펄스 전착된 크롬-카본 도금층의 특성 (Characterization of Electro-deposited Chrome-Carbon Layer Prepared by Pulse Plating)

  • Lee, J.J.;Lee, B.K.;Y.S. Pyun;Kim, Man;S.C. Kwon
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2002년도 춘계학술발표회 초록집
    • /
    • pp.36-36
    • /
    • 2002
  • Effects of pulse-plating on the wear and corrosion resistance of chrome-carbon layers were studied. The plating were carried out at $06A/\textrm{cm}^2$ in modified Sargent bath containing formic acid at $53^{\circ}C$. The chrome layer were super-saturated with carbon up to 2.0wt. %, which precipitated as chrome carbide such as $Cr_{23}C_6$ after vacuum aging above $200^{\circ}C$ for 1 hour. This resulted in improvement of hardness and wear resistance of the chrome layer. Considering the reduction of corrosion resistance due to the thermal effect, optimum vacuum aging condition of the chrome layer in this study was I-hour at $200^{\circ}C$.

  • PDF

저항클래딩법을 응용하여 형성된 내마모성 WC-6.5Co 클래딩층의 미크로조직 특성 (Characterization of Microstructure of WC-6.5%Co Cladding Layer by Electric Resistance Welding)

  • 이진우;고준빈;이영호
    • Journal of Welding and Joining
    • /
    • 제25권3호
    • /
    • pp.72-77
    • /
    • 2007
  • This study deals with characterizations of microstructure and wear performance of a cladding layer, product on 1.9 mm-thick mild steel plate by the electric resistance welding, of composite metal powder of Coarse WC-6.5%Co and high carbon alloy (SHA). The cladding layer was examined and tested for microstructural features, chemical composition, hardness, and bondability. The cladding layer have two different matrix were observed by an optical microscope and EPMA. The one was the coarse WC-6.5Co structure. The other was the melted SHA with surrounding the WC-6.5Co structure. The hardness of WC-6.5Co was 1210HV. The hardness of SHA was 640HV.

증착방법에 따른 DLC 막의 마찰-마모 특성평가 (Characterization of Tribological Properties of DLC Films Prepared by Different Deposition Method)

  • 오윤석
    • 한국세라믹학회지
    • /
    • 제46권5호
    • /
    • pp.497-504
    • /
    • 2009
  • DLC is considered as the candidate material for application of moving parts in automotive components relatively in high pressure and temperature operating conditions for its high hardness with self lubrication and chemical inertness. Different deposition method such as arc plating, ion gun plating and PECVD were used for comparing mechanical and tribological properties of each DLCs deposited on stainless steel with 1 um thick respectively. Among these 3 types of DLCs, the arc plated DLC film showed highest value for wear resistance in dry condition. From the results of analysis for physical properties of DLC films, it seems that the adhesion force and crack initiation modes were more important factors than intrinsic mechanical properties such as hardness, elastic modulus and/or roughness to the wear resistance of DLC films. Raman spectroscopy was used for understanding chemical bonding natures of each type of DLC films. Typical D and G peaks were identified based on the deposition method. Hardness of the coating layers were identified by nanoindentation method and the adhesions were checked by scratch method.

기능화된 다중벽 탄소나노튜브 복합재료의 제조 및 물성 평가에 대한 연구 (Manufacturing and Characterization of Nano-composites with Chemically Functionalized Multiwalled Carbon Nanotubes)

  • 박주혁;김태구
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.126-131
    • /
    • 2004
  • Chemically modified multiwalled carbon nanotubes with acids were incorporated into a epoxy matrix by in situ polymerization process, to improve the transfer of mechanical load through chemical bonds, which were demonstrated by infrared spectroscopy. And the mechanical properties of epoxy/carbon nanotube composites were measured to investigate the role of carbon nanotubes. The epoxy/carbon nanotube composites shows higher tensile strength and wear resistance than existing epoxy, with 1 or 2 wt. % addition of functionalized carbon nanotubes. The tensile strength with 7 wt. % carbon nanotibes is increased by a 28% and the wear resistance in exceptionally increased by an outstanding 100 times.

