• 제목/요약/키워드: TiC layer thickness

검색결과 191건 처리시간 0.028초

Electrochemical Metallization방법을 이용한 GaN Schottky Diode의 제작과 전기적 특성 향상 및 분석 (Electrical Characteristics of n-GaN Schottky Diode fabricated by using Electrochemical Metallization)

  • 이철호;;이명재;곽성관;김동식;정관수;강태원
    • 대한전자공학회:학술대회논문집
    • /
    • 대한전자공학회 2001년도 하계종합학술대회 논문집(2)
    • /
    • pp.205-208
    • /
    • 2001
  • Schottky barrier diodes are fabricated on a intrinsic GaN(4${\mu}{\textrm}{m}$) epitaxial structure grown by rf plasma molecular beam epitaxy (MBE) on sapphire substrates. First, We make Ohmic electrodes (Ti/Al/Ti/Au) by evaporator. Next, we contact RuO$_2$ by dipping in the solution (RuCl$_3$.HClO$_4$), and then we deposit Ni/Au on the surface of RuO$_2$ by evaporator. We study the electrical characteristics of GaN Schottky barrier diodes made by these methods. Measurements are C-V, I-V, SEM, EDX, and XRD for the characteristics of devices. Thickness of RuO$_2$ layer depends on supplied voltage and dipping time. Device of thinner RuO$_2$ layer have a good Schottky characteristics compare with device of thicker RuO$_2$ layer

  • PDF

Interfaces of Stacking $TiO_2$ Thin Layers Affected on Photocatalytic Activities

  • 주동우;부진효
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2013년도 제45회 하계 정기학술대회 초록집
    • /
    • pp.189.1-189.1
    • /
    • 2013
  • Titanium dioxide (TiO2) is a wide bandgap semiconductor possessing photochemical stability and thus widely used for photocatalysis. However, enhancing photocatalytic efficiency is still a challenging issue. In general, the efficiency is affected by physio-chemical properties such as crystalline phase, crystallinity, exposed crystal facets, crystallite size, porosity, and surface/bulk defects. Here we propose an alternative approach to enhance the efficiency by studying interfaces between thin TiO2 layers to be stacked; that is, the interfacial phenomena influencing on the formation of porous structures, controlling crystallite sizes and crystallinity. To do so, multi-layered TiO2 thin films were fabricated by using a sol-gel method. Specifically, a single TiO2 thin layer with a thickness range of 20~40 nm was deposited on a silicon wafer and annealed at $600^{\circ}C$. The processing step was repeated up to 6 times. The resulting structures were characterized by conventional electron microscopes, and followed by carrying out photocatalytic performances. The multi-layered TiO2 thin films with enhancing photocatalytic efficiency can be readily applied for bio- and gas sensing devices.

  • PDF

Role of HCl in Atomic Layer Deposition of TiO2 Thin Films from Titanium Tetrachloride and Water

  • Leem, Jina;Park, Inhye;Li, Yinshi;Zhou, Wenhao;Jin, Zhenyu;Shin, Seokhee;Min, Yo-Sep
    • Bulletin of the Korean Chemical Society
    • /
    • 제35권4호
    • /
    • pp.1195-1201
    • /
    • 2014
  • Atomic layer deposition (ALD) of $TiO_2$ thin film from $TiCl_4$ and $H_2O$ has been intensively studied since the invention of ALD method to grow thin films via chemical adsorptions of two precursors. However the role of HCl which is a gaseous byproduct in ALD chemistry for $TiO_2$ growth is still intriguing in terms of the growth mechanism. In order to investigate the role of HCl in $TiO_2$ ALD, HCl pulse and its purging steps are inserted in a typical sequence of $TiCl_4$ pulse-purge-$H_2O$ pulse-purge. When they are inserted after the first-half reaction (chemisorption of $TiCl_4$), the grown thickness of $TiO_2$ becomes thinner or thicker at lower or higher growth temperatures than $300^{\circ}C$, respectively. However the insertion after the second-half reaction (chemisorption of $H_2O$) results in severely reduced thicknesses in all growth temperatures. By using the result, we explain the growth mechanism and the role of HCl in $TiO_2$ ALD.

상온분사분말공정에 의해 SrTiO3 (100), (110) Seed에 코팅된 BaTiO3의 고온 성장 거동 분석 (High Temperature Grain Growth Behavior of Aerosol Deposited BaTiO3 Film on (100), (110) Oriented SrTiO3 Single Crystal)

