Optical Properties of Sputtered Ta2O5 Thin Films Using Spectroscopic Ellipsometty (분광타원법을 이용한 스퍼터된 Ta2O5 박막의 광학적 특성)

  • Kim, Sun-Hee;Lee, Eui-Hyun;Jung, In-Woo;Hyun, Jang-Hoon;Lee, Sung-Young;Kang, Man-Il;Ryu, Ji-Wook
    • Journal of the Korean Vacuum Society
    • /
    • v.18 no.2
    • /
    • pp.133-140
    • /
    • 2009
  • $Ta_{2}O_{5}$ thin films were deposited by RF magnetron sputtering method under various RF power, substrates and oxygen partial pressure. Elliptic constants were measured by using a phase modulated spectroscopic ellipsometer and analyzed with the Tauc-Lorentz dispersion formula and best fit method in the range of 310$\sim$1239 nm. Also, transmittance spectra of the films were measured by UV -Vis spectrophotometer in the range of 300$\sim$1000 nm. From these data, thickness of $Ta_{2}O_{5}$ and surface layer were analyzed and changes of magnitude and shape of dispersion of optical constants according to fabricated conditions were measured. Also, to evaluate thickness and optical constants data analyzed by Tauc-Lorentz dispersion formula, the measured and analyzed transmittance spectra were compared. In result of the comparison, two spectra were in good agreement each other. Accordingly, it indicates that our ellipsometric analysis is valid.

Investigation of Co- and Pr-doped yttria-stabilized cubic zirconia (YSZ) single crystal grown by skull melting method (스컬용융법에 의해 성장시킨 Co와 Pr이 첨가된 이트리아안정화큐빅지르코니아(YSZ) 단결정의 연구)

  • Moon, So-I;Seok, Jeong-Won
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.24 no.4
    • /
    • pp.140-144
    • /
    • 2014
  • Co-(0.7 wt%) and Pr-(2.0, 3.5 or 5.0 wt%) doped cubic zirconia ($ZrO_2:Y_2O_3=50:50wt%$) single crystals grown by a skull melting method were heat-treated in $N_2$ at $1150^{\circ}C$ for 5 hrs. The brown colored as-grown single crystals were changed into either dark brownish green, greenish blue and light green color after the heat treatment. Before and after the heat treatment, the YSZ (yttria-stabilized zirconia) single crystals were cut for wafer form (${\phi}7.5mm{\times}t3mm$). The optical and structural properties were examined by UV-VIS spectrophotometer and X-ray diffraction. Absorption by $Co^{2+}$(${\fallingdotseq}589nm$: ${\Gamma}_8[^4A_2(^4F)]{\rightarrow}{\Gamma}_8+{\Gamma}_7[^4T_1(^4F)]$, ${\fallingdotseq}610nm$: ${\Gamma}_8[^4A_2(^4F)]{\rightarrow}{\Gamma}_8[^4T_1(^4F)]$], ${\fallingdotseq}661nm$: ${\Gamma}_8[^4A_2(^4F)]{\rightarrow}{\Gamma}_6[^4T_1(^4F)]$]) and $Pr^{3+}$(${\fallingdotseq}450nm$: ${^3}H{_4}-{^3}P{_2}$, ${\fallingdotseq}473nm$: ${^3}H{_4}{\rightarrow}{^3}P{_1}$, ${\fallingdotseq}484nm$: ${^3}H{_4}{\rightarrow}{^3}P{_0}$), change of ionization energy and lattice parameter were confirmed.

Synthesis and characterization of thermally stable pink-red inorganic pigment for digital color (디지털 컬러용 pink-red 고온발색 무기안료의 합성 및 특성평가)

  • Lee, Won-Jun;Hwang, Hae-Jin;Kim, Jin-Ho;Cho, Woo-Suk;Han, Kyu-Sung
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.24 no.4
    • /
    • pp.169-175
    • /
    • 2014
  • Digital ink-jet printing system has many advantages such as fast and fine printing of various images, high efficiency and low cost process. Generally digital ink-jet printing requires ceramic pigments of cyan, magenta, yellow and black with thermal and glaze stability above $1000^{\circ}C$ for the application of porcelain product design. In this study, pink-red colored $CaO-SnO_2-Cr_2O_3-SiO_2$ pigment was synthesized using solid state reaction. The synthesis conditions of $Ca(Cr,Sn)SiO_5$ pigment such as annealing temperature, amount of mineralizer and non-stoichiometric composition were optimized. Crystal structure and morphology of the obtained $Ca(Cr,Sn)SiO_5$ pigment were analyzed using XRD, SEM, PSA, FT-IR and effect of Cr substitution on the pigment color was analyzed using Uv-vis. spectrophotometer and CIE $L^*a^*b^*$ measurement.

