• Title/Summary/Keyword: Tin

Search Result 2,461, Processing Time 0.042 seconds

Hepatotoxicity of Rifampicin and Pyrazinamide Treatment Excluding Isoniazid (Isoniazid를 제외한 Rifampicin과 Pyrazinamide 병합치료의 간독성 빈도)

  • Choi, Ik Su;Park, I-Nae;Hong, Sang-Bum;Oh, Yeon-Mok;Lim, Chae-Man;Lee, Sang Do;Koh, Younsuck;Kim, Woo Sung;Kim, Dong Soon;Kim, Won Dong;Shim, Tae Sun
    • Tuberculosis and Respiratory Diseases
    • /
    • v.60 no.1
    • /
    • pp.38-43
    • /
    • 2006
  • Background : Even though two-month rifampicin (RMP, R) and pyrazinamide (PZA, P) treatment has some advantages over isoniazid (INH, H) treatment for latent tuberculosis infection (LTBI), it was withdrawn from the list of treatment regimens for LTBI because of reported cases of severe hepatotoxicity. The purpose of this study was to estimate the frequency of hepatotoxicity of RMP and PZA treatment excluding INH in a Korean population. Method : TIn order to recruit patients who were prescribed RMP and PZA excluding INH, 256 INH-resistant tuberculosis patients were investigated through retrospective medical record analysis. A standard four-drug regimen was changed to a RMP/PZA-containing regimen excluding INH in 64 patients (RZ+ group). In the same study period, 146 patients who were prescribed an INH/RMP/PZA-containing standard regimen were randomly selected as a control (HRZ+ group). Clinical characteristics including liver diseases and the frequency of drug-induced hepatitis were compared between the RZ+ and HRZ+ groups. Result : The mean age of patients in the RZ+ group was 50.2 (${\pm}16.2$) and the male-to-female ratio was 36:28. The frequency of underlying liver diseases was 10.9% (7/64), which was not significantly different from that of the HRZ+ group (4.1%, 6/146). Even though the treatment duration of RZ+ ($5.5{\pm}4.8months$) was longer that than that of HRZ+ ($2.7{\pm}2.3months$), the frequency of toxic hepatitis was not significantly different between RZ+ and HRZ+ groups, 3.5% (2/57) and 7.1% (10/140), respectively. Conclusion : Hepatotoxicity was mild and occurred in a minor proportion of patients in a Korean population prescribed an RMP/PZA-containing regimen. A future prospective study including more patients is needed.

Comparison of the Results in Gastric Carcinoma Patients undergoing Billroth I and Billroth II Gastrectomiesy (원위부 위암에서 위절제술 후 위재건술식에 따른 잔위기능 및 영양 증상학적 삶의 질 비교)

  • Kim, Sung Geun;Kim, Young Kyun;Heo, Youn Jung;Song, Kyo Young;Kim, Jin Jo;Jin, Hyung Min;Kim, Wook;Park, Cho Hyun;Park, Seung Man;Lim, Keun Woo;Kim, Seung Nam;Jeon, Hae Myung
    • Journal of Gastric Cancer
    • /
    • v.7 no.1
    • /
    • pp.16-22
    • /
    • 2007
  • Purpose: The proper reconstruction technique to use after a distal subtotal gastrectomy for a gastric carcinoma, there has been a subject for debated what is the proper reconstruction technique. The aim of this study was to compare the gastricemptying time and the quality of life following both B-I and B-II reconstructions after a distal gastrectomy for a gastric adenocarcinoma. Materials and Methods: We studied 122 patients who had undergone a distal gastrectomy for a gastric adenocarcinoma between June 1999 and July 2002 at our hospital. 51 patients underwent B-I group, and 71 patients underwent B-II group. To evaluate the gastric-emptying time, we analyzed the T1/2 time by means of radionuclide scintigraphy using a gamma camera after ingestion of an $^{99m}Tc$-tin-colloid steamed egg. The nutritional status was measured by the weight change. Postgastrectomy syndrome was evaluated using an abdominal symptoms survey. Dumping syndrome was measured using the Sigstad dumping score. Results: The gastric-emptying time was somewhat delayed in the B-I group after a 6 month period, but there was no difference after 12 months between the two groups. There was less weight loss in the B-I group than in the B-II group (P=0.023). Fewer abdominal symptoms were occurred in the B-I group than in the B-II group. Dumping syndrome occurred less frequently in the B-I group than in the B-II group (P=0.013). Conclusion: In our study, the Billroth I reconstruction led to less weight loss, a better nutritional status, and a better quality of life than the Billroth II reconstruction. We concluded that after a distal subtotal gastrectomy, the Billroth I reconstruction would be considered when the procedure is oncologically suitable.

