Transactions of the Korean Society of Mechanical Engineers A
/
v.32
no.6
/
pp.519-525
/
2008
For this study, SM45C steel rods using generally for power transmission shafts and machine components was selected and welded by butt-GMAW method. And then it was studied about estimation of fatigue strength and the region of infinite life by Haigh diagram using Goodman's equation. Fatigue strength in weld zone presents highly in order of the boundary between deposited metal zone and heat affected zone, deposited metal zone, heat affected zone. This result agrees with distribution of hardness in weld zone. Fatigue strength in base metal zone presents highly compared with weld zone in low cycles between $10^4$ cycles and $10^6$cycles, but it presents the lowest fatigue strength on the order of heat affected zone in the vicinity of $10^6$cycles. It is the result that the first high compressive residual stress distributed by drawing process of the steel rods is released and the base metal is softened by alternating stresses. The region of infinite life by Haigh diagram presents highly in order of the boundary between deposited metal zone and heat affected zone, deposited metal zone, heat affected zone. From this results, it is demanded that the stress for safety design of machine components using SM45C butt-welded steel rods must be selected in the region of the lowest infinite life of heat affected zone.
This study is to compare the welding quality of API 5L-X65 Steel- pipe's for natural gas transmission piping applied by SAW at shop and by GTAW-SMAW at site. The results can be summarized as follows; 1) Tensile strength of the welded zone by SAW(611.5 MPa) and by GTAW-SMAW(608.6 MPa) was maintained greater than that of the base metal(583.5 MPa). 2) Hardness of the welded zone and HAZ by SAW(Hv 194.8) & GTAW-SMAW (Hv 196.1) was slightly increased above that of the base metal (Hv 168.8), but less than the maximum allowable hardness(Hv 248). 3) Impact value of the welded zone by SAW(126.8 J) & GTAW-SMAW(88 J) became lower than that of the base metal(282.5 J), but was above the requirement of API 5L(68J). 4) Microscopic structure of the welded zone and HAZ by both SAW & GTAW-SMAW became fine-grained.
In an attempt to evaluate the feasibility of friction stir welding(FSW) for joining carbon steels, microstructures and mechanical properties of friction stir welded carbon steels with different grain structures were investigated. In comparison of O-type stir zone(SZ) appeared in various aluminium alloys, configuration of SZ in friction stir welded carbon steels displayed U-type. Plastically deformed pearlite band structure was identified to surround the SZ, indicating the existence of so-called thermo-mechanically affected zone(TMAZ). However, the TMAZ of carbon steels was much narrower than that of Al alloys. The microstructures of both stir zone and TMAZ revealed bainite matrix in a conventional carbon steel for shipbuilding, while, in the same region, ferrite matrix microstructures were formed in a low carbon fine grained steel. The conventional carbon steel showed superior stirring workability to that of the fine grained carbon steel. The yield and tensile strength of the friction stir welded joints were comparable to those of the base metals, and the elongation in welded joints demonstrated excellent ductility. Absorbed energy in SZ of the fine grained carbon steel was ten times higher than that obtained from conventional submerged arc weld metal of the same steel. Based on these results, the application FSW to carbon steels was found to be feasible.
By using miniature SENB specimens, the fracture properties of the materials in the region of welded metal, 321 stainless steel heat affected zone, 690 alloy heat affected zone of 321/690 dissimilar metal girth welded joints were tested. Both the J-resistance curves and critical fracture toughness of the three different materials are affected by the crack size because of the effect of crack tip constraint. Groups of constraint corrected J-resistance curves of the three materials are obtained according to J-Q-M approach. The welded metals exhibit the best fracture resistance but the worst fracture resistance is observed in the material of 690 alloy heat affected zone.
In this study, dissimilar friction welding were produced using 15mm diameter solid bar in chrome molybedenum steel(SCM440) to carbon steel(S45C) to investigate their mechanical properties and the relationship between the weld parameters and the nondestructive coefficients, such as AE counts and ultrasonic attenuation coefficient. The main friction welding parameters were selected to endure good quality welds on the basis of visual examination, tensile tests, Vickers hardness surveys of the bond of area and heat affected zone. The specimens were tested as-welded and post weld heat treated(PWHT). The tensile strength of the friction welded steel bars was increased up to 100% of the S45C base metal under the condition of all heating time. The ductility of PWHT specimens is higher than as-welded.
