• 제목/요약/키워드: Ti-Zr-Ni

검색결과 289건 처리시간 0.028초

Ni/MH 2차 전지용 고용량 Ti계 수소저장합금의 설계에 관한 연구 (A Study on the Alloy Design of High Capacity Ti-Based Metal Hydride for Ni/MH Rechargeable Battery)

  • 이한호;이재영
    • 한국수소및신에너지학회논문집
    • /
    • 제7권1호
    • /
    • pp.19-28
    • /
    • 1996
  • Ti-Mn based hydrogen storage alloy were modified by substituting alloying elements such as Zr, V and Ni in order to design a high capacity MH electrode for Ni/MH rechargeable battery. When V was substituted in Ti-Mn binary system, the crystal structure was maintained as $Cl_4$ Laves phase at a composition of $Ti_{0.2}V_{0.4}Mn_{0.4}$ and $Ti_{0.4}V_{0.2}Mn_{0.4}$ and equilibrium pressure decreased below 1 atm without decreasing hydrogen storage capacity considerably. It was found that Ni should be included in Ti-V-Mn alloy in order to hydrogenate it electrochemically in KOH electrolyte. But substitution of Ni for Mn in Ti-V-Mn system caused the increase of equilibrium pressure above 1atm and decrease of hydrogen storage capacity. Zr was able to increase the reversible hydrogen storage capacity of Ti-V-Mn-Ni alloy without considerable change of hydrogenation properties. The electrochemical discharge capacity of Ti-Zr-V-Mn-Ni system were in the range of 350 - 464mAh/g and among them $Ti_{0.8}Zr_{0.2}V_{0.5}Mn_{0.5}Ni_{1.0}$ alloy had $Cl_4$ Laves single phase and very high electrochemical discharge capacity of 464mAh/g.

  • PDF

$Fe_2O_3$가 첨가된 $0.4Pb(Ni_{1/3}Nb_{2/3})O_3-0.6Pb(Zr_xTi_{1-x})O_3$ 세라믹스에서의 PZ/PT비 변화에 따른 유전 및 압전 특성 (Dielectric and Piezoelectric Properties of $Fe_2O_3$-Added $0.4Pb(Ni_{1/3}Nb_{2/3})O_3-0.6Pb(Zr_xTi_{1-x})O_3$ Ceramics with Variatior of Zr/Ti Ratio)

  • 백종후;임은경;김세기;이미재;지미정;최병현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.338-339
    • /
    • 2005
  • 본 연구에서는 $Fe_2O_3$를 첨가한 $Pb(Ni_{1/3}Nb_{2/3})O_3-Pb(Zr_xTi_{1-x})O_3$ 세라믹스에서 Zr/Ti 비 변화에 따른 소결 및 압전, 유전특성을 조사하였다. $0.4Pb(Ni_{1/3}Nb_{2/3})O_3-0.6Pb(Zr_xTi_{1-x})O_3$+0.25Wt% $Fe_2O_3$ 계에서 Zr/(Ti+Zr)비(x)를 0.39에서 0.42까지 변화시킨 조성을 1100 - $1250^{\circ}C$ 온도에서 2시간 소결하여 이의 결정구조 및 미세조직을 분석하였고, 압전, 유전 특성 및 RAINBOW 액츄에이터로의 응용을 조사하였다. $1150^{\circ}C$에서 소결한 0.405 조성(x)에서 유전상수(${\varepsilon}r$) = 4669, 전기기계결합계수(kp) = 0.75, 압전상수($d_{33}$) = 810 pC/N의 우수한 특성 값을 나타내었으며, 닥터블레이드법에 의해 RAINBOW 액츄에이터를 제작하여 변위특성을 조사하였다.

  • PDF

벌크 비정질 Zr-Ti-Cu-Ni-Be 합금의 고온 소성 변형 특성 (High Temperature Plastic Deformation Behaviors of the Bulk Metallic Glass Zr-Ti-Cu-Ni-Be Alloy)

