Materials Integrity Analysis for Application of Hyper Duplex Stainless Steels to Korean Nuclear Power Plants

  • Chang, Hyun-Young;Park, Heung-Bae;Park, Yong-Soo;Kim, Soon-Tae;Kim, Young-Sik;Kim, Kwang-Tae;Jhang, Yoon-Young
    • Corrosion Science and Technology
    • /
    • v.9 no.5
    • /
    • pp.187-195
    • /
    • 2010
  • Hyper duplex stainless steels have been developed in Korea for the purpose of application to the seawater system of Korean nuclear power plants. This system supplies seawater to cooling water heat exchanger tubes, related pipes and chlorine injection system. In normal operation, seawater is supplied to heat exchanger through the exit of circulating water pump headers, and the heat exchanged sea water is extracted to the discharge pipes in circulating water system connected to the circulating water discharge lines. The high flow velocity of some part of seawater system in nuclear power plants accelerates damages of components. Therefore, high strength and high corrosion resistant steels need to be applied for this environment. Hyper duplex stainless steel (27Cr-7.0Ni-2.5Mo-3.2W-0.35N) has been newly developed in Korea and is being improved for applying to nuclear power plants. In this study, the physical & mechanical properties and corrosion resistance of newly developed materials are quantitatively evaluated in comparative to commercial stainless steels in other countries. The properties of weld & HAZ (heat affected zone) are analyzed and the best compositions are suggested. The optimum conditions in welding process are derived for ensuring the volume fraction of ferrite(${\alpha}$) and austenite(${\gamma}$) in HAZ and controlling weld cracks. For applying these materials to the seawater heat exchanger, CCT and CPT in weldments are measured. As a result of all experiments, it was found that the newly developed hyper duplex stainless steel WREMBA has higher corrosion resistance and mechanical properties than those of super austenitic stainless steels including welded area. It is expected to be a promising material for seawater systems of Korean nuclear power plants.

A Study on the Fatigue Crack Growth threshold Characteristic for Steel of Pressure Vessel at Low Temperature (압력용기용강의 저온피로 크랙전락 하한계 특성에 관한 연구)

  • 박경동;하경준
    • Proceedings of the KWS Conference
    • /
    • 2001.05a
    • /
    • pp.224-227
    • /
    • 2001
  • In this study, CT specimens were prepared hem ASTM SA516 which was used for pressure vessel plates for room and low temperature service. And we got the following characteristics from fatigue crack growth test carried out in the environment of room and low temperature at $25^{\circ}C$, -3$0^{\circ}C$, -6$0^{\circ}C$, -8$0^{\circ}C$, -l$0^{\circ}C$ and -l2$0^{\circ}C$ and in the range of stress ratio of 0.1, 0.3 by means of opening mode displacement. At the constant stress ratio, the threshold stress intensity factor range $\Delta K_{th}$ in the early stage of fatigue crack growth ( Region I ) and stress intensity factor range $\Delta$K in the stable of fatigue crack growth ( Region II) was increased in proportion to descend temperature. It assumed that the fatigue resistance characteristics and fracture strength at low temperature is considerable higher than that of room temperature in the early stage and stable of fatigue crack growth region. The straight line slope relation of logarithm da/dN - $\Delta$K in Region II, that is, the fatigue crack growth exponent m increased with descending temperature at the constant stress ratio. It assumed that the fatigue crack growth rate da/dN is rapid in proportion to descend temperature in Region H and the cryogenic-brittleness greatly affect a material with decreasing temperature.

  • PDF

Repair Procedure and Structural Strength Analysis to Damage of Moon-Pool Structure for Drillship During Construction (드릴쉽 건조 중 문풀 구조 수정 작업 및 구조적 안정성 검토)

  • Yoo, In-Sang;Sohn, Sang-Young;Baek, Seung-Jung;Choi, Young-Lack;Yoo, Hae-Kun;Yoon, Ki-Jeong
    • Special Issue of the Society of Naval Architects of Korea
    • /
    • 2011.09a
    • /
    • pp.12-16
    • /
    • 2011
  • During the shipbuilding construction, the repair works will be occurred by various reasons such as the natural disaster, mistakes of engineers or workers, defect of material, and so on. The one of the engineer's responsibilities is to design considering every possibility and to prevent the repair works due to the mistakes during construction stages, but actually it is very difficult and impossible to avoid every mistake. However, it is also the responsibility of engineers to find the best solution for the unavoidable mistakes which is to maintain the capacity of vessel and guarantee the safety for the repair works considering the construction schedules and economic cost. In this paper, it will be introduced the brief of repair works to the structural damage of the moon-pool structure in drillship which is built in our shipyard. For the verification of the structural strength, the fatigue analysis has been carried out based on the guide of Classification society. Furthermore, the modifications of structure design and welding procedure have been applied to avoid the stress concentration in the moon-pool structure.

