• 제목/요약/키워드: TiAl Alloys

검색결과 336건 처리시간 0.022초

Investigation of Interface Reaction between TiAl Alloys and Mold Materials

  • 김명균;김영직
    • 소성∙가공
    • /
    • 제8권3호
    • /
    • pp.289-289
    • /
    • 1999
  • This paper describes the investment casting of TiAl alloys. The effects of mold material and mold preheating temperature for the investment casting of TiAl on metal-mold interfacial reaction were investigated by means of optical micrography, hardness profiles and an electron probe microanalyzer. The mold materials examined were colloidal silica bonded ZrO₂, ZrSiO₄, A1₂O₃and CaO stabilized ZrO₂. When compared with conventional titanium a1loy, the high aluminum concentration of TiAl alloys helps to lower their reactivity in the molten state. The A1₂O₃mold is a promising mold material for the investment casting of TiAl in terms of the thermal stability, formability and cost. Special attention need to be paid to thermal stability and mold preheating when developing the investment calling of TiAl alloys.

상향식 연속주조법에 의한 Al-Cr 및 Al-Ti 2원계 포정합금의 결정성장 (Crystal Growth of Al-Cr and Al-Ti Peritectic Alloys by the Upward Continuous Casting Proces)

  • 백승일;최정철;신현진;홍준표
    • 한국주조공학회지
    • /
    • 제12권3호
    • /
    • pp.203-209
    • /
    • 1992
  • Directional solidification of Al-Ti peritetic alloys was carried out using Upward Continuous Casting Process. The morphology of a solid-liquid interface and solidification microstructures were investigated under various crystal growing conditions. The experimental results were compared with those attained by the Bridgman method. The cell spacing of the Al-Ti peritetic alloys and the primary dendrite arm spacing of the Al-Ti peritetic alloys decreased with an increase in pulling speed. The primary ${\beta}$ phase of the Al-Cr and Al-Ti peritectic alloys did not appear in solidification microstructures because of the depleted solute contents in the melt ahead of the solid-liquid interface.

  • PDF

Ti-10wt.%Al-xMn 분말합금의 Mn첨가에 따른 소결특성 평가 (Effect of Mn Addition on Sintering Properties of Ti-10wt.%Al-xMn Powder Alloy)

  • 신기승;현용택;박노광;박용호;이동근
    • 한국분말재료학회지
    • /
    • 제24권3호
    • /
    • pp.235-241
    • /
    • 2017
  • Titanium alloys have high specific strength, excellent corrosion and wear resistance, as well as high heat-resistant strength compared to conventional steel materials. As intermetallic compounds based on Ti, TiAl alloys are becoming increasingly popular in the aerospace field because these alloys have low density and high creep properties. In spite of those advantages, the low ductility at room temperature and difficult machining performance of TiAl and $Ti_3Al$ materials has limited their potential applications. Titanium powder can be used in such cases for weight and cost reduction. Herein, pre-forms of Ti-Al-xMn powder alloys are fabricated by compression forming. In this process, Ti powder is added to Al and Mn powders and compressed, and the resulting mixture is subjected to various sintering temperature and holding times. The density of the powder-sintered specimens is measured and evaluated by correlation with phase formation, Mn addition, Kirkendall void, etc. Strong Al-Mn reactions can restrain Kirkendall void formation in Ti-Al-xMn powder alloys and result in increased density of the powder alloys. The effect of Al-Mn reactions and microstructural changes as well as Mn addition on the high-temperature compression properties are also analyzed for the Ti-Al-xMn powder alloys.

TiN 코팅된 Ti 및 Ti-6Al-4V합금의 부식거동 (Corrosion behaviors of Cp-Ti and Ti-6Al-4V alloys by TiN coating)

  • 이순현;정용훈;최한철;고영무
    • 대한치과기공학회지
    • /
    • 제30권1호
    • /
    • pp.25-31
    • /
    • 2008
  • Cp-Ti and Ti-6Al-4V alloys commonly used dental implant materials, particularly for orthopaedic and osteosynthesis because of its suitable mechanical properties and excellent biocompatibility. This alloys have excellent corrosion behavior in the clinical environment. The first factor to decide the success of dental implantation is sufficient osseointegration and high corrosion resistance between on implant fixture and its surrounding bone tissue. In this study, in order to increase corrosion resistance and biocompatibility of Cp-Ti and Ti-6Al-4V alloy that surface of manufactured alloy was coated with TiN by RF-magnetron sputtering method. The electrochemical behavior of TiN coated Cp-Ti and Ti-6Al-4V alloy were investigated using potentiodynamic (EG&G Co, PARSTAT 2273. USA) and potentiostatic test (250mV) in 0.9% NaCl solution at 36.5 $\pm$ 1$^{\circ}C$. These results are as follows : 1. From the microstructure analysis, Cp-Ti showed the acicular structure of $\alpha$-phase and Ti-6Al-4V showed the micro-acicular structure of ${\alpha}+{\beta}$ phase. 2. From the potentiodynamic test, Ecorr value of Cp-Ti and Ti-6Al-4V alloys showed -702.48mV and -319.87mV, respectively. Ti-6Al-4V alloy value was higher than Cp-Ti alloy. 3. From the analysis of TiN and coated layer, TIN coated surface showed columnar structure with 800 nm thickness. 4. The corrosion resistance of TiN coated Cp-Ti and Ti-6Al-4V alloys were higher than those of the non-coated Ti alloys in 0.9% NaCl solution from potentiodynamic test, indicating better protective effect. 5. The passivation current density of TiN coated Cp-Ti and Ti-6Al-4V alloys were smaller than that of the noncoated implant fixture in 0.9% NaCl solution, indicating the good protective effect resulting from more compact and homogeneous layer formation.