  • PDF

화염급냉 표면처리된 Cu-8.8Al-4.5Ni-4.5Fe 합금의 미세구조 분석 및 내마모성에 관한 연구 (Characterization of the Microstructure and the Wear Resistance of the Flame-Quenched Cu-8.8Al-4.5Ni-4.5Fe Alloy)

  • 이민구;홍성모;김광호;김경호;김흥회
    • 열처리공학회지
    • /
    • 제17권6호
    • /
    • pp.346-355
    • /
    • 2004
  • The flame quenching process has been employed to modify the surfaces of commercial marine propeller material, aluminum bronze alloy (Cu-8.8Al-5Ni-5Fe), and the microstructure, hardness and wear properties of the flame-quenched layers have been studied. The thermal history was accurately monitored during the process with respect to both the designed maximum surface temperature and holding time. The XRD and EDX analyses have shown that at temperatures above $T_{\beta}$, the microstructure consisting of ${\alpha}+{\kappa}$ phases changed into the ${\alpha}+{\beta}^{\prime}$ martensite due to an eutectoid reaction of ${\alpha}+{\kappa}{\rightarrow}{\beta}$ and a martensitic transformation of ${\beta}{\rightarrow}{\beta}^{\prime}$. The ${\beta}^{\prime}$ martensite phase formed showed a face-centered cubic (FCC) crystal structure with the typical twinned structure. The hardness of the flame-quenched layer having the ${\alpha}+{\beta}^{\prime}$ structure was similar to that of the ${\alpha}+{\kappa}$ structure and depended sensitively on the size and distribution of hard ${\kappa}$ and ${\beta}^{\prime}$ phases with depth from the surface. As a result of the sliding wear test, the wear resistance of the flame-quenched layer was markedly enhanced with the formation of the ${\beta}^{\prime}$ martensite.

플라즈마 코팅재료의 파괴인성과 마모 거동 (Characterization of Fracture Toughness and Wear Behavior for Plasma Ceramic Coated Materials)

  • 하선호;이동우;아따 울 레만;압둘 와지;송정일
    • 한국기계가공학회지
    • /
    • 제12권4호
    • /
    • pp.123-130
    • /
    • 2013
  • Zirconia is well known in industrial applications for its mechanical characteristics. DLC (diamond-like carbon) have high elastic modulus, high electric resistivity, high dielectric constant, high wear resistance, low friction coefficient, bio compatibility, chemically inert and thermally stable. Because of all these physical and chemical properties these types of coatings have become key procedure for thin coating. Friction coefficient of DLC films is already evaluated and the current work is a further advancement by calculating the fracture toughness and wear resistance of these coatings. In the present study DLC thin film coatings are developed on $ZrO_2$ alloy surface using Plasma Enhanced Chemical Vapor Deposition (PECVD) method. Vicker hardness test is employed and it was concluded that, DLC coatings increase the Vickers hardness of ceramics.

Ti-6Al-4V 합금의 미세조직 및 기계적 특성에 미치는 Plasma 침탄 처리의 영향 (Improvement of Microstructural and Mechanical Properties of Ti-6Al-4V Alloy by Plasma Carburization)

  • 박용권;김택수;지태구;위명용
    • 한국재료학회지
    • /
    • 제12권5호
    • /
    • pp.341-346
    • /
    • 2002
  • In order to improve the low wear resistance of Ti-6Al-4V alloy, plasma carburization treatment was newly carried out without consumption of its good specific strength and fatigue life over the temperature. Effect of the plasma carburization was analyzed and compared with the non-treated alloy by microstructural observation, structure characterization and mechanical property test. The plasma treated alloy formed a carburized layer of about 150$\mu\textrm{m}$ in depth from the surface, where a fine and hard particles of TiC and $V_4C_3$ were homogeneously dispersed through the layer. It was also found that an increase of the wear resistance, fatigue life and hardness, due to the hard and fine dispersoids.