  • 임지호;이승희;김기현;지성엽;정승운;박춘길;정한보;정대용
    • 한국재료학회지
    • /
    • 제29권11호
    • /
    • pp.684-689
    • /
    • 2019
  • Single crystals, which have complexed composition, are fabricated by solid state grain growth. However, it is hard to achieve stable properties in a single crystal due to trapped pores. Aerosol deposition (AD) is suitable for fabrication of single crystals with stable properties because this process can make a high density coating layer. Because of their unique features (nano sized grains, stress inner site), it is hard to fabricate single crystals, and so studies of grain growth behavior of AD film are essential. In this study, a $BaTiO_3$ coating layer with ${\sim}9{\mu}m$ thickness is fabricated using an aerosol deposition method on (100) and (110) cut $SrTiO_3$ single crystal substrates, which are adopted as seeds for grain growth. Each specimen is heat-treated at various conditions (900, 1,100, and $1,300^{\circ}C$ for 5 h). $BaTiO_3$ layer shows different growth behavior and X-ray diffraction depending on cutting direction of $SrTiO_3$ seed. Rectangular pillars at $SrTiO_3$ (100) and laminating thin plates at $SrTiO_3$ (110), respectively, are observed.

Surface Protection Obtained by Anodic Oxidation of New Ti-Ta-Zr Alloy

  • Vasilescu, C.;Drob, S.I.;Calderon Moreno, J.M.;Drob, P.;Popa, M.;Vasilescu, E.
    • Corrosion Science and Technology
    • /
    • 제17권2호
    • /
    • pp.45-53
    • /
    • 2018
  • A new 80Ti-15Ta-5Zr wt% alloy surface was protected by anodic oxidation in phosphoric acid solution. The protective oxide layer (TiO2, ZrO2 and Ta suboxides and thickness of 15.5 nm) incorporated $PO{_4}^{3-}$ ions from the solution, according to high resolution XPS spectra. The AFM analysis determined a high roughness with SEM detected pores (20 - 50 nm). The electrochemical studies of bare and anodically oxidized Ti-15Ta-5Zr alloy in Carter-Brugirard saliva of different pH values and saliva with 0.05M NaF, pointed to a nobler surface for the protected alloy, with a thicker electrodeposited oxide layer acting as a barrier against aggressive ions. The oxidized alloy significantly decreased corrosion current densities and total quantity of ions released into the oral environment in comparison with the bare one, at higher polarisation resistance and protective capacity of the electrodeposited layer. The impedance data revealed a bi-layered oxidation film formed by: a dense, compact, barrier layer in contact with the metallic substrate, decreasing the potential gradient across the metal/oxide layer/solution interface, reducing the anodic dissolution and a more permissive, porous layer in contact with the electrolyte. The open circuit potential for protected alloy shifted to nobler values, with thickening of the oxidation film signifying long-term protection.

Hardness and Oxidation Resistance of Ti0.33Al0.67N/CrN Nano-multilayered Superlattice Coatings

  • Ahn, Seung-Su;Oh, Kyung-Sik;Chung, Tai-Joo;Park, Jong-Keuk
    • 한국세라믹학회지
    • /
    • 제56권1호
    • /
    • pp.49-55
    • /
    • 2019
  • $Ti_{0.33}Al_{0.67}N/CrN$ nano-multilayers, which are known to have excellent wear resistance, were prepared using an unbalanced magnetron sputter to have various periods of 2-5 nm. $Ti_{0.33}Al_{0.67}N$ had a hexagonal structure in a single layer, but converted to a cubic structure by forming a multilayer with CrN, which has a cubic structure. Thus, $Ti_{0.33}Al_{0.67}N$ formed a superlattice in the multilayer. The $Ti_{0.33}Al_{0.67}/CrN$ multilayer with a period of 2.5 nm greatly exceeded the hardness of the $Ti_{0.33}Al_{0.67}N$ and the CrN single layer, reaching 39 GPa. According to the low angle X-ray diffraction results, the $Ti_{0.33}Al_{0.67}N/CrN$ multilayer maintained its as-coated structure to a temperature as high as $700^{\circ}C$ and exhibited hardness of 30 GPa. The thickness of the oxide layer of the $Ti_{0.33}Al_{0.67}N/CrN$ multilayered coating was less than one-tenth of those of the single layers. Thus, $Ti_{0.33}Al_{0.67}N/CrN$ multilayered coating had hardness and oxidation resistance far superior to those of its constituent single layers.

$TiO_2$ 정밀여과막의 제조 및 특성 (Preparation and Characterization of $TiO_2$ Membranes for Microfiltration)

  • 한상욱;최세영;현상훈;조철구;강한규
    • 한국세라믹학회지
    • /
    • 제33권6호
    • /
    • pp.700-708
    • /
    • 1996
  • TiO2 membranes for microfiltration were prepared on $\alpha$-alumina support tube by slurry coating. The coating layer was obtained by flowing TiO2 slip on the inner surface of the alumina support. TiO2 membranes were heat-treated at 9$25^{\circ}C$ for 2 hrs. The thickness of the unsupported membrane was about 10${\mu}{\textrm}{m}$. The mean pore diameter of the membranes were 0.09 and 0.15${\mu}{\textrm}{m}$ respectively and the pure water flux was 900~1,200ι/m2.hr at room temperature and 1 bar. For a possible application of oily wastewater treatement an kerosene/wa-ter emulsion was separated in terms of flux and removal efficiency. In 60 min of operating time the flux of TiO2 membranes was 50~100 ι/m2.hr and removal efficiency was over 97% at 3kgf/cm2 of operating pres-sure and 600 ml/min of flow rate. TiO2 membranes could be recycled by reheat treatments at $600^{\circ}C$ for 2 hrs.

