금속 3D 프린팅 소재와 폴리머 레이저접합에 관한 연구 (A Study on Laser Welding for 3D Printed Metal Plate and Polymer)

  • 예강현;김성욱;박거동;최해운
    • Journal of Welding and Joining
    • /
    • 제34권4호
    • /
    • pp.23-27
    • /
    • 2016
  • A 3D printed metal part and thermal plastic polymer part were joined by direct laser irradiation. The 3D metal part was fabricated by using DED(Direct Energy Deposition) with STS316 material. The experiment was carried out through no patterned metal surface, 3D metal printed surface and micro laser patterned surface. The most secure joining quality was obtained at the laser micro patterned surface specimen and the counterparts of polymers were PLA and PE based thermo plastics. The applied laser power was 350Watt and the distance of patterns was maintained at $150{\mu}m$. The laser line width was optimized at $450{\mu}m$ and the laser micro pattern depth was $180{\mu}m$ for the best joining quality. Based on the result analysis, the possibility of laser material joining for metal to polymer was proposed and multi-material joining will be possible in 3D laser direct material fabrication.

A Study on Remaining Efficiency of Thermal Straightening after Block Lifting

  • Ha, Yunsok;Yi, Myungsu
    • Journal of Advanced Research in Ocean Engineering
    • /
    • 제1권3호
    • /
    • pp.148-156
    • /
    • 2015
  • Deck plates of ships or offshore structures would make out-of-plane distortion for their thin thickness. These distortions are usually straightened by thermal straightening such as flame heating method. After thermal straightening, the blocks are lifted and moved by cranes to assemble it at dry-dock stage. After this lifting process, out-of-plane deformation again happens frequently. And then, they continuously cause quality and accuracy problems in the final dry-dock process. So, it takes more time for repair and correction working. According to preceding research, the lifting process by cranes would offset the effect on thermal straightening. The target of this study is to develop a methodology analyzing the remaining efficiency of thermal straightening after block lifting. The development was based on the assumption of yield state at straightening region. Therefore the remaining efficiency was obtained by different stiffness slope while lifting & relieving. The efficiency formula was designed using inherent strain, and we made a table of zero-efficiency by cooling speed and class rule's steels. As a result, if the stress orthogonal to straightened line is calculated during lifting analysis by FEA, the efficiency can be obtained linearly to the values in the table. Finally, even optimized carling position can be designed by considering the regional data from series project and welding region on deck.

LASER WELDING OF TI-NI SHAPE MEMORY ALLOY WIRE

  • Kim, Young-Sik;Kim, Jong-Do
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.139-144
    • /
    • 2002
  • Ti-50.9at%Ni wires were welded using pulsed YAG laser. The laser welded wires were tested for investigating the shape memo교 effect and the ability of super elasticity. The fatigue properties of the welded wires were investigated using the rotary bending fatigue tester specially designed for wires. Moreover, the effect of defocusing distance during laser welding on the static and fatigue properties was investigated. The shape memory effect and super elasticity of the laser welded wires were approximately identical with that of base metal at the test temperature below 353K. However, the welded wires were broken within elastic limit at the test temperature above 353k. Under the cyclic bending loading conditions, the welded wires could be useful only below the elastic limit, while the base metal had sufficient fatigue life even the stress induced M-phase region. The fatigue strength of the welded wires was about half of that of the base metal. The deterioration of the static and fatigue properties in the welded wires was proven to be from the large difference of the transformation behavior between the base metal and welded part that is caused by vaporization of Ni-content at the welded part during the welding process. The defocusing distance below 3mm acted more largely on lowering the strength of the welded wires than that of 6mm or 8mm.

  • PDF

디지털 화상처리에 의한 강.구조물의 용접부 치수 결함 검출의 자동화에 관한 연구 (A study on the Automatic Detection of the Welding Dimension Defect of Steel Construct using Digital Image Processing)

  • 김재열;유신;박기형
    • 한국생산제조학회지
    • /
    • 제8권3호
    • /
    • pp.92-99
    • /
    • 1999
  • The inspection unit which is developed and used in this study, is processed the shape data from the CCD camera to seek welding bite section shape, and then calculated as a real dimension from measuring the value of each inspection item. The reason of measuring with the real in this study is came out from the image method which used for a long time, which is extricated the characteristic as the dimension of pixel by recognize pixel. The measurement method of the section shape is that we decide the thresholding value after we drew the histogram to binarizate the object. After that, we make flat the object to get rid of the noise and measure the shape of welded part through the boundarization of the object. The shape measurement is that measure the value of the welding part to adapt the actual operation program from using the ratio between the actual dimension of the standard specimen and the dimension of image, to measure the ratio between the actual product and the camera image. The inspection algorithm which estimates the quality of welded product is developed and also, the software GUI(Graphic User Interface) which processes the automatic test function of the inspection system is developed. We make the foundation of the inspection automatic system and we will help to apply other welding machine.