Evaluation of Blue-light Blocking Ratio and Luminous Transmittance of Blue-light Blocking Lens based on International Standard (국제표준에 의거한 청색광차단렌즈의 청색광차단율 및 시감투과율 평가)

  • Kim, Chang-Jin;Choi, Sung Wook;Yang, Seok Jun;Oh, Sang-Young;Choi, Eun Jung
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.19 no.2
    • /
    • pp.135-143
    • /
    • 2014
  • Purpose: To evaluate the blue-light blocking ratio and luminous transmittance of blue-light blocking lenses using the blue-light hazard function as specified in international standard. Methods: In order to calculate the blue-light blocking ratio and luminous transmittance for a total of 41 blue-light blocking lenses from 8 manufacturers, UV-Vis spectrophotometer was used for measuring the spectral transmittance of wavelengths from 380 to 780 nm. Blue-light blocking ratio was calculated using blue-light hazard function as specified in ANSI Z80.3:2010 and ISO 13666(or Korean Standard KS B ISO 13666:2004). Results: The range of the blue-light blocking ratio was from 9.3 to 96.8%, the range of the transmittance from 53.5 to 92.7%, and the range of the luminous transmittance from 58.0% to 98.1%. In general the blue-light blocking lens prepared by coating tended to have a higher luminous transmittance, while those prepared by tinting a higher blue-light blocking ratio. Conclusions: The behavior of the spectral distribution of lenses showed the possibility of the performance improvement in the blue-light blocking lenses. Manufactures need to acquire their own technology that can evaluate the performance of blue-light blocking lens based in international standard.

Phosphate Adsorption-Desorption of Kaolinite KGa-2 (Source Clay) (카올리나이트 KGa-2 (표준 점토)의 인산염 흡착-탈착 특성)

  • Cho, Hyen-Goo;Choi, Jae-Ho;Moon, Dong-Hyuk;Kim, Soo-Oh;Do, Jin-Youn
    • Journal of the Mineralogical Society of Korea
    • /
    • v.21 no.2
    • /
    • pp.117-127
    • /
    • 2008
  • The characteristics of phosphate adsorption-desorption on kaolinite was studied by batch adsorption experiments and detailed adsorbed state of phosphate on kaolinite surface was investigated using ATR-FTIR (Attenuated Total Reflectance-Fourier Transform Infrared) spectroscopy. The phosphorous contents were measured using UV-VIS-IR spectrophotometer with 820 nm wavelength. The adsorbed P was generally increased with increasing pH value in the range of pH 4 to pH 9, however it is not distinct. Moreover the adsorbed P was significantly changed with different initial phosphate concentration. The adsorption isotherms were well fitted with the Langmuir equation, Temkin equation, and Freundlich equation in descending order. The maximum Langmuir adsorption capacity of kaolinite KGa-2 is 232.5 ($204.1{\sim}256.5$) mg/kg and has very higher value than that of kaolinite KGa-1b. Most of adsorbed phosphate on kaolinite were not easily desorbed to aqueous solution, but might fixed on kaolinite surface. However it needs further research about the exact desorption experiment. It was impossible to recognize phosphorous adsorption bands on kaolinite in ATR-FTIR spectrum from kaolinite bands themselves, because the absorption peaks of phosphorous have very similar positions with those of kaolinite, and the intensities of the former were very weak in comparison with those of the latter.

Residual Stress Behavior and Physical Properties of Colorless and Transparent Polyimide Films (무색 투명 폴리이미드 박막의 잔류응력 거동 및 특성분석)

  • Nam, Ki-Ho;Lee, Wansoo;Seo, Kwangwon;Han, Haksoo
    • Polymer(Korea)
    • /
    • v.38 no.4
    • /
    • pp.510-517
    • /
    • 2014
  • A series of polyimide (PI) was prepared by reacting 4,4'-(hexafluoroisopropylidene)-diphthalic anhydride (6FDA) as the anhydride and bis(3-aminophenyl) sulfone (APS), bis[4-(3-aminophenoxy)-phenyl] sulfone (BAPS), 2,2-bis(4-aminophenyl)-hexafluoropropane (6FPD), 2,2-bis[4-(4-aminophenoxy)-phenyl]hexafluoropropane (6FBAPP), 2,2'-bis(trifluoromethyl)benzidine (TFDB), or 1,4-phenylenediamine (PDA) as the diamine. Residual stress behaviors were detected in-situ during thermal imidization of the polyimide precursors using a thin film stress analyzer (TFSA), and interpreted with respect to their morphology. According to the molecular orientation and packing order, the residual stress varied from 23.1 to 12.5 MPa, decreased with increasing chain rigidity. The thermal properties of the PI films were investigated using differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), and thermomechanical analysis (TMA). Their optical properties were measured by ultraviolet-visible spectrophotometer (UV-vis), and spectrophotometry. The properties of PI films were found to be strongly dependent upon the morphological structure. However, trade-offs between residual stress and optical properties were identified.

