• Title/Summary/Keyword: Zeolite A/X

Search Result 268, Processing Time 0.028 seconds

Structural Study of Selenium Sorption Complex of Fully Dehydrated, Partially Ca2+-exchanged Zeolite A (완전히 탈수되고 부분적으로 칼슘 이온으로 교환된 제올라이트 A의 셀레늄 수착 화합물의 구조 연구)

  • Kim, Hu Sik;Park, Jong Sam;Lim, Woo Taik
    • Korean Journal of Mineralogy and Petrology
    • /
    • v.33 no.3
    • /
    • pp.251-258
    • /
    • 2020
  • Single crystal of fully dehydrated and partially Ca2+-exchanged zeolites A (|Ca4Na4|[Si12Al12O48]-LTA) was brought into contact with Se in fine pyrex capillary at 523 K for 5 days. Crystal structure of Se-sorbed |Ca4Na4|[Si12Al12O48]-LTA has been determined by single-crystal X-ray diffraction techniques at 294 K in the cubic space group $Pm{\bar{3}}m$ (a = 12.2787(13) Å). The crystal structure of yellow |Ca4Na4Se4|[Si12Al12O48]-LTA has been refined to the final error indices of R1/wR2 = 0.0960/0.3483 with 327 reflections for which Fo > 4s(Fo). In this structure, 4 Na+ and 4 Ca2+ ions fill every 6-ring site: These ions are all found at three crystallographic positions, on 3-fold axes equipoints of opposite 6-rings. Selenium atoms are found at three crystallographically distinct positions: 2 Se atoms per unit cell at Se(1) are located opposite 6-rings in the sodalite cavity (Se(1)-Na(1) = 2.53(5) Å) and 1 at Se(2) opposite 4-rings (Se(2)-O(1) = 2.76(10) Å) and 1 at Se(3) opposite 6-rings in the large cavity (Se(3)-Na(1) = 2.48(5) Å). Two molecular of Se2 (Se(1)-Se(1) = 2.37(7) or 2.90(8) Å and Se(2)-Se(3) = 2.91(5) ) Å) are found in all sodalite cavity and large cavity. Other clusters such as Se4 and Se8 could be existed in large cavity. The inter-selenium distances turned out to be longer that of gases Se2 molecule.

Adsorption of Gaseous Benzene onto Mesoporous Silicates (메조포러스 실리케이트에 의한 기상 벤젠 흡착)

  • Lee, Chae Young;Moon, Nam Gu;Chung, Jin Suk;Shin, Eun Woo
    • Applied Chemistry for Engineering
    • /
    • v.19 no.4
    • /
    • pp.452-456
    • /
    • 2008
  • Mesoporous silicate materials have been used as adsorbents due to the advantage of high specific surface area and regular mesopores. In this study, conventional mesoporous silicates (MCM-41, and SBA-15) were utilized as adsorbents for gaseous benzene, one of volatile organic compounds. In the results of the breakthrough curves of gaseous benzene, SBA-15 showed a higher benzene adsorption capacity in adsorption condition of this study. Especially, compared to benzene adsorption of zeolite X, that of SBA-15 was higher by a factor of 2.7. With increasing adsorption temperature, adsorption capacity for benzene of SBA-15 was decreased rapidly. This indicates that benzene adsorbed weakly on SBA-15.

Site Competition of Ca2+ and Cs+ Ions in the Framework of Zeolite Y (Si/Al = 1.56) and Their Crystallographic Studies (제올라이트 Y (Si/Al = 1.56) 골격 내의 Ca2+과 Cs+ 이온의 자리 경쟁 및 그들의 결정학적 연구)

