Microwave Sol-Gel Derived NaGd(MoO4)2:Ho3+/Yb3+ Phosphors and Their Upconversion Photoluminescence Properties

  • Lim, Chang Sung
    • Transactions on Electrical and Electronic Materials
    • /
    • v.18 no.6
    • /
    • pp.364-369
    • /
    • 2017
  • Double molybdate $NaGd_{1-x}(MoO_4)_2:Ho^{3+}/Yb^{3+}$ phosphors with proper doping concentrations of $Ho^{3+}$ and $Yb^{3+}$ ($x=Ho^{3+}+Yb^{3+}$, $Ho^{3+}=0$ and 0.05, and $Yb^{3+}=0$, 0.35, 0.40, 0.45, and 0.50) were successfully synthesized using the microwave sol-gel method. Well-crystallized particles formed after heat-treatment at $800^{\circ}C$ for 16 h showed fine and homogeneous morphologies with particle sizes of $1{\sim}3{\mu}m$. The spectroscopic properties were examined using photoluminescence emission and Raman spectroscopy. Under excitation at 980 nm, the upconversion doped samples exhibited strong yellow emissions, from the combination of strong emission bands at 545 nm and 655 nm in the green and red spectral regions, respectively. The strong 545 nm emission band in the green region corresponded to the $^5S_2/^5F_4{\rightarrow}^5I_8$ transition in the $Ho^{3+}$ ions, while the strong 655 nm band in the red region appeared because of the $^5F_5{\rightarrow}^5I_8$ transition in the $Ho^{3+}$ ions. The pump power dependence and the Commission Internationale de L'Eclairage chromaticity of the upconversion emission intensity were evaluated in detail.

Luminescent Properties and Anti-Counterfeiting Applications of SrWO4:RE3+ (RE=Dy, Sm, Dy/Sm) Phosphors Doped with Several Activator Ions (다양한 활성제 이온이 도핑된 SrWO4:RE3+ (RE=Dy, Sm, Dy/Sm) 형광체의 특성과 위조 방지 응용)

  • Yoon, Soohwan;Cho, Shinho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.33 no.5
    • /
    • pp.393-399
    • /
    • 2020
  • A series of phosphors, SrWO4:5 mol% Dy3+, SrWO4:5 mol% Sm3+, and SrWO4:5 mol% Dy3+:x Sm3+ (x=1~15 mol%), were prepared using a facile co-precipitation. The crystal structure, morphology, photoluminescence properties, and application in anti-counterfeiting fields were investigated. The crystalline structures of the prepared phosphors were found to be tetragonal systems with the dominant peak occurring at the (112) plane. The excitation spectra of the Dy3+ singly-doped SrWO4 phosphors were composed of an intense charge-transfer band centered at 246 nm in the range of 210~270 nm and two weak peaks at 351 nm and 387 nm due to the 6H15/26P7/2 and 6H15/24I13/2 transitions of Dy3+ ions, respectively. The wavelength of 246 nm was optimum for exciting the luminescence of Dy3+ and Sm3+ co-doped SrWO4 phosphors. The emission spectra consisted of two intense blue and yellow emission bands at 480 nm and 573 nm corresponding to the 4F9/26H15/2 and 4F9/26H13/2 transitions of Dy3+, and two strong emission peaks at 599 nm and 643 nm originating from the 4G5/26H7/2 and 4G5/26H9/2 transitions of Sm3+, respectively. As the concentration of Sm3+ ions increased, the emission intensities of Dy3+ rapidly decreased, while the emission intensities of Sm3+ gradually increased. These results suggest that the color of the emission light can be tuned from yellow to white by changing the concentration of Sm3+ ions at a fixed 5 mol% Dy3+. Furthermore, the fluorescent security inks were synthesized for use in anti-counterfeiting applications.

Optical Properties of MgMoO4:Dy3+,Eu3+ Phosphors Prepared with Different Eu3+ Molar Ratios (Eu3+ 이온의 몰 비 변화에 따른 MgMoO4:Dy3+,Eu3+ 형광체의 광학 특성)

