• 제목/요약/키워드: Wood properties

검색결과 1,416건 처리시간 0.021초

난기류 혼합법을 이용한 목섬유-열가소성 섬유 복합재에 관한 연구(I) - 공정변수가 복합재의 물리적 성질에 미치는 영향 - (Wood Fiber-Thermoplastic Fiber Composites by Turbulent Air Mixing Process(I) - Effects of Process Variables on the Physical Properties of Composites -)

  • 윤형운;이필우
    • Journal of the Korean Wood Science and Technology
    • /
    • 제24권3호
    • /
    • pp.101-109
    • /
    • 1996
  • Effects of process variables were evaluated in physical properties of the wood fiber-thermoplastic fiber composites using nonwoven web method. Turbulent air mixer using compressed air was employed to mix wood fiber with two types of thermoplastic polypropylene and nylon 6 fibers. The optimal hot press temperature and time were found to be $190^{\circ}C$ and 9 minutes in wood fiber-polypropylene fiber composite and to be $220^{\circ}C$ and 9 minutes in wood fiber-nylon 6 fiber composite. As the density of wood fiber-polypropylene fiber composite and wood fiber-nylon 6 fiber composite increased, the physical properties were improved The density appeared to be the most significant factor on physical properties in the statistical analysis. The composition ratio of polypropylene or nylon 6 fiber to wood fiber was considered not to be statistically significant factor. The thickness swelling decreased somewhat in wood fiber-polypropylene fiber composite and wood fiber-nylon 6 fiber composite as the content of synthetic fiber increased. As the increase of mat moisture content, dimensional stability was improved in wood fiber-polypropylene fiber composite but not in wood fiber-nylon 6 fiber composite.

  • PDF

Effects of Density, Resin and Particle Types on Properties of Composites from Wood Particle Mixed with Coating Paper

  • Lee, Phil-Woo
    • Journal of the Korean Wood Science and Technology
    • /
    • 제27권4호
    • /
    • pp.57-64
    • /
    • 1999
  • This research was carried out to investigate the effects of density, resin and particle types on the physical and mechanical properties of the composites made from various wood particles mixed with coating paper. The experiment was designed to apply with three particles (flake, chip, and fiber) and three resin types (urea, phenol and PMDI resin). The mixed ratio of coating paper to wood particle was fixed on 50 to 50% in each board making. And also it was designed to apply for four density levels (0.6, 0.7, 0.8 and 0.9 g/$cm^3$) and four mixed formulations of coating paper to wood particle (10:90, 20:80, 30:70, and 40:60 %) to analyze clearly the effects of PMDI resin. Coating paper-wood particle composites have acceptable bending strength (MOR, MOE) though the mixed ratio of coating paper was increased, but have low internal bond strength and poor dimensional stability (WA, TS, LE). Composites with high density had higher mechanical properties but showed lower physical properties than composites with low density. In conclusion, at least up to 20% mixed ratios, coating paper-wood particle composites have acceptable physical and mechanical properties, and PMDI resin has possibility for coating paper-wood particle composite manufacture.

  • PDF

Preparation and Characterization of Chemically Modified Wood Flour Reinforced Phenol-formaldehyde Composites

  • Nam, Byeong-Uk;Mun, Jun-Yeong
    • 반도체디스플레이기술학회지
    • /
    • 제17권1호
    • /
    • pp.1-5
    • /
    • 2018
  • Wood Polymer Composites(WPC) have attracted significant attention because of ecological and environmental concerns. However, the structure of Wood Flour containing many hydroxyl groups(-OH) reduces the interface adhesion to Phenol-formaldehyde(PF) and it decreases the mechanical properties of the PF/Wood Flour Composites. The present work involves the modification of Wood Flour using silanes reinforced with Phenol-formaldehyde to enhance the mechanical properties of the composites. The spectroscopic properties of the composites were analyzed using FT-IR, XPS(X-ray Photoelectron Spectroscopy) and the mechanical properties i.e., tensile strength, flexural strength and impact strength were studied. We confirmed the modification effect of silanes by spectroscopic analysis, and the mechanical properties of the composites using wood flour modified by silanes were significantly improved.

