Journal of the Korean Crystal Growth and Crystal Technology
/
v.29
no.3
/
pp.123-131
/
2019
In this study, the development of transparent UV blocking material using $TiO_{2-x}$ oxide thin film process was developed. A process technology is related to a process technology for making a sample with ultraviolet-shielding property of visible light transmittance of 78 % or more (total light transmittance at 550 nm) and of a UV cut-off characteristic of more than 95 % at 315 nm in ultraviolet wavelength band. In this study, it is possible to establish a flexible device process condition of high performance ultraviolet (UV) shielding thin film, to design mixed type of transparent flexible device with heterogeneous characteristics and to formulate composite deposition technology, according to various market demands. Establishment of actual roll-to-roll continuous process and equipment and process technology will affect related industries greatly.
Proceedings of the Korean Vacuum Society Conference
/
2016.02a
/
pp.312.1-312.1
/
2016
We have deposited ZnO thin films by ultraviolet (UV) enhanced atomic layer deposition using diethylznic (DEZ) and water (H2O) as precursors with UV light. The atomic layer deposition relies on alternating dose of the precursor on the surface and subsequent chemisorption of the precursors with self-limiting growth mechanism. Though ALD is useful to deposition conformal and precise thin film, the surface reactions of the atomic layer deposition are not completed at low temperature in many cases. In this experiment, we focused on the effects of UV radiation during the ALD process on the properties of the inorganic thin films. The surface reactions were found to be complementary enough to yield uniform inorganic thin films and fully react between DEZ and H2O at the low temperature by using UV irradiation. The UV light was effective to obtain conductive ZnO film. And the stability of TFT with UV-enhanced ZnO was improved than ZnO by thermal ALD method. High conductive UV-enhanced ZnO film have the potential to applicability of the transparent electrode.
In the paper, we have demonstrated an azobenzene-coated fiber Bragg grating (FBG) for monitoring ultraviolet light (UV) intensity in remote measurement. The elasticity of the coated azobenzene polymer is changed by the UV light, which induces a center wavelength change corresponding to the change of the FBG's grating period. The wavelength shift resulting from both UV light and other light with the wavelength out of the UV range was about 0.18 nm. In order to improve the accuracy of the measurement, the center wavelength shift caused by radiant heat of the light source was sufficiently removed by using a thermal filter. The amount of the center wavelength shift was consequently reduced to 0.06 nm, compared to the result without the thermal filter. Also, the FBGs coated by using azobenzene polymer were produced by two different methods; thermal casting and UV curing. Considering temperature dependence, UV curing is more suitable than thermal casting in UV sensor application of the azobenzene-coated FBG. In addition, we have confirmed the wavelength dependence of the optical sensor by means of four different band pass filters. Thus, we found out that the center wavelength shift per unit intensity is 0.029 [arb. unit] as a maximum value at 370 nm wavelength region and that the absorption spectrum of the azobenzene polymer was very consistent with the wavelength dependence of the azobenzene-coated FBG.
Kim, Woo Young;Kim, Chan-Young;Kim, Hyun-Kyoung;Ahn, Tae-Jung
Korean Journal of Optics and Photonics
/
v.26
no.2
/
pp.83-87
/
2015
This study was focused on developing an optical sensor that monitors ultraviolet (UV) light. Recently, we proposed and demonstrated a novel, highly sensitive UV sensor based on a fiber Bragg grating (FBG). To ensure that the incident UV light is focused on the FBG surface, the sensor was coated with an azobenzene polymer material that acts as a UV-induced stretchable functional material, in combination with a cylindrical focal lens. In this study we have improved the sensitivity of the sensor by employing a cylindrical focal mirror as a curved reflector, to refocus the UV light passing through the FBG. We considered the performance of several different types of reflectors and chose the optimal radius of curvature for the reflector. Compared to the UV sensor without an auxiliary device, the sensitivity of the FBG sensor with a focal lens and a curved reflector was 15 times as high.
