The Variation of Mechanical Properties by Thermomechanical Treatment in Fe-30%Ni-0.1 %C Alloy (가공열처리에 의한 Fe-30% Ni-0.1%C 합금의 기계적성질 변화)

  • Ahn, H.K.;Kim, H.S.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.7 no.2
    • /
    • pp.88-95
    • /
    • 1994
  • In order to compare mechanical properties of ausformed martensite with those of marformed martemsite in Fe-30%Ni-0.1%C alloy and to investigate their strengthening mechanisms, ausformed martensite and marformed martensite were prepared by ausforming treatment and marforming treatment respectively. The microstructures were observed and the quantities of retained austenite, hardness, yield strength, ultimate tensile strength and elongation were examined. The strength of ausformed martensite was mainly increased because of the lattice defects inherited from austenite. The ductility of ausformed martensite was constant at the rate of 7-8% by ductile matrix formation of the retained austenite in spite of the increase in strength. The strength of marformed martensite was increased by the increment in dislocation density, the crossing of transformation twin with deformation twin and the mutual crossing of deformation twin. The ductility of mar formed martensite was slightly lower than that of ausformed martensite, but the strength of mar formed martensite was prominently higher.

  • PDF

Ultimate Fracture Strength Analysis of Initially Cracked Plate (초기균열을 가진 판의 최종파괴 강도해석)

  • 백점기;서흥원
    • Proceedings of the Computational Structural Engineering Institute Conference
    • /
    • 1991.10a
    • /
    • pp.133-138
    • /
    • 1991
  • The aim of the present paper is to develop a computer program predicting ultimate fracture strength of initially cracked structure under monotonically increasing external loads. For this purpose, two kinds of 3-D isoparametric solid elements, one 6-node wedge element and another 8-node brick element are formulated along the small deformation theory. Plasticity in the element is checked using von Mises' yield criterion. Elasto-plastic stiffness matrix of the element is calculated taking account of strain hardening effect. If the principal strain at crack tip which is one nodal point exceeds the critical strain dependin on the material property, crack tip is supposed to be opened and the crack tip node which was previously constrained in the direction perpendicular to the crack line is released. After that, the crack lay be propagated to the adjacent node. Once a crack tip node is fractured, the energy of the newly fractured node should be released which is to be absorbed by the remaining part. The accumulated reaction force which was carried by the newly fractured node so far is then applied in the opposite direction. During the action of crack tip relief force, since unloading may be occured in the plastic element, unloading check should be made. If a plastic element unloads, elastic stress-strain equation is used in the calculation of the stiffness matrix of the element, while for a loading element, elasto-plastic stress-strain equation is continuously used. Verification of the computer program is made comparing with the experimental results for center cracked panel subjected to uniform tensile load. Also some factors affecting ultimate fracture strength of initially cracked plate are investigated. It is concluded that the computer program developed here gives an accurate solution and becomes useful tool for predicting ultimate fracture load of initially cracked structural system under monotonically increasing external loads.

  • PDF

Flexural Tensile Strength of Concrete Block Masonry (비보강 콘크리트 조적조의 휨인장강도)

  • Kim, Young-Sang
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.9 no.4
    • /
    • pp.119-126
    • /
    • 2005
  • The objective of this paper is to evaluate the flexural tensile strength of unreinforced concrete masonry wall to ensure the structural safety in out-of-plane behaviors under the wind or earthquake loads. Flexural tensile strength of unreinforced concrete masonry wall has been obtained from the full scale tests of total 327 specimens and the statistical analysis are performed for each of the cases. The flexural tensile strength derived from experiments is classified as 13 groups according to masorny units, mortar ingredients, and the direction of tensile stresses and the mean tensile strength and the variable coefficient are obtained for each case. The uniform and concentrated transverse loads have been applied over the face of the wall specimens. The ultimate mean flexural tensile strengths are distributed from 1,564 kPa to 363 kPa according to masonry units, mortar ingredients, and other factors. The allowable flexural tension stress criteria will be established based on the mean flexural tensile strengths in the future.

Design and ultimate behavior of RC plates and shells: two case studies

  • Min, Chang-Shik
    • Structural Engineering and Mechanics
    • /
    • v.14 no.2
    • /
    • pp.171-190
    • /
    • 2002
  • Two cases of design are performed for the hyperbolic paraboloid saddle shell (Lin-Scordelis saddle shell) and the hyperbolic cooling tower (Grand Gulf cooling tower) to check the design strength against a consistent design load, therefore to verify the adequacy of the design algorithm. An iterative numerical computational algorithm is developed for combined membrane and flexural forces, which is based on equilibrium consideration for the limit state of reinforcement and cracked concrete. The design algorithm is implemented in a finite element analysis computer program developed by Mahmoud and Gupta. The amount of reinforcement is then determined at the center of each element by an elastic finite element analysis with the design ultimate load. Based on ultimate nonlinear analyses performed with designed saddle shell, the analytically calculated ultimate load exceeded the design ultimate load from 7% to 34% for analyses with various magnitude of tension stiffening. For the cooling tower problem the calculated ultimate load exceeded the design ultimate load from 26% to 63% with similar types of analyses. Since the effective tension stiffening would vary over the life of the shells due to environmental factors, a degree of uncertainty seems inevitable in calculating the actual failure load by means of numerical analysis. Even though the ultimate loads are strongly dependent on the tensile properties of concrete, the calculated ultimate loads are higher than the design ultimate loads for both design cases. For the cases designed, the design algorithm gives a lower bound on the design ultimate load with respect to the lower bound theorem. This shows the adequacy of the design algorithm developed, at least for the shells studied. The presented design algorithm for the combined membrane and flexural forces can be evolved as a general design method for reinforced concrete plates and shells through further studies involving the performance of multiple designs and the analyses of differing shell configurations.

