• Title/Summary/Keyword: Ti-Zr-Be-Cu-Ni

검색결과 56건 처리시간 0.416초

DEVELOPMENT OF TITANIUM-BASED BRAZING FILLER METALS WITH LOW-MELTING-POING

  • Onzawa, Tadao;Tiyama, Takashi
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.539-544
    • /
    • 2002
  • Titanium and titanium alloy are excellent in corrosion resistance and specific intensity, and also in the biocompatibility. On the other hand, the brazing is bonding method of which productivity and reliability are high, when the complicated and precise structure of the thin plate is constructed. However, though conventional titanium-based brazing filler metal was excellent in bond strength and corrosion resistance, it was disadvantageous that metal structure and mechanical property of the base metal deteriorated, since the brazing temperature (about 1000 C) is considerably high. Authors developed new brazing filler metal which added Zr to Ti-Cu (-Ni) alloy which can be brazed at 900 C or less about 15 years ago. In this paper, the development of more low-melting-point brazing filler metal was tried by the addition of the fourth elements such as Ni, Co, Cr for the Ti-Zr-Cu alloy. As a method for finding the low-melting-point composition, eutectic composition exploration method was used in order to reduce the experiment point. As the result, several kinds of new brazing filler metal such as 37.5Ti-37.5-Zr-25Cu alloy (melting point 825 C) and 30Ti-43Zr-25Cu-2Cr alloy (melting point: 825 C) was developed. Then, the brazing joint showed the characteristics which were almost equal to the base metal from the result of obtaining metallic structure and strength of joint of brazing joint. However, the brazing filler metal composition of the melting point of 820 C or less could not be found. Consequentially, it was clarified that the brazing filler metal developed in this study could be practically sufficiently used from results such as metal structure of brazing joint and tensile test of the joint.

  • PDF

Development of Titanium-based Brazing Filler Metals with Low-melting-point

  • Onzawa, T.;Iiyama, T.
    • International Journal of Korean Welding Society
    • /
    • 제2권2호
    • /
    • pp.14-18
    • /
    • 2002
  • Titanium and titanium alloy are excellent in corrosion resistance and specific intensity, and also in the biocompatibility. On the other hand, the brazing is bonding method of which productivity and reliability are high, when the complicated and precise structure of the thin plate is constructed. However, though conventional titanium-based brazing filler metal was excellent in bond strength and corrosion resistance, it was disadvantageous that metal structure and mechanical property of the base metal deteriorated, since the brazing temperature ( about $1000^{\circ}C$ ) is considerably high. Authors developed new brazing filler metal which added Zr to Ti-Cu (-Ni) alloy which can be brazed at $900^{\circ}C$ or less about 15 years ago. In this paper, the development of more low-melting-point brazing filler metal was tried by the addition of the fourth elements such as Ni, Co, Cr for the Ti-Zr-Cu alloy. As a method for finding the low-melting-point composition, eutectic composition exploration method was used in order to reduce the experiment point. As the result, several kinds of new brazing filler metal such as 37.5Ti-37.5-Zr-25Cu alloy (melting point: $825^{\circ}C$) and 30Ti-43Zr-25Cu-2Cr alloy (melting point: $825^{\circ}C$) was developed. Then, the brazing joint showed the characteristics which were almost equal to the base metal from the result of obtaining metallic structure and strength of joint of brazing joint. However, the brazing filler metal composition of the melting point of $820^{\circ}C$ or less could not be found. Consequentially, it was clarified that the brazing filler metal developed in this study could be practically sufficiently used from results such as metal structure of brazing joint and tensile test of the joint.

  • PDF

Cu기 비정질 합금의 과냉각 액상구간에서 온간 압연시 Roll 온도의 영향 (Evolution of temperature gradients during rolling of $Cu_{54}Ni_6Zr_{22}Ti_{18}$ bulk metallic glass in the super cooled liquid region)

  • 박은수;이주호;김휘준;배정찬;허무영
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.409-412
    • /
    • 2006
  • Bulk metallic glass (BMG) strips of $Cu_{54}Ni_6Zr_{22}Ti_{18}$ were produced by warm rolling of the amorphous powder canned with copper. Controlling of temperatures of the rolled sample and rolls was essential for the successive rolling process. Because improper controlling of the sample temperature gave rise to the crystallization of BMG loading to the catastrophic fracture of BMG strips, the temperature of rolls should be properly controlled for achieving successful powder rolling of BMG. The variations of the strain state and temperature in the roll gap was simulated by the finite element method(FEM) using various roll temperatures.

