• 제목/요약/키워드: Zinc borosilicate glass

검색결과 31건 처리시간 0.028초

저온소결용 $Zr1-x(Zn_{1/3}Nb_{2/3})xTiO_4$ 세라믹스의 소결 및 마이크로파 유전 특성 (Sinterability and microwave dielectric properties of $Zr1-x(Zn_{1/3}Nb_{2/3})xTiO_4$ system ceramics sintered at low temperature)

  • 김관수;윤상옥;이주영;김남협;이주식;심상흥;박종국
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 Vol.19
    • /
    • pp.208-209
    • /
    • 2006
  • Sinterability and microwave dielectric properties of the $Zr1-x(Zn_{1/3}Nb_{2/3})xTiO_4$(x=4, 6) system ceramics have been investigated as functions of zinc-borosilicate(ZBS) glass contents and amount of $Zn_{1/3}Nb_{2/3}O_2$ substitution with a view to applying the composition to LTCC technology. The addition of 25 wt% ZBS glass ensured successful sintering below $925^{\circ}C$. With increasing ZBS glass and $Zn_{1/3}Nb_{2/3}O_2$ contents increased dielectric constant and sinterability but addition ZBS glass decreased the quality factor significantly due to the formation of an excessive liquid and second phases. The sintered $Zr4(Zn_{1/3}Nb_{2/3})6TiO_4$ system ceramics at $925^{\circ}C$ with 25 wt% ZBS glass demonstrated 27.7 in dielectric constant (${\varepsilon}_r$), 3,850 m quality factor($Q{\times}f_0$), and +6 ppm/$^{\circ}C$ in temperature coefficient of resonant frequency($\tau_f$).

  • PDF

저온 소결용 xZnWO4-(1-x)TiO2 세라믹스의 소결 및 마이크로파 유전 특성 (Sinterability and Microwave Dielectric Properties of xZnWO4-(1-x)TiO2 Ceramics Sintered at Low Temperature)

  • 윤상옥;김관수;심상흥;박종국
    • 한국전기전자재료학회논문지
    • /
    • 제19권9호
    • /
    • pp.855-861
    • /
    • 2006
  • Sinterability and microwave dielectric properties of $xZWO_{4}-(1-x)TiO_{2}$ ceramic systems with zinc-borosilicate glass and $TiO_{2}$ contents for LTCC(Low Temperature Co-fired Ceramics) were investigated. The addition of $3{\sim}10\;wt%$ ZBS glass ensured the sinterability below $900^{\circ}C$. In general, increasing ZBS glass content seemed to enhance the sinterability, but the quality factor($Qxf_{0}$) significantly decreased due to the formation of an excessive liquid and second phases. As for the addition of $TiO_{2}$, the dielectric constant(${\varepsilon}_{r}$) and temperature coefficient of resonant frequency(${\tau}_{f}$) showed to increase, while the quality factor($Qxf_{0}$) did not show an apparent change. The composition of $0.7xZnWO_{4}-0.3TiO_{2}$ ceramics sintered at $900^{\circ}C$ with 5 wt% ZBS glass demonstrated 21.6 in dielectric constant(${\varepsilon}_{r}$), 14,800 in quality factor($Qxf_{0}$), and $+5\;ppm/^{\circ}C$ in temperature coefficient of resonant frequency(${\tau}_{f}$).

$1-xBiNbO_4-xZnNb_2O_6$ 세라믹스의 저온소결 및 유전특성 (Low-temperature sintering and dielectric properties of the $1-xBiNbO_4-xZnNb_2O_6$ ceramics)

  • 김윤한;윤상옥;김관수;이주식;김경미;박종국
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.260-260
    • /
    • 2007
  • Low-temperature sintering and dielectric properties of the $1-xBiNbO_4-xZnNb_2O_6$ ceramics (x=0.3, 0.5, and 0.7) with 10 wt% zinc borosilicate (ZBS) glass was investigated as a function of the substitution of $ZnNb_2O_6$ with a view to applying this system to LTCC technology. The all composition addition of 10 wt% ZBS glass ensured a successful sintering below $900^{\circ}C$. The the amount of $ZnNb_2O_6$ on $ZnNb_2O_6$ ceramics increased the $Q{\times}f$ values, but it decreased the sinterability and dielectric constant due to the higher $Q{\times}f$ value and sintering temperature of $ZnNb_2O_6$ than that of $ZnNb_2O_6$ ceramics. The increase of $ZnNb_2O_6$ content from 0.3 to 0.7 in the $1-xBiNbO_4-xZnNb_2O_6$ ceramics with 10 wt% ZBS glass sintered at $900^{\circ}C$ demonstrated 30~20 in the dielectric constant (${\varepsilon}_r$), 3,500~4,500 GHz in the $Q{\times}f$ value.