Mechanical Properties of Precious Metal-Ceramic Alloy Joined by the Laser-Welding and the Soldering Method (레이저 용접과 납착법으로 연결된 귀금속성 금속-도재 합금의 물리적 성질)

  • Oh, Jung-Ran;Lee, Seok-Hyung;Woo, Yi-Hyung
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.19 no.4
    • /
    • pp.269-279
    • /
    • 2003
  • This study investigated the mechanical properties of precious metal-ceramic alloy joined by the laser-welding and the soldering compared with the parent metal. Twenty-four tensile specimens were cast in precious metal-ceramic alloy and divided into three groups of eight. All specimens in the control group(group 1) were left in the as-cast condition. Group 2 and 3 were the test specimens, which were sectioned at the center. Eight of sectioned specimens were joined by soldering with a propane-oxygen torch, and the remaining specimens were joined by laser-welding. After joining, each joint diameter was measured, and then tested to tensile failure on an Instron machine. Failure loads were recorded, and then fracture stress(ultimate tensile strength), 0.2% yield strength and % elongation calculated. These data for three groups were subjected to a one-way analysis of variance(ANOVA). Neuman-Keuls post hoc test was then used to determine any significant differences between groups. The fracture locations, fracture surfaces were examined by SEM(scanning electron microscope). The results were as follows: 1) The tensile strength and 0.2% yield strength of the soldered group($280.28{\pm}49.35MPa$, $160.24{\pm}26.67MPa$) were significantly less than both the as-cast group($410.99{\pm}13.07MPa$, $217.82{\pm}17.99MPa$) and the laser-welded group($383.56{\pm}59.08MPa$, $217.18{\pm}12.96MPa$). 2) The tensile strength and 0.2% yield strength of the laser-welded group were about each 98%, 99.7% of the as-cast group. There were no statistically significant differences in these two groups(p<0.05). 3) The percentage elongations of the soldered group($3.94{\pm}2.32%$) and the laser-welded group($5.06{\pm}1.08%$) were significantly less than the as-cast group($14.25{\pm}4.05%$) (p<0.05). 4) The fracture of the soldered specimens occurred in the solder material and many porosities were showed at the fracture site. 5) The fracture of the laser-welded specimens occurred also in the welding area, and lack of fusion and a large void was observed at the center of the fracture surface. However, the laser-welded specimens showed a ductile failure mode like the as- cast specimens. The results of this study indicated that the tensile strengths of the laser-welded joints were comparable to those of the as-cast joints and superior to those of the soldered joints.

A Study on the Elasto-Plasticity Behaviour According to the Yield Strength of a Ship's Plate (항복강도에 따른 선체판의 탄소성거동에 관한 연구)

  • 고재용;박주신
    • Proceedings of the Korean Institute of Navigation and Port Research Conference
    • /
    • 2003.05a
    • /
    • pp.27-31
    • /
    • 2003
  • Recently, buckling is easy to happen as that High tensile steel that is the thin plate absence is used comprehensively for the structure. Specially, buckling is getting into important design standard in hull construction which use High tensile steel. Therefore, that grasp conduct exactly after buckling is important in stability of hull structure. In this study, examined closely about conduct and secondary buckling after initial buckling of thin plate structure which receive compressive load according to various kinds yield strength under simply supported condition that make by buckling strength formula standard in each payment in advance rule to place that is representative construction of hull in this research. Analysis method is F.E.M by ANSYS and complicated nonlinear behaviour to analyze such as secondary buckling in used arc-length method.

