• 제목/요약/키워드: X-Ray diffraction measurement

검색결과 519건 처리시간 0.025초

염료 감응형 태양전지에서 Mesoproso $TiO_2$/FTO 사이에 완충층으로써의 PLD로 증착한 $TiO_2$ 박막에 관한 연구 (A Study on $TiO_2$ Thin Film by PLD for Buffer Layer between Mesoproso $TiO_2$ and FTO of Dye-sensitized Solar Cell)

  • 송상우;김성수;노지형;이경주;문병무;김현주
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.424-424
    • /
    • 2008
  • Dye-sensitized Solar Cell (DSC) is a new type of solar cell by using photocatalytic properties of $TiO_2$. The electric potential distribution in DSCs has played a major role in the operation of such cells. Models based on a built-in electric field which sets the upper limit for the open circuit voltage(Voc) and/or the possibility of a Schottky barrier at the interface between the mesoporous wide band gap semiconductor and the transparent conducting substrate have been presented. $TiO_2$ thin films were deposited on the FTO substrate by Nd:YAG Pulsed Laser Deposition(PLD) at room temperature and post-deposition annealing at $500^{\circ}C$ in flowing $O_2$ atmosphere for 1 hour. The structural properties of $TiO_2$ thin films have investigated by X-ray diffraction(XRD) and atomic force microscope(AFM). Thickness of $TiO_2$ thin films were controlled deference deposition time and measurement by scanning electron microscope(SEM). Then we manufactured a DSC unit cells and I-V and efficiency were tested using solar simulator.

  • PDF

기계적 합금화법에 의해 제조된 Al+Al3Ti합금 및 Al+10wt.%Ti합금의 고용현상 (Solid Solution Phenomena of Al+Al3Ti Alloy and Al+10wt.%Ti Alloy using Mechanical Alloying Process)

  • 김혜성;이정일;김긍호;금동화;서동수
    • 열처리공학회지
    • /
    • 제9권2호
    • /
    • pp.121-129
    • /
    • 1996
  • The solubility of Ti in Al matrix was determined by X-ray diffraction method on two different mechanical alloying systems, i.e Al+$Al_3Ti$ and Al+Ti alloys. Starting powder compositions of two systems were chosen for final volume fraction of $Al_3Ti$ phase being 25%. The solubility of Ti in ${\alpha}$-Al was estimated by the lattice parameter measurement of Al. For Al+$Al_3Ti$ mixture, it appeared that some of $Al_3Ti$ particles decomposed during milling and maximum solubility of Ti in Al was about 0.99%. The majority of $Al_3Ti$ particles were dispersed uniformly in Al matrix, having approximate size of 100~200 nm. On the other hand, higher Ti solubility of 1.24 wt.% was found in Al+Ti system, with starting composition of Al+10 wt.%Ti. After 15 hours of milling, Ti phase was identified as 20 nm sized particles embedded in Al matrix. The annealing of mechanically alloyed powders from Al+$Al_3Ti$ and Al+10 wt.%Ti systems was followed in the temperature range of 200 to $600^{\circ}C$ to study thermal stability of supersaturated solution of Al(Ti). After annealing, the lattice parameter of Al reverted back to that of pure Al, and the peak intensity ratio of $Al_3Ti$/Al was increased more than the original value before annealing. These results suggest that Ti dissolve into alpha-Al solutions during milling, and by annealing, $Do_{22}-Al_3Ti$ phase forms from Al(Ti) solution.

  • PDF

인쇄회로기판 용 Epoxy/BaTiO$_3$내장형 커패시터 필름에 관한 연구 (Study on the Epoxy/BaTiO$_3$Embedded Capacitor Films for PWB Applications)

