Vicker's hardness and pore size distribution of mortar adhered to the recycled coarse aggregate were tested according to the strength level of original concrete of recycled coarse aggregate to find the change of mortar adhered to the recycled coarse aggregate in cement paste. The strength levels of original concrete of recycled coarse aggregate were 25.5MPa, 41.7MPa and 60.1MPa and the aggregates were used at the state of saturated surface dry condition and oven dry condition. The results of this experimentation indicated that the mean value of Vicker's hardness was increased according to age and strength of original concrete of recycled aggregate. Porosity of $100nm{\sim}10{\mu}m$ size was reduced and porosity of 6nm~100nm size was increased in cement paste.
Quarternary $Li_2O-B_2O_3-Al_2O_3-SiO_2$ glasses were fabricated by the function of $R({\equiv}Li_2Omole%/B_2O_3mole%)$ and $K({\equiv}(Al_2O_3mole%+SiO_2mole%/B_2O_3mole%)$. The structures of these glasses were investigated through refractive index and Vicker's hardness. The refractive index increased as the increase of the polarizability in the glass network. In the region of low $Li_2O$ content, the refractive index increased due to the increase of the polarizability in the glass network but, in the region of high $Li_2O$ content, the rate of increase of the refractive index decreased due to the increase of the molar volume caused by the formation of $BO_3{^-}$ units with relatively high molar volume. And, the refractive index decreased as the increase of $Al_2O_3+SiO_2$ content with the molar volume in the glass network. The increase and decrease of vicker's hardness values for those glasses depended on the fraction of tetrahedral $BO_4$ units and it of triangle $BO_3{^-}$ units with non-bridging oxygen, respectively.
Quarternary $Na_2O-B_2O_3-Al_2O_3-SiO_2$ glasses were fabricated by the function of $R({\equiv}Na_2O\;mole%/B_2O_3\;mole%)$ and $K({\equiv}(Al_2O_3\;mole%+SiO_2\;mole%)/B_2O_3mole%)$. The structures of these glasses were investigated through refractive index and vicker's hardness. The refractive index increased as the increase of the polarizability in the glass network. In the region of low $Na_2O$ content, the refractive index increased due to the increase of the polarizability in the glass network, but in the region of high $Na_2O$ content, the rate of increase of the refractive index decreased due to the increase of the molar volume caused by the formation of $BO_3{^-}$ units with relatively high molar volume. And, the refractive index decreased as the increase of $Al_2O_3+SiO_2$ content with the molar volume in the glass network. The increase and decrease of vicker's hardness values for those glasses depended on the fraction of tetrahedral $BO_4$ units and it of triangle $BO_3{^-}$ units with non-bridging oxygen, respectively.
In this study, we have examined the possibility to improve the material properties and biocompatibility of the 630 stainless steel for the application of medical instruments. The evaluation of mechanical properties and biocompatibility of the 630 stainless steel were studied by aging, nitriding, SEM measurement, Vicker's hardness, tensile strength and MTT cytotoxicity using IGF cells, respectively. The results showed that the tensile strength and Vicker's hardness of 630 stainless steel was increased with aging and ion nitriding time. The cytotoxicities of the 630 stainless decreased compared with the 420 stainless on MTT cytotoxicity using IGF cells. Ion nitriding of 630 stainless led to an enhanced application of medical instruments and biocompatibility performance.