  • 이광석;하태권;안상호;장영원
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2001년도 추계학술대회 논문집
    • /
    • pp.272-276
    • /
    • 2001
  • Multicomponent $Zr_{41.2}Ti_{13.8}Cu_{12.5}Ni_{10}Be_{22.5}$ bulk matallic glass alloy shows good bulk glass forming ability due to its high resistance to crystallization in the undercooled liquid state.1) In this study, DSC and X-ray diffractometry have been performed to confirm the amorphous structure of the master $Zr_{41.2}Ti_{13.8}Cu_{12.5}Ni_{10}Be_{22.5}$ alloy. To investigate the mechanical properties and deformation behaviors of the bulk metallic $Zr_{41.2}Ti_{13.8}Cu_{12.5}Ni_{10}Be_{22.5}$ alloy, a series of compression tests has been carried out at the temperatures ranging from $351^{\circ}C$ to $461^{\circ}C$ and at the various initial strain rates from $2{\times}10^{-4}s^{-1}\;to\;2{\times}10^{-2}s^{-1}$. There are two types of nominal stress-strain curves. The one shows linear stress-strain relationship meaning fracture at maximum stress, the other shows plastic deformation including steady-state flow. Also DSC analysis for the compressed specimens has been performed to investigate the change of thermal stability and crystallization behavior for the various test conditions.

  • PDF

벌크 비정질 Zr-Ti-Cu-Ni-Be 합금의 고온 압축 변형 특성 (High Temperature Compressive Deformation Behavior of the Bulk Metallic Glass Zr-Ti-Cu-Ni-Be Alloy)

  • 이광석;하태권;안상호;장영원
    • 소성∙가공
    • /
    • 제10권7호
    • /
    • pp.565-572
    • /
    • 2001
  • It is well known that a multicomponent $Zr_{4l.2}Ti_{13.8}Cu_{12.5}Ni_{10}Be_{22.5}$ bulk metallic glass alloy shows good bulk glass forming ability due to its high resistance to crystallization in the undercooled liquid state. DSC and XRD have been performed to confirm the amorphous structure of the master alloy. To investigate the mechanical properties and deformation behavior of the bulk metallic $Zr_{4l.2}Ti_{13.8}Cu_{12.5}Ni_{10}Be_{22.5}$ alloy, a series of compression tests has been carried out at the temperatures ranging from $351^{\circ}C$ to $461^{\circ}C$at the various initial strain rates from $2{\times}10^4s^1$ to $2{\times}10^2s^1$. Three types of nominal stress-strain curves have been identified such as linear stress-strain relationship meaning fracture at maximum stress, plastic deformation including stress overshoot and steady-state flow, plastic deformation without stress overshoot depending on the strain rate and test temperature. Also DSC analysis for the compressed specimens was carried out to investigate the change of structure, thermal stability and crystallization behavior for the various test conditions.

  • PDF

비행입자의 열 에너지에 따른 NiTiZrSiSn 벌크 비정질 분말의 적층 거동 (Effect of Thermal Energy of In-Flight Particles on Impacting Behavior for NiTiZrSiSn Bulk Metallic Glass during Kinetic Spraying)

  • 윤상훈;김수기;이창희
    • Journal of Welding and Joining
    • /
    • 제25권3호
    • /
    • pp.37-44
    • /
    • 2007
  • Mechanical and thermomechanical properties of the bulk metallic glass (BMG) are so unique that the deformation behavior is largely dependent on the temperature and the strain rate. Impacting behavior of NiTiZrSiSn bulk metallic glass powder during kinetic spraying was investigated in this study. Considering the impact behavior of the BMG, the kinetic spraying system was modified and attached the powder preheating system to make the transition from the inhomogeneous deformation to the homogeneous deformation of impacting BMG particle easy BMG splat formation is considered from the viewpoint of the adiabatic shear instability. It is suggested that the impact behavior of bulk metallic glass particle is determined by the competition between fracture and deformation. The bonding of the impacting NiTiZrSiSn bulk amorphous particle was primarily caused by the temperature-dependent deformation and fracture (local liquid formation) behavior.

