Fabrication and Properties of Thin Microwave Absorbers of Ferroelectric Materials Used in Mobile Telecommunication Frequency Bands (강유전체를 이용한 이동통신주파수 대역용 박형 전파흡수체의 제조 및 특성)

  • Lee, Yeong-Jong;Yun, Yeo-Chun;Kim, Seong-Su
    • Korean Journal of Materials Research
    • /
    • v.12 no.2
    • /
    • pp.160-165
    • /
    • 2002
  • High-frequency dielectric and microwave absorbing properties have been investigated in ferroelectric materials (BaTiO$_3$(BT), (1-x)Pb$Mg_{\frac{1}{3}}Nb_{\frac{2}{3}}$)O$_3$-xPbTiO$_3$(PMN-PT), (1-x)Pb$Mg_{\frac{1}{3}}Nb_{\frac{2}{3}}$O$_3$-xPb(Zn_{\frac{1}{3}}Nb_{\frac{2}{3}}$)O$_3$(PMN-PZN) for the aim of thin microwave absorbers in the frequency range of mobile telecommunication. The specimenns are prepared by conventional ceramic processing and complex permittivity has been measured by transmission/reflection method. The ferroelectric materials show high dielectric constant and dielectric loss in the microwave range and their domiant loss mechanism is considered to be domain wall relaxation. The microwave absorbance of BT 0.9PMN-0.1PT, and 0.8PMN-0.2PZN specimen (determined at 2) are found to be 99.5% (at a thickness of 4.5 mm), 50% (2.5 mm), and 30% (2.5 mm), respectively. It is suggested that PMN-PT or PMN-PZN ferroelectrics are good candidate materials for the spacer of λ/4 absorber. The use of ferroelectric materials is effective in reducing the thickness of absorber with their advantage of high dielectric constant.

A study on the development of SRM for XRF analysis of PZT[$Pb(ZrTi)O_3$] (PZT[$Pb(ZrTi)O_3$]의 XRF 분석용 SRM 개발에 관한 연구)

  • Kim, Young Man;Jeong, Chan Yee;Lim, Chang Ho;Choi, Beom Suk
    • Analytical Science and Technology
    • /
    • v.10 no.6
    • /
    • pp.439-444
    • /
    • 1997
  • Twelve kinds (1set) standard materials of chemical ingredients of lead zirconate titanate[$Pb(ZrTi)O_3$] have been developed in order to determine fast and accurate measurement of X-ray fluorescence spectrometry. Especially, we used diluted(ahout sixteen times) filling compound($Li_2B_4O_7/LiBO_2=4/1$) to consider removal effect of matrix, storage convenience, and homogenous characteristics. As a result from the four different laboratories, we obtained extremly good agreement about the standard curve on twelve standard materials which containing eleven elements, PbO, $ZrO_2$, $TiO_2$, SrO, $WO_3$, $La_2O_3$, $Cr_2O_3$, MgO, $Nb_2O_5$, and $MnO_2$. The correlation factor of standard curve was over 0.998. However, ZnO has relatively low correlation factor, 0.977, because the concentration was 10ppm lower than other original materials. This analysis reveals that ZnO has shown the poor linearity as well as low fluorescence intensity. In present work, XRF standard materials are useful for determining a rapid and accurate results for major and minor elements concentration among PZT.

  • PDF

Fabrication of SAW filter using PZT ceramics (PZT압전세라믹을 이용한 SAW필터의 제작)

  • 정연호;송준태
    • Electrical & Electronic Materials
    • /
    • v.10 no.1
    • /
    • pp.1-7
    • /
    • 1997
  • SAW filter has been used in mobile communication device, bandpass filter and resonator for merits )f miniaturization and high reliability. Materials for substrate mainly used single crystal such as LiNbO$_{3}$, LiTaO$_{3}$, ZnO. In this study, it was attempted that LiNbO$_{3}$ was substituted for piezoelectric ceramics(PZT4, PZT5A and PZT8) which had simple fabrication process because fabrication of crystal is difficult and it's cost is high. SAW filters were fabricated by the photolithography on piezoelectric ceramics substrates in order to compare their characteristics with LiNbO$_{3}$'s. The experimental value of center frequency was compared with theoretical one. The average difference of center frequency was 3.7%. PZT8 showed the best bandwidth properties among them. It is considered that PZT8 has higher mechanical quality factor and propagation velocity than others.