  • PDF

가토의 경골에 이식된 새로운 티타늄계 합금 주위의 골형성에 관한 형태학적 연구 (A HISTOMORPHOMETRIC STUDY OF BONE APPOSITION TO NEWLY DEVELOPED TI-BASED ALLOYS IN RABBIT BONE)

  • 김태인
    • 대한치과보철학회지
    • /
    • 제36권5호
    • /
    • pp.701-720
    • /
    • 1998
  • Research advances in dental implantology have led to the development of several different types of materials and it is anticipated that continued research will lead to advanced dental implant materials. Currently used pure titanium has relatively low hardness and strength which may limit its ability to resist functional loads as a dental implant. Ti-6Al-4V also has potential problems such as corrosion resistance. osseointegration properties and neurologic disorder due to aluminium and vanadium, known as highly toxic elements, contained in Ti-6Al-4V. Newly developed titanium based alloys(Ti-20Zr-3Nb-3Ta-0.2Pd-1In, Ti-20Zr-3Nb-3Ta-0.2Pd) which do not contain toxic metallic components were designed by the Korea Institute of Science and Technology (KIST) with alloy design techniques using Zr, Nb, Ta, Pd, and In which are known as non-toxic elements. Biocompatibility and osseointegration properties of these newly designed alloys were evaluated after implantation in rabbit femur for 3 months. The conclusions were as follows : 1. Mechanical properties of the new designed Ti based alloys(Ti-20Zr-3Nb-3Ta-0.2Pd-1In, Ti-20Zr-3Nb-3Ta-0.2Pd) demonstrated close hardness and tensile strength values to Ti-6Al-4V. 2. New desinged experimental alloys showed stable corrosion resistance similar to the pure Ti but better than Ti-6Al-4V. However, the corrosion rate was higher for the new alloys. 3. Cell culture test showed that the new alloys have similar cell response compared with pure Ti and Ti-6Al-4V with no cell adverse reaction. 4. New designed alloys showed similar bone-metal contact ratio and osseointegration properties compared to pure Ti and Ti-6Al-4V after 3 months implantation in rabbit femur. 5. Four different surface treatments of the metals did not show any statistical difference of the cell growth and bone-metal contact ratio.

  • PDF

Ti-43%Al-2%W-0.1%Si 합금의 고온산화 (High Temperature Oxidation of Ti-43%Al-2%W-0.1%Si Alloys)

  • 심웅식;이동복
    • 한국표면공학회지
    • /
    • 제36권2호
    • /
    • pp.128-134
    • /
    • 2003
  • Alloys of Ti-43%Al-2%W-0.1%Si were oxidized isothermally and cyclically between $900^{\circ}C$ and$ 1050^{\circ}C$, and their oxidation characteristics were studied. During isothermal tests, the alloys oxidized slowly up to 100$0^{\circ}C$, but fast at $1050^{\circ}C$. Though the scale adherence was not good above $900^{\circ}C$, the alloys displayed better oxidation behavior than unalloyed TiAl alloys. The oxide scales consisted primarily of an outer $TiO_2$ layer, intermediate $Al_2$$O_3$-rich layer, and an inner mixed layer of (TiO$_2$ $+Al_2$$O_3$). Tungsten was present mainly at the lower part of the oxide scale, while Si over the whole oxide scale.

열처리 조건에 따른 TiAl화합물의 미세조직과 기계적 성질에 관하여 (Effect of Heattreatment condition on structure and properties of TiAl alloys)

  • 박정종;이철형;최진일
    • 열처리공학회지
    • /
    • 제8권1호
    • /
    • pp.84-88
    • /
    • 1995
  • Various heat-treatments were conducted to Ti-48.1at%Al and Ti-48.3at%Al-1.2at%Mn alloys casted by plasma arc melting system. Mechanical properties, microstructure and high temperature oxidizing behaviors of as-casted and heat-treatment alloys were investigated. Ti-48.1Al and Ti-48.3Al-1.2Mn alloys were decreased in strength according to increased of heattreatment temperature. Oxidizing weight gain of Ti-48.1Al alloy which conducted at $1273^{\circ}K$ was linearly increased. In case of adding Mn to alloy, there was no rapid increase of oxidizing weight gain during early time.

