• Title/Summary/Keyword: TiNi Alloy

Search Result 393, Processing Time 0.024 seconds

Fatigue Properties of Ti-Ni Shape Memory Alloy Wire Welded by Nd: YAG Laser

  • Kim, Y.S.;Kim, J.D.;Kil, B.L.
    • International Journal of Korean Welding Society
    • /
    • v.3 no.1
    • /
    • pp.39-44
    • /
    • 2003
  • The welded specimens were made by butt welding of the 2 wires of 50mm length using the pulsed YAG laser. The laser welded wires were tested for investigating the shape memory effect and the ability of super elasticity. The fatigue properties of the welded wires were investigated using the rotary bending fatigue tester specially designed for wires. Moreover, the effect of defocusing distance during laser welding on the static and fatigue properties was Investigated. The shape memory effect and super elasticity of the laser welded wires were approximately identical with that of base metal at the test temperature below 353K. However, the welded wires were broken within elastic limit at the test temperature above 353k. Under the cyclic bending loading conditions, the welded wires could be useful only below the elastic limit, while the base metal had sufficient fatigue life even the stress induced M-phase region. The fatigue strength of the welded wires was about half of that of the base metal. The deterioration of the static and fatigue properties in the welded wires was proven to be from the large difference of the transformation behavior between the base metal and welded part that is caused by vaporization of Ni-content at the welded part during the welding process. The defocusing distance below 3mm acted more largely on lowering the strength of the welded wires than that of 6mm or 8mm.

  • PDF

The Formation and Crystallization of Amorphous Ti50Cu50Ni20Al10 Powder Prepared by High-Energy Ball Milling

  • Viet, Nguyen Hoang;Kim, Jin-Chun;Kim, Ji-Soon;Kwon, Young-Soon
    • Journal of Powder Materials
    • /
    • v.16 no.1
    • /
    • pp.9-15
    • /
    • 2009
  • Amorphization and crystallization behaviors of $Ti_{50}Cu_{50}Ni_{20}Al_{10}$ powders during high-energy ball milling and subsequent heat treatment were studied. Full amorphization obtained after milling for 30 h was confirmed by X-ray diffraction and transmission electron microscope. The morphology of powders prepared using different milling times was observed by field-emission scanning electron microscope. The powders developed a fine, layered, homogeneous structure with prolonged milling. The crystallization behavior showed that the glass transition, $T_g$, onset crystallization, $T_x$, and super cooled liquid range ${\Delta}T=T_x-T_g$ were 691,771 and 80 K, respectively. The isothermal transformation kinetics was analyzed by the John-Mehn-Avrami equation. The Avrami exponent was close to 2.5, which corresponds to the transformation process with a diffusion-controlled type at nearly constant nucleation rate. The activation energy of crystallization for the alloy in the isothermal annealing process calculated using an Arrhenius plot was 345 kJ/mol.

Comparison of mechanical properties of nickel-titanium rotary files: Aurum Blue vs. Aurum Pro (니켈티타늄 전동 파일의 기계적 특성 비교: Aurum Blue vs. Aurum Pro)

  • Kwak, Sang Won;Ha, Jung-Hong;Ahn, Sang Mi;Kim, Hyeon-Cheol
    • The Journal of the Korean dental association
    • /
    • v.57 no.11
    • /
    • pp.672-678
    • /
    • 2019
  • AIM: The purpose of this study was to evaluate and compare the torsional fracture resistances, cyclic fatigue resistance, and bending stiffness of two nickel-titanium (NiTi) rotary instruments made of different heat-treated alloy: Aurum Blue (heat-treated) and Aurum Pro (conventional). Methods: Forty-five Aurum Blue and Aurum Pro NiTi files were selected for the three mechanical tests (n=15). For the torsional resistance test, 3 mm file tip was fixed and the shaft was driven clockwise at 2 rpm until fracture occurred by using a customized device. Cyclic fatigue resistance was evaluated by rotating instruments in artificial canal with dynamic mode. Bending stiffness was tested by observation of the bending moment on attaining a 45° bend. The results were analyzed by student-t tests at a significance level of 95%. The fractured surface of each groups were examined under a scanning electron microscope (SEM). Results: Aurum Blue showed significantly higher toughness, ultimate strength, distortion angle, and number of cycles to failure than those of Aurum Pro (p < 0.05). However, Aurum Blue and Aurum Pro did not differ significantly in terms of bending stiffness. SEM showed typical topographic appearances of the cyclic fatigue and torsional fracture. Conclusions: Under the limitations of this study, heat-treated instruments showed higher flexibility and fracture resistances than conventional NiTi instruments.