  • PDF

The Effect of Tin Ion-plating on the Bond Strength of Orthodontic Bracket (TiN Ion-Plating이 교정용 브라켓의 접착강도에 미치는 영향)

  • KIM, Seok-Yong;KWON, Oh-Won;KIM, Kyo-Han
    • The korean journal of orthodontics
    • /
    • v.27 no.1
    • /
    • pp.157-171
    • /
    • 1997
  • This study was conducted to see the effect of TiN ion-plating on the bond strength of orthodontic bracket. Three stainless-steel brackets with different base types were chosen; when TiN ion-plated brackets and non iorrplated brackets were bonded to the teeth, initial and long-term bond strength were measured, The observations oi bonding surface and failure sites through the scanning electron microscope were analysed and compared. The summary of this study was as follows; ${\cdot}$ When TiN ion-plating was not applied, the Micro-Loc type was the highest in bond strength atter 24 hours as $5.89{\pm}1.77$ MPa, followed by $4,27{\pm}1.12MPa$ for Foil Mesh type and $2.64{\pm}0.58MPa$ for Undercut type(P<0.05). ${\cdot}$ Under TiN ion-plating, the bond strength after 24 hours showed: Micro-Loc type $-6.26{\pm}1.51MPa$, Foil Mesh type $-7.45{\pm}2.01MPa$, Undercut type $-2.93{\pm}0.84MPa$. Unlike in the case of non ion-plating, Foil Mesh type showed a higher strength than Micro-Loc type, with Undercut type still showing the lowest bond strength(P<0.05). The bond strength, after 24 hours, increased in case of ion-plated in all 3 types, but a significant increase was shown only in Foil Mesh type(P<0.001). ${\cdot}$ Under a long-term immersion, regardless of ion or non ion-plating, bond strength in general increased over the initial bond strength(one day), with more stability. ${\cdot}$ Through scanning electron microscopic observation of bonding surface, it was found that, regardless of the bracket base type or the application of ion-plating, the resin was thoroughly spreaded into bracket base to form a solid bonding surface between the bracket and the tooth. This was also true in case of a long-term immersion. ${\cdot}$ The scanning electron microscopic observation of failure sites revealed diverse failure patterns.

  • PDF

Some Chemical Properties and Composition of Lipid Extracts of Riced Dehydrated Potato Granules (감자분말(粉末)의 지방질조성(脂肪質組成)과 저장중(貯藏中)의 변화(變化)에 관(關한) 연구(硏究))