This study compared tooth's remineralization using enamel surface artificially demineralized with 0.1M lactate and HCL solution using Vicker's Hardness Number(VHN) to compare CPP-ACP and remineralization of nano-sized Carbonate Apatite's initial caries. Using pH circulation models divided into 0% nano-CA, 5% nano-CA, 10% nano-CA, 10% CPP-ACP and D.W. they were treated for 5 minutes, three times a day for 14 days to get the following results. 1. There were no significant differences among the initial surface hardness of samples demineralized surface of front tooth in 5 groups. and all 5 groups' surface hardness reduced significantly after demineralization of enamel. 2. When inquiring into hardness changes through pH circulation model, the highest hardness change was in 5% nano-CA group. Also. 10% nano-CA and 10% CPP-ACP groups increased significantly. but there was no significant difference statistically. In generalizing the above experiment results, nano-sized Carbonate Apatite showed remineralization, and compared to 10% CPP-ACP group, 5% nano-CA had remineralization to artificial caries. thus implies that when we develop method to contact with tooth of nano-CA in the future, it is expected to gain synergy effect on function of saliva, a natural remineralization material.
Proceedings of the Korean Vacuum Society Conference
/
2016.02a
/
pp.166.1-166.1
/
2016
각종 부품의 내마모성 및 내식성을 개선하기 위해서 금속물질에 나노두께의 보호막층을 입혀 경도를 높이는 표면처리 기술이 개발되고 있다. TiN막은 기계적 경도, 내마모성 및 내식성이 우수하여 수없이 연구되어 왔으며 박막의 두께에 따라 다양한 색상표현이 가능하다는 연구도 진행되고 있다. 이러한 TiN 박막의 연구결과로 높은 경도와 강도를 요하는 절삭공구에 하드 코팅을 이용하여 높은 절삭력으로 고효율적인 작업환경을 조성할 수 있다. 기존에 연구되어 온 TiN박막은 Ar과 N2의 혼합가스 분위기에서 증착된 반면 본 실험에서는 영구자석을 이용한 고밀도 플라즈마로 높은 점착성과 균일한 박막 및 대면적 공정이 가능한 RF-magnetron sputtering방법을 이용하여 N2 분위기에서 TiN박막을 $100^{\circ}C{\sim}400^{\circ}C$의 온도범위에서 $100^{\circ}C$간격으로 열처리 후 증착하여 비교실험을 하였다. 이와 같이 제작된 TiN박막을 XRD(X-ray Diffraction)를 사용하여 결정성을 확인한 결과 온도가 높을수록 (111)방향의 결정성장이 뚜렷하게 나타났으며 그 외 Scratch Test와 HM-220(Micro-vicker's tester)를 사용하여 경도특성을 확인하고 SEM(Scanning Electron Microscope), AFM(Atomic Force Microscope)를 이용하여 박막의 표면형상을 측정하였다. 이러한 측정 결과로 향후에는 높은 내마모성 및 초경도가 요구되는 절삭공구 및 경질표면코팅이 필요한 금속산업분야에 적용이 가능 할 것이라 사료된다.
Moon, Seong Jun;Kim, Hyun Teh;Shim, Moon Sik;Park, Kwang Ho
Journal of Korean Ophthalmic Optics Society
/
v.7
no.1
/
pp.57-61
/
2002
Ternary $SrO-B_2O_3-SiO_2$ glasses were fabricated as a function of R(${\equiv}SrO\;mole%/B_2O_3\;mole%$) and K(${\equiv}SiO_2\;mole%/B_2O_3\;mole%$). The structures of these glasses were investigated through Infrared transmittance, vicker's hardness, and refractive index. The results indicated : First, in the infrared transmittance spectra, when R increased, the intensities of the absorption bands around $1200{\sim}1600cm^{-1}$ resulting from the B-O stretching vibration bond in the symmetrical trigonal $BO_3$ units decreased, and these of the absorption bands around $800{\sim}1200cm^{-1}$ caused by the B-O stretching vibration bond of the tetrahedral $BO_4$ units varied. Also, the intensities of the absorption bands for the B-O stretching vibration bond in trigonal $BO_3$ units increased and these of the bands for B-O stretching vibration bond in tetrahedral $BO_4$ units decreased as K increased. Second, the increase and the decrease of vicker's hardness values for these glasses depended on the fraction of $BO_4$ units and it of $BO_3$ units, respectively. The refractive index of these glasses mostly depended on the SrO contents and only slightly depended on the fraction of $BO_4$ and $BO_3{^-}$ units.