  • 조성동;이주연;백경욱
    • 마이크로전자및패키징학회지
    • /
    • 제8권4호
    • /
    • pp.59-65
    • /
    • 2001
  • 경화 전 상온 보관성이 우수하며 넓은 면적에 균일한 두께와 균일한 유전특성의 커패시터를 쉽게 형성할 수 있는 epoxy/$BaTiO_3$composite커패시터 필름을 제조하였다. 이 필름은 필름 형성특성과 가공성, 그리고 상온 보관성이 우수한 에폭시계 이방성 전도 필름(Anisotropic Conductive Film: ACF)용으로 개발된 레진을 기본으로 하고, 유전상수를 높이기 위한 충진제로 2종류의 $BaTiO_3$분말을 사용하였다. X선 회절을 통하여 두 분말의 결정구조와 이에 따른 유전상수의 변화를 살펴보았으며, 점포 측정을 통해 분산제의 양을 정하였다. 필름의 경화온도와 적정한 경화제의 양을 결정해주기 위해 differential scanning calorimeter (DSC)와 커패시터의 특성 분석을 통해 경화제 양에 따른 필름 및 커패시터 특성에 미치는 영향을 살펴보았다. 이 필름을 이용하여 두께 7 $\mu\textrm{m}$에서 10 nF/$\textrm{cm}^2$ (이때의 유전상수는 80)의 높은 전기용량을 가진 우수한 커패시터를 성공적으로 제작하였다.

  • PDF

Li2O.Al2O3.2SiO2의 조성을 갖는 유리에서 $\beta$-eucryptite의 핵생성 및 결정성장 (Nucleation and Crystal Growth of $\beta$-eucryptite in a Glass of the Molecular Composition Li2O.Al2O3.2SiO2)

  • 이상현;장수진
    • 한국세라믹학회지
    • /
    • 제22권3호
    • /
    • pp.53-59
    • /
    • 1985
  • Nucleation and crystallization of $\beta$-eucryptite in a glass of molecular percentage composition Li2O.Al2O3.2SiO2 are studied. The glasses are made by quenching of the melts from 143$0^{\circ}C$ to room temperature. Heat-treatment for nucleation and crystal growth are caried out at various temperature in the range between 50$0^{\circ}C$ and 80$0^{\circ}C$ with different duration of time. The amounts of crystallization are estimated by the method of x-ray powder diffraction. As the results a time-temperature-transformation relation for crystallization is derived. The maximum rate of crystallization is observed at about 75$0^{\circ}C$ from the T-T-T-curve while the crystallization temperature is detected at 67$0^{\circ}C$ by DTA measurement. The crystallization temperature moved to 62$0^{\circ}C$ by adding 5 weight percents of TiO2 and it moved to 78$0^{\circ}C$ by adding 2 weight percents of V2O5. The crystallization temperature moved to 62$0^{\circ}C$ by adding 5 weight percent of TiO2 it moved to 78$0^{\circ}C$ by adding 2 weight percents of V2O5 The activation energy for crystallization from the pure glass is calculated as 68 Kcal/mol and it varied to 53 Kcal/mol and 110Kcal/mol when 5 weight percents of TiO2 and weight percents of V2O5 are added respectively.

  • PDF

SnO2-TiO2-V2O5계의 노랑안료 합성 (Synthesis of SnO2-TiO2-V2O5 System Yellow Pigment)

  • 주인돈;황동하;이현수;박주석;이병하
    • 한국세라믹학회지
    • /
    • 제46권6호
    • /
    • pp.639-642
    • /
    • 2009
  • The research was performed to find out the optimum firing condition for the $SnO_2-TiO_2-V_2O_5$ system yellow pigment. The pigment based on $SnO_2-V_2O_5$ system showed very intense yellow color and it was used widely in ceramics industry. Synthesized pigment, with partial substitutions of $SnO_2\;by\;TiO_2$, was fired at $1300{^{\circ}C}$ soaking 1h and it showed bright yellow color. $SnO_2-TiO_2-V_2O_5$ system was very more intensive changes in yellow color by colorimetric value $b^*$ than $SnO_2-V_2O_5$ system. Synthesized yellow pigments were characterized by X-ray diffraction (XRD), FT-IR, and UV-vis spectroscopy. The best composition for yellow pigment was 93:7:0.5(mole%) for $SnO_2-V_2O_5-TiO_2$. The measurement of CIE $L^*a^*b^*$ of pigment was $L^*(78.82),\;a^*(-4.88)\;and\;b^*$(59.25).