Physical and Mechanical Properties of Wood Fiber-Polypropylene Fiber Composite Panel

  • Kim, Jee-Woong;Eom, Young-Geun
    • Journal of the Korean Wood Science and Technology
    • /
    • 제29권3호
    • /
    • pp.36-46
    • /
    • 2001
  • This study was to find a way of reusing wood and plastic wastes, which considered as a troublesome problem to be solved in this age of mass production and consumption, in manufacturing wood fiber-polypropylene fiber composite panel. And the feasibility of this composite panel as a substitute for existing headliner base panel of automobile was also discussed, especially based on physical and mechanical performance. Nonwoven web composite panels were made from wood fiber and polypropylene fiber formulations of 50 : 50, 60 : 40, and 70 : 30, based on oven-dry weight, with densities of 0.4, 0.5, 0.6, and 0.7 g/$cm^3$. At the same density levels, control fiberboards were also manufactured for performance comparison with the composite panels. Their physical and mechanical properties were tested according to ASTM D 1037-93. To elucidate thickness swelling mechanism of composite panel through the observation of morphological change of internal structures, the specimens before and after thickness swelling test by 24-hour immersion in water were used in scanning electron microscopy. Test results in this study showed that nonwoven web composite panel from wood fibers and polypropylene fibers had superior physical and mechanical properties to control fiberboard. In the physical properties of composite panel, dimensional stability improved as the content of polypropylene fiber increased, and the formulation of wood fiber and polypropylene fiber was considered to be a significant factor in the physical properties. Water absorption decreased but thickness swelling slightly increased with the increase of panel density. In the mechanical properties of composite panel, the bending modulus of rupture (MOR) and modulus of elasticity (MOE) appeared to improve with the increase of panel density under all the tested conditions of dry, heated, and wet. The formulation of wood fiber and polypropylene fiber was considered not to be a significant factor in the mechanical properties. All the bending MOR values under the dry, heated, and wet conditions met the requirements in the existing headliner base panel of resin felt.

  • PDF

폐타이어를 이용한 목질고무 복합패널의 물성에 관한 연구 - 원료혼합비율에 따른 복합패널의 재질변화 - (Studies on Physical Properties of Wood-based Composite Panel with Recycled Tire Chip - Change of Properties on Composite Panel by Mixing Ratio of Combined Materials -)

  • 이원희;변희섭;배현미
    • Journal of the Korean Wood Science and Technology
    • /
    • 제26권1호
    • /
    • pp.70-75
    • /
    • 1998
  • In this paper, the relationships between volumetric mixing ratio of rubber chip and physical and mechanical properties of wood/rubber composite panel was examined in order to investigate the mixture characteristics of wood and rubber chip. Because of the specific gravity of rubber differed from wood chip, physical properties of wood/rubber composite panel was shown very different values by mixing rate of chip element. Specific gravity in air-dry of composite panel was increased rapidly as volumetric percent of rubber chip was increased. Moisture content of composite panel was decreased as volumetric percent of rubber chip element was increased. This results was considered that wood weight is light and porosity material for moisture absorption. Compressive strength and modulus of rupture in bending test were decreased as volumetric percent of rubber chip increased. By mixing ratio control of chip elements, various wood/rubber composite panel can be applicable to every interior materials such as subfloor, playground, and exterior materials such as road blocks for recreational facilities in garden and forest and city parks.

  • PDF

Evaluation of the Basic Properties for the Korean Major Domestic Wood Species I. Korean Red Pine (Pinus densiflora) in Pyeongchang-gun, Gangwon-do

  • Yonggun PARK;Chul-ki KIM;Hanseob JEONG;Hyun Mi LEE;Kwang-Mo KIM;In-Hwan LEE;Min-Ji KIM;Gyu Bin KWON;Nayoung YOON;Namhee LEE
    • Journal of the Korean Wood Science and Technology
    • /
    • 제52권1호
    • /
    • pp.87-100
    • /
    • 2024
  • Wood has different properties depending on the species or growth area. Therefore, in order to use wood efficiently, it is necessary to have a proper understanding of the characteristics of wood depending on the species and the appropriate use for them. In particular, in order to effectively use more than 1,000 species of woody plants in South Korea as wood, it is necessary to evaluate the characteristics of various Korean domestic woods and make a database of them. In this study, the anatomical properties (length and width of tracheid, cell wall thickness), physical properties (specific gravity and shrinkage), mechanical properties (bending strength, compressive strength, tensile strength, shear strength, hardness), and chemical composition (ash, extract, lignin, total sugar content) of Korean red pine which was grown in Pyeongchang-gun, Gangwon-do, South Korea were evaluated.