  • Kim, Jung Dae;Cho, Shinho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.29 no.3
    • /
    • pp.186-191
    • /
    • 2016
  • The effects of $Eu^{3+}$ doping on the structural, morphological, and optical properties of $MgMoO_4:Dy^{3+},Eu^{3+}$ phosphors prepared by solid-state reaction technique were investigated. XRD patterns exhibited that all the synthesized phosphors showed a monoclinic system with a dominant (220) diffraction peak, irrespective of the content of $Eu^{3+}$ ions. The surface morphology of $MgMoO_4:Dy^{3+},Eu^{3+}$ phosphors was studied using scanning electron microscopy and the grains showed a tendency to agglomerate as the content of $Eu^{3+}$ ions increased. The excitation spectra of the phosphor powders were composed of a strong charge transfer band centered at 294 nm in the range of 230~340 nm and two intense peaks at 354 and 389 nm, respectively, arising from the $^6H_{15/2}{\rightarrow}^6P_{7/2}$ and $^6H_{15/2}{\rightarrow}^4M_{21/2}$ transitions of $Dy^{3+}$ ions. The emission spectra of the $Mg_{0.85}MoO_4$:10 mol% $Dy^{3+}$ phosphors without incorporating $Eu^{3+}$ ions revealed a strong yellow band centered at 573 nm resulting from the $^4F_{9/2}{\rightarrow}^6H_{13/2}$ transition of $Dy^{3+}$. As the content of $Eu^{3+}$ was increased, the intensity of the yellow emission was gradually decreased, while that of red emission band located at 614 nm began to appear, approached a maximum value at 10 mol%, and then decreased at 15 mol% of $Eu^{3+}$. These results indicated that white light emission could be achieved by controlling the contents of the $Dy^{3+}$ and $Eu^{3+}$ ions incorporated into the $MgMoO_4$ host crystal.

Influence of Fluxing Agents in Sr3SiO5:Eu2+ Phosphors for Fabrication of Warm White Light Emitting Diodes (따뜻한 백색 LED의 제조를 위한 Sr3SiO5:Eu2+ 형광체에서의 융제 첨가 영향)

  • Kim, Hyun-Ho;Chung, Kang-Sup;Lee, Seoung-Won;Kim, Byoung-Gyu
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.1
    • /
    • pp.105-110
    • /
    • 2012
  • In this paper, a yellow phosphor $Sr_3SiO_5:Eu^{2+}$ that emits efficiently at the 450 nm excitation for warm white LED is studied. In addition, the effects of various flux $BaF_2$, $NH_4Cl$ on the emission spectra were investigated. The samples were synthesized through conventional solid state reaction under reducing atmosphere of 95% $N_2$-5% $H_2$ mixture at the high temperature. All phosphors showed a excitation band from 450 nm and broad band emission peaking at region of 580 nm. The optimal concentration of $BaF_2$ flux is 3 wt% for $Sr_3SiO_5$ with doping 0.05mol Eu phosphors fired in a reductive atmosphere. The phosphor showed highest emission peaking at 582 nm.

White Electroluminescent Device by ZnS: Mn, Cu, Cl Phosphors

  • Kim, Jong-Su;Park, Je-Hong;Lee, Sung-Hun;Kim, Gwang-Chul;Kwon, Ae-Kyung;Park, Hong-Lee
    • Journal of the Semiconductor & Display Technology
    • /
    • v.5 no.3 s.16
    • /
    • pp.1-4
    • /
    • 2006
  • White-light-emitting ZnS:Mn, Cu, Cl phosphors with spherical shape and the size of $20\;{\mu}m$ are successfully synthesized. They have the double phases of cubic and hexagonal structures. They are applied to electroluminescent (EL) devices by silk screen method with the following structure: $electrode/BaTiO_3$ insulator layer ($50{\sim}60\;{\mu}m$)/ ZnS:Mn, Cu, Cl phosphor layer ($30{\sim}50\;{\mu}m$)/ITO glass. The EL devices are driven with the voltage of 100 V and the frequency of 400 Hz. The EL devices show the three emission peaks. The blue and green emission bands are originated from $CICu^{2+}$ transition and $ClCu^+$ transition, respectively. The yellow emission band results from $^4T^6A$ transition of $Mn^{2+}$ ion. As an increase of Cu concentrations, the blue and green emission intensities decrease whereas the yellow emission intensity increases; the quality becomes warm white. It is due to the energy transfer from the blue and green bands to the yellow band.

  • PDF

Spectral Properties of Various $Y_3Al_5O_{12}:Ce^{3+}$ Nanocrystalline Phosphors for the Application of White LEDs

  • Yang, Hee-Sun;Jeon, Mi-Jung;Huh, Young-Duk
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2007.08b
    • /
    • pp.1593-1596
    • /
    • 2007
  • Various yellow-emitting $Y_3Al_5O_{12}:Ce^{3+}$ (YAG:Ce) nanocrystalline phosphors, where some $Al^{3+}$ sites are substituted with $Ga^{3+}$ or some Y sites with Gd3+, have been synthesized. The rare earth ions such as $Pr^{3+}$ and $Tb^{3+}$ were also co-doped into YAG:Ce system, leading to the tunability of CIE coordinates of emission.