  • PDF

Re-distribution of Welding Residual Stress Due to Tensile Pre-load and Its Effects on Fatigue Strength in Padding Plate Weldment (Padding plate 용접구조의 인장 정하중 이력에 의한 용접잔류응력 변화 및 피로강도에의 영향)

  • S.W. Kang;Y.W. Kim;W.S. Kim;D.H. Kim
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.38 no.4
    • /
    • pp.75-82
    • /
    • 2001
  • Static loadings on ship structure induced either by water pressure before service such as a tank test and ballasting or by cargo pressure during first laden voyage cause relatively much greater stress than dynamic loadings induced by wave. With these static pre-loadings, the initial residual stresses around welded joint, where fatigue strength is concerned(in most cases, where stress concentration occurs) are expected to be shaken-down in a great extent by the elasto-plastic deformation behavior of material. Therefore, it is more resonable to assess the fatigue strength of ship structure with S-N data which have taken into account the effect of shaken-down residual stresses(re-distributed stresses) on the fatigue strength. In this research work, the re-distribution of residual stresses by the tensile pre-loading is measured using an ordinary sectioning method for specimens of padding plate weldment. Fatigue tests are performed also to evaluate the fatigue strength of the both as-welded and pre-loaded specimens.

  • PDF

Development of Localized Roots Type Medium-Vacuum Pump (루츠형 중진공펌프 국산화 개발)

  • Tak, Bong-Yeol;Kim, Byung-Duk;Yang, Hea-Gyeong;Han, Gi-Young;Lee, So-A
    • The KSFM Journal of Fluid Machinery
    • /
    • v.14 no.3
    • /
    • pp.23-27
    • /
    • 2011
  • Due to a roots type medium vacuum pump is operated in condition of $1{\sim}10^{-3}$ torr vacuum, it could be applied for production and process of industrial parts, such as precise processing, vaporization, enrichment, separation, casting, metaling, welding, transportation. Therefore, the demand of this pump is increasing nowadays in our industrial markets of semiconductor, electric, electronic, automobile, material, environmental and transporting industries. However, the pumps are almost imported, because the domestic pumps are inferior in fields of vacuum range as under $10^{-1}$torr, relevant techniques(design, fabrication, casting, test, etc.) to the imported ones. In this study, essential parts of the development pump are designed with using of CFD and 3D decodes, FEM for analysing strength and deformation, generated heat, vibration and noise control, and are casted with using of mechanochemistry techniques for decreasing of weights, increasing of heat resistances and abrasion durability of materials for pump caing and impellers especially. Besides, in order to achieve ultimate vacuum around $10^{-3}$torr, this pump is composed of 6 stages, among which 1st stage is operated separately from remained stages. Additionally, a test rig for prototype pumps(300$m^3/h$ and 2,500$m^3/h$) is designed and procured as to apply for multi-staged rootz type vacuum pump, with modification of the test method recommended by KS B 6314 "Positive-displacement oil-sealed rotary vacuum pumps".

Evaluation of Microscopic Damage to TIG Welded Carbon Steel using Acoustic Emission and Ultrasonic Test (음향방출과 초음파를 이용한 TIG 용접탄소강의 미시적 손상평가)

  • Lee, Joon-Hyun;Lee, Jin-Kyung
    • Journal of Ocean Engineering and Technology
    • /
    • v.26 no.5
    • /
    • pp.5-10
    • /
    • 2012
  • In this study, carbon steel (A53) is used as the material for the pipes in a marine plant and ship industry. Welds are necessary to join the carbon steel, and the effect of this welding on the properties of the carbon steel has been studied by many researchers. In this study, the dynamic behavior of welded carbon steel was studied using an acoustic emission (AE) technique, which is a nondestructive test. There are numerous AE parameters that can be used to analyze the damage behavior of carbon steel by external loading. The AE parameters of energy, cumulative count, amplitude, and AE event were used, and each parameter was differentiated according to the degree of damage to the carbon steel. The energy showed a high level at the elastic range of the load curve, while the amplitude had the highest value at the hardening region. The cumulative count showed a growth tendency similar to the loading curve. In addition, an ultrasonic technique and hardness test were applied to evaluate the mechanical properties according to the base zone, HAZ region, and weld zone of the weld specimen. The velocity and attenuation ratio showed little change between zones, and an evaluation of the ultrasonic waves on each zone of the specimen was found to be a useful method to clarify the mechanical properties of the carbon steel.

Optimization of SWCNT-Coated Fabric Sensors for Human Joint Motion Sensing

  • Cho, Hyun-Seung;Park, Seon-Hyung;Yang, Jin-Hee;Park, Su-Youn;Han, Bo-Ram;Kim, Jin-Sun;Lee, Hae-Dong;Lee, Kang-Hwi;Lee, Jeong-Whan;Kang, Bok-Ku;Chon, Chang-Soo;Kim, Han-Sung;Lee, Joo-Hyeon
    • Journal of Electrical Engineering and Technology
    • /
    • v.13 no.5
    • /
    • pp.2059-2066
    • /
    • 2018
  • This study explored the feasibility of utilizing an SWCNT-coated fabric sensor for the development of a wearable motion sensing device. The extent of variation in electric resistance of the sensor material was evaluated by varying the fiber composition of the SWCNT-coated base fabrics, attachment methods, number of layers, and sensor width and length. 32 sensors were fabricated by employing different combinations of these variables. Using a custom-built experimental jig, the amount of voltage change in a fabric sensor as a function of the length was measured as the fabric sensors underwent loading-unloading test with induced strains of 30 %, 40 %, and 50 % at a frequency of 0.5 Hz. First-step analysis revealed the following: characteristics of the strain-voltage curves of the fabric sensors confirmed that 14 out of 32 sensors were evaluated as more suitable for measuring human joint movement, as they yield stable resistance values under tension-release conditions; furthermore, significantly stable resistance values were observed at each level of strain. Secondly, we analyzed the averaged maximum, minimum, and standard deviations at various strain levels. From this analysis, it was determined that the two-layer sensor structure and welding attachment method contributed to the improvement of sensing accuracy.