  • Yoon, Jeong-Won;Hong, Bum-Shik;Yang, Han-Chul;Kim, Dong-Hoon
    • Korean Journal of Food Science and Technology
    • /
    • v.10 no.3
    • /
    • pp.320-330
    • /
    • 1978
  • Riced dehydrated potato granules with a good reconstituton quality was made from Irish Cobber (IC) and Shimabara which are representative varieties in Korea. A part of IC potato granules was packed in small vinyl-bags while the rest, including some BHA (75ppm)-treated granules, was packed in $301{\times}407$ plain tin cans. These granules were stored in a room at room temperature, and their physico-chemical properties and lipid composition were studied. The color of the granules was measured with a Hunter-type Tristimules colorimeter. L, $a_L,$ and $b_L-values$ were respectively 83.8, -1.1 and 18.3. Variety and package-type did not affect the color. In general, it was darker than that of commercial wheat flour, but whiter than that of commercial defatted soy flour. At $100^{\circ}C$, the granules, irrespective of variety and package-type, absorbed water rapidly, and reached the maximum moisture content of $90{\sim}92%$ in 3 min., whereas they absorbed water more slowly at $8{\sim}14^{\circ}C$, and reached the maximum content of $72{\sim}74%$ in 5 minutes. Peroxide, TBA, carbonyl, acid, and iodine values of the granules after 3 months storage were respetively $150{\sim}460\;meq/kg,\;20{\sim}26,\;154{\sim}380$ micromole, $24{\sim}59,\;and\;70{\sim}78$. Except iodine values, all the chemical values were affected by variety and package-type. Ether and $CHCl_3-extracts$ of the granules from IC and Shimabara were subjected to GLC and TLC analyses. In case of IC, the major fatty acids were palmitic, stearic, and oleic (30.0, 18.8, 40.6), while in case of Shimabara they were palmitic, oleic, and linoleic acids (26.7, 39.6, 23.4%). The major lipid classes were, in both cases, triglycerides and phospholipids. Their contents were raspectively 19.1 and 43.1 (IC), and 30.1 and 37.4% (Shimabara).

  • PDF

Macroporous Thick Tin Foil Negative Electrode via Chemical Etching for Lithium-ion Batteries (화학적 식각을 통해 제조한 리튬이온 이차전지용 고용량 다공성 주석후막 음극)

  • Kim, Hae Been;Lee, Pyung Woo;Lee, Dong Geun;Oh, Ji Seon;Ryu, Ji Heon
    • Journal of the Korean Electrochemical Society
    • /
    • v.22 no.1
    • /
    • pp.36-42
    • /
    • 2019
  • A macroporous Sn thick film as a high capacity negative electrode for a lithium ion secondary battery was prepared by using a chemical etching method using nitric acid for a Sn film having a thickness of $52{\mu}m$. The porous Sn thick film greatly reduced the over-voltage for the alloying reaction with lithium by the increased reaction area. At the same time. The porous structure of active Sn film plays a part in the buffer and reduces the damage by the volume change during cycles. Since the porous Sn thick film electrode does not require the use of the binder and the conductive carbon black, it has substantially larger energy density. As the concentration of nitric acid in etching solution increased, the degree of the etching increased. The etching of the Sn film effectively proceeded with nitric acid of 3 M concentration or more. The porous Sn film could not be recovered because the most of Sn was eluted within 60 seconds by the rapid etching rate in the 5 M nitric acid. In the case of etching with 4 M nitric acid for 60 seconds, the appropriate porous Sn film was formed with 48.9% of weight loss and 40.3% of thickness change during chemical acid etching process. As the degree of etching of Sn film increased, the electrochemical activity and the reversible capacity for the lithium storage of the Sn film electrode were increased. The highest reversible specific capacity of 650 mAh/g was achieved at the etching condition with 4 M nitric acid. The porous Sn film electrode showed better cycle performance than the conventional electrode using a Sn powder.