  • PDF

입도분포에 따른 하상퇴적물의 지구화학적 분산 및 부화 (Geochemical Dispersion and Enrichment of Fluvial Sediments Depending on the Particla Size Distribution)

  • 이현구
    • 자원환경지질
    • /
    • 제32권3호
    • /
    • pp.247-260
    • /
    • 1999
  • Geochermical characteristics of the fluvial sediments deprnding on particle size distribution size were investigated in the respect of majir, minor and rare eath element chemisitry. Ratios of $Al_{2}O_{3}/Na_{2}O$ and $K_{2}O/Na_{2}O$ of the sediments show the homogeneous valus, and partly positive correlation with $SiO_{2}/Al_{2}O_{3}$, respecively. Characteristics of minor element ratios (V/Ni, Cr/V, Ni/Co and Zr/Hf)are within the lower and narrow range. Thesesuggested that sediment sources may be acidic to intermediate granitic rock, and may be explained by simple weathering and sedimentation. With increasing SiO2 contents, concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, CaO and MgO decreased, but those of $K_{2}O$ and $Na_{2}O$ increased, Concentrations of Ba, Be, Cs, Cu, Li, Ni, Sr, V and Zr show comparatively normal negative and some positive trends. Compared with the mean composition of granite, concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, MnO, CaO and MgO in the sediments of the study area were highly enriced. Among some minor and rare earth elements, concentrations of As, Cd, Cu, and V were enriched, but those of Be, Ce, Rb, Sc, Sr and Zn were depleted when compared with average composition of granite. By decreasing of particle size fractions, SiO2, Rb and Sr conterts decreased, but concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, CaO, MgO, $TiO_{2}$, MgO, $P_{2}O_{5}$, Be, Cu, Hf, Pb, V and Zr increased. From the correlations between particle size fractions and element concenreations, some elements of $Fe_{2}O_{3}$, CaO, MgO, $P_{2}O_{5}$, Cu, Ni, Zn and Zr showed typical trends in the secondary contramination sediments. These trends are typically shown under 100 mesh fractions. It indicates that the fraction of minus 100 mesh is the optimum size fraction for geochemical and environmental survey.

  • PDF

벌크비정질합금의 액상 성형성 평가 (Evaluation on Liquid Formability of Bulk Amorphous Alloys)

  • 주혜숙;강복현;김기영
    • 한국주조공학회지
    • /
    • 제26권5호
    • /
    • pp.227-231
    • /
    • 2006
  • Liquid formability of bulk amorphous alloys is known to be very poor due to their high viscosity comparing with conventional metallic materials. It is important to have the fabricating technology of bulk amorphous alloys in order to make the components with complicated shape. Liquid formability includes the mold cavity filling ability and the hot tear(crack) resistance during solidification. A mold made of a commercial tool steel for the formability test was designed. Melting was performed by the arc melting furnace with melting capacity of 200 g in an argon atmosphere. Liquid formability and glass forming ability of Cu base and Ni base bulk amorphous alloys were measured and evaluated. Mold filling ability of Ni-Zr-Ti-Si-Sn alloy was better than that of Cu-Ni-Zr-Ti alloy, however the reverse is the hot tear resistance. Bulk amorphous alloy is very susceptible to crack if partial crystallization occurs during solidification. Crack resistance was thought to be closely related with the glass forming ability.

동합금의 가공열처리법에 의한 기계적·전기적 성질 (The Effect of Thermo-Mechanical Treatment on Mechanical and Electrical Behavior of Cu Alloys)

  • 김형석;전채홍;송건;권숙인
    • 열처리공학회지
    • /
    • 제10권1호
    • /
    • pp.20-29
    • /
    • 1997
  • Pure copper is widely used for base material for electrical and electronic parts because of its good electrical conductivity. However, it has such a low strength that various alloying elements are added to copper to increase its strength. Nevertheless, alloying elements which exist as solid solution elements in copper matrix severely reduce the electrical conductivity. The reduction of electrical conductivity can be minimized and the strengthening can be maximized by TMT(Thermo-Mechanical Treatment) in copper alloys. In this research, the effects of TMT on mechanical and electrical properties of Cu-Ni-Al-Si-P, Cu-Ni-Al-Si-P-Zr and Cu-Ni-Si-P-Ti alloys aged at various temperatures were investigated. The Cu alloy with Ti showed the hardness of Hv 225, electrical conductivity of 59.8%IACS, tensile strength of 572MPa and elongation of 6.4%.