Micro Joining Process Using Solderable Anisotropic Conductive Adhesive (Solderable 이방성 도전성 접착제를 이용한 마이크로 접합 프로세스)

  • Yim, Byung-Seung;Jeon, Sung-Ho;Song, Yong;Kim, Yeon-Hee;Kim, Joo-Heon;Kim, Jong-Min
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.73-73
    • /
    • 2009
  • In this sutdy, a new class ACA(Anisotropic Conductive Adhesive) with low-melting-point alloy(LMPA) and self-organized interconnection method were developed. This developed self-organized interconnection method are achieved by the flow, melting, coalescence and wetting characteristics of the LMPA fillers in ACA. In order to observe self-interconnection characteristic, the QFP($14{\times}14{\times}2.7mm$ size and 1mm lead pitch) was used. Thermal characteristic of the ACA and temperature-dependant viscosity characteristics of the polymer were observed by differential scanning calorimetry(DSC) and torsional parallel rheometer, respectively. A electrical and mechanical characteristics of QFP bonding were measured using multimeter and pull tester, respectively. Wetting and coalescence characteristics of LMPA filler particles and morphology of conduction path were observed by microfocus X-ray inspection systems and cross-sectional optical microscope. As a result, the developed self-organized interconnection method has a good electrical characteristic($2.41m{\Omega}$) and bonding strength(17.19N) by metallurgical interconnection of molten solder particles in ACA.

  • PDF

Dynamic Analysis to Select Main Parts of Four-Axis Palletizing Robots (4축 이적재 로봇의 주요 부품 선정을 위한 동적 해석)

  • Park, Il-Hwan;Jeon, Yong-Jae;Go, A-Ra;Seol, Sang-Seok;Hong, Dae-Sun
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.19 no.12
    • /
    • pp.62-69
    • /
    • 2020
  • The demand for industrial robots is proliferating with production automation. Industrial robots are used in various fields, such as logistics, welding, and assembly. Generally, six degrees of freedom are required to move freely in space. However, the palletizing robot used for material management and logistics systems typically has four degrees of freedom. In designing such robots, their main parts, such as motors and reducers, need to be adequately selected while satisfying payload requirements and speed. Hence, this study proposes a practical method for selecting the major parts based on dynamic analysis using ADAMS. First, the acceleration torques for the robot motion were found from the analysis, and then the friction torques were evaluated. This study introduces a constant-speed torque constant instead of friction coefficient. The RMS torque and maximum power of each motor were found considering the above torques. After that, this study recommends the major specifications of all motors and reducers. The proposed method was applied to a palletizing robot to verify the suitability of the pre-selected main parts. The verification result shows that the proposed method can be successfully applied to the early design stage of industrial robots.

Fabrication and Characterization of Cu-based Amorphous Coatings by Cold Spray Process (저온 분사를 이용한 Cu계 비정질 코팅층의 제조 및 특성 연구)

  • Jung, Dong-jin;Park, Dong-Yong;Lee, Jin Kyu;Kim, Hyung Jun;Lee, Kee-Ahn
    • Korean Journal of Metals and Materials
    • /
    • v.46 no.5
    • /
    • pp.321-327
    • /
    • 2008
  • Cu based amorphous ($Cu_{54}Zr_{22}Ti_{18}Ni_6$) coating was produced by cold spraying as a new fabrication process. The microstructure and macroscopic properties of amorphous coating layer was investigated and compared with those of cold sprayed pure Cu coating. Amorphous powders were prepared by gas atomization and Al 6061 was used as the substrate plate. X-ray diffraction results showed that Cu based amorphous powder could be successfully deposited by cold spraying without any crystallization. The Cu based amorphous coating layer ($300{\sim}400{\mu}m$ thickness) contained 4.87% porosity. The hardness of Cu based amorphous coating represented $412.8H_v$, which was correspond to 68% of the hardness of injection casted bulk amorphous material. The wear resistance of Cu based amorphous coating was found to be three times higher than that of pure Cu coating. The 3-point bending test results showed that the adhesion strength of Cu based amorphous coating layer was higher than that pure Cu coating. It was also observed that hard Cu base amorphous particle could easily deform soft substrate by particle collisions and thus generated strong adhesion between coating and substrate. However, the amorphous coating layer unexpectedly represented lower corrosion resistance than pure Cu coating, which might be resulted from the higher content of porosity in the cold sprayed amorphous coating.