  • PDF

Electric properties of PZN-PNN-PT-PZ piezoelectric ceramics prepared by molten salt method (용융염 합성법으로 제조한 PZN-PNN-PT-PZ계 압전세라믹스의 전기적 특성)

  • 어수해;이기태
    • Electrical & Electronic Materials
    • /
    • v.9 no.4
    • /
    • pp.351-356
    • /
    • 1996
  • The quartemary system ceramics 0.5[xPb(Zn$_{1}$3/Nb$_{2}$3/)O$_{3}$-(1-x)Pb(Ni$_{1}$3/Nb$_{2}$3/)O$_{3}$]-0.5[yPbTiO$_{3}$-(1-y) PbZrO$_{3}$ for piezoelectric actuators were prepared bv the were added to the raw materials up to 5 mole. Sintering temperature was varied form 1000.deg. C to 1200.deg. C. Sintering characteristrics, dielectric and piezoelectric properties were then investigated. Piezoelectric properties of sample prepared by the molten salt method were improved compared to those prepared by the conventional method. Addition of PZN shifted morphotropic phase boundary to more Zr-rich composition and decreased the piezoelectric properties.

  • PDF

Effect of A-Site Substitution on the Dielectric Properties of PZN Ceramics (A-자리 치환에 따른 PZN 세라믹스의 유전특성)

  • 조상희;백종갑;손정호;김정주;김남경
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.5
    • /
    • pp.635-641
    • /
    • 1995
  • The effects of A-site substitution with alkaline-earth ions (Ca, Sr and Ba) on the perovskite-phase formation and dielectric properties for Pb1-xMx(Zn1/3Nb2/3)O3 (0.0 x 0.5)-based relaxors were studied. Considerable improvements in the sinterability and the extent fo perovskite formation were observed with increasing the A-site substitution (x) and sintering temperature. The maximum dielectric permittivity appeared at x=0.1 for Sr and Ba substitutiion, while the relative dielectric permittivity was almost invariant in the case of Ca ion substitution. Curie temperature decreased with increasing relative amount of Sr and Ba ions but was almost invariant in case of Ca ion substitution. With increasing the amount of x, the diffuseness parameter ($\delta$) increased but the maximum dielectric constant decreased, demonstrating an enhanced diffuse phase transition (DPT) in the presence of alkaline-earth cations.

  • PDF

A High Tunable Capacitor Embedding Its Electrodes in Tunable Thin Film Dielectrics (가변형 박막 유전체에 전극을 임베디드 시킨 고가 변형 커패시터)

  • Lee Young-Chul;Hong Young-Pyo;Ko Kyung-Hyun
    • The Journal of Korean Institute of Electromagnetic Engineering and Science
    • /
    • v.17 no.9 s.112
    • /
    • pp.860-865
    • /
    • 2006
  • In this paper, a novel tunable inter-digital capacitor using dielectric tunable $Bi_2O_3-ZnO-Nb_2O_5(BZN)$ pyrochlore thin films is proposed. In order to improve the tunability and reduce DC bias voltage using the fringing electric field, the electrodes of the inter-digital capacitor are embedded in the thin film. Designed results using a 2.5 D simulator show that the tunability of the proposed inter-digital capacitor improves by 10 %, compared to the conventional inter-digital capacitor. The proposed IDC, which is based on the simulation results, was fabricated, using the BZN thin film deposited by a reactive RF magnetron sputtering on the on the silicon substrate. The fabricated inter-digital capacitor shows the maximum tunability of 50 % at 5.8 GHz and 18 V DC applied.

Structure and Electrical Properties of Pb($Zn_{1/3}Nb_{2/3})O_3-Pb(Zr_xTi{1-x})O_3$ Ceramics (Pb($Zn_{1/3}Nb_{2/3})O_3-Pb(Zr_xTi{1-x})O_3$세라믹의 구조적, 전기적 특성)

  • 조현무;이성갑;이영희
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.07a
    • /
    • pp.357-360
    • /
    • 2000
  • Ferroelectric 0.05PZN-xPZT(90/10)-(0.95-x)PZT(10/90) (x=0.65, 0.85) specimens were fabricated by the mixed-oxide method and cold-pressing method using sol-gel derived PZT(90/10) and PZT(10/90) powders. All specimens show a uniform ferroelectric grain without the presence of the pyrocholre phase. Average grain size increased with an increase in sintering temperature, the value for the x=0.65 specimen sintered at 125$0^{\circ}C$ was 14.4${\mu}{\textrm}{m}$. The dielectric constant and dielectric loss of the x=0.65 specimen sintered at 125$0^{\circ}C$ were 1247, 2.05%, respectively. All specimens showed fairly good temperature and frequency stability of dielectric constant with the range from -2$0^{\circ}C$ to 6$0^{\circ}C$ and 100Hz to 10MHz. The coercive electric field and the remanent polarization of x = 0.65 specimen sintered at 125$0^{\circ}C$ were 8.5 kV/cm and 13 $\mu$C/cm$^2$, respectively.