  • PDF

Effects of Holding Temperatures on Microstructure and Mechanical Properties of CP Titanium and Ti-6Al-4V Alloy and Its low Temperature Brazing Characteristics (열노출 온도에 따른 CP 티타늄, Ti-6Al-4V 합금의 미세조직/기계적성질 변화 및 저온브레이징 특성)

  • Sun, J.H.;Shin, S.Y.;Hong, J.W.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.23 no.1
    • /
    • pp.3-9
    • /
    • 2010
  • Titanium and its alloys were brazed in the range of $850-950^{\circ}C$ within 10 min. of brazing time using expensive infra red or other heating methods. However, brazing time needs to be extended to get temperature-uniformity for mass production by using continuous belt type furnace or high vacuum furnace with low heating rate. This study examined effects of holding temperature for 60 min, on microstructure and mechanical properties of titanium alloys. Mechanical properties of titanium alloys were drastically deteriorated with increasing holding temperature followed by grain growth. Maximum holding temperatures for CP (commercial pure) titanium and Ti-6Al-4V were confirmed as $800^{\circ}C$ and $850^{\circ}C$, respectively. Both titanium alloys were successfully brazed at $800^{\circ}C$ for 60 min. with the level of base metal strengths by using Zr based filler metal, $Zr_{54}Ti_{22}Ni_{16}Cu_8$.

Flow Stress and Deformation Behavior of Zr-based Bulk Metallic Glass Composite in Supercooled Liquid Region (Zr계 비정질 복상 합금의 과냉 액상 영역에서의 유동 음력과 변형거동)

  • Jun, H.J.;Lee, K.S.;Chang, Y.W.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2006.05a
    • /
    • pp.417-420
    • /
    • 2006
  • The composition and structure of dendrite phase within $Zr_{76.11}Ti_{4.20}Cu_{4.51}Ni_{3.16}Be_{1.49}Nb_{10.53}$ bulk metallic glass (BMG) were confirmed by using an EPMA, XRD and TEM, respectively. The chief elements of dendrite phase were Zr-Ti-Nb and had a BCC structure. The thermal properties of this BMG have been then subsequently investigated by using a differential scanning calorimeter (DSC). The glass transition and crystallization onset temperatures were determined as $339.7^{\circ}C$ and $375.8^{\circ}C$ for this alloy, respectively. Mechanical properties have also been examined by conducting a series of uniaxial compression tests at various temperatures within supercooled liquid region under the strain rates between $10^{-4}/s$ and $3{\times}10^{-2}/s$. The deformation behavior of BMG composite within supercooled liquid region is similar to one of Vit-1 exhibiting amorphous single phase alloy. The flow stresses of BMG composite, however, are entirely higher than those of Vit-1 because dendrite phases are interfere with moving of atoms.

  • PDF

Research of Diffusion Bonding of Tungsten/Copper and Their Properties under High Heat Flux