  • PDF

해양구조물용 RE36강 용접부의 부식거동 및 기계적 특성에 미치는 용접후 열처리 효과에 관한 연구 (A Study on the Post-Weld Heat Treatment Effect Affecting Corrosion Behavior and Mechanical Property of Welding Part of RE36 Steel for Marine Structure)

  • 김성종;문경만
    • Journal of Welding and Joining
    • /
    • 제19권1호
    • /
    • pp.65-74
    • /
    • 2001
  • A study on the corrosion behavior in case of As-welded and PWHT temperature 55$0^{\circ}C$ of welding part of RE36 steel for marine structure was investigated with parameters such as micro-Vickers hardness, corrosion potential measurement of weld metal(WM), base metal(BM) and heat affected zone(HAZ), both Al anode generating current and Al anode weight loss quantity under sacrificial anode cathodic protection conditions. And also we carried out slow strain rate test(SSRT) in order to research both limiting cathodic polarization potential for hydrogen embrittlement and optimum cathodic protection potential as well as mechanical properties by post-weld heat treatment(PWHT) effect. Hardness of HAZ was the highest among three parts(WM, BM and HAZ) and the highest galvanic corrosion susceptibility was HAZ. And the optimum cathodic polarization potential showing the best mechanical properties by SSRT method was from -770mV to -875mV(SCE). In analysis of SEM fractography, applied cathodic potential from -770mV to -875mV(SCE) it appeared dimple pattern with ductile fracture while it showed transgranular pattern (Q. C : quasicleavage) under -900mV(SCE). However it is suggested that limiting cathodic polarization potential indicating hydrogen embrittlement was under -900mV(SCE).

  • PDF

CAE 를 통한 하이브리드 용접 후 차체부품 변형예측 및 검증 (Prediction and Verification of the Twist Deformation of Automotive Structure Parts after Hybrid Welding Using CAE)

  • 이덕영;최보성;최원호;안장호
    • 한국정밀공학회지
    • /
    • 제29권1호
    • /
    • pp.87-95
    • /
    • 2012
  • In recent years, laser-arc hybrid welding has begun to be adopted for assembly welding of automotive bodies and parts, because the hybrid welding process can weld lapped steel sheets having a larger gap than is possible with laser welding. In this paper, to predict the twist deformation by the hybrid welding when brackets are welded in B pillar of a passenger car, the residual stress using CAE is analyzed and the deformation result of CAE is compared with the measured deformation. First of all, after modeling heat source as intended to be expressed with laser-arc hybrid welding method, heat source fitting is done with welding conditions and a section of welding part obtained through specimen test. In case of heat source functions, laser used conical source and arc used double ellipsoid source. Through the local model analysis, elements which are located in the center of the model are selected. The elements are called WME(Welding Macro Element). This WME is extruded in the welding lines and welding phenomenon of complex parts is accomplished. The deformation amount after hybrid welding is got through a simulation, the validity of simulation is verified by measuring the panel and comparing with the simulation result.

조선강재의 최적 용접조건에 관한 연구 (Study on Optimal Welding Condition for Shipbuilding Steel Materials)

  • 김옥환
    • 한국기계가공학회지
    • /
    • 제10권6호
    • /
    • pp.128-133
    • /
    • 2011
  • In this study, the steel material for shipbuilding(LR-A class) was used, and FCAW was taken advantage of 3G attitude and they are welded by different welding ways. As a result of analyzing wave with welding monitoring system, the stable values are obtained which are the first floor(electronic current 164~182 A, voltage 24 V), the second floor(electronic current 174~190 A, voltage 22~25 V), the third floor(electronic current 158~188 A, voltage 22~25 V), and fourth floor(electronic current 172~184 A, voltage 22~25 V), at this time, the stable wave standard deviation and changing coefficient could be obtained. When the welding testing through nondestructive inspection was analyzed know defect of welding, there was no defect of welding in A, D, E, but some porosities in B, and slag conclusion near the surface in C, because the length of arc was not accurate, and the electronic current and voltage was not stable. After observing the change of heat affect zone through micro testing, each organization of floor formed as Grain Refinement, so welding part was fine, the distance of heat affect zone is getting wider up to change the values of the electronic current and voltage. As a result of degree of hardness testing, the hardness orders were the heat affect zone(HAZ), Welding Zone(WZ), and Base Metal(BM). When the distribution of degree of hardness is observed. B is the highest degree of hardness The reason why heat effect zone is higher than welding zone and base metal, welding zone is boiled over melting point($1539^{\circ}C$) and it starts to melt after the result of analysis through metal microscope, so we can know that delicate tissue is created at the welding zone. Therefore, in order to get the optimal conditions of the welding, the proper current of the welding and voltage is needed. Furthermore the precise work of welding is required.

