An experimental study was performed to discover the effect of environment on the tribological behavior of Si-incorporated diamond-like carbon(Si-DLC) film slid on a steel ball. The films were deposited on Si(100) wafers by a radio-frequency glow discharge of mixtures of benzene and dilute silane gases. Experiments using a ball-on-disk test-rig was performed in vacuum, dry air and ambient air conditions. It was observed that coefficient of friction decreased as the environment changed from vacuum, to dry air. Chemical analyses of debris suggested that low and stable friction is closely related to the formation of silicon-rich oxide debris and the rolling action.
Lim Jong Hoon;Je Sung Uk;Ryu Shi Hyoung;Chu Chong Nam
International Journal of Precision Engineering and Manufacturing
/
제6권4호
/
pp.44-48
/
2005
As mechanical components are miniaturized, the demands on micro die/mold are increasing. Micro mechanical components usually have high hardness and good conductivity. Micro electrical discharge machining (MEDM) can thus be an effective way to machine those components. In micro cavity fabrication using MEDM, it is observed that the bottom surface of the cavity is distorted. Electric charges tend to be concentrated at the sharp edge, and debris cannot be drawn off easily at the center of the bottom surface. These two phenomena make the bottom surface of electrode and workpiece distort. As machining depth increases, the distorted shape of the electrode approaches hemisphere. This process is affected by both capacitance and the size of electrode. By using a smaller electrode than the desired cavity size and appropriate tool movement, bottom shape distortion can be prevented.
WC-CrC-Ni coatings were prepared by nine processes of the Taguchi program with three levels for the four spray parameters: spray distance, flow rates of hydrogen and oxygen, and powder feed rate. The optimal coating process (OCP) was oxygen flow rate of 38 FMR, hydrogen flow rate of 53 FMR, powder feed rate of 25 g/min, and spray distance of 7 inches. Hardness of 1150 Hv and porosity of 1.2 %, were obtained by OCP; these are better results compared with the highest 1033 Hv and the lowest 1.5 % porosity obtained by nine processes of the Taguchi program. Friction coefficient of the WC-CrC-Ni coating decreased from $0.36{\pm}0.07$ at $25^{\circ}C$ to $0.23{\pm}0.07$ at $450^{\circ}C$. These values were smaller than those of the EHC (electrolytic hard chrome) plating at both temperatures due to lubrication from the oxide debris. The wear trace and wear depth of the coating are smaller than those of the EHC at both temperatures. Pitting was not found in the WC-CrC-Ni coating sample, while it did appear in the EHC sample.
Micron size Co-alloy(T800) powder was coated on Inconel 718 by HVOF thermal spraying for the studies of the improvement of durability of high speed spindle by using Taguchi program for the parameters of spray distance, flow rates of hydrogen and oxygen and powder feed rate. The optimal coating process was determined by the studies of coating properties such as micro-structure, porosity, surface roughness and micro hardness. Friction and wear behaviors of coatings were investigated by sliding wear test at room temperature and $1000^{\circ}F(538^{\circ}C)$. At both room temperature and $538^{\circ}C$ the sliding wear debris and friction coefficients of the coating were drastically reduced compared with the surface of non-coated parent material. This shows that Co-alloy powder coating is highly recommendable for the durability improvement surface coating of high speed air-bearing spindle. At high temperature wear traces and friction coefficients of both coating and non-coating were drastically reduced compared with those of room temperature since the brittle oxides were formed easily on the surface, and the brittle oxide phases were attrited by the reciprocating sliding wear according to the complicated mixed wear mechanisms These oxide particles, partially melts and the melts play role as lubricant and reduce the wear and friction coefficient. This also shows that Co-alloy powder coating is highly recommendable far the durability improvement surface coating on the surface vulnerable to frictional heat such as high speed spindles.
Tripathi, Khagendra;Joshi, Bhupendra;Gyawali, Gobinda;Kim, Seung-Ho;Lee, Soo Wohn
한국표면공학회:학술대회논문집
/
한국표면공학회 2014년도 추계학술대회 논문집
/
pp.182-183
/
2014
Hemispherical dimples with diameter, ø=$60{\mu}m$ and depth, d= $30{\mu}m$ were created on the metal and ceramics surfaces using INYA 10 watt Laser of 1064 nm wavelength. This study reports the influence of dimple pitch on friction and wear behavior rather than dimple size, depth and density. LST was performed on the specimens with dimple pitch and density in the range of 80 to-$200{\mu}m$ and 44 to 7 %, respectively. Surface topography was analyzed by using roughness measurement, scanning electron microscopy (SEM), and optical microscopy. Friction and wear characteristics were analyzed on textured surfaces at lubricating environment to observe the effect of surface texturing on reduction of friction and wear. Reduction on coefficient of friction was achieved by more than 70% due to the dual behavior of dimples as wear (debris) traps and lubricant reservoirs. Wear reduced significantly for the textured surface as compared to the polished surface. Moreover, the friction coefficient of the textured specimens reduced with increasing load and speed which may be attributed to the transition of lubrication regime.