  • Kim, Hu Sik;Park, Jong Sam;Lim, Woo Taik
    • Journal of the Mineralogical Society of Korea
    • /
    • v.31 no.4
    • /
    • pp.235-248
    • /
    • 2018
  • The present work was performed in order to study the effect of competing cation of $Ca^{2+}$ ion on ion exchange of $Cs^+$ on zeolite Y (Si/Al = 1.56). Three single-crystals of fully dehydrated and partially $Cs^+$-exchanged zeolites Y (Si/Al = 1.56) were prepared by the flow method using mixed ion-exchange solutions. The $CsNO_3:Ca(NO_3)_2$ molar ratios of the ion exchange solution were 1 : 1 (crystal 1), 1 : 100 (crystal 2), and 1 : 250 (crystal 3) with a total concentration of 0.05 M. The single-crystals were then vacuum dehydrated at 723 K and $1{\times}10^{-4}Pa$ for 2 days. The structures of the crystals were determined by single-crystal synchrotron X-ray diffraction technique in the cubic space group $Fd{\bar{3}}m$, at 100(1) K. The unit-cell formulas of crystals 1, 2, and 3 were ${\mid}Cs_{21}Ca_{27}{\mid}[Si_{117}Al_{75}O_{384}]-FAU$, ${\mid}Cs_2Ca_{36.5}{\mid}[Si_{117}Al_{75}O_{384}]-FAU$, and ${\mid}Cs_1Ca_{37}{\mid}[Si_{117}Al_{75}O_{384}]-FAU$, respectively. In all three crystals, the $Ca^{2+}$ ions preferred to occupy site I in the D6Rs, with the remainder occupying sites I', II', and II. On the other hand, the significant differences in the fractional distribution of $Cs^+$ ions are observed depending on the intial $Cs^+$ concentrations in given ion exchange solution. In Crystal 1, $Cs^+$ ion are located at sites II', II, III, and III', and in crystal 2, at sites II, IIIa, and IIIb. In crystal 3, $Cs^+$ ions are only located at sites IIIa and IIIb. The degree of $Cs^+$ ion exchange decreased sharply from 28.0 to 2.7 to 1.3 % as the initial $Ca^{2+}$ concentration increases and the $Cs^+$ content decreases.

Comparative Crystal Chemistry of Exchanged by Cs-, Cd-, Pb-, and Sr-synthetic Mordenite Using High Resolution X-ray Powder Diffraction (고분해능 X-선 분말 회절을 이용한 Cs-, Cd-, Pb-, Sr-으로 치환된 합성 모데나이트의 격자상수 비교 연구)

  • Lee, Soojin;Lee, Hyunseung;Seoung, Donghoon;Kim, Pyosang;Kim, Hyeonsu;Lee, Yongmoon
    • Korean Journal of Mineralogy and Petrology
    • /
    • v.35 no.3
    • /
    • pp.345-353
    • /
    • 2022
  • This study aimed to fundamentally understand changes of cell parameters of cation-exchanged mordenites using high resolution X-ray powder diffraction for studies that immobilization of various heavy metal cation using synthesis mordenite (Na6.6Al6.6Si41.4O96·20.4H2O, Na-MOR). As a results of measurement by Thermogravimetric analysis (TGA), it was confirmed that 19.4, 20.4 water molecules per unit cell were present in monovalent-cation substituted MOR (Cs-MOR, Na-MOR), and 21, 23.1, 23.2 water molecules per unit cell were present in divalent-cation substituted MOR (Pb-MOR, Sr-MOR, Cd-MOR). The space group of all the samples were identified as Cmcm belonging to the orthorhombic crystal system. Compared to Na-MOR, starting material, relative peak intensity of (110) and (200) is significantly changed after cation substitution whereas peak position is almost similar. Also, (220) peak that was not found in Na-MOR was clearly observed in Pb-, Cd- and Sr-exchanged MOR. Thus, it was estimated that changes of atomic distribution usually occurred on ab-plane while changes of cell parameters were little. Detailed changes in the cell parameters of cation-exchanged mordenites were derived from whole profile fitting method using the GSAS suite program. Changes in the axial lengths and unit cell volume of cation substitution showed different relationship depending on ionic radius and charge number. In case of monovalent-cation substituted MOR, the length of a-axis increases whereas the length of b- and c-axis decrease by absorbed cation radius. In the case of divalent-cation exchanged MOR, the length of a-axis usually decreases while the length of b- and c-axis increases by cation radius. It was confirmed that unit cell volume of monovalent and divalent cation substituted MORs had an independent tendency by cation radius.

