• Title/Summary/Keyword: ZnO nanostructure

Search Result 79, Processing Time 0.04 seconds

Investigation of the luminescence properties of ZnO nanostructures (ZnO 나노 구조의 형상에 따른 발광 특성에 관한 연구)

  • Jung, Mi-Na;Ha, Seon-Yeo;Park, Seung-Hwan;Yang, Min;Kim, Hong-Seung;Lee, Uk-Hyeon;Yao, Takafumi;Chang, Ji-Ho
    • Proceedings of the Korean Institute of Information and Commucation Sciences Conference
    • /
    • v.9 no.1
    • /
    • pp.1013-1016
    • /
    • 2005
  • ZnO nanostructure was fabricated by catalyst-free method using Zn powder in air. The growth temperature was controlled from 450$^{\circ}$C to 600$^{\circ}$C, and the structural and optical properties were investigated by scanning electron microscopy (SEM), photoluminescence (PL), energy dispersive X-ray spectroscopy (EDX) and cathodoluminescence (CL). From all samples both ZnO tetrapods and clusters were observed. No significant dispersion was observed from the ZnO tetrapods, however, ZnO clusters show considerable change in density and size. From the EDX results, atomic composition difference was found. The clusters have O-deficiencies, while tetrapods have stoichiometric composition. Strong luminescence was observed at room temperature. From room temperature PL, UV emission at 380 nm and green emission at 500 nm were observed, and the intensity ratio ($I_{uv}/I_{green}$) increased as growth temperature increases. CL measurements show that the UV emission is closely related with tetrapods and the green emission is dominated from the clusters.

  • PDF

Surface and small scale effects on the dynamic buckling of carbon nanotubes with smart layers assuming structural damping

  • Farokhian, Ahmad;Salmani-Tehrani, Mehdi
    • Steel and Composite Structures
    • /
    • v.37 no.2
    • /
    • pp.229-251
    • /
    • 2020
  • In this paper, dynamic buckling of a smart sandwich nanotube is studied. The nanostructure is composed of a carbon-nanotube with inner and outer surfaces coated with ZnO piezoelectric layers, which play the role of sensor and actuator. Nanotube is under magnetic field and ZnO layers are under electric field. The nanostructure is located in a viscoelastic environment, which is assumed to obey Visco-Pasternak model. Non-local piezo-elasticity theory is used to consider the small-scale effect, and Kelvin model is used to describe the structural damping effects. Surface stresses are taken into account based on Gurtin-Murdoch theory. Hamilton principle in conjunction with zigzag shear-deformation theory is used to obtain the governing equations. The governing equations are then solved using the differential quadrature method, to determine dynamic stability region of the nanostructure. To validate the analysis, the results for simpler case studies are compared with others reported in the literature. Then, the effect of various parameters such as small-scale, surface stresses, Visco-Pasternak environment and electric and magnetic fields on the dynamic stability region is investigated. The results show that considering the surface stresses leads to an increase in the excitation frequency and the dynamic stability region happens at higher frequencies.

Effect of ON/OFF Cycles of Ar Gas on Structural and Optical Properties of ZnO Nanostructure Grown by Vapor Phase Transport

  • Nam, Gi-Woong;Kim, Min-Su;Cho, Min-Young;Kim, So-A-Ram;Leem, Jae-Young
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.02a
    • /
    • pp.415-415
    • /
    • 2012
  • ZnO nanostructures were synthesized by a vapor phase transport process in a single-zone furnace within a horizontal quartz tube with an inner diameter of 38 mm and a length of 485 mm. The ZnO nanostructures were grown on Au-catalyzed Si(100) substrates by using a mixture of zinc oxide and graphite powders. The growth of ZnO nanostructures was conducted at $800^{\circ}C$ for 30 min. High-purity Ar and $O_2$ gases were pushed through the quartz tube during the process at a flow rate of 100 and 10 sccm, respectively. The sequence of ON/OFF cycles of the Ar gas flow was repeated, while the $O_2$ flow is kept constant during the growth time. The Ar gas flow was ON for 1 min/cycle and that was OFF for 2 min/cycle. The structure and optical properties of the ZnO nanostructures were investigated by field-emission scanning electron microscope, X-ray diffraction, temperature-dependent photoluminescence. The preferred orientation of the ZnO nanostructures was along c-axis with hexagonal wurtzite structure.