  • PDF

Comparison and prediction of seismic performance for shear walls composed with fiber reinforced concrete

  • Zhang, Hongmei;Chen, Zhiyuan
    • Advances in concrete construction
    • /
    • v.11 no.2
    • /
    • pp.111-126
    • /
    • 2021
  • Concrete cracking due to brittle tension strength significantly prevents fully utilization of the materials for "flexural-shear failure" type shear walls. Theoretical and experimental studies applying fiber reinforced concrete (FRC) have achieved fruitful results in improving the seismic performance of "flexural-shear failure" reinforced concrete shear walls. To come to an understanding of an optimal design strategy and find common performance prediction method for design methodology in terms to FRC shear walls, seismic performance on shear walls with PVA and steel FRC at edge columns and plastic region are compared in this study. The seismic behavior including damage mode, lateral bearing capacity, deformation capacity, and energy dissipation capacity are analyzed on different fiber reinforcing strategies. The experimental comparison realized that the lateral strength and deformation capacity are significantly improved for the shear walls with PVA and steel FRC in the plastic region and PVA FRC in the edge columns; PVA FRC improves both in tensile crack prevention and shear tolerance while steel FRC shows enhancement mainly in shear resistance. Moreover, the tensile strength of the FRC are suggested to be considered, and the steel bars in the tension edge reaches the ultimate strength for the confinement of the FRC in the yield and maximum lateral bearing capacity prediction comparing with the model specified in provisions.

Failure Properties of Common Tendon Origins at the Human Elbow after Static and Repetitive Loading (정적 및 반복하중 시의 주관절 Tendon의 파괴 물성치 측정)

  • Han, Jeong-Su;Lee, Gwan-Hui;Yu, Jae-Yeong
    • Journal of Biomedical Engineering Research
    • /
    • v.19 no.4
    • /
    • pp.393-401
    • /
    • 1998
  • Based on clinical observations, it is suspected that the bone-tendon origin is the site where piratical failure, leading to pathophysiological changes in the humeral epicondyle after repetitive loading, is initiated Mechanical properties and failure patterns of the common extensor and flexor tendons of the humeral epicondyle under static and repetitive loading have not been well documented. Our goal was to determine mechanical properties of failure strength and strain changes, to correlate strain changes and the number of cyclic repetitions, and to identify the failure pattern of bone-tendon specimens of common extensor and flexor tendons of the humeral epicondyle. Mechnaical properties of human cadaver bone-tendon specimens of the common extensor and flexor tendons of the humeral epicondyle were tested under two different loading rates. No statistically significant difference in ultimate tensile strength was found between male and female specimens or between slow (10 mm/sec) and fast elongation (100 mm/sec) rates. However, a statistically significant difference in ultimate tensile strength between the common extensor (1190.0 N/$cm^2{\pm}$388.8) and flexor 1922.0 N/$cm^2{\pm}$764.4)tendons was found (p<0.05). When loads of 25%, 33%, and 41% of the ultimate tensile strength of their contralateral sides were applied, the number of cycles required to reach 24% strain change for the common extersor and flexor tendons were approximately 8,893, 1,907, and 410, respectively. The relationship between cycles and loads was correlated ($R^2$=0.46) Histological observation showed that complete or partial failure after tensile or cyclic loadings occurred at the transitional zone, which is the uncalcified fibrocartilage zone between tendon and bone of the humeral epicondyle. Sequential histological sections revealed that failure initiated at the upper, medial aspect of the extensor carpi radialis brevis tendon origin. Biomechanical and hstological data obtained in this study indicated that the uncalcified fibrocartilage zone at the bone-tendon origin of the common extensor and flexor tendons is the weak anatomical structure of the humeral epicondyle.

  • PDF

The effect of neutron irradiation on hydride reorientation and mechanical property degradation of zirconium alloy cladding

  • Jang, Ki-Nam;Kim, Kyu-Tae
    • Nuclear Engineering and Technology
    • /
    • v.49 no.7
    • /
    • pp.1472-1482
    • /
    • 2017
  • Zirconium alloy cladding tube specimens were irradiated at $380^{\circ}C$ up to a fast neutron fluence of $7.5{\times}10^{24}n/m^2$ in a research reactor to investigate the effect of neutron irradiation on hydride reorientation and mechanical property degradation. Cool-down tests from $400^{\circ}C$ to $200^{\circ}C$ under 150 MPa tensile hoop stress were performed. These tests indicate that the irradiated specimens generated a smaller radial hydride fraction than did the unirradiated specimens and that higher hydrogen content generated a smaller radial hydride fraction. The irradiated specimens of 500 ppm-H showed smaller ultimate tensile strength and plastic strain than those characteristics of the 250 ppm-H specimens. This mechanical property degradation caused by neutron irradiation can be explained by tensile hoop stress-induced microcrack formation on the hydrides in the irradiation-damaged matrix and subsequent microcrack propagation along the hydrides and/or through the matrix.

A New Model for Nonlinear Analysis of Prestressed Concrete Members Subjected to Torsion (비틀림하중을 받는 프리스트레스트 콘크리트 부재의 새로운 비선형 해석모델)

  • 오병환;박창규
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1993.10a
    • /
    • pp.290-295
    • /
    • 1993
  • The purpose of the present study is to propose a realistic method to analyze the prestressed concrete members subjected to pure torsion. The present study device a method to realistically take into account the tensile stiffness of concrete after cracking. The effect of biaxial compressive and tensile loading on the compressive and tensile strength of concrete is also taken into account in the present model. The present model can predict not only the service load behavior, but also up to the behavior of ultimate load stages. The comparison of the present theory with experimental data indicates that the proposed model dipicts reasonably well the actual behavior of prestressed concrete members.