Crystal Structures of Dehydrated Partially $Sr^{2+}$-Exchanged Zeolite X, $Sr_{31}K_{30}Si_{100}A1_{92}O_{384}\;and\;Sr_{8.5}TI_{75}Si_{100}AI_{92}O_{384}$ (부분적으로 스트론튬이온으로 교환되고 탈수된, 제올라이트 X의 결정구조)

  • Kim Mi Jung;Kim Yang;Seff Karl
    • Korean Journal of Crystallography
    • /
    • v.8 no.1
    • /
    • pp.6-14
    • /
    • 1997
  • The crystal structures of $Sr_{31}K_{30}-X\;(Sr_{31}K_{30}Si_{100}A1_{92}O_{384};\;a=25.169(5) {\AA}$) and $Sr_{8.5}Tl_{75}-X (Sr_{8.5}Tl_{75}Si_{100}A1_{92}O_{384};\;a=25.041(5) {\AA}$) have been determined by single-crystal X-ray diffraction techniques in the cubic space group $\=F{d3}\;at\;21(1)^{\circ}C$. Each crystal was prepared by ion exchange in a flowing stream of aqueous $Sr(ClO_4)_2\;and\;(K\;or\;T1)NO_3$ whose mole ratio was 1 : 5 for five days. Vacuum dehydration was done at $360^{\circ}C$ for 2d. Their structures were refined to the final error indices $R_1=0.072\;and\;R_w=0.057$ with 293 reflections, and $R_1= 0.058\;and\;R_w=0.044$ with 351 reflections, for which $I>2{\sigma}(I)$, respectively. In dehydrated $Sr_{31}K_{30}-X,\;all\;Sr^{2+}$ ions and $K^+$ ions are located at five different crystallographic sites. Six-teen $Sr^{2+}$ ions per unit cell are at the centers of the double six-rings (site I), filling that position. The remaining 15 $Sr^{2+}$ ions and 17 $K^+$ ions fill site II in the supercage. These $Sr^{2+}$ and $K^+$ ions are recessed ca $0.45{\AA}\;and\;1.06{\AA}$ into the supercage, respectively, from the plane of three oxygens to which each is bound. ($Sr-O=2.45(1){\AA}\;and\;K-O=2.64(1){\AA}$) Eight $K^+$ ons occupy site III'($K-O=3.09(7){\AA}\;and\;3.11(10){\AA}$) and the remaining five $K^+$ ions occupy another site III'($K-O=2.88(7){\AA}\;and\;2.76(7){\AA}$). In $Sr_{8.5}Tl_{75}-X,\;Sr^{2+}\;and\;Tl^+$ ions also occupy five different crystallographic sites. About 8.5 $Sr^{2+}$ ions are at site I. Fifteen $Tl^+$ ions are at site I' in the sodalite cavities on threefold axes opposite double six-rings: each is $1.68{\AA}$ from the plane of its three oxygens ($T1-O=2.70(2){\AA}$). Together these fill the double six-rings. Another 32 $Tl^+$ ions fill site II opposite single six-rings in the supercage, each being $1.48{\AA}$ from the plane of three oxygens ($T1-O=2.70(1){\AA}$). About 18 $Tl^+$ ions occupy site III in the supercage ($T1-O=2.86(2){\AA}$), and the remaining 10 are found at site III' in the supercage ($T1-O=2.96(4){\AA}$).

  • PDF

Study on the Fuel Decomposition Characteristics and Coke Formation by Type of Endothermic Fuel and Method of Catalyst Molding (흡열연료 종류와 촉매 성형 방법에 따른 분해특성과 코크 생성에 관한 연구)