Ni-K2TixOy 촉매를 이용한 해조류 유래 수열 액화 원료의 수증기 개질 반응 연구 (Steam Reforming of Hydrothermal Liquefaction Liquid from Macro Algae over Ni-K2TixOy Catalysts)

  • 박용범;임한권;우희철
    • 청정기술
    • /
    • 제23권1호
    • /
    • pp.104-112
    • /
    • 2017
  • 해조류로부터 수열 액화 반응을 통해 생성된 원료를 이용하여 수소가스를 생산하기 위해 개질 반응용 상용화 촉매와 $K_2Ti_xO_y$가 첨가된 니켈(Ni) 제조 촉매를 사용하여 반응온도에 따른 수증기 개질 반응을 수행하였다. 반응원료는 해조류 바이오매스를 503 K의 반응온도에서 2시간 동안 수열 액화를 통해 생성된 액화 원료를 사용하였으며, 상용화 촉매(FCR-4-02)와 제조 촉매($Ni/K_2Ti_xO_y-Al_2O_3$, $Ni/K_2Ti_xO_y-SiO_2$, $Ni/K_2Ti_xO_y-ZrO_2/CeO_2$, Ni/$K_2Ti_xO_y$-MgO) 및 반응온도에 따른 수증기 개질 반응의 활성을 비교 연구하였다. 실험결과 제조 촉매 4종 모두 상용화 촉매와 비교하여 반응활성이 높게 나타나는 것이 확인되었으며, 제조 촉매의 지지체에 따라 생성되는 가스의 조성이 달라지는 것이 확인되었다. 특히, 산성이나 염기성을 띄는 $Al_2O_3$와 MgO의 지지체와 중성을 띄는 $SiO_2$의 지지체에서는 CO가 선택적으로 높게 생성이 되었으며 환원성을 띄는 $CeO_2$를 포함하는 지지체에서는 수성가스 전환 반응이 일어나 $CO_2$가 높게 생성됨을 보였다.

$(Zr_{0.65}Sn_{0.35})Ti_{1.04}O_4$ 세라믹스의 NiO 첨가량 및 소결온도에 따른 고주파 유전특성 (Microwave Dielectric Properties of $(Zr_{0.65}Sn_{0.35})Ti_{1.04}O_4$ Ceramics according to Doped NiO and Sintering Temperature)

  • 윤중락;홍성용;이헌용;권정열;김경용
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1994년도 하계학술대회 논문집 C
    • /
    • pp.1487-1489
    • /
    • 1994
  • $(Zr_{0.65}Sn_{0.35})Ti_{1.04}O_4$ system which has a dielectric constant, low dielectric loss and temperature coefficient was investigated. Temperature coefficient varied from positive to negative with increasing of NiO. For the NiO content 1.0wt%. i.e $(Zr_{0.65}Sn_{0.35})Ti_{1.04}O_4$, the ceramic showed very good dielectric properties such as ${\epsilon}$=37.8, $Q{\times}f_o=49.000$ and ${\tau}_r= 4{\pm}1ppm/^{\circ}C$.

  • PDF

급냉응고법으로 제조한 Zr-Ni-Cu-Al-Ti 합금의 열적, 기계적 성질 (Thermal and Mechanical Properties of Rapidly Solidified Zr-Ni-Cu-Al-Ti Alloy)

  • 최익석;한태교;지용권;임병문;김영환;김인배
    • 한국재료학회지
    • /
    • 제11권3호
    • /
    • pp.171-177
    • /
    • 2001
  • 급냉응고방식으로 제조한 비정질 Z $r_{62-x}$N $i_{10}$C $u_{20}$A $l_{8}$ $Ti_{x}$ (x=3, 6, 9at%) 합금을 사용하여 열적, 기계적 성질을 조사하였다. 시효온도에 따른 결정화 거동은 Ti 3at%에서는 비정질$\longrightarrow$비정질+Z $r_2$A $l_3$+Zr+(Ni,Ti)$\longrightarrow$Z $r_2$Cu+Al+(Ni,Ti)의 결정화 거동을 나타내었으며, Ti 6at%에서는 비정질$\longrightarrow$비정질+Al$\longrightarrow$A $l_2$Ti+NiZr+CuTi, Ti 9at%에서는 비정질$\longrightarrow$비정질+Zr+Al$\longrightarrow$Zr+A $l_2$Zr+Al $Ti_3$+CuTi의 결정화 거동을 보였다. 시효온도가 증가할수록 비정질 모상에 석출상의 체적율( $V_{f}$ )이 증가하고 그에 따라 비커스 경도 ( $H_{v}$ )간이 증가하였다. 파괴인장강도($\sigma_{f}$ )는 $V_{f}$ 의 증가에 따라 증가하다가 Z $r_{59}$A $l_{10}$N $i_{20}$C $u_{8}$ $Ti_3$$V_{f}$ =38%에서 1219MPa의 최대값을 보이고, Z $r_{56}$A $l_{10}$N $i_{20}$C $u_{8}$ $Ti_{6}$$V_{f}$ =2%에서 1203MPa의 최대값을 보이고, Z $r_{53}$A $l_{10}$N $i_{20}$C $u_{8}$ $Ti_{9}$ $V_{f}$ =5%에서 1350MPa의 최대값을 나타낸 후 그 이상의 $V_{f}$ 에서는 급격히 감소하였다. $\sigma_{f}$ 가 급격히 감소하는 $V_{f}$ 와 연성 파면에서 취성파면으로 천이되는 $V_{f}$ 가 일치하였다.f/가 일치하였다.