  • PDF

RF 마그네트론 스퍼터링법으로 성장시킨 0.5 % Ce-doped Ba($Zr_{0.2}Ti_{0.8}$)$O_3$(BCZT) 박막의 특성분석 (Characterization of 0.5 % Ce-doped Ba($Zr_{0.2}Ti_{0.8}$)$O_3$ Thin Films Grown by RF Magnetron Sputtering Method)

  • 최원석;박용섭;이준신;홍병유
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.301-304
    • /
    • 2002
  • We investigated the structural and electrical properties of Ce-doped Ba($Zr_{0.2}Ti_{0.8}$)$O_3$(BCZT) thin films with a mole fraction of x=0.2 and a thickness about 100 nm. BCZT films were prepared on Pt/Ti/$SiO_2$/Si substrate by a RF magnetron sputtering system. We have measured the thickness profile with Ar/$O_2$ ratio and the surface roughness. It was observed that the oxygen gas, which introduced during the film deposition, have an influence on the roughness of the film and the film roughness was reduced by annealing from 2.33 nm to 2.02 m (RMS at $500^{\circ}C$, Ar:6 scrim, $O_2$:6 sccm). We have found that annealing procedure after top electrode deposit can reduce the dissipation factor.

  • PDF

RF 마그네트론 스퍼터링법으로 성장시킨 0.5% Ce-doped Ba(Zr0.2Ti0.8)O3 (BCZT) 박막의 열처리 특성분석 (Characterization of the Annealing Effect of 0.5 % Ce-doped Ba(Zr0.2Ti0.8)O3 Thin Films Grown by Rf Magnetron Sputtering Method)

  • 최원석;박용섭;이준신;홍병유
    • 한국전기전자재료학회논문지
    • /
    • 제16권5호
    • /
    • pp.361-364
    • /
    • 2003
  • It was investigated that the structural and electrical Properties of Ce-doped Ba(Zr$_{x}$Ti$_{1-x}$ )O$_3$ (BCZT) thin films with a mole fraction of x=0.2 and a thickness about 100 nm. BCZT films were prepared on Pt/Ti/SiO$_2$/Si substrate by a RF magnetron sputtering system. We have measured the thickness profile with Ar/O$_2$ ratio and the surface roughness. It was observed that the oxygen gas, which introduced during the film deposition, have an influence on the roughness of the film and the film roughness was reduced by annealing from 2.33 nm to 2.02 nm (RMS at 500 $^{\circ}C$, Ar:6 sccm, $O_2$:6 sccm). It was found that annealing procedure after top electrode deposit can reduce the dissipation factor.

PZT 박막의 압전 특성 및 MEMS 기술로 제작된 PZT cantilever의 전기기계적 물성 평가 (Piezoelectric and electromechanical properties of PZT films and PZT microcantilever)

  • 이정훈;황교선;윤기현;김태송
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.177-180
    • /
    • 2002
  • Thickness dependence of crystallographic orientation of diol based sol-gel derived PZT(52/48) films on dielectric and piezoelectric properties was investigated The thickness of each layer by one time spinning was about 0.2 $\mu\textrm{m}$, and crack-free films was successfully deposited on 4 inches Pt/Ti/SiO$_2$/Si substrates by 0.5 mol solutions in the range from 0.2 $\mu\textrm{m}$ to 3.8 $\mu\textrm{m}$. Excellent P-E hysteresis curves were achieved without pores or any defects between interlayers. As the thickness increased , the (111) preferred orientation disappeared from 1$\mu\textrm{m}$ to 3 $\mu\textrm{m}$ region, and the orientation of films became random above 3 $\mu\textrm{m}$. Dielectric constants and longitudinal piezoelectric coefficient d$\_$33/, measured by pneumatic method were saturated around the value of about 1400 and 300 pC/N respectively above the thickness of 0.8 7m. A micromachined piezoelectric cantilever have been fabricated using 0.8 $\mu\textrm{m}$ thickness PZT (52/48) films. PZT films were prepared on Si/SiN$\_$x/SiO$_2$/Ta/Pt substrate and fabricated unimorph cantilever consist of a 0.8 fm thick PZT layer on a SiNx elastic supporting layer, which becomes vibration when ac voltage is applied to the piezoelectric layer. The dielectric constant (at 100 kHz) and remanent polarization of PZT films were 1050 and 25 ${\mu}$C/$\textrm{cm}^2$, respectively. Electromechanical characteristics of the micromachined PZT cantilever in air with 200-600 $\mu\textrm{m}$ lengths are discussed in this presentation.

  • PDF