Technological Diversities Observed in Bronze Objects of the Late Goryo Period - Case Study on the Bronze Bowls Excavated from the Burial Complex at Deobu-gol in Goyang - (고려 말 청동용기에 적용된 제작기술의 다양성 연구 - 고양 더부골 고분군 출토 청동용기를 중심으로 -)

  • Jeon, Ik Hwan;Lee, Jae Sung;Park, Jang Sik
    • Korean Journal of Heritage: History & Science
    • /
    • v.46 no.1
    • /
    • pp.208-227
    • /
    • 2013
  • Twenty-seven bronze bowls excavated from the Goryo burial complex at Deobu-gol were examined for their microstructure and chemical composition to characterize the bronze technology practiced by commoners at the time. Results showed that the objects examined can be classified into four groups: 1) objects forged out of Cu-near 22%Sn alloys and then quenched; 2) objects cast from Cu-below 10% Sn alloys containing lead; 3) objects cast from Cu-10%~20% Sn alloys containing lead and then quenched; 4) objects forged out of Cu-10~20% Sn alloys containing lead and then quenched. This study revealed that the fabrication technique as determined by alloy compositions plays an important role in bronze technology. The use of lead was clearly associated with the selection of quenching temperatures, the character of inclusions and the color characteristics of bronze surfaces. It was found that the objects containing lead were quenched at temperatures of $520^{\circ}{\sim}586^{\circ}C$ while those without lead were quenched at the range of $586^{\circ}{\sim}799^{\circ}C$. The presence of selenium in impurity inclusions was detected only in alloys containing lead, suggesting that the raw materials, Cu and Sn, used in making the lead-free alloys for the first group were carefully selected from those smelted using ores without lead contamination. Furthermore, the addition of lead was found to have significant effects on the color characteristics of the surface of bronze alloys when they are subjected to corrosion during interment. In leaded alloys, corrosion turns the surface light green or dark green while in unleaded alloys, corrosion turns the surface dark brown or black. It was found that in fabrication, the wall thickness of the bronze bowls varies depending on the application of quenching; most of the quenched objects have walls 1mm thick or below while those without quenching have walls 1mm thick or above. Fabrication techniques in bronze making usually reflect social environments of a community. It is likely that in the late Goryo period, experiencing lack of skilled bronze workers, the increased demand for bronze was met in two ways; by the use of chief lead instead of expensive tin and by the use of casting suitable for mass production. The above results show that the Goryo bronze workers tried to overcome such a resource-limited environment through technological innovations as apparent in the use of varying fabrication techniques for different alloys. Recently, numerous bronze objects are excavated and available for investigation. This study shows that with the use of proper analytical techniques they can serve as a valuable source of information required for the characterization of the associated technology as well as the social environment leading to the establishment of such technology.

A Review on Treasure No.1167, Unified Silla Buddhist Bell from Uncheon-dong, Cheongju, about Its Form and Conservational Scientific Features (보물 제1167호 청주 운천동 출토 통일신라 범종의 형태와 보존과학적 특성 고찰)

  • Kim, Hyun-jeong;Kim, Su-gi
    • Korean Journal of Heritage: History & Science
    • /
    • v.40
    • /
    • pp.357-386
    • /
    • 2007
  • At present, thirteen Buddhist bells of Unified Silla are known to the world: Six in Korea, five in Japan and two other bells, and three out of them are impossible to make out its original form. Therefore, we divided the form of Unified Silla Buddhist bells based on the ten other bells, and we tried out to prove the manufacturing technology by the comparison of the research material of Uncheon-dong bell and existing research materials of other bells, in other to find their linkage based on the alloy elemental composition. We divided Unified Silla Buddhist bell into two types: Type I has symmetric apsaras and regular patterns on its face and it was made in early Silla period; type II has asymmetric apsaras and irregular pattern arrangement and made in late Silla period. In particular, Uncheon-dong Buddhist bells is very similar to Komyoji[光明寺] temple bell from ninth century in Japan. It is peculiar that the apsaras on Uncheon-dong bell play vertical music instruments that are never seen in Unified Silla Buddhist bell. Most of Unified Silla Buddhist bell are compounded with Cu-Sn or Cu-Sn-Pb system. From eighth and ninth century, bells were cast with even composition of copper, tin and lead, and the bronze alloy ratio was similar to the record in Gogonggi[考工記], Jurye[周禮], a book from ancient China. Particularly, Uncheon-dong bell is in a rare case of Cu-Sn-Pb-As system. As had been rarely used in Unified Silla Buddhist bells, so we presented the relative research materials. As has the same nature as Pb. Because As easily volatilize at high temperature, it is hard to use. But it has its merit of solidity and durability. Pb enhances fluidity and thereby expresses the patterns more distinct; As makes the bell stronger. The result of lead isotope ratio could not exactly reveal a concrete producing center. However, over the analysis of our samples, hereby we suggest Uncheon-dong bell was made of materials from just one ore deposit.