아미노실란으로 개질된 목분/PVC/나노점토 복합재의 기계적 특성 (Mechanical Properties of Aminosilane-Treated Wood Flour/PVC/Nanoclay Composites)

  • 박솔몬;김대수
    • 폴리머
    • /
    • 제36권5호
    • /
    • pp.573-578
    • /
    • 2012
  • 일반적으로 목분/PVC 복합재가 갖는 대부분의 물리적 특성은 소수성인 PVC와 친수성인 목분 사이의 낮은 계면결합력으로 인해 순수한 PVC에 비해서도 낮다. 그러므로 본 연구에서는 목분/PVC의 계면결합력을 향상시키기 위해 세 가지 아미노실란을 각각 사용하여 목분을 개질하였으며, 아미노실란으로 개질된 목분, 무중금속 PVC 컴파운드, 나노점토를 용융혼합하여 환경친화적인 목분/PVC/나노점토 복합재를 제조하였다. 목분의 아미노실란 개질 및 나노점토의 첨가가 복합재의 기계적 특성에 미치는 영향을 조사하였다. 복합재의 기계적 특성은 만능재료시험기, 아이조드 충격시험기, DMA, TMA를 이용하여 조사하였다. 아미노실란으로 개질된 목분을 이용한 복합재의 인장특성은 순수한 목분을 이용한 복합재의 인장특성보다 훨씬 높았다. 또한 적은 양의 나노점토가 복합재의 기계적 특성을 향상시켰다. 아미노실란으로 개질된 목분과 나노점토를 사용함으로써 목분/PVC 복합재의 성능이 크게 향상되었다.

한국산 가구용 주요 수종의 재질 (Properties of Major Korean Wood Species for Furniture Manufacturing)

  • 김병로;박원규;최태호
    • 한국가구학회지
    • /
    • 제19권5호
    • /
    • pp.365-374
    • /
    • 2008
  • Understanding of the properties of woods is important in wood utilization. Until now, traditional wooden houses(Korean-style house, Buddhist temple, royal palaces) and furniture have been made of domestic woods with the experience of a craftsman rather than the scientific knowledge on woods. Because of concrete-based houses and imported wood products and furniture, even wood craftsmen decrease in number, too. This study was carried out to collect wood samples growing in Korea and to measure wood characteristics. Anatomical, physical and mechanical properties of 37 wood species were investigated.

  • PDF

Dowel-embedment Properties-Based Finite Solid Element Model for Bolted Connections

  • Hong, Jung-Pyo;Kim, Hyun-Bae;Oh, Jung-Kwon;Lee, Jun-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • 제42권5호
    • /
    • pp.563-570
    • /
    • 2014
  • Two transversely isotropic plasticity-based models for wood, derived from the standard compression properties and the embedment properties were investigated for suitability of application for bolted connections. It was found that the conventional connection models involving the compression properties were incapable of simulating the real behaviour of the connections because the compression properties provided too stiff foundation to represent embedding behaviour of wood under the bolt. However, wood foundation-based connection model that was newly developed using the bolt embedment properties showed good agreement with the actual behaviour of bolted connections.

인도네시아산 미이용 수종의 목재성질(III) - Kebambang, Bawang-bawang 및 Garu buaya 목재의 기초성질 - (Studies on the Wood Properties of Lesser-Known Species Grown in Indonesia(III) - The Fundamental Wood Properties of Kebambang, Bawang-bawang and Garu buaya -)

  • 정성호;정두진;박병수;이도식;조성택
    • 한국가구학회지
    • /
    • 제11권1호
    • /
    • pp.13-23
    • /
    • 2000
  • This study was carried out to investigate the wood properties for development the proper uses of lesser-known tree species. The tested species are Kebambang(Pentace sp.), Bawang-bawang(Dysoxylum alliaceum Bl .), Garu buaya( Gonystylus brunescens A. Shaw)grown in Indonesia. fundamental wood properties such as anatomical, physical, mechanical and chemical properties and characteristics related to wood processing were examined. The results are summarized as follows : The woods of these species are diffuse porous, coarse textured, and interlocked grained. The heartwood of Kebambang is distinguished clearly to the sapwood, but the heartwood of other species are not distinguished clearly to the softwood. The woods of Kebambang and Bawang-bawang have the moderate weight density and the low strength properties, but Garu buaya has the high weight density and the high strength properties. The woods of these species has high shrinkage. The sawing characteristics of Kebambang are excellent but the other species are moderate. The machining characteristics by planer and drying characteristics of these species are moderate. These woods has poor characteristics in bending processing and decay durability. The wood of Bawang-bawang has high content of the extractives and lignin.