Fabrication of ATO thin film for IR-cut off by sol-gel method (솔-젤 법에 의한 적외선 차단 ATO 박막 제조)

  • Kim, Jin-Ho;Lee, Kwang-Hee;Lee, Mi-Jai;Hwang, Jonghee;Lim, Tae-Young
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.23 no.5
    • /
    • pp.230-234
    • /
    • 2013
  • IR cut-off thin films consisted of ATO nanoparticles were successfully fabricated by sol-gel method. The coating solution was synthesized with organic/inorganic hybrid binder and ATO colloidal solution and ATO thin films were coated on a slide glass with the withdrawal speed of 5~40 mm/s. As the withdrawal speed increased from 5 mm/s to 40 mm/s, the thickness of coating thin films also increased from $1.05{\mu}m$ to $4.25{\mu}m$ and the IR cut-off in wavelength of 780~2500 nm increased from 49.5 % to 66.7 %. In addition, the pencil hardness of ATO thin films dried at $80^{\circ}C$ was ca. 5H and the coating films were not removed after a cross cutter tape test because of the hybrid binder synthesized with tetraethylorthosilicate and methyltrimethoxysilane. The surface morphologies, optical properties and film thickness of prepared thin films with a different withdrawal speed were measured by field emission scanning electron microscope (FE-SEM), UV-Vis spectrophotometer, and Dektak.

Fabrication of superhydrophobic $TiO_2$ thin films by wet process (습식 공정법에 의한 초발수 $TiO_2$ 박막 제조)

  • Kim, Jin-Ho;Jung, Hyun-Ho;Hwang, Jong-Hee;Lim, Tae-Young;Choi, Duk-Gun;Cheong, Deock-Soo;Kim, Sae-Hoon
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.19 no.5
    • /
    • pp.262-267
    • /
    • 2009
  • Superhydrophobic $TiO_2$ thin films were successfully fabricated on a glass substrate by wet process. Layer-by-layer (LBL) deposition and liquid phase deposition (LPD) methods were used to fabricate the thin films of micro-nano complex structure with a high roughness. To fabricate superhydrophobic $TiO_2$ thin films, the (PAH/PAA) thin films were assembled on a glass substrate by LBL method and then $TiO_2$ nanoparticles were deposited on the surface of (PAH/PAA) thin film by LPD method, Subsequently, hydrophobic treatment using fluoroalkyltrimethoxysilane (FAS) was carried out on the surface of prepared $TiO_2$ thin films. The $TiO_2$ thin film fabricated with 45 minutes immersion time on $(PAH/PAA)_{10}$ showed the RMS roughness of 65.6nm, water contact angel of $155^{\circ}$ and high transmittance of above 80% (>650nm in wavelength) after the hydrophobic treatment. The Surface morphologies, optical properties and contact angel of prepared thin films with different experimental conditions were measured by field emission scanning electron microscope (FE-SEM), atomic force microscope (AFM), UV-Vis spectrophotometer and contact angle meter.

A Study on Blue Light Blocking Performance and Prescription for Blue Light Blocking Lens (청광차단렌즈의 청광차단성능과 처방에 관한 고찰)

  • Yu, Young Guk;Choi, Eun Jung
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.18 no.3
    • /
    • pp.297-304
    • /
    • 2013
  • Purpose: To investigate blue light rejection and the percentage of blue light in the visible light of blue light blocking lens according to light source, and to study prescriptions for blue light blocking lens Methods: UV-VIS spectrophotometer was used for blue light rejection and the percentage of blue light in the visible light according to light source, and the percentage of blue light in solar light was used to evaluate the prescription for blue light blocking lens. Results: The blue light rejection and the percentage of blue light in the visible light of each lens were depending on light sources. Through the way to compare the percentages of blue light in the visible light passing through the lens with that in solar light, blue light blocking lenses suitable to each light source could been selected. Conclusions: In the prescription for blue light blocking lens, inquiry for user's display must be preceded. And then the percentages of blue light in the visible light passing through the lens based on that in solar light may be useful as a method of evaluating the prescription for blue light blocking lens.

The optical and structural properties by ZrO2 and Y2O3 compositional ratio of Co- and Ce-doped cubic zirconia (YSZ) single crystals (ZrO2와 Y2O3 조성비에 따른 Co와 Ce 첨가 큐빅지르코니아(YSZ) 단결정의 광학적 및 구조적 특성)

  • Moon, So-I.;Park, Hee-Yul;Seok, Jeong-Won
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.22 no.2
    • /
    • pp.73-77
    • /
    • 2012
  • Co-(0.8 wt%) and Ce-(0.4 wt%) doped cubic zirconia ($ZrO_2$ : $Y_2O_3$ = 80 : 20, 70 : 30, 60 : 40, 50 : 50 wt%) single crystals grown by a skull melting method were heat-treated in $N_2$ at $1000^{\circ}C$ for 5 hrs. The orange, yellowish brown and brown colored as-grown single crystals were changed into either brownish red, yellow and green color after the heat treatment. Before and after the heat treatment, the YSZ (yttria-stabilized zirconia) single crystals were cut for wafer form (${\phi}6.5mm{\times}t2mm$). The optical and structural properties were examined by UV-VIS spectrophotometer and X-ray diffraction. Absorption by $Ce^{3+}(^2F_{5/2,7/2}(4f){\rightarrow}^2T_g(5d^1))$, $Co^{2+}(^4A_2(^4F){\rightarrow}^4T_1(^4F)$ or $^4T_1(^4P))$ and $Co^{3+}$, change of ionization energy and lattice parameter were confirmed.