Research on Radiation Shielding Film for Replacement of Lead(Pb) through Roll-to-Roll Sputtering Deposition (롤투롤 스퍼터링 증착을 통한 납(Pb) 대체용 방사선 차폐필름 개발)

  • Sung-Hun Kim;Jung-Sup Byun;Young-Bin Ji
    • Journal of the Korean Society of Radiology
    • /
    • v.17 no.3
    • /
    • pp.441-447
    • /
    • 2023
  • Lead(Pb), which is currently mainly used for shielding purposes in the medical radiation, has excellent radiation shielding functions, but is continuously exposed to radiation directly or indirectly due to the harmfulness of lead itself to the human body and the inconvenience caused by its heavy weight. Research on shielding materials that are human-friendly, lightweight, and convenient to use that can block risks and replace lead is continuously being conducted. In this study, based on the commonly used polyethylene terephthalate (PET) film and the fabric material used in actual radiation protective clothing, a multi-layer thin film was realized through sputtering and vacuum deposition of bismuth, tungsten, and tin, which are metal materials that can shield radiation. Thus, a shielding film was produced and its applicability as a radiation shielding material was evaluated. The radiation shielding film was manufactured by establishing the optimized conditions for each shielding material while controlling the applied voltage, roll driving speed, and gas supply amount to manufacture the shielding film. The adhesion between the parent material and the shielding metal thin film was confirmed by Cross-cut 100/100, and the stability of the thin film was confirmed through a hot water test for 1 hour to measure the change of the thin film over time. The shielding performance of the finally realized shielding film was measured by the Korea association for radiation application (KARA), and the test conditions (inverse wide beam, tube voltage 50 kV, half layer 1.828 mmAl) were set to obtain an attenuation ratio of 16.4 (initial value 0.300 mGy/s, measured value 0.018 mGy/s) and damping ratio 4.31 (initial value 0.300 mGy/s, measured value 0.069 mGy/s) were obtained. by securing process efficiency for future commercialization, light and shielding films and fabrics were used to lay the foundation for the application of films to radiation protective clothing or construction materials with shielding functions.

Conservation Treatment and Study on Manufacturing Techniques of Jija Chongtong Gun in the Middle of Joseon Dynasty (조선 중기 제작된 지자총통의 보존처리와 제작기법 연구 -동아대학교 석당박물관 소장 보물 지자총통을 중심으로-)