  • Li, Jun;Yang, Jianfeng
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.05a
    • /
    • pp.14-14
    • /
    • 2011
  • W (tungsten)-alloys will be the most promising plasma facing armor materials in highly loaded plasma interactive components of the next step fusion reactors due to its high melting point, high sputtering resistance and low deuterium/tritium retention. The bonding technology of tungsten to Cu alloy was one of the key issues. In this paper, W/CuCrZr diffusion bonding has been performed successfully by inserting pure metal interlay. The joint microstructure, interfacial elements migration and phase composition were analyzed by SEM, EDS, XRD, and the joint shear strength and micro-hardness were investigated. The mock-ups were fabricated successfully with diffusion bonding and the cladding technology respectively, and the high heat flux test and thermal fatigue test were carried out under actively cooling condition. When Ni foil was used for the bonding of tungsten to CuCrZr, two reaction layers, Ni4W and Ni(W) layer, appeared between the tungsten and Ni interlayer with the optimized condition. Even though Ni4W is hard and brittle, and the strength of the joint was oppositely increased (217 MPa) due primarily to extremely small thicknesses (2~3 ${\mu}m$). When Ti foil was selected as the interlayer, the Ti foil diffused quickly with Cu and was transformed into liquid phase at $1,000^{\circ}C$. Almost all of the liquid was extruded out of the interface zone under bonding pressure, and an extremely thin residual layer (1~2 ${\mu}m$) of the liquid phase was retained between the tungsten and CuCrZr, which shear strength exceeded 160 MPa. When Ni/Ti/Ni multiple interlayers were used for bonding of tungsten to CuCrZr, a large number of intermetallic compound ($Ni_4W/NiTi_2/NiTi/Ni_3T$) were formed for the interdiffusion among W, Ni and Ti. Therefore, the shear strength of the joint was low and just about 85 MPa. The residual stresses in the clad samples with flat, arc, rectangle and trapezoid interface were estimated by Finite Element Analysis. The simulation results show that the flat clad sample was subjected maximum residual stress at the edge of the interface, which could be cracked at the edge and propagated along the interface. As for the rectangle and trapezoid interface, the residual stresses of the interface were lower than that of the flat interface, and the interface of the arc clad sample have lowest residual stress and all of the residual stress with arc interface were divided into different grooved zones, so the probabilities of cracking and propagation were lower than other interfaces. The residual stresses of the mock-ups under high heat flux of 10 $MW/m^2$ were estimated by Finite Element Analysis. The tungsten of the flat interfaces was subjected to tensile stresses (positive $S_x$), and the CuCrZr was subjected to compressive stresses (negative $S_x$). If the interface have a little microcrack, the tungsten of joint was more liable to propagate than the CuCrZr due to the brittle of the tungsten. However, when the flat interface was substituted by arc interfaces, the periodical residual stresses in the joining region were either released or formed a stress field prohibiting the growth or nucleation of the interfacial cracks. Thermal fatigue tests were performed on the mock-ups of flat and arc interface under the heat flux of 10 $MW/m^2$ with the cooling water velocity of 10 m/s. After thermal cycle experiments, a large number of microcracks appeared at the tungsten substrate due to large radial tensile stress on the flat mock-up. The defects would largely affect the heat transfer capability and the structure reliability of the mock-up. As for the arc mock-up, even though some microcracks were found at the interface of the regions, all microcracks with arc interface were divided into different arc-grooved zones, so the propagation of microcracks is difficult.

  • PDF

A study on the diffusion bonding of the $Al_2$O$_3$ ceramics to metal (A$_2$O$_3$세라믹과 Ni-Cr-Mo鋼과의 인서트 合金을 이용한 擴散接合에 關한 硏究)

  • 김영식;박훈종;김정일
    • Journal of Welding and Joining
    • /
    • v.10 no.3
    • /
    • pp.63-72
    • /
    • 1992
  • The joining methods of ceramics to metals which can be expected to obtain high temperature strength are mainly classified into the solid-state diffusion bonding method and the active brazing method. Between these two, the solid-state diffusion bonding method is given attentions as substituting method for active brazing method due to being capable of obtaining higher bonding strength at high temperature and accurate bonding. In this paper, the solid-state diffusion bonding of $Al_{2}$O$_{3}$ ceramics to Ni-Cr-Mo alloy steel (SNCM21) using insert metal was carried out. The insert metal employed in this study was experimentally home-made, Ag-Cu-Ti alloy. Influence of several bonding parameters of $Al_{2}$O$_{3}$SNCM21 joint was quantitatively evaluated by bonding strength test, and microstructural analyses at the interlayer were performed by SEM/EDX. From above experiments, the optimum bonding condition of the solid-state diffusion bonding of $Al_{2}$O$_{3}$/SNCM21 using Ag-Cu-Ti insert metal was determined. Futhermore, high temperature strength and thermal-shock properties of $Al_{2}$O$_{3}$/SNCM21 joint were also examined. The results obtained are as follows. 1. The maximum bonding strength was obtained at the temperature of 95% melting point of insert metal. 2. The high temperature strength of $Al_{2}$O$_{3}$/SNCM21 joint appeared to bemaximum value at test temperature 500.deg.C and the bonding strength with increasingtemperature showed parabolic curve. 3. The strength of thermal-shocked specimens was far deteriorated than those of as-bonded specimens. Especially, water-quenched specimen after heated up to 600.deg. C was directly fractured in quenching.