DLC(Diamond-Like Carbon) 코팅에 의한 오목 폴리머인쇄판의 내구성 및 인쇄 품질 특성 (Characterization of Plate Wear and Printing Quality of Concave Polymer Printing Plate Prepared by Diamond-Like Carbon Deposition Conditions)

  • 유한솔;김준형;문경일;황택성;이혁원
    • 한국재료학회지
    • /
    • 제22권10호
    • /
    • pp.552-561
    • /
    • 2012
  • Diamond-like carbon (DLC) films have been widely used in many industrial applications because of their outstanding mechanical and chemical properties like hardness, wear resistance, lubricous property, chemical stability, and uniformity of deposition. Also, DLC films coated on paper, polymer, and metal substrates have been extensively used. In this work, in order to improve the printing quality and plate wear of polymer printing plates, different deposition conditions were used for depositing DLC on the polymer printing plates using the Pulsed DC PECVD method. The deposition temperature of the DLC films was under $100^{\circ}C$, in order to prevent the deformation of the polymer plates. The properties of each DLC coating on the polymer concave printing plate were analyzed by measuring properties such as the roughness, surface morphology, chemical bonding, hardness, plate wear resistance, contact angle, and printing quality of DLC films. From the results of the analysis of the properties of each of the different DLC deposition conditions, the deposition conditions of DLC + F and DLC + Si + F were found to have been successful at improving the printing quality and plate wear of polymer printing plates because the properties were improved compared to those of polymer concave printing plates.

Pulse Electrodeposition and Characterization of Ni-Si3N4 Composite Coatings

  • Gyawali, Gobinda;Woo, Dong-Jin;Lee, Soo-Wohn
    • 한국표면공학회지
    • /
    • 제43권5호
    • /
    • pp.224-229
    • /
    • 2010
  • $Ni-Si_3N_4$ nano-composite coatings were prepared by pulse current (PC) electrodeposition and direct current (DC) electrodeposition techniques. The micro-structure of the coatings was characterized by scanning electron microscopy (SEM), vickers microhardness, X-Ray Diffraction (XRD) and wear-friction tests. The results showed that the micro-structure and wear performance of the coatings were affected by the electrodeposition techniques. Pulse current electrodeposited $Ni-Si_3N_4$ composite coatings exhibited higher microhardness, smooth surface, and better wear resistance properties as compared to coatings prepared under DC condition. The $Ni-Si_3N_4$ composite coatings prepared at 50 Hz pulse frequency with 10% duty cycles has shown higher codeposition of nano-particles. Consequently, increased microhardness and less plastic deformations occurred in coatings during sliding wear test. The XRD patterns revealed that the increased pulse frequencies changed the preferred (100) nickel crystallite orientations into mixed (111) and (100) orientations.

Microstructural Characterization and Plasma Etching Resistance of Thermally Sprayed $Al_2O_3$ and $Y_2O_3$ Coatings

  • Baik, Kyeong-Ho;Lee, Young-Ra
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.234-235
    • /
    • 2006
  • In this study, the plasma sprayed $Al_2O_3$ and $Y_2O_3$ coatings have been investigated for applications of microelectronic components. The plasma sprayed coatings had a well-defined splatted lamellae microstructure, intersplat pores and a higher amount of microcracks within the splats. The plasma sprayed $Y_2O_3$ coating had a relatively lower hardness of 300-400Hv, compared to 650-800Hv for $Al_2O_3$ coating, and would be readily damaged by mechanical attacks such as erosion, wear and friction. For a reactive ion etching against F-containing plasmas, however, the $Y_2O_3$ coating had a much higher resistance than the $Al_2O_3$ coating because of the reduced erosion rate of by-products.

  • PDF