  • PDF

Morphology control and optical properties of ZnO nanostructures grown by ultrasonic synthesis

  • Morales-Flores, N.;Galeazzi, R.;Rosendo, E.;Diaz1d, T.;Velumani, S.;Pal, U.
    • Advances in nano research
    • /
    • v.1 no.1
    • /
    • pp.59-70
    • /
    • 2013
  • ZnO nanostructures of rod-like, faceted bar, cup-end bars, and spindle shaped morphologies could be grown by a low power ultrasonic synthesis process. pH of the reaction mixture seems to plays an important role for defining the final morphology of ZnO nanostructures. While the solution pH as low as 7 produces long, uniform rod-like nanostructures of mixed phase (ZnO and $Zn(OH)_2$), higher pH of the reaction mixture produces ZnO nanostructures of different morphologies in pure hexagonal wurtzite phase. pH of the reaction as high as 10 produces bar shaped uniform nanostructures with lower specific surface area and lower surface and lattice defects, reducing the defect emissions of ZnO in the visible region of their photoluminescence spectra.

Photoluminescence Studies of ZnO Nanostructures Fabricated by Using Combination of Hydrothermal Method and Plasma-Assisted Molecular Beam Epitaxy Regrowth

  • Nam, Giwoong;Kim, Byunggu;Park, Youngbin;Kim, Soaram;Lee, Sang-Heon;Kim, Jong Su;Leem, Jae-Young
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.08a
    • /
    • pp.202.1-202.1
    • /
    • 2013
  • ZnO nanostructure was fabricated on a Si substrate using two-step growth. The seed layer was grown on the Si substrate by a sol-gel spin-coating. In the first step, ZnO nanorods were grown by a hydrothermal method at $140^{\circ}C$ for 5 min. In the second step, a ZnO thin film was grown on the ZnO nanorods by spin-coating. After growth, these films were annealed at $800^{\circ}C$ for 10 min. Electrical and optical properties of ZnO nanostructures have modified by plasma-assisted molecular beam epitaxy (PA-MBE) regrowth. The carrier concentration and resistivity increased by PA-MBE regrowth. In the photoluminescence, the full width at half maximum and intensity were decreased and increased, respectively, by PA-MBE regrowth.

  • PDF

Zinc Oxide Nanostructured Thin Film as an Efficient Photoanode for Photoelectrochemical Water Oxidation

  • Park, Jong-Hyun;Kim, Hyojin
    • Korean Journal of Materials Research
    • /
    • v.30 no.9
    • /
    • pp.441-446
    • /
    • 2020
  • Synthesizing nanostructured thin films of oxide semiconductors is a promising approach to fabricate highly efficient photoelectrodes for hydrogen production via photoelectrochemical (PEC) water splitting. In this work, we investigate the feasibility as an efficient photoanode for PEC water oxidation of zinc oxide (ZnO) nanostructured thin films synthesized via a simple method combined with sputtering Zn metallic films on a fluorine-doped tin oxide (FTO) coated glass substrate and subsequent thermal oxidation of the sputtered Zn metallic films in dry air. Characterization of the structural, optical, and PEC properties of the ZnO nanostructured thin film synthesized at varying Zn sputtering powers reveals that we can obtain an optimum ZnO nanostructured thin film as PEC photoanode at a sputtering power of 40 W. The photocurrent density and optimal photocurrent conversion efficiency for the optimum ZnO nanostructured thin film photoanode are found to be 0.1 mA/㎠ and 0.51 %, respectively, at a potential of 0.72 V vs. RHE. Our results illustrate that the ZnO nanostructured thin film has promising potential as an efficient photoanode for PEC water splitting.