  • PDF

$MnO_2$ 가 첨가된 0.4P$(Ni_{1/3}Nb_{2/3})O_3-xPbTiO_3-yPbZrO_3$ 세라믹스에서의 PZ/PT비 변화에 따른 유전 및 압전 특성 (Dielectric and Piezoelectric Properties of $MnO_2$-Added 0.4P$(Ni_{1/3}Nb_{2/3})O_3-xPbTiO_3-yPbZrO_3$ Ceramics with Variation of PZ/PT Ratio)

  • 백종후;김창일;임은경;이미재;지미정;최병현;김세기
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.169-170
    • /
    • 2005
  • 본 연구에서는 초음파 센서에 응용 가능한 $0.4Pb(Ni_{1/3}Nb_{2/3})O_3-0.6Pb(Zr_xTi_{1-x})O_3+0.5Wt%$ $MnO_2$ 세라믹스에 Zr/(Ti+Zr)비를 0.37에서 0.41로 변화시킨 조성을 1175 $\sim$ 1200$^{\circ}C$ 온도에서 소결하여 이의 결정구조 및 미세조직을 분석하였고, 압전, 유전 특성을 고찰하였다. 본조성에서 x=0.385 조성에서 최대 유전상수 값 3490 이 나타났으며, 그 이상의 첨가에서는 감소하였다. 상경계 영역인 x=0.385 조성에서 $\varepsilon$r, $K_p$, $d_{33}$ 값이 최대값을 나타내었다. $0.4Pb(Ni_{1/3}Nb_{2/3})O_3-0.6Pb(Zr_xTi_{1-x})O_3+0.5Wt%$ $MnO_2$, 세라믹스에서는 kp 와 $d_{33}$ 는 Zr/(Ti+Zr)비 0.385조성까지 증가하였다가 그 이상 조성에서 감소하였다. $1175^{\circ}C$에서 2시간 소결한 x=0.385조성에서 $\varepsilon$r=3490, kp=0.71, Qm=476의 우수한 압전 특성을 나타내었다.

  • PDF

Zr-based 수소저장합금을 음극으로 사용한 밀패형 Ni-MH 2차전지의 내압특성에 관한 연구 (A study on the characteristics of inner cell pressure for sealed type Ni-MH rechargeable battery using Zr-based hydrogen storage alloy as anode)

  • 김동명;이호;장국진;이재영
    • 한국수소및신에너지학회논문집
    • /
    • 제8권2호
    • /
    • pp.79-90
    • /
    • 1997
  • Extensive work has been done on investigating the inner cell pressure characteristics of sealed type Ni-MH battery in which Zr-Ti-Mn-V-Ni alloy is used as anode. The inner cell pressure of this type Ni-MH battery much more increases with the charge/discharge cycling than that of the other type Ni-MH battery where commercialized $AB_5$ type alloy is used as anode. The increase of inner cell pressure in the sealed type Ni/MH battery using Zr-Ti-Mn-V-Ni alloy system is mainly due to the accumulation of oxygen gas during charge/discharge cycling. The accumulation of oxygen gas arises mainly due to the low rate of oxygen recombination on the MH electrode surface during charge/discharge cycling. The difference of oxygen recombination rate between $AB_5$ type electrode and Zr-Ti-Mn-V-Ni electrode is caused by the difference of electrode reaction surface area resulting from different particle size after their activation and the difference of surface catalytic activity for oxygen recombination reaction, respectively. After EIS analysis, it is identified that the surface catalytic activity affects much more dominantly on the oxygen recombination reaction than the reaction surface area does. In order to suppress the inner cell pressure of Ni-MH battery where Zr-Ti-Mn-V-Ni is used as anode, it is suggested that the surface catalytic activity for oxygen recombination should be improved.