팔라듐-은 합금 도재소부전장 가공의치의 잔류응력과 변형에 관한 연구 (A STUDY FOR THE MEASUREMENTS OF THE RESIDUAL STRESS AND THE DISTORTIONS IN THE CERAMO-METAL BRIDGE OF Pd-Ag ALLOY)

  • 전영찬;이호용
    • 대한치과보철학회지
    • /
    • 제27권2호
    • /
    • pp.53-78
    • /
    • 1989
  • This study was taken to observe the changes of the residual stress in the alloy and to measure 3 dimensional distortions of the long span ceramo-metal bridge. The materials used in this study were Pors-on 4 (Pd-Ag alloy), and Ceramco and Vita VMK 68 powders. The residual stress of the alloy was measured on the six specimens (dia. 8m/m) by the X-ray diffraction stress analyzer according to the kind of ceramic powder and different measuring stages. And, for the measurement of the distortions, fifteen specimens of the anterior 8-unit ceramo-metal brige were fabricated and subjected to the 3-D coordinate measuring machine. Variables included the 2 kinds of a ceramic powder and the presence or absence of a splint bar at the cast metal framework. The measuring stages in both were after casting, after degassing and after glazing. The following conclusions were obtained : 1. The residual stress of the alloy showed increasing tendency for the tension by the ceramic fusing, but there was not significance. 2. The tendency of the distortions in the cast metal frameworks were decrease of the width, the anterior displacement and sagging. 3. The amount of the distortions at the degassing stage were greater than that at the ceramic fusing stage. 4. The splint bar was effective to control the distortion only at ceramic fusing stage. 5. The sagging distortion in the Ceramco firing were even through all measuring stages, but in the Vita firing, pronounced at degassing stage.

  • PDF

Growth of zinc oxide thin films by oxygen plasma-assisted pulsed laser deposition

  • Pak, Sang-Woo;Suh, Joo-Young;Lee, Dong-Uk;Kim, Eun-Kyu
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2010년도 제39회 하계학술대회 초록집
    • /
    • pp.208-208
    • /
    • 2010
  • Zinc oxide (ZnO) is a functional material with interesting optical and electrical properties, a wide band gap (more than 3.3 eV), a high transmittance in the visible light region, piezoelectric properties, and a high n-type conductivity. This material has been investigated for use in many applications, such as transparent electrodes, blue light-emitting diodes, and ultra-violet detector. ZnO films grown under low oxygen pressure by thin film deposition methods show low resistivity and large free electron concentration. Therefore, reducing the background carrier concentration in ZnO films is one of the major challenges ahead of realizing high-performance ZnO-based optoelectronic devices. In this study, we deposited ZnO thin films on sapphire substrates by pulsed laser deposition (PLD) with employing an oxygen plasma source to decrease the background free-electron concentration and enhance the crystalline quality. Then, the substrate temperature was varied between 200 'C to 900 'C The vacuum chamber was initially evacuated to a pressure of $10^{-6}$ Torr, and then a pure $O_2$ gas was introduced into the chamber and the pressure during deposition was maintained at $10^{-2}$ Torr. Crystallinity and orientation of ZnO films were investigated by X-ray diffraction (XRD). The film surface was analyzed with atomic force microscope (AFM). And electrical properties were measured at room temperature by Hall measurement.

  • PDF

키토산/Bombyx mori 견 피브로인 블렌드 필름의 구조와 특성 (Structure and Characteristic of Chitosan/Bombyx mori Silk Fibroin Blend Filems)

  • 김동건;김홍성
    • 폴리머
    • /
    • 제29권4호
    • /
    • pp.408-412
    • /
    • 2005
  • 생체재료로 이용하기 위하여 키토산을 기질로 하여 Bembyx mori로부터 추출한 견 피브로인을 블렌드한 필름에 대한 구조와 특성을 X선 회절분석, 열분석, 적외선 분광분석, 전자현미경 관찰, 접촉각 측정, 흡수율 측정으로 조사하였다. $-\~30wt\%$ 피브로인을 포함하는 블렌드 필름은 리튬이온을 포함하는 초산수용액으로 제조되었다. 키토산/피브로인 블렌드 필름은 키토산의 아미노기와 피브로인의 아미드 카보닐기 사이의 수소결합과 같은 분자간 상호작용의 형성에 의해 결정성이 감소되었다. 피브로인의 비율이 증가할수록 키토산의 무수혈 견정상은 소실되었고, 수화형 결정상은 감소되었으며, 퍼브로인의 P형 결정이 형성되어 혼재된 결정구조를 이루었다. 표면 친수성과 수분 흡수성은 피브로인의 비율이 클수록 증가되었으며, 20 $wt\%$, 이상에서 수화젤 상의 필름을 형성하였다. 전자현미경에 의한 블렌드 필름의 표면과 단면은 균일한 상을 나타내었다.