  • Lee, Tae Ho;Kang, Saetbyeol;Kim, Sung Hyun
    • Korean Chemical Engineering Research
    • /
    • v.57 no.5
    • /
    • pp.611-619
    • /
    • 2019
  • This study was carried out to investigate fuel decomposition characteristics and coke formation according to types of endothermic fuels and methods of catalyst molding. Methylcyclohexane (MCH), n-dodecane, and exo-tetrahydrodipentadiene (exo-THDCP) were used as the endothermic fuels. As a catalyst, USY720 supported with platinum was used. It was manufactured by only using pressure to disk-type, or pelletized with a binder and a silica solution. The characteristics of the catalysts according to the molding method were analyzed by X-ray diffraction analysis, scanning electron microscopy, nitrogen adsorption-desorption isotherm, and ammonia temperature programmed desorption analysis. The reaction was carried out under conditions of high temperature and high pressure ($500^{\circ}C$, 50 bar) in which the fuel could exist in a supercritical state. The product was analyzed by gas chromatograph/mass spectrometer and the coke produced by the catalyst was analyzed by thermogravimetric analyzer. After the reaction, the composition of the products varied greatly depending on the structure of the fuel. In addition, the crystallinity and surface properties of the catalysts were not changed by the method of catalyst molding, but the changes of the acid sites and the pore characteristics were observed, which resulted in changes in the amount and composition of products and coke.

Synthesis and Structural Characterization of Benzene-sorbed Cd2+-Y(FAU) Zeolite (벤젠이 흡착된 Cd2+-Y(FAU) 제올라이트의 합성 및 구조연구)

  • Moon, Dae Jun;Suh, Jeong-Min;Park, Jong Sam;Choi, Sik Young;Lim, Woo Taik
    • Journal of the Mineralogical Society of Korea
    • /
    • v.30 no.2
    • /
    • pp.45-57
    • /
    • 2017
  • Two single crystals of fully dehydrated $Cd^{2+}$-exchanged zeolites Y were prepared by the exchange of ${\mid}Na_{75}{\mid}[Si_{117}Al_{75}O_{384}]-FAU$ ($Na_{75}-Y$, Si/Al = 1.56) with aqueous $0.05M\;Cd(NO_3)_2$ (pH = 3.65) at 294 K, followed by vacuum dehydration at 723 K (crystal 1) and a second crystal, similarly prepared, was exposed to zeolitically dried benzene for 72 hours at 294 K and evacuated (crystal 2). Their structures were determined crystallographically using synchrotron X-rays and were refined to the final error indices using $F_o$>$4{\sigma}(F_o)$ of $R_1/wR_2=0.040/0.121$ and 0.052/0.168, respectively. In crystal $1({\mid}Cd_{36}H_3{\mid}[Si_{117}Al_{75}O_{384}]-FAU)$, $Cd^{2+}$ ions primarily occupy sites I and II, with additional $Cd^{2+}$ ions at sites I', II', and a second site II. In crystal $2({\mid}Cd_{35}(C_6H_6)_{24}H_5{\mid}[Si_{117}Al_{75}O_{384}]-FAU)$, $Cd^{2+}$ ions occupy five crystallographic sites. The 24 benzene molecules are found at two distinct positions within the supercages. The 17 benzene molecules are found on the 3-fold axes in the supercages where each interacts facially with one of site IIa $Cd^{2+}$ ions. The remaining 7 benzene molecules lie on the planes of the 12-rings where each is stabilized by multiple weak electrostatic and van der Waals interactions with framework oxygens.

Synthesis of Single Crystalline Analcime and Its Single-crystal Structure, |Na0.94(H2O)|[Si2.06Al0.94O6]-ANA: Determination of Cation Sites, Water Positions, and Si/Al Ratios (결정성 아날심(|Na0.94(H2O)|[Si2.06Al0.94O6]-ANA)의 합성 및 단결정구조: 양이온 및 물 분자의 위치, Si/Al 비의 결정)