The purpose of this study was to measure Micro vicker's hardness of 4 kinds of anterior Composite resins (Pyrofil light bond anterior, Lite-fil anterior, Photo clear fil anterior, Silux) and 6 kinds of posterior Composite resin (Pyrofil light bond posterior. Lite-fil posterior, Photo clear fil posterior, Occlusin posterior, Palfique light posterior, P-30, posterior) according to deference of depth and distance of light tip from surface of composite resin. Each composite resin was filled into Teflon tube of 5mm in diameter and 5mm in depth, celluloid matrix was covered and the light in accordance with each composite resin was irradiated in distance of zero millimeter and 1 cm from light tip to surface of composite resin for 30 seconds. Specimens were sectioned longitudinally with cutting device. Microvicker's hardness measurements ware made at the depth of surface, 1mm, 2mm, 3mm, 4mm and 5mm from the surface to deep portion. Vicker's hardness numbers were taken on each depth under 200gm load for 30 seconds with MVK-E. The following results were: 1. The highest hardness value was measured at 1 mm depth. Then the deeper the depth, the lesser the hardness was observed. 2. The hardness value of anterior composite resins is lower than one of posterior composite resins. 3. Hardness number of composite resin irradiated in distance of zero millimeter from surface of composite resin was higher than one of 1 cm from surface of composite resin. 4. The pattern of hardness change at varying depth was similar to all the experimental material with no relation to distance of light from specimen.
The objective of this investigation was to compare the effects of water storage on the aspect of hardness and diametral tensile strengths of four hybrid glass ionomer cements(two compomers and two resin-reinforced glass ionomers) with a resin composite material. One composite resin(Degufill Ultra), two compomers(Dyract, Compoglass Cavifil), and two resin-reinforced glass ionomers(Fuji Duet, Vitremer) were used in this study. Cylindrical specimens were prepared and stored at $36{\pm}1^{\circ}C$ in distilled water for 10 minutes after set, and then tested on an Instron testing machine(No.4467) at 1.0 mm/min displacement rate. Vicker's hardness and diametral tensile strengths as time elapsed were measured after aging in water for 10 minutes, 1 hour, 3 hours, 1 day, 3 days, 5 days and 7 days at $36{\pm}1^{\circ}C$. During the test of diametral tensile strength, stress-strain curves were obtained, from which the compressive modulus were calculated and compared. The structure of four set glass ionomer cement mass was observed on SEM(Hitachi, S-2300) after being etched with 9.6% hydrofluoric acid for 1 minute. The results were as follows; 1. The hardness of the experimental group(compomer and the resin reinforced glass ionomer cement) did not exceed the value of control group(Degufill Ultra). 2. Vicker's hardness of the Fuji Duet tended to increase succeedingly, Dyract was decreased after 3 hours in water, and Vitremer was the lowest. 3. The control group(Degufill Ultra) presented progressively on increased diametral tensile strength with time, Fuji Duet were decreased after 3 days, Compoglass Cavifil and Vitremer were decreased after 5 days in water storage. 4. Compressive modulus of the control group(Degufill Ultra) and Dyract were increased sharply timely, Fuji Duet and Vitremer were increased smoothly by lapse of time in water. Fuji Duet were stronger than Vitremer. On the other hand, Vitremer exhibited the lowest toughness. 5. The microstructure of compomer was similar with that of the composite resin(Degufill Ultra), and the fillers in resin-reinforced glass ionomer cements were noticed. It can be concluded that mechanical properties of hybrid glass ionomer cements is weaker than composite resin, and that the compomers or the resin-reinforced glass ionomers can not substitute the composite resins. A plenty of considerations should be done on the application of them to the area under the loading and high wear has a little adverse effect on the mechanical properties on the water storage for 7 days. The further research should be needed to confirm the advantage of the compomer.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.