CO2 용접결함 감소를 위한 원격 제어 토치 성능 평가 연구 (Study on an Evaluation of Remote Control Torch Performance to reduce CO2 Welding Defects)

  • 김정혁;오석형;이해길
    • 한국산학기술학회논문지
    • /
    • 제15권10호
    • /
    • pp.6282-6288
    • /
    • 2014
  • 본 논문은 용접 산업현장에서 많이 사용 되는 $CO_2$ 용접에서는 차량내부 및 탱크내부 용접에서 제어 패널을 볼 수 없는 곳, 작업장이 먼 곳 등에서 용접사가 용접을 하면서 용접조건에 맞는 전류와 전압을 조절할 수가 없고, 전류와 전압을 조절하기 위해 용접을 중단하고 잦은 이동으로 용접 구조물의 순간적인 냉각에 의해 용접결함이 발생된다. 본 연구에서는 기존의 $CO_2$ 용접기 3종류를 각각 사용하여 원격제어 토치의 용접에 대해 SS400 용접구조용 압연강재를 사용하여 원격제어 토치와 기존 $CO_2$ 용접 토치를 V형 맞대기 수직자세로 용접실험을 실시하고 용접 부의 표면비드 상태의 형상을 육안검사 관찰하고 또한 이를 침투탐상검사 및 굽힘 시험을 통해 용접부의 외관품질에 대하여 중점적으로 수행하여 용접결함 감소 및 기존 상용용접기에 교체사용에 대한 성능 및 호환성여부에 미치는 영향에 대해 평가하였다.

GTAW 펄스 용접 조건에 따른 타이타늄 정밀관의 용입, 변색 및 굽힘특성 (Effects of GTAW Pulse Condition on Penetration, Discoloration and Bending Property for Titanium Tube)

  • 민성환;안성용;박지태;박영도;강남현
    • Journal of Welding and Joining
    • /
    • 제32권6호
    • /
    • pp.47-55
    • /
    • 2014
  • The purpose of the study is to produce a mechanically improved weld and minimum variation of color through comparing unpulsed and pulsed GTAW (Gas Tungsten Arc Welding) for pure titanium (CP grade7) tube. Pulsed GTAW using 60 A peak current and 20 A background current (1:9) achieved the wider window of welding conditions having part and full penetration without burn-through than the case of unpulsed GTAW. Moreover, the pulsed welding reduced a discoloration on the back bead of the weld and the size of microstructures (basket weave and serrated ${\alpha}$). That is because the pulsed welding has it's a low heat input and severe weld flow induced from electric current variation. Furthermore, the pulsed welding improved the bending property of the welded Ti tube. The enhanced bending property for the pulsed GTAW was due to the insignificant discoloration on the weld surface with maintaining the metal polish.

자동차 브레이크 부품용 S45C 소재의 레이저 용접특성 평가 (Laser Welding Properties of the S45C using Automobile Brake Parts)

  • 심기중;조원용;김용관;최규재
    • 한국자동차공학회논문집
    • /
    • 제22권1호
    • /
    • pp.103-109
    • /
    • 2014
  • This paper represents the s-cam manufacturing process with the high-carbon steel like S45C using laser welding system. Laser welding of the high-carbon steel is generally difficult because of hardening of the weld zone. Also, existing s-cam manufacturing process, electric resistance welding system, have some problems like increase of production and development cost. To solve those problems, we are introduced the laser welding system with the pre-heating system for precision welding of s-cam with separated shaft and cam part. S-cam manufactured with optimum laser welding conditions is verified the performance like tensile strength, torsional strength and fatigue test. Strength and fatigue test results are described.