  • PDF

Inorganic phosphors for LED applications

  • Winkler, Holger;Barnekow, Peter;Benker, Andreas;Petry, Ralf;Tews, Stefan;Vosgroene, Tim
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2009.10a
    • /
    • pp.56-59
    • /
    • 2009
  • In the nineties the invention of the InGaN blue LED has innovated illumination technology. Currently LCD backlighting and more and more general lighting applications are based on white LEDs comprising of inorganic phosphors and blue emitting InGaN chip. Well established phosphor materials are ortho silicates and garnets like yellow emitting YAG:Ce. In our paper we demonstrate that garnet materials also allow for green light emission for both, general lighting and backlighting LED applications.

  • PDF

Synthesis and luminescent properties of $Sr_2SiO_4:Eu^{2+}$ phosphors ($Sr_2SiO_4:Eu^{2+}$ 형광체의 합성 및 발광특성)

  • Kim, Jong-Min;Park, Yong-Seo;Choi, Hyung-Wook
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.06a
    • /
    • pp.430-431
    • /
    • 2009
  • In this study, europium doped strontium silicate ($Sr_2SiO_4:Eu^{2+}$) phosphor has been synthesized by conventional solid-state method and investigated luminescent characteristic. $SrCO_3$ and $SiO_2$ were mixed together by 2:1 mole ratio. Also $NH_4Cl$ was added as a flux. The mixture were sintered at $800^{\circ}C$, $1000^{\circ}C$ for 3h under the atmosphere (5% $H_2$/95% $N_2$). This phosphor can be applicated to the yellow phosphor for white LED because it has yellow emission band (540nm), which emits efficiently under the 370nm excitaion energy.

  • PDF

Synthesis and Properties of Ca8Gd2(PO4)6O2 Nano-Crystalline Structures

  • Bharat, L. Krishna;Yu, Jae Su
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.08a
    • /
    • pp.286.1-286.1
    • /
    • 2013
  • Nowadays, the glare towards the light-emitting diode (LED) lighting source has much attention due to its eco-friendly nature, reduced energy consumption, and low CO2 emission. LEDs can show versatile colors by changing the composition ratio of semiconductors. Phosphors re-emit light by absorbing light from LED, which is the key factor for emission. The endeavor to make replica of natural white light is increasing day by day. Industrially, blue LED chip crowned with a yellow phosphor coated lens gives low quality white light. Newly, many researchers are introducing modern approaches, adding red phosphor to the yellow phosphor to increase the quality of white light. Here, we synthesized structurally and chemically stable europium doped oxyapatite Ca8Gd2(PO4)6O2 nano-crystalline structures by a hydrothermal method. The ultrafine structures were formed due to the effect of ethylenediaminetetraacetic acid, which is confirmed by the transmission electron microscope images. The structural properties were analyzed using the X-ray diffraction patterns.

  • PDF

Color Tuning of a Mn4+ Doped Phosphor : Sr1-xBaxGe4O9:MnMn4+0.005 (0.00 ≤ x ≤ 1.00) (Mn4+ 도핑된 형광체, Sr1-xBaxGe4O9:MnMn4+0.005 (0.00 ≤ x ≤ 1.00)의 Color Tuning)

  • Park, Woon Bae
    • Journal of the Korean Chemical Society
    • /
    • v.61 no.4
    • /
    • pp.163-167
    • /
    • 2017
  • Along with the progress of white LED technology, red phosphors have become increasingly important in industry and academia, and a more specific demand has steadily increased in the market. Red phosphors are used in high efficiency and high rendering LED lightings. However, using red phosphors with $Eu^{2+}$ activators caused color rewarming and reduced emission intensity in white LED chips due to strong reabsorption in the green or yellow wavelength range caused by the 4f-5d transition. $Mn^{4+}$ doped phosphors which have no such drawbacks and which can further improve the color rendering index (CRI) are now of great interest. However, $Mn^{4+}$-doped phosphors have a disadvantage in that the emission wavelength is determined depending on the host due to the $^2E_g{\rightarrow}^4A_2$ transition. In this study, the $SrO-BaO-GeO_2$ solid-solution was selected, and $Sr_{1-x}B_axGe_4O_9:Mn^{4+}{_{0.005}}$ ($0{\leq}x{\leq}1$) phosphors were synthesized and characterized. This led to a versatile color tuning in LED technology.