Journal of the Society of Cosmetic Scientists of Korea
/
v.17
no.1
/
pp.1-17
/
1991
Multiport-600 Solar SimulatorR is one of the most recent and convenient in-strument for evaluation of sun protection factor(SPF). In this study, we examined the practicability of the SPF determining system using Multiport -600 and the effects of several factors-light sources, seasons and experimental animals-on the minimal erythema dose(MED) and SPF. We also tested the UV sensitivity according to the sites of Korean people, And the ultraviolet radiation reaching the earth's surface In Seoul have been observed for one year. As a result of this study, the determinig system for SPF using Multiport-600 was proved to be a good system in accuracy and time-saving. The biological activity of fluorescence UV lamp of PUVA-800R was significantly higher than natural light or solar simulator with Xe arc lamp, and the determined MED became lower in inverse proportion to room temperature rise. Skin sensitivity by ultraviolet adiation was hights. in order \circled1 back \circled2 inns, upper arm \circled3 outer upper arm \circled4 foream. We also observed that UV radiation intensity was highest at noon in july and 1 sun burn unit(MED) was 28 minutes at that time.
Kim, Dong-Yeon;Lee, Gwang-Young;Kang, Hoo-Won;Yang, Cheon-Seung
Journal of Technologic Dentistry
/
v.42
no.3
/
pp.208-212
/
2020
Purpose: This study aimed to analyze the shrinkage and expansion strain of ultraviolet (UV)-cured resin according to the wavelength of the light source and compare the shrinkage and expansion. Methods: We prepared the mold with according to the ISO 4049 specimen. The size of the circle in the mold was prepared with a height of 6.02 mm and a diameter of 4 mm. UV-curable resin for three-dimensional (3D) printing was injected into the circular mold. The control group was irradiated with a wavelength of 400~405 nm using UV-curing equipment (400 group), and the experimental group was irradiated with a wavelength of 460~465 nm (460 group). Both groups were produced ten specimens. The produced specimen was first measured with a digital micrometer. After the first measurement, the specimen was immersed in a constant temperature water bath for 15 days, after which the second measurement was performed, and the third measurement was taken after 30 days. The measured values were analyzed using the independent sample t-test (α=0.05). Results: In the non-immersion water tank, the contraction was 0.9% in the 400 group and 1.3% in the 460 group. In the constant temperature bath, the expansion was high at -0.4% in the 400 group for 15 days, and the smallest expansion was -0.03% for the 400 group for 30 days. There were significant differences between the two groups (p<0.05). Conclusion: The 400 group had a lower UV resin specimen strain than the 460 group. Therefore, it is recommended to use the wavelength required by the UV-curing resin.
$KSrPO_4$ and $Sr_3(Al_2O_5)Cl_2$ phosphors doped with $Eu^{2+}$ emit a blue and orange-yellow luminescence under ultraviolet (UV) excitation at ~ 400 nm, respectivel, which can be used for making white light emitting diodes.
The external electrode fluorescent lamp(EEFL) has recently been applied to backlight of LCD TV as a new light source. The dependence of the electro-optic characteristics of the EEFL used in direct-lit backlights on the glass thickness was examined in detail, and the ultraviolet(UV)-light efficiency was estimated. It was found that the lamp efficiency became larger as the glass thickness decreased if other conditions were the same.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
1998.06a
/
pp.113-116
/
1998
In this paper, we studied the electro-optical(EO) performance of photo-aligned twisted nematic(TN)-liquid crystal display(LCD) with oblique non-polarized ultraviolet(UV) light irradiation on polyimide(Pl) surface. We observed that the voltage-transmittance and response time characteristics of photo-aligned TN-LCD is almost same compared to conventional TN-LCD. Also, we observed that the voltage-holding-ratio(VHR) of photo-aligned TN-LCD is almost same compared to conventional TN-LCD.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.11
no.6
/
pp.481-485
/
1998
We investigated the generation of high pretilt angle for nematic liquid crystal (NLC) in a cell with obilique non-polarized ultraviolet (UV) light irradiation on mixtured polyimide surface. It was found that the monodomain alignment of NLC is obtained with an angle of incidence of 75∼85 degrees on PI surface. We consider that the monodomain alignment of NLC is attributed to anisotropic dispersion force effect to photo-depolymerization of polymer. We successfully observed that the pretilt angle of NLC is generated above 5 degree with an angle of incidence of 75∼85 degrees. It is considered that the pretilt angle generation NLC is attributed to interaction between the LC molecules and the polymer surfaces.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.