Self-assembly of ZnO Stripes Prepared by Anodization in an Ethanolic Sulfuric Acid (에탄올/황산 혼압액에서 양극산화법을 이용한 자기정렬된 ZnO 줄무늬 구조 제조 연구)

  • Kim, Sung Joong;Choi, Jinsub
    • Korean Chemical Engineering Research
    • /
    • v.46 no.4
    • /
    • pp.686-691
    • /
    • 2008
  • There are no many research reports on the preparation of ZnO by electrochemical oxidation since the zinc oxide is very easily dissolved in an acidic or basic environment, even though zinc oxides have attracted many attentions because of their optical/electrical properties. In this paper, we describe the fabrication of self-ordered stripes of ZnO by anodization of Zn in an ethanolic sulfuric acid. The formation of stripes of ZnO originating from Zn is attributed to water-selective dissolution of ZnO during anodization. We study in detail the effects of concentration of $H_2SO_4$, applied potential, anodization time, and addition of a small amount of water on the fabrication of stripes of ZnO. Mechanisms for the fabrication of ZnO stripes are discussed in terms of the above-mentioned effects.

ZnO Nanostructure Characteristics by VLS Synthesis (VLS 합성법을 이용한 ZnO 나노구조의 특성)

  • Choi, Yuri;Jung, Il Hyun
    • Applied Chemistry for Engineering
    • /
    • v.20 no.6
    • /
    • pp.617-621
    • /
    • 2009
  • Zinc oxide (ZnO) nanorods were grown on the pre-oxidized silicon substrate with the assistance of Au and the fluorine-doped tin oxide (FTO) based on the catalysts by vapor-liquid-solid (VLS) synthesis. Two types of ZnO powder particle size, 20nm, $20{\mu}m$, were used as a source material, respectively The properties of the nanorods such as morphological characteristics, chemical composition and crystalline properties were examined by X-ray diffraction (XRD), energy-dispersive X-ray spectroscopy (EDX) and field-emission scanning electron microscope (FE-SEM). The particle size of ZnO source strongly affected the growth of ZnO nanostructures as well as the crystallographic structure. All the ZnO nanostructures are hexagonal and single crystal in nature. It is found that $1030^{\circ}C$ is a suitable optimum growth temperature and 20 nm is a optimum ZnO powder particle size. Nanorods were fabricated on the FTO deposition with large electronegativity and we found that the electric potential of nanorods rises as the ratio of current rises, there is direct relationship with the catalysts, Therefore, it was considered that Sn can be the alternative material of Au in the formation of ZnO nanostructures.

Effects of Co Doping on NO Gas Sensing Characteristics of ZnO-Carbon Nanotube Composites (산화아연-탄소나노튜브 복합체의 일산화질소 가스 감지 특성에 미치는 코발트 첨가 효과)

  • Jung, Hoon-Chul;Ahn, Eun-Seong;Hung, Nguyen Le;Oh, Dong-Hoon;Kim, Hyo-Jin;Kim, Do-Jin
    • Korean Journal of Materials Research
    • /
    • v.19 no.11
    • /
    • pp.607-612
    • /
    • 2009
  • We investigated the effects of Co doping on the NO gas sensing characteristics of ZnO-carbon nanotube (ZnO-CNT) layered composites fabricated by coaxial coating of single-walled CNTs with ZnO using pulsed laser deposition. Structural examinations clearly confirmed a distinct nanostructure of the CNTs coated with ZnO nanoparticles of an average diameter as small as 10 nm and showed little influence of doping 1 at.% Co into ZnO on the morphology of the ZnO-CNT composites. It was found from the gas sensing measurements that 1 at.% Co doping into ZnO gave rise to a significant improvement in the response of the ZnO-CNT composite sensor to NO gas exposure. In particular, the Co-doped ZnO-CNT composite sensor shows a highly sensitive and fast response to NO gas at relatively low temperatures and even at low NO concentrations. The observed significant improvement of the NO gas sensing properties is attributed to an increase in the specific surface area and the role as a catalyst of the doped Co elements. These results suggest that Co-doped ZnOCNT composites are suitable for use as practical high-performance NO gas sensors.