• Title/Summary/Keyword: UV curing resin

Search Result 73, Processing Time 0.018 seconds

A Study on the Development of BIPV Module Equipped with Vacuum Glass for Improved Thermal Performance (단열성능 개선을 위한 진공유리가 부착된 BIPV Module 개발에 관한 연구)

  • Eom, Jae-Yong;Lee, Hyun-Soo;Suh, Seung-Jik
    • Journal of the Korean Solar Energy Society
    • /
    • v.34 no.2
    • /
    • pp.44-52
    • /
    • 2014
  • The main purpose of this paper is to develop the new BIPV module equipped with vacuum glass. Beacuse BIPV module has a function of architectural materials, thermal and PV performance should be simultaneously evaluated. To improve the thermal performance of BIPV module, this study developed BIPV module equipped with a vacuum glass. Those BIPV module was tested with a variety of encapsulants. The results are as follows. When a vacuum glass is laminated with EVA or PVB, it was broken. The reason seems to be bending by unbalance of heat expansion with center and edge of vacuum glass. In case of lamination with resin, there is no breakage and no bending of vacuum glass. Because production was conducted in low pressure & low temperature conditions. And it was also found that vacuum glass does not interfere with the UV curing process.

Effect of Washing Solvent and Washing Method on Flexural Strength of 3D-Printed Temporary Resin Material (세척 용액 및 세척 방법이 3D 프린팅 임시수복용 레진의 굴곡강도에 미치는 영향)

  • Hae-Bom Kim;Jae-Won Choi
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.27 no.2_2
    • /
    • pp.389-395
    • /
    • 2024
  • The purpose of this study was to evaluate the effect of different washing solvents and washing methods on the flexural strength of 3D printed temporary resin. A bar(25 × 2 × 2 mm) was produced with a layer thickness of 50 ㎛ using an LCD-type 3D printer and divided into 15 groups(n = 10, each) according to washing solution(IPA; 99% isopropyl alcohol, TPM; 93% Tripropylene glycol monomethylether, ETL; Ethanol, TWC; Twin 3D Cleaner, and DNC; DIO navi Cleaner) and washing method(Dip; Dip washing, Ultra; Ultrasonic washing, and Auto; Automated washing). All groups were washed for 5 minutes, and post-cured for 5 minutes using a UV LED light curing machine. The Flexural strength was measured using a three-point bending test using a universal testing machine. For statistical analysis, one-way ANOVA, Tukey HSD post hoc test, Kruskal-Wallis test and post-hoc by Bonferroni-Dunn test(𝛼=.05) were performed depending on whether the normality test was satisfied. In all washing solvents except TPM and DNC, the Dip group showed the lowest flexural strength values, while the Auto group showed the highest flexural strength values except for DNC. Additionally, the washing solution showed completely different flexural strength values depending on the washing method.

Solvent-free UV-curable Acrylic Adhesives for 3D printer build sheet (3D 프린터 빌드시트용 무용제 UV 경화형 아크릴 점착제의 제조)

  • Lee, Bae Hwa;Park, Dong Hyup;Kim, Byung Jick
    • Journal of Adhesion and Interface
    • /
    • v.21 no.3
    • /
    • pp.93-100
    • /
    • 2020
  • 3D printing technology enables proper objects to be made through an additive manufacturing method, but resulting in dimension deviation of the product due to contraction phenomenon as cooling melted filament resin injected from high-temperature use environment. In this research, we studied on acrylic adhesives for 3D printer build sheet in order to fabricate high-quality products with a precise shape and to well-mount without distortion. The solvent-free UV-curable acrylic adhesive formulation was designed by adding 4-acryloylmorpholine (ACMO) with high adhesion, toughness, glass transition temperature so that adhesion properties are stable at high temperature and products are easily mounted/detached from the adhesives. The designed formulation was polymerized through two-steps using post-addition of monomers. Using this, the acrylic adhesive was coated to make a film and then analyzed using various experimental techniques. As a result, the fabricated adhesive exhibited high glass transition temperature and there was little gap in peel strength before and after thermal treatment. Moreover, it was confirmed by rheological analysis that this adhesive can provide great bonding/debonding ability without distortion. We demonstrated the fabrication of a rectangular product using a 3D printing method using our acrylic adhesive as a build sheet. Mounting ability and workability were satisfactory and dimension deviation of the product was tiny. Because the product is easily detachable from the acrylic adhesive developed here than conventional build sheets, it is expected that this will provide work convenience to users who use the 3D printer.