• 제목/요약/키워드: Ultra-Fine Powder

검색결과 148건 처리시간 0.025초

AACH 를 이용한 고순도 알루미나 분말 제조 (Preparation of Ultra Fine Alumina Powder Via Ammonium Aluminium Carbonate Hydroxide)

  • 주돈;신건철
    • 산업기술연구
    • /
    • 제24권B호
    • /
    • pp.65-71
    • /
    • 2004
  • The ultra fine gamma-alumina powder was prepared via ammonium aluminium carbonate hydroxide (AACH). The XRD, SEM, BET, thermal analysis were used to characterize the samples. The effects of various reaction parameters as concentration, of solution, anion on specific area, PH, aging time and thermal decomposition condition on the produced AACH and alumina were discussed.

  • PDF

전자렌지를 이용한 초미세 대두분말두부의 신속제조 (Rapid Preparation of Soybean Curd Using of Ultra Fine Soy Powder by Microwave Oven)

  • 김순동;김미경;김미향;이명숙
    • 동아시아식생활학회지
    • /
    • 제4권2호
    • /
    • pp.45-49
    • /
    • 1994
  • The rapid preparaton method of soybean curd with ultra fine soy powder at home was investigated. The microwave oven of this study used common microwave attached sensor for the volume and temperature control, The temperature of the microwave oven was maintained at 98, not boiling over. It took 9 minutes to make 300g of soybean curd, 10 minutes to make 600g, 14 minutes to make 900g, and 17 minutes to make 1200g. Beany flavor and trypsin inhibitor could be removed by this conditon. It took only 5 min to make coaguation of the curd by glucono-$\delta$-lactone.

습식직접합성 Ferrite 분말의 전파흡수능 (Microwave Absorption of Ferrite Powders by Wet-Direct Synthesis)

  • 남경호;이경희;이병하
    • 한국세라믹학회지
    • /
    • 제28권11호
    • /
    • pp.843-850
    • /
    • 1991
  • There is a growing demend for absorptive electromagentic shielding materials for wide band frequency application. In this study, the absorber which consists of a rubber plus Ni-Zn ferrite which have been prepared by direct-wet method. A rubber ferrite composite for electromagnetic shielding, it is most importan facter the homogeneous ultra fine size and high dispersitive ferrite powder. Direct-wet method and solid-solid reaction method for preparing of ultra fine ferrite powder was used. It has been experimentally verified that the powder which prepared by direct-wet method was very fine and almost same size spherical powder, the composite ferrite have excellent electromagnetic wave absorption in X-band.

  • PDF

Development of Granulated Powders by SUS316L Ultra Fine Powder

  • Kadomura, Takeshi;Maeta, Yu;Otuka, Isamu
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.733-734
    • /
    • 2006
  • Granulated powders, prepared from PF-5F($D_{50}=4(\mu}m$), PF-10F($D_{50}=6{\mu}m$) and PF-20F($D_{50}=10{\mu}m$) water atomized powder, were compacted, debound and sintered to evaluate the properties of sintered parts. As a result, the relative sintered density of about 97% at sintering temperature of 1423K was obtained. It can be considered that by using granulated finer particle size powder, mechanical properties of sintered parts were also improved.

  • PDF

수열반응으로 합성한 Hydroxyapatite 초미분말의 소결특성 (Sintering Behavior of Ultra-fine Hydroxyapatite Powders Synthesized by Hydrothermal Reaction)

  • 최재웅;조성원;최상홀
    • 한국세라믹학회지
    • /
    • 제31권11호
    • /
    • pp.1265-1270
    • /
    • 1994
  • Ultra-fine hydroxyapatite powder were synthesized by the hydrothermal reaction at 10 atm, 3 hrs of Ca(OH)2 suspension with (NH4)2HPO4 solution, and were characterized sintering behavior. Sintered bodies of hydroxyapatite powders which synthesized by hydrothermal reaction method has less weight loss, less sintering shrinkage and superior mechanical property, and was more dense than sintered bodies of hydroxyapatite powder which synthesized by wet method. Sintered bodies were hydroxyapatite single phase. When soack in Ringer's solution for 2 weeks, hydroxyapatite powders preserved hydroxyapatite and sintered body absorbed trace of Ca2+ ion with soaked time.

  • PDF

Ultra Fine Soft Magnetic Powders Produced by High Pressure Water Atomization Process

  • Watanabe, Atsushi;Otsuka, Isamu;Wada, Kimio
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.794-795
    • /
    • 2006
  • Metal powder for dust core application was developed. The powder can be produced improved high-pressure water atomization process. The process has produced powder of spherical shape and lower coercivity. The dust core obta ined shows lower core loss.

  • PDF

난각으로부터 합성된 초미립 CaO 분말을 이용한 C3S, C2S, C3A 분말 합성 및 혼합 경화체에 미치는 C3A 함량의 영향 (Synthesis of C3S, C2S, C3A Powders using Ultra-fine Calcium Oxide Powder Synthesized from Eggshell and Effect of C3A Content on Hardened Mixed Aggregates)

  • 공헌;권기범;박상진;노효섭;이상진
    • 한국분말재료학회지
    • /
    • 제26권6호
    • /
    • pp.493-501
    • /
    • 2019
  • In this work, ultra-fine calcium oxide (CaO) powder derived from eggshells is used as the starting material to synthesize mineral trioxide aggregate (MTA). The prepared CaO powder is confirmed to have an average particle size of 500 nm. MTAs are synthesized with three types of fine CaO-based powders, namely, tricalcium silicate (C3S), dicalcium silicate (C2S), and tricalcium aluminate (C3A). The synthesis behavior of C3S, C2S and C3A with ultra-fine CaO powder and the effects of C3A content and curing time on the properties of MTA are investigated. The characteristics of the synthesized MTA powders are examined by X-ray diffraction (XRD), field emission-scanning electron microscope (FE-SEM), and a universal testing machine (UTM). The microstructure and compressive strength characteristics of the synthesized MTA powders are strongly dependent on the C3A wt.% and curing time. Furthermore, MTA with 5 wt.% C3A is found to increase the compressive strength and shorten the curing time.

초미세 느릅 분말의 항산화 활성 연구 (Antioxidant Activities of Powdered and Ultra-fine Powdered Ulmus Davidiana var. Japonica)

  • 박재호;안정좌
    • 한국지역사회생활과학회지
    • /
    • 제27권3호
    • /
    • pp.343-350
    • /
    • 2016
  • The antioxidant activity was examined on ultra-fine powdered (UFP) Ulmus davidiana (U. davidiana) var. japonica. The average particle size of UFP or commercial powdered (CP) was $1-3{\mu}m$ or $100{\mu}m$. The extraction was performed using either ethanol (EtOH) or hot-water. Contents of phenolic compound of CP and UFP U. davidiana extracts in EtOH was 40.38 and 65.61 mg/g, respectively. In DPPH, EtOH extract of UFP U. davidiana showed a significantly greater activity than hot-water extract at 40 and $200{\mu}g/mL$. At $200{\mu}g/mL$, the activity was over 90% in all groups. The reducing power of UFP U. davidiana var. japonica in EtOH extraction was 74.3%, which was significantly greater than in other samples (p<0.05). In addition, reducing powder was significantly higher in UFP-EtOH than in other samples at all concentrations except for $0.32{\mu}g/mL$. The above results suggest that EtOH extraction of U. davidiana showed slightly higher DPPH radical scavenging activity, and ultra-fine powder of U. davidiana extracts may show higher antioxidative activities based on reducing power.