  • PDF

과냉각 액체 영역에서의 변형거동을 이용한 벌크 비정질 합금의 미세성형 기술 개발 (Micro Forming of Bulk Metallic Glass using the Deformation Behavior in the Supercooled Liquid Region)

  • 옥명렬;서진유;홍경태
    • 소성∙가공
    • /
    • 제13권1호
    • /
    • pp.9-14
    • /
    • 2004
  • Recently, various bulk metallic glasses (BMG's) having good mechanical and chemical properties were developed. BMG's can easily be deformed in the supercooled liquid region, via viscous flow mechanism. By using the viscous flow, the very low pressure is needed to deform the materials. In this study, we investigated the structural transition and deformation behavior of Vitreloy 1 (Zr/sub 41.2/Ti/sub 13.8/Cu/sub 12.5/Ni/sub 10/Be/sub 22.5/) using TMA and DSC. We applied the results to the micro forming process. The forming condition was chosen based on the viscosity data from TMA, and Si wafer with micro patterns on the surface was used as a forming die. The deformed surface was analyzed by SEM and 3D Surface Profiling System. The alloy showed good replication of the patterns. Quantitative measurement of roughness was useful to evaluate the replication. Surface condition of the deformed surface was determined by the initial surface condition.

역사시대에 분화한 백두산 화산재의 화학 성분 (Geochemical Composition of Volcanic Ash from Historical Eruptions of Mt. Baekdu, Korea)

  • 윤성효;고정선;장철우
    • 암석학회지
    • /
    • 제27권1호
    • /
    • pp.37-47
    • /
    • 2018
  • 백두산에서 역사시대에 분화한 화산재의 시료에 대하여 다양한 방법으로 주성분과 미량성분을 분석하였다. 화산재의 주성분 원소 함량은 $SiO_2$ 58.8~71.1 wt.%, $Al_2O_3$ 9.6~16.8 wt.%, ${Fe_2O_3}^T$ 4.5~6.9 wt.%, MgO 0.1~1.7 wt.%, CaO 0.3~1.6 wt.%, $Na_2O$ 5.2~6.3 wt.%, $K_2O$ 4.3~5.9 wt.% 그리고 $TiO_2$ 1.2 wt.%이하로 분석되었다. Ba, Cu, Cr. Co, Ni, Sr, V, Zn와 Zr을 포함하는 32개 미량원소가 분석되었는데, 이들 화산재는 일부 미량원소와 경희토류 원소의 부화정도에 따라 두 그룹(그룹 A, 그룹 B)으로 구분되며, 그룹 A에는 1천년 전의 밀레니엄 분화물, 1668년과 1903년 분화물이, 그룹 B에는 1702년 분화물이 해당된다. 중금속원소인 Cu, Co, Zn, Mn 등은 소량 함유되어 나타난다. 백두산 화산재는, 섭입대 기원의 일본 사쿠라지마 화산의 화산재와 비교하여, 미량성분원소 중 Y, Nb, Pb, U, Sc, V, Ni 그리고 Cu 함량은 낮게 나타나며, Zr, Ba, Hf, Cr, Co, Zn 그리고 희토류(Eu제외) 등은 높은 함량을 나타낸다.

Y$Ba_{2}$$Cu_{3}$$O_{7-\delta}$ coated conductors의 응용을 위한 단일완충층에 대한 연구 (A study on the single buffer layers for the application of $YBa_{2}$$Cu_{3}$$O_{7-\delta}$ coated conductors)

  • 정준기;최수정;고락길;;신기철;박유미;하홍수;김호섭;송규정
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2003년도 추계학술대회 논문집
    • /
    • pp.120-122
    • /
    • 2003
  • BaZrO$_3$and SrTiO$_3$(STO) thin films were Pulsed laser deposited on biaxially textured Ni and Ni-W alloy substrates to be used as single buffer layer for coated conductor. The texture of the films were analysed using the GADDS (general area detector diffraction system). Both films deposited on the metal tape were strongly (001) oriented, and in-plane textured (Δø (BZO) =9$^{\circ}$, Δø (STO) = 10$^{\circ}$).

  • PDF

열노출 온도에 따른 CP 티타늄, Ti-6Al-4V 합금의 미세조직/기계적성질 변화 및 저온브레이징 특성 (Effects of Holding Temperatures on Microstructure and Mechanical Properties of CP Titanium and Ti-6Al-4V Alloy and Its low Temperature Brazing Characteristics)

  • 선주현;신승용;홍주화
    • 열처리공학회지
    • /
    • 제23권1호
    • /
    • pp.3-9
    • /
    • 2010
  • Titanium and its alloys were brazed in the range of $850-950^{\circ}C$ within 10 min. of brazing time using expensive infra red or other heating methods. However, brazing time needs to be extended to get temperature-uniformity for mass production by using continuous belt type furnace or high vacuum furnace with low heating rate. This study examined effects of holding temperature for 60 min, on microstructure and mechanical properties of titanium alloys. Mechanical properties of titanium alloys were drastically deteriorated with increasing holding temperature followed by grain growth. Maximum holding temperatures for CP (commercial pure) titanium and Ti-6Al-4V were confirmed as $800^{\circ}C$ and $850^{\circ}C$, respectively. Both titanium alloys were successfully brazed at $800^{\circ}C$ for 60 min. with the level of base metal strengths by using Zr based filler metal, $Zr_{54}Ti_{22}Ni_{16}Cu_8$.