  • Seo, Sung-Man;Suh, Jeong-Min;Ko, Seong-Oon;Lim, Woo-Taik
    • Journal of the Korean Chemical Society
    • /
    • v.55 no.4
    • /
    • pp.570-574
    • /
    • 2011
  • Large colorless single crystals of analcime with diameters up to 0.20 mm have been synthesized from gels with the composition of $3.00SiO_2$ : $1.50NaAlO_2$ : 8.02NaOH : $454H_2O$ : 5.00TEA. The fully $Na^+$-exchanged analcime have been prepared with aqueous 0.1 M NaCl (pH adjusted from 6 to 11 by dropwise addition of NaOH). The single-crystal structure of hydrated $|Na_{0.94}(H_2O)|[Si_{2.06}Al_{0.94}O_6]$-ANA per unit cell, a=13.703(3) ${\AA}$, has been determined by single-crystal X-ray diffraction technique in the orthorhombic space group Ibca at 294 K. The structure was refined using all intenties to the final error indices (using only the 1,446 reflections for which $F_o$ > $4{\sigma}(F_o))R_1/wR_2$ = 0.054/0.143. About 15 $Na^+$ ions are located at three nonequivalent positions and octahedrally coordinated. The chemical composition is $Na_{0.94}(H_2O)Si_{2.06}Al_{0.94}O_6$. The Si/Al ratio of synthetic analcime is 2.19 determined by the occupations of cations, 14.79, in the single-crystal determination work.

Quality Characteristics of Cherry Tomato and Unshiu Orange Packaged with Box Incorporated with Antimicrobial Agents (항균소재 함유 박스로 포장한 방울토마토와 밀감의 저장중 품질 특성)

  • Park Woo-Po;Kim Chul-Hwan;Cho Sung-Hwan
    • Food Science and Preservation
    • /
    • v.13 no.3
    • /
    • pp.273-278
    • /
    • 2006
  • In order to help the preservation of the cherry tomato and unshiu orange, antimicrobial paper incorporating grapefruit seed extract and zeolite was applied to the package. Cherry tomato and unshiu orange were packed in a box (38x25x20 cm) attached with antimicrobial paper and then stored respectively at $5^{\circ}C$. During the storage, weight loss, pH total acidity, soluble solid content microbial load and decay ratio were measured as quality indices. pH increase in cherry tomato was observed until 20 days, and decreased with litle difference between the packaging treatments thereafter pH and total acidity decrease in unshiu orange were shown till 30 days, and abrupt change was revealed by 40 days. This was due to physiological disorders. The microbial loads of total aerobic bacteria, and yeast/mold count were suppressed during storage by the box packaging incorporated with antimicrobial agents, which also contributed to reducing the decayed cherry tomato and unshiu orange. Antimicrobial paper was useful fur the reduction of microbial load in cherry tomato and unshiu orange pear without other quality deterioration.

Mineralogical Properties and Paragenesis of H-smectite (H-스멕타이트의 광물학적 특성과 생성관계)

  • Noh, Jin-Hwan;Hong, Jin-Sung
    • Journal of the Mineralogical Society of Korea
    • /
    • v.23 no.4
    • /
    • pp.377-393
    • /
    • 2010
  • Pumiceous tuffs occurring in the Beomgockri Group are examined applied-mineralogical characteristics and their controling factors to evaluate their potentials as the adsorption-functional mineral resources. The pumiceous tuffs are diagenetically altered to low-grade zeolitcs and bentonites in the Janggi area. Compositional specialty due to the presence of pumice fragments induces the altered tuffs to exhibit the characteristic adsorption property combined with cation exchange capacity, specific surface area, and acidic pH. Unusual lower pH in the adsorption-functional mineral substances is turned out to be originated from the presence of H-smectite having $H^+$ in the interlayer site of the sheet structure. On account of disordered crystallinity resulting from the exchanged $H^+$ in the interlayer site, the smectite commonly forms crenulated edges in the planar crystal form and exhibits characteristic X-ray diffraction patterns showing comparatively lower intensities of basal spacings including (001) peak than conventional Ca-smectite. Based on the interpretation of paragenetic relations and precursor of the H-smectite, a genetic model of the peculiar clay mineral was proposed. The smectite formation may be facilitated resulting from the precipitation of opal-CT at decreasing pH condition caused by the release of H+ during diagenetic alteration of pumice fragments. Because of the acidic smectite, the low-grade mineral resources from the Beomgockri Group may be applicable to the adsorption industry as the raw materials of acid clays and bed-soil.