  • PDF

저온소결용 $Bi(Nb_{0.7}Ta_{0.3})O_4$ 세라믹스의 유전특성에 미치는 $TiO_2$ 영향 (Influence of $TiO_2$ on the dielectric properties of $Bi(Nb_{0.7}Ta_{0.3})O_4$ ceramics for low-firing)

  • 김대민;윤상옥;김관수;김신;김재찬;김경주;박종국
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.298-298
    • /
    • 2007
  • Influence of $TiO_2$ on the dielectric properties of the $Bi(Nb_{0.7}Ta_{0.3})O_4$ ceramic with 7 wt% zinc borosilicate(ZBS) glass was investigated as a function of the $TiO_2$ contents with a view to applying this system to LTCC technology. The $Bi(Nb_{0.7}Ta_{0.3})O_4$ ceramic addition of 7 wt% ZBS glass ensured successful sintering below $900^{\circ}C$. But, TCF of $Bi(Nb_{0.7}Ta_{0.3})O_4$ ceramic is large negative values, respectively, it is necessary to adjust to zero TCF for practical applications Therefore, the addition of materials having positive TCF, such as $TiO_2$, might be an effective method for the improvement. In general, increasing addition of $TiO_2$ increased dielectric constant and TCF but it decreased the sinterability and $Q{\tiems}f$ value significantly due to the dielectric property and high sintering temperature of $TiO_2$. $Bi(Nb_{0.7}Ta_{0.3})O_4$ ceramic with 7 wt% ZBS glass and then addition 0.5 wt% $TiO_2$ sintered at $900^{\circ}C$ demonstrated 42 in the dielectric constant(${\varepsilon}_r$), 1,000 GHz in the $Q{\times}f$ value, and $10{\pm}5\;ppm/^{\circ}C$ in the temperature coefficient of resonant frequency(${\tau}_f$).

  • PDF

(1-x)$BiNbO_4-(x)ZnNb_2O_6$ 세라믹스의 저온 소결 및 유전 특성 (Low-temperature sintering and dielectric properties of the (1-x)$BiNbO_4-(x)ZnNb_2O_6$ ceramics)

  • 김윤한;윤상옥;김신;김관수;김경주;박종국
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.284-284
    • /
    • 2007
  • In this study, the microwave dielectric property variations of (1-x)$BiNbO_4-(x)ZnNb_2O_6$ composites (x=0.3, 0.5 and 0.7) with 10wt% zinc borosilicate(ZBS) glass was investigated as a function of the substitution of $ZnNb_2O_6$ with a view to applying thes system to LTCC technology. The all composition addition of 10wt% ZBS glass ensured a successful sintering below $900^{\circ}C$. In addition, a small amount of $Bi_2SiO_5$ as the secondary phase was observed in the all composition. The substitution of $ZnNb_2O_6$ on the $BiNbO_4$ composites increased the $Q{\times}f$ values, but it decreased the sinterability and dielectric constant due to the high sintering temperature and low dielectric constant of $ZnNb_2O_6\;than\;BiNbO_4$ ceramics. The increasing of $ZnNb_2O_6$ content from 0.3 to 0.7 in the (1-x)$BiNbO_4-(x)ZnNb_2O_6$ composites with 10wt% ZBS glass sintered at $900^{\circ}C$ demonstrated 28.1~15.6 in the dielectric constant$({\varepsilon}_r)$, 5,500~8,700GHz in the $Q{\times}f$ value.

  • PDF

전자장치용 Passivation 유리의 결정화에 관한 연구 (Crystallization of Passivation Glass for Electronic Devices)

  • 손명모;박희찬;이헌수
    • 한국세라믹학회지
    • /
    • 제30권2호
    • /
    • pp.107-114
    • /
    • 1993
  • Zinc-Borosilicate(ZnO 65.0wt%, B2O3 21.5wt%, SiO2 9.0wt%, PbO or tiO2 4wt%) passivation glasses were studied using differential thermal analysis(DTA), scanning electron microscopy(SEM) observations, X-ray diffraction (XRD) patterns and measurement of thermal expansion coefficients. Passivation glasses containing 4wt% TiO2 and 4wt% PbO had crystallization temperature of 680~73$0^{\circ}C$ and major crystalline phases were identified by X-ray diffraction as $\alpha$-ZnO.B2O3 and $\alpha$-5ZnO.2B2O3. As increasing firing temperature, the size of crystalline phases increased by observation of SEM. The thermal expansion coefficient of crystallized glass frits was smaller than that of unfired glass.

  • PDF

고출력 ICP (RF) 열플라즈마 시스템을 이용한 다성분계 나노 복합체 합성

  • 이미연;김정수;최채홍;김민호;서준호;홍봉근
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제43회 하계 정기 학술대회 초록집
    • /
    • pp.415-415
    • /
    • 2012
  • ICP (RF) 열 플라즈마 분말 합성법은 초고온 열플라즈마(~10,000 K) 속으로 원료물질을 투입한 뒤, 용융, 기화 및 재합성의 과정을 거쳐 초미분(<1 ${\mu}s$)을 합성하는 방법으로 고출력 시스템의 경우 고온/고 엔탈피 열 유동을 통한 고융점 및 저융점 복합물질의 동시 기화에 의한 물질 조성이 제어된 나노 복합체의 대량 합성이 가능할 것으로 기대되고 있다. 본 연구에서는 전북대학교 고온플라즈마 응용연구센터의 60&200 kW의 고출력 ICP (RF) 열 플라즈마 시스템을 이용하여 LTO (Lithium Titanium Oxide)와 IZTO (Indium Zinc Tin Oxide), Barium Borosilicate Glass (K2O-BaO-B2O3-SiO2)의 다성분계 나노 복합체를 합성하였으며, FE-SEM, TEM, XRD, ICP-OES를 이용하여 그 특성을 분석하였다.