  • PDF

Study on Corrosion Characteristics of Zr-Sn and Zr-Nb-Sn Alloys (Zr-Sn 및 Zr-Nb-Sn 합금의 부식특성에 관한 연구)

  • Jeon, Chi-Jung;Jeong, Yong-Hwan;Kim, Seon-Jin
    • Korean Journal of Materials Research
    • /
    • v.9 no.4
    • /
    • pp.378-385
    • /
    • 1999
  • To evaluate the effect of Sn on the corrosion behavior of Zr alloys for nuclear fuel claddings, the corrosion tests on the binary Zr-xSn and the ternary Zr-0.4Nb-xSn alloys were performed in water at $360^{\circ}C$. The binary alloys containing 0.5, 0.8 and 1.5wt.% Sn showed the transition corrosion rate at 15 days. On the other hand, the binary alloy containing 2.0wt.% Sn showed a good corrosion resistance without the transition of corrosion rate up to 80 days. The corrosion rate of the ternary alloy increased with increasing Sn content. The difference of corrosion behaviors between binary and ternary alloys is considered due to the different solubility of Sn, Nb content and precipitates. The corrosions of Zr-xSn and Zr-0.4Nb-xSn alloys would be controlled by the fraction of tetragonal-$ZrO_2$and the amount of hydrogen pick-up.

  • PDF

Piezoelectric properties and microstructure of 0.01Pb(Mg1/2W1/2)O3-0.41Pb(Ni1/3Nb2/3)O3-0.35PbTiO3-0.23PbZrO3thick film with particle size distribution (입자 크기 분포에 따른 0.01Pb(Mg1/2W1/2)O3-0.41Pb(Ni1/3Nb2/3)O3-0.35PbTiO3-0.23PbZrO3 후막의 미세구조 및 압전특성)

  • Moon, Hi-Gyu;Song, Hyun-Cheol;Kim, Sang-Jong;Choi, Ji-Won;Kang, Chong-Yun;Yoon, Seok-Jin
    • Journal of Sensor Science and Technology
    • /
    • v.17 no.6
    • /
    • pp.418-424
    • /
    • 2008
  • The PZT based piezoelectric thick films prepared by screen printing method have been mainly used as a functional material for MEMS applications due to their compatibility of MEMS process. However the screen printed thick films generally reveal poor electrical and mechanical properties because of their porous microstructure. To improve microstructure we mixed attrition milled powder with ball milled powder of 0.01Pb$(Mg_{1/2}W_{1/2})O_3$-0.41Pb$(Ni_{1/3}Nb_{2/3})O_3$-$0.35PbTiO_3$-$0.23PbZrO_3$+0.1 wt% ${Y_2}{O_3}$+1.5 wt% ZnO composition. By mixing 25 % of attrition milled powder and 75 % of ball milled powder, the broadest particle size distribution was obtained, leading to a dense thick film with crack-free microstructure and improved dielectric properties. The X-ray diffraction analysis revealed that the film was in wellcrystallized perovskite phase. The remanent polarization was increased from $13.7{\mu}C/cm^2$ to $23.3{\mu}C/cm^2$ at the addition of 25 % attrition milled powder.

Effect of Pb based flux on the Microwave Dielectric Properties of PCFN-PZW System (PCFN-PZW계의 마이크로파 유전 특성에 미치는 Pb계 Flux의 영향)

  • 강동헌;설충의;차훈주;김영호;길상근;조봉희
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.15 no.12
    • /
    • pp.1027-1032
    • /
    • 2002
  • (Pb$\_$0.4/Ca$\_$0.6/)(Fe$\_$1/2/Nb$\_$1/2/)O$_3$ system was modified by 10 mol% Pb(Zn$\_$1/2/W$\_$1/2/)O$_3$ addition and their sinterability and microwave properties were investigated as a function of the amount of flux (0.975PbO-0.025SnO$_2$). With increasing flux content, single perovskite phase was maintained up to 3 wt% flux addition and further addition led to the presence of Pb-rich second phase which was confirmed by EDS analysis. The apparent densities of PCFN-PZW specimen increased and showed maximum values at 2.5 wt% flux addition for the Ts=1000$^{\circ}C$ and 2.0wt% flux addition for the Ts=1050$^{\circ}C$, respectively. The dielectric constant and Q$.$f values strongly depended on the variation of density and microstructure, where the optimum values of $\varepsilon$$\_$r/ = 91.95, Q$.$f = 5938GHz, TCF = +8.15ppm/$^{\circ}C$ were obtained for the 2.5wt% flux added PCFN-PZW specimen sintered at 1000$^{\circ}C$ for 4h.