This paper describes an empherical equation which is to predict the engine condition of the supersonic aircraft. The equation, which is a function of running time of engine and engine oil, is derived from the trend analysis of JOAP data. Qualitative analysis is carried out to make up for the weak points in the current JOAP system. Also wear debris collected from the abnormal engine is analyzed by EDS to detect the damaged parts of engine.
R.F. PACVD법을 이용하여, 벤젠을 반응기체로 사용하여 순수한 DLC필름을 증착하였다. DLC필름의 마찰마모특성은 시험 환경을 제어하기 위하여 챔버로 고립된 ball-on-disk형식의 마모시험기를 이용하여 측정하였다. 상대습도에 따른 필름의 마찰특성을 관찰하기 위하여, 상압에서 챔버 내의 습도를 0-90%로 조절하면서 관찰하였다. 그리고 상대면 물질의 영향을 알아보기 위하여 스틸볼과 함께 DLC필름이 코팅된 스틸볼을 사용하였다. 스틸볼을 사용시 습도가 0%에서 90%로 증가함에 따라 마찰계수가 0.025에서 0.2로 크게 증가하였다. Ferich debris가 생성되지 않는 DLC가 코팅된 볼을 사용하여 실험한 경우에, 마찰계수는 상대 습도가 90%인 경우에도 0.08정도로, 스틸볼을 사용하였을 경우보다 훨씬 더 낮은 습도의존성을 보여주었다. 스틸볼 사용시 나타나는 DLC필름의 마찰계수의 큰 습도의존성은 습도가 증가함에 따라 debris의 크기 증가와 함께 스틸볼의 마모로 인한 Fe-rich debris의 생성과 밀접한 관계가 있음을 확인 할 수 있었다. 그리고 스틸볼을 사용하여 90%의 습도에서 마모시험을 하는 중간에 습도를 0%로 변화시키며 관찰한 결과, 마찰계수 값이 급격히 감소하였다. 이와 같은 결과를 통하여, Fe-rich debris가 마찰계수에 미치는 영향은 debris내의 Fe원소가 습도에 매우 민감한 흑연상의 전이층을 형성시킨다는 것을 확인 할 수 있었다.
Damage of hydraulic concrete structures by the abrasion and erosion process is very severe and it indicates that the necessity of considering the influence of this process while designing concrete mixtures. Abrasion wear of concrete in hydraulic structures is caused by the movement of particles, water-borne debris. The resistance against erosion for high-strength self-consolidating concrete(SCC) was examined in this paper. A newly designed testing method is presented in order to quantitatively estimate the erosion of concrete. It was shown that loss of volume in abraded concrete can be explained as function of material parameters such as the amount of fly ash and blast furnace slag. Those admixtures have been widely used to reduce heat of hydration and improve resistance against sulfate attack. The results of current study can be used as a guideline in selecting the composition of concrete exposed to abrasion-wear.
Condition monitoring technology has recently been received much attention in the light of its significance on the maintenance of complex machineries such as turbines in power plants. Currently, turbines in power plants are maintained by scheduled overhaul based on the manufacturer's recommendations and the utility's experience. Although this preventive maintenance is known to be very effective, operators have less access to identify failure of elements when it happens between overhaul period. Therefore, in this study, a development of a on-line condition monitoring system through wear debris analysis of lubricating oils is aimed with a view to detecting abnormal wear behaviour of bearings and other wet-components at an early stage, allowing better outage scheduling and minimizing forced outages. For field application purposes, the on-line system developed was installed on the turbine of the No.4 unit at Ulsan Power Plant and its performance has been evaluated on site.
Surface damage accumulation of alumina ceramics under the cyclic stress state was analyzed. The alternating stress state in repeat pass sliding contact was simulated by a synchronized biaxial (normal and tangential) repeated indentation technique. Wear debris formation mechanism through damage accumulation and fatigue grain failure in both alumina ceramic balls and flat disks was confirmed, and the contact induced surface degradation due to fatigue cracking accumulation was quantified by measuring vertical contact displacement. Variation of structural compliance (slope of load-displacement curve) of two contacting bodies was expressed as a variation of the apparent elastic property, called pseudo-elastic constant, of the contact system.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.