  • PDF

세라믹 입자가 혼합된 유리분말의 소결, 결정화 및 고주파 유전특성 (Sintering, Crystallization and Microwave Dielectric properties of a Ceramic Particle Incorporated Glass Powder)

  • 김선영;이경호
    • 한국마이크로전자및패키징학회:학술대회논문집
    • /
    • 한국마이크로전자및패키징학회 2002년도 추계기술심포지움논문집
    • /
    • pp.59-63
    • /
    • 2002
  • Zinc-Magnesium borosilicate 유리에 CaF$_2$입자를 충진재로 첨가하여 혼합체의 소결거동, 결정화 거동 및 최종 소결체의 마이크로파 유전특성을 측정하였다. CaF$_2$첨가는 유리의 점도를 감소 시켜 결정화 및 수축개시온도를 감소시켰다. 이러한 CaF$_2$의 최대 첨가량은 주어진 유리조성에 있어서 15 vol. % 이었다. 이러한 소결성 및 결정화 개시온도의 변화는 모 유리와 CaF$_2$의 반응에 의한 결과로 보여지며 이 반응은 결정상의 변화나 이차상의 형성에는 영향을 미치지 않았다. 따라서 유전율 6.1에 품질계수가 40000GHz 인 CaF$_2$입자를 15 vol.% 첨가시 유전상수는 7.1에서 5.6로 품질계수는 2200에서 5000GHz로 유전특성이 향상되었고 소결온도는 75$0^{\circ}C$이었다.

  • PDF

Thermal Expansion and Dielectric Properties of CaO-ZnO-B2O3-SiO2 Glass-Added Al2O3 Composites for LTCC Applications

  • Byeon, Tae-Hun;Park, Hyo-Sung;Shin, Hyun-Ho;Yoon, Sang-Ok;Oh, Chang-Yong
    • 한국세라믹학회지
    • /
    • 제47권4호
    • /
    • pp.325-328
    • /
    • 2010
  • Varying quantities of a high-thermal-expansion glass, 50CaO-20ZnO-$20B_2O_3-10SiO_2$ (CZBS), were added to alumina and sintered at $875^{\circ}C$ for 2 h for low temperature co-firing ceramic (LTCC) applications. As the amount of glass addition increased from 40 wt% to 70 wt%, the apparent density of the sintered product increased from 88.8% to 91.5%, which was also qualitatively confirmed by microstructural observation. When the glass addition was very high, e.g., 70 wt%, an apparent formation of secondary phases such as $CaZn_2AlZnSiAlO_7$, $Ca_2Al(AlSi)O_7$, $Ca_2Al_2SiO_7$, $Ca_2ZnSi_2O_7$ and ZnO, was observed. Both the dielectric constant and the coefficient of thermal expansion increased with the glass addition, which was qualitatively consistent with the analytical models, while the experimental values were lower than the predicted ones due to the presence of pores and secondary phases.

저온소결 기판재료용 Glass/Ceramic 소결체의 제조 및 특성 (Fabrication and Characteristics of Glass/Ceramic Composites for low temperature sintering substrate material)

  • 윤상옥;조태현;김관수;심상흥;박종국
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.185-186
    • /
    • 2005
  • 저온소결 Glass/Ceramic계 기판재료 조성으로 $Al_2O_3$, $SiO_2$, Cordierite, $Al_2O_3{\cdot}3SiO_2$의 4가지 filler에 zinc-borosilicate(ZBS) glass를 첨가하여 기판재료로의 사용가능성을 조사하였다. 4가지 filer에 ZBS glass를 30$\sim$50vol%첨가하여 $700\sim950^{\circ}C$에서 2시간 소결한 결과 40, 50vol%첨가 했을 때 900$^{\circ}C$에서 치밀한 소결체를 얻을 수 있었다. LSI칩 신호라인의 빠른 신호전달에 직접적인 영향을 주는 유전율은 기존의 $Al_2O_3$기관($\fallingdotseq$9.7)보다 저유전율 ($900^{\circ}C$에서 $Al_2O_3$-50vol%ZBS 5.7, $SiO_2$-50vol%ZBS 5.9, Cordierite-40vo1%ZBS 5.9, $Al_2O_3${\cdot}3SiO_2$-50vol%ZBS 4.9)을 나타내어 저온소결 기판재료로 사용이 가능함을 확인하였다.