T-type and H-type section steels were generally used in shipbuilding and offshore plants and were produced by welding technology. These section steels were produced by handwork, and the supplying amounts can't satisfy the demand amounts of the fabrication companies. In case of fillet welding, there are some gaps in weld-joint region due to no groove preparation processing and it can occur crack initiation in the welded region. It is important to evaluate the microstructural and mechanical properties of welded zone to solve these problems. To satisfy the demand amounts of T-bar parts, automatic welding technology was introduced and several conditions as a function of welding speeds were carried out to improve the manufacturing speed. Heat-affected zone may be affected by variation of heat input and cooling rate through automatic welding speed and welding speed is necessary to be optimized. In this study, fusion zone and heat-affected zone were investigated by microstructural and mechanical analysis and were evaluated whether the welded parts were sound or not.
The seawater pipes in the engine rooms of ships are surrounded by severely corrosive environments caused by fast flowing seawater containing chloride ions, high conductivity, etc. Therefore, it has been reported that seawater leakage often occurs at a seawater pipe because of local corrosion. In addition, the leakage area is usually welded using shielded metal arc welding with various electrodes. In this study, when seawater pipes were welded with four types of electrodes(E4311, E4301, E4313, and E4316), the difference between the corrosion resistance values in their welding zones was investigated using an electrochemical method. Although the corrosion potential of a weld metal zone welded with the E4316 electrode showed the lowest value compared to the other electrodes, its corrosion resistance exhibited the best value compared to the other electrodes. In addition, a heat affected zone welded with the E4316 electrode also appeared to have the best corrosion resistance among the electrodes. Furthermore, the corrosion resistance of the weld metal zone and heat affected zone exhibited relatively better properties than that of the base metal zone in all of the cases welded with the four types of electrodes. Furthermore, the hardness values of all the weld metal zones were higher than the base metal zone.
Transactions of the Korean Society of Mechanical Engineers A
/
v.31
no.4
/
pp.532-539
/
2007
The 7075-T651 Al alloy was welded by friction stir welding. Microstructure, macro behaviors and fracture type in the nugget, thermo-mechanically affected zone(TMAZ) and heat affected zone(HAZ) of the welded part were compared to base metal. The microsturctures of nugget zone were compared with tool rotation speeds and various tool transition speed. When the rotation speeds were decreased and transition speeds were increased, the hardness of nugget zone were decreased. Also, the optimal microstructure was observed at the low rotation speed of 800rpm and the high transition speed of 124mm/min. The transgranular dimple and quasi-cleavage at fractured part of nugget zone were investigated.
The conventional SCC(stress corrosion cracking) test methods have much difficulty in evaluating the SCC behaviors of the localized zone like HAZ, bond line and weld metal because of the specimen size. Accordingly, the purpose of this paper is to develop the new SCC test method of the welded zone by evaluating the SCC susceptibility on parent metal and various microstructures of the welded zone by SP(small punch) test method using miniaturized small specimen and SSRT(slow strain rate test) method(SP-SSRT). Besides, this study is to verify the efficiency of the SP-SSRT results through AE(acoustic emission) test which is a useful technique to monitor the microfracture processes of the material. From the results of SCC susceptibility, SEM observation and AE test, it can be concluded that the SP-SSRT test using miniaturized small specimen(10mm*10mm*0.5mm) will be a good test method to evaluate the SCC susceptibility on the local zone such as the welded zone.
It is reported that about more than 45% of damage shown in railroad rails include breakage of rail end which cross the center of Thermit welded zone. Thermite welding is always accompanied by numerous aluminum oxide and secondary inclusions, which may have a negative influence on the ductility and toughness of the weld metal. In this study the aluminum powder recycled by waste aluminum can was used for iron oxide generated after the process of welding rod and the remain aluminum was reduced by minimizing the quantity of aluminum. And complete dissolution was induced by using ferro Mn powder as the additive element. This study reviewed the applicability of heat treatment in the welded zone of rail using ceramic heating pad by carrying it out. This study could observe the improvement of the mechanical characteristics (UTS and elongation) and the changes of failure mechanism from brittleness to ductility. It could be found that improved strength and elongation result from pearilte fine structure.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.