  • Nam Dohyeon;Park Younghwan;Lee Jaesung
    • Conservation Science in Museum
    • /
    • v.30
    • /
    • pp.23-46
    • /
    • 2023
  • The Jija Chongtong Gun, owned by Seokdang Museum of Dong-A University, is a tubedstyle heavy weapon of the battlefield in the mid-Joseon Dynasty and is the second largest firearm after Cheonja Chongtong. The original surface color of the Jija Chongtong Gun was obscured by foreign substances and therefore it was judged that its condition requires the conservation treatment. For stable conservation treatment, gamma ray and X-ray non-destructive transmission surveys was conducted to determine the internal structure and conservation condition. And the component analysis on the material components and surface contaminants of Jija Chongtong Gun was conducted by utilizing the p-XRF component analysis, SEM-EDS component analysis, and XRD analysis. As a result of the gamma-ray and X-ray non-destructive transmission investigation, a large amount of air bubbles was observed inside Jija Chongtong Gun, and the part that appeared to be a chaplet by visual observation was not identified. As a result of gamma-ray and p-XRF component analysis, it was confirmed that Jija Chongtong Gun was bronze made of copper (Cu), tin (Sn), and lead (Pb) alloy. As a result of surface analysis of foreign substances using SEM-EDS, it was confirmed that the main components of white foreign substances were calcium (Ca), sulfur (S), and titanium (Ti). Titanium was presumed to be titanium dioxide (TiO2), the main component of white correction fluid. The red foreign substance was confirmed to contain barium (Ba) as its main ingredient, and was presumed to be barium sulfate (BaSO4), an extender pigment in paint. White and red contaminants, mainly composed of titanium and barium, are presumed to have been deposited on the surface in recent years. The yellow foreign substances were confirmed to be aluminum (Al) and silicon (Si), and were presumed to have originated from soil components. As a result of SEM-EDS and XRD component analysis, the white foreign substance was confirmed to be gypsum (CaS). Based on the results of component analysis, surface impurities were removed, stabilization treatment, and strengthening treatment were performed. During the conservation process, unknown inscriptions Woo (右), Byeong (兵), Sang (上), and Yi (二) were discovered through a portable microscope and precise 3D scanning. In addition, the carving method, depth, and width of the inscription were measured. Woo Byeong Sang is located above Happo Fortress in Changwon, and Yi can be identified as the second hill.

Manufacturing Techniques of Bronze Seated Bodhisattva Statue of Goseongsa Temple in Gangjin (강진 고성사 청동보살좌상의 제작기술 연구)

  • LEE Seungchan;BAE Gowoon;CHUNG Kwangyong
    • Korean Journal of Heritage: History & Science
    • /
    • v.57 no.1
    • /
    • pp.146-159
    • /
    • 2024
  • In this study, a study on the production technology of the Buddha statue and the production of raw material origin was conducted through scientific analysis on the Bronze seated Bodhisattva Statue of Goseongsa Temple, a treasure. As a result of microstructure analysis through a metal microscope, it was confirmed that the microstructure of the Bronze seated Bodhisattva Statue of Goseongsa Temple was a process-type dendritic structure, and the casting structure of bronze was well represented, so it was manufactured through casting. Subsequently, as a result of analyzing the alloy composition ratio through SEM-EDS, it was identified as a ternary alloy with 81.26 wt% of copper (Cu) and 16.42 wt% of tin (Sn) and 1.72 wt% of lead (Pb). The results of the analysis of lead isotope ratios using a thermal ionization mass spectrometer (TIMS) were substituted into the distribution of lead isotope ratios on the Korean Peninsula, it was shown in corresponding to Jeolla-do and Chungcheong-do regions and North and South Gyeongsang Province. This suggests that the raw materials used in their production were likely sourced from the mines around Goseong Temple in Gangjin. Despite the fact that the statue is a medium and large Buddha with a total height of 51 centimeters, 1.72 wt% of lead (Pb) was found as a result of alloy composition ratio analysis, which showed a similar composition to the lead content ratio of small bronze and gilt-bronze Buddha statues. Therefore, we compared and analyzed the results of the analysis of the composition ratio of the alloys of bronze and gilt bronze statues, which has been scientifically analyzed with a compositional age similar to that of the Bronze seated Bodhisattva Statue of Goseongsa Temple. Comparison results, Various factors, such as the size of the Buddha statue as well as its stylistic characteristics and the age of composition, may exist in determining the alloy composition ratio of the bronze and gilt bronze Buddha statues, and it was confirmed that the alloy composition ratio or casting technology was properly adjusted when the Buddha statue was created. In other words, it is judged that a more comprehensive system of Buddha statue production technology should be investigated by conducting archaeological and art history studies on stylistic characteristics and age of composition, as well as scientific analysis results such as observation of internal structure, microstructure observation, and analysis of alloy composition ratio using radiation transmission irradiation.