토코페롤을 함유하는 생분해성 폴리($\varepsilon$-카프로락톤) 마이크로캡슐의 제조 및 방출 특성 (Preparation and Release Characterization of Biodegradable Poly($\varepsilon$-caprolactone) Microcapsules Containing Tocopherol)

  • 박수진;김기석;민병각;홍성권
    • 폴리머
    • /
    • 제28권2호
    • /
    • pp.103-110
    • /
    • 2004
  • 토코페롤을 함유하는 폴리($\varepsilon$-카프로락톤)(PCL) 마이크로캡슐은 액중건조법에 의하여 제조하였고, 제조 조건에 따른 마이크로캡슐의 특성과 PCL 필름을 사용하여 PCL의 분해거동을 측정하였다 제조된 마이크로캡슐의 크기 및 형태와 구조적 특성은 각각 SEM과 XRD를 이용하여 관찰하였다. 또한, 접촉각 측정을 통하여 심물질의 농도에 따른 마이크로캡슐의 표면자유에너지를 측정하였다. 실험결과, 마이크로캡슐은 유화제로 폴리(비닐 알코올)을 사용한 경우 안정된 구형의 마이크로캡슐이 형성되었고, 마이크로캡슐의 표면자유에너지와 PCL의 결정성은 감소하고, PCL 필름은 악 21일 후 분해가 시작되었다. 토코페롤의 방출특성은 UV/vis.에 의하여 측정하였으며, 마이크로캡슐의 방출속도는 교반속도의 증가와 함께 증가하였다. 이는 교반속도의 증가와 함께 감소된 마이크로캡슐 입자 크기에 의한 방출용액과 마이크로캡슐 사이의 계면의 증가에 의한 것으로 판단된다.

고성능 투명박막트랜지스터 Source/Drain용 AZO박막 특성연구

  • 박온전;노지형;박재호;신주홍;조슬기;여인형;문병무
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제42회 동계 정기 학술대회 초록집
    • /
    • pp.357-357
    • /
    • 2012
  • 박막트랜지스터의 전극으로 Au, Ag, Mo, ITO와 같은 물질들이 이미 많이 연구되어 왔으며, 투명 Source/Drain 전극을 활용한 물질로는 ITO에 초점이 맞춰져 왔다. 하지만 ITO의 높은 가격과 Indium의 인체 유해한 독성 때문에 ITO를 대체하는 물질에 대해 많은 연구가 진행되고 있다. 그 중 Al이 도핑된 ZnO (AZO) 는 가시광 영역에서 85% 이상의 높은 투과율과 높은 전도성, 낮은 비저항으로 다양한 광전소자의 전극과 윈도우 물질로 많은 응용 가능성을 보여주고 있다. 본 실험에서는 고 품질의 박막성장이 가능하고, 박막의 두께를 세밀하게 조절할 수 있는 Pulsed Laser Deposition (PLD) 을 이용하여 온도변화에 따라 AZO 박막을 성장시키고 구조적, 전기적, 광학적 특성을 조사하였다. 또한 온도변화가 AZO 박막 특성에 미치는 영향을 분석하여 Source/Drain 전극으로 사용하기 위한 조건을 최적화하였고, 실제 투명박막트랜지스터 제작을 통해 소자의 I-V Curve 와 Transfer 특성을 확인하고, Transfer Length Method 방법을 이용하여 투명박막트랜지스터의 접촉저항, 채널 비저항 등을 확인해 보았다. 소결된 타겟으로는 99.99%의 순도를 갖는 ZnO-$Al_2O_3$ (98:2 wt%) 타겟을 이용하였으며, 장비조건으로는 355 nm의 파장대역을 갖는 Nd:YAG 레이저를 사용하였고, 실험변수로는 온도범위 RT, $200^{\circ}C$, $400^{\circ}C$, $600^{\circ}C$에서 실험을 진행하였다. AZO 박막의 구조적, 전기적 특성을 분석하기 위해 각각 X-Ray Diffraction (XRD), Hall measurement 장비를 사용하였으며, 광학적 특성을 분석하기 위한 투과도의 측정은 UV-Visible spectrophotometer 장비를 사용하였다.

  • PDF