  • PDF

Fe-30at.%A1 합금의 압연성에 미치는 Cr, B, Ti 및 Si 첨가효과 (Effects of Cr, B, Ti and Si on Rolling Characteristics in Fe-30at.%A1 Alloy)

  • 최답천;이지성
    • 한국주조공학회지
    • /
    • 제23권2호
    • /
    • pp.77-85
    • /
    • 2003
  • Some alloying elements such as Cr, B, Ti and Si were added individually or as a mixture to Fe-30 at.%Al alloys. The alloys were melted using an arc furnace and then heat-treated for homogenization at 1000$^{\circ}C$ for 7 days and followed by rolling at 1000$^{\circ}C$. The alloying elements on rolling characteristics were investigated by the microstructures and fracture mode before and after rolling. The microstructures before rolling showed that all of the alloys had equiaxed grains. On the other hand, the microstructures of rolling plane as well as its perpendicular plane became elongated after rolling. The alloys such as Fe-30Al, Fe-30Al-3Ti, Fe-30Al-0.5B, Fe-30Al-5Cr and Fe-30Al-3Ti-0.5B revealed better rolling behaviour from the point that intergranular and cleavage fractures were not fundamentally occurred. But the addition of 5Ti or 3Si to Fe-Al alloys had detrimental effects. The Ti-added alloy system such as Fe-30Al-5Ti, Fe-30Al-5Ti-5Cr, Fe-30Al-3Ti-5Cr and Fe-30Al-5Ti-0.5B were cracked through grain and showed cleavage fracture. The Si-added alloy system such as Fe-30Al-5Si, Fe-27Al-3Si and Fe-27Al-5Cr-3Si were cracked along the grain boundary and showed intergranular fracture. $DO_3{\leftrightarrow}B_2$ transition temperature of Fe-30at.%Al alloy was 520$^{\circ}C$, whereas the addition of 3Ti and 3Ti+0.5B comparably increased the temperature to 797 and 773$^{\circ}C$, respectively.

Effects of Cr and Fe Addition on Microstructure and Tensile Properties of Ti-6Al-4V Prepared by Direct Energy Deposition

  • Byun, Yool;Lee, Sangwon;Seo, Seong-Moon;Yeom, Jong-taek;Kim, Seung Eon;Kang, Namhyun;Hong, Jaekeun
    • Metals and materials international
    • /
    • 제24권6호
    • /
    • pp.1213-1220
    • /
    • 2018
  • The effects of Cr and Fe addition on the mechanical properties of Ti-6Al-4V alloys prepared by direct energy deposition were investigated. As the Cr and Fe concentrations were increased from 0 to 2 mass%, the tensile strength increased because of the fine-grained equiaxed prior ${\beta}$ phase and martensite. An excellent combination of strength and ductility was obtained in these alloys. When the Cr and Fe concentrations were increased to 4 mass%, extremely fine-grained martensitic structures with poor ductility were obtained. In addition, Fe-added Ti-6Al-4V resulted in a partially melted Ti-6Al-4V powder because of the large difference between the melting temperatures of the Fe eutectic phase (Ti-33Fe) and the Ti-6Al-4V powder, which induced the formation of a thick liquid layer surrounding Ti-6Al-4V. The ductility of Fe-added Ti-6Al-4V was thus poorer than that of Cr-added Ti-6Al-4V.

기계적 합금화한 Al-8wt.%(Ti+V+Zr) 4원계 합금의 열적 안정성에 관한 연구 (The Thermal Stability of Mechanically Alloyed Quaternary Al-8wt.%(Ti+V+Zr) Alloys)

  • 김주영
    • 한국분말재료학회지
    • /
    • 제2권3호
    • /
    • pp.247-254
    • /
    • 1995
  • The theoretical optimum quaternary composition for improving the thermal stability of Al-Ti alloy was recently proposed. On the basis of the suggestion, quaternary Al-Ti-V-Zr alloy powders corresponding to the optimum compositions, one of which belongs to the region of the smallest lattice misfit between the matrix and the precipitates and the other belongs to the region of the smallest rate constant of coarsening, were prepared by mechanical alloying and the powders were vacuum-hot-pressed at $430^{\circ}C$ under the pressure of 800 MPa. The thermal stability of the specimens was evaluated by hardness testing after isothermal aging up to 400 hrs at various temperatures. The decrease of hardness of Al-Ti-V-Zr alloys was smaller than that of Al-Ti alloys. It was considered to be due to the formation of $Al_3Zr$ type and$Al_3Ti$ type quaternary precipitates having smaller lattice misfit than $Al_3Ti$ and the increase of volume fraction of All0v during the isothermal aging. The quaternary Al-Ti-V-Zr alloys corresponding to the smallest lattice misfit showed the most improved thermal stablilty and it was mainly considered to be due to the formation of All0v.

  • PDF