  • PDF

Dynamic Deformation Behavior of Zr-Based Bulk Amorphous Alloy after Annealing Treatments (벌크형 비정질 Zr계 합금의 결정화 열처리에 따른 동적변형 거동)

  • Chang J. J;Lee B. J;Hwang J. I;Park I. M;Cho K. M;Cho Y. R
    • Korean Journal of Materials Research
    • /
    • v.14 no.3
    • /
    • pp.181-185
    • /
    • 2004
  • The mechanical properties of a bulk amorphous alloy ($Zr_{41.2}$ $Ti_{13.8}$ /$Cu_{10}$ $Ni_{10}$ $Be_{22.5}$ /at.%) before and after an annealing treatment were investigated. For the bulk amorphous alloy, the compressive strength was about 2.0 GPa, irrespective of the strain rates in the range of $10^{-4}$ to $10^3$$ sec^{-1}$ . Fine-sized nanocrystalline particles (10~100 nm) were precipitated homogeneously in the bulk amorphous matrix after the annealing treatments. Compared to the bulk amorphous materials, these composite materials, composed of the nanocrystalline phases and a bulk amorphous matrix had much different mechanical properties. The strength and strain of coposite materials measured by a compressive test showed a peak-maximum values at 7 vol.% of the nanocrystalline phases. The values in higher volume fraction of the crystalline phases in the amorphous matrix were decreased, as measured by both quasi-static and high strain rate. The decrease in fracture strength is due to presence of the dispersed large-crystalline phases in the amorphous matrix.

The Study of Ni-Pd Alloy Characteristics to Form a NiSi for Shallow S/D Junction (Shallow S/D Junction에 적용 가능한 NiSi를 형성하기 위한 Ni-Pd 합금의 특성 연구)

  • Lee, Won-Jae;Oh, Soon-Young;Agchbayar, Tuya;Yun, Jang-Gn;Kim, Yong-Jin;Zhang, Ying-Ying;Zhong, Zhun;Kim, Do-Woo;Cha, Han-Seob;Heo, Sang-Bum;Wang, Jin-Suk;Lee, Hi-Deok
    • Proceedings of the IEEK Conference
    • /
    • 2005.11a
    • /
    • pp.603-606
    • /
    • 2005
  • In this paper, the formation and thermal stability of Ni-silicide using Ni-Pd alloys is studied for ultra shallow S/D junction of nano-scale CMOSFETs. There are no different effects when Ni-Pd is used in single structure and TiN capping structure. But, in case of Cobalt interlayer structure, it was found that Pure Ni had lower sheet resistance than Ni-Pd, because of a thick silicide. Also, Ni-Pd has merits that surface of silicide and interface between silicide and silicon have a good morphology characteristics. As a result, Ni-Pd is an optimal candidate for shallow S/D junction when cobalt is used for thermal stability.

  • PDF

Crystallization behavior of Cu-base bulk metallic glass in supercooled liquid region during compression and tension (과냉각 액상구간에서 압축.인장시 Cu기 비정질 합금의 결정화 거동)

  • Park, E.S.;Kim, S.H.;Huh, M.Y.;Kim, H.W.;Bae, J.C.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.10a
    • /
    • pp.215-217
    • /
    • 2008
  • Crystallization behavior of the bulk metallic glass (BMG) during compression and tension was studied in the supercooled liquid region (SLR). Rod samples of the BMG alloy were produced by consolidating gas atomized powders of $Cu_{54}Zr_{22}Ti_{18}Ni_6$ using spark plasma sintering. The crystallization behavior in these samples was examined by tackling changes in thermal property during heating the samples in DSC. The present BMG alloy was firstly decomposed and then crystallized during annealing in the SLR. The phase decomposition from the original amorphous phase was retarded by the compressive stress, while it was accelerated by the tensile stress.

  • PDF