further through the upper and lower gates. The computed temperature gradient G and G/R values at 70% solidified temperature were used for prediction of microshrinkage formation during casting. The effect of mold preheat on the thermal history of the casting displayed minute effect on the microshrinkage formation.

  • PDF