• 제목/요약/키워드: Ti powder

검색결과 1,433건 처리시간 0.023초

Ta20Nb20V20W20Ti20 하이엔트로피 합금의 미세조직 및 기계적 특성에 미치는 밀링 시간의 영향 (Effect of Milling Time on the Microstructure and Mechanical Properties of Ta20Nb20V20W20Ti20 High Entropy Alloy)

  • 송다혜;김영겸;이진규
    • 한국분말재료학회지
    • /
    • 제27권1호
    • /
    • pp.52-57
    • /
    • 2020
  • In this study, we report the microstructure and characterization of Ta20Nb20V20W20Ti20 high-entropy alloy powders and sintered samples. The effects of milling time on the microstructure and mechanical properties were investigated in detail. Microstructure and structural characterization were performed by scanning electron microscopy and X-ray diffraction. The mechanical properties of the sintered samples were analyzed through a compressive test at room temperature with a strain rate of 1 × 10-4 s-1. The microstructure of sintered Ta20Nb20V20W20Ti20 high-entropy alloy is composed of a BCC phase and a TiO phase. A better combination of compressive strength and strain was achieved by using prealloyed Ta20Nb20V20W20Ti20 powder with low oxygen content. The results suggest that the oxide formed during the sintering process affects the mechanical properties of Ta20Nb20V20W20Ti20 high-entropy alloys, which are related to the interfacial stability between the BCC matrix and TiO phase.

카본블랙을 첨가하여 제조한 다공성 BaTiO3계 세라믹스의 미세구조 및 PTCR 특성 변화 (Microstructure and PTCR Characteristics of Porous BaTiO3-based Ceramics Prepared by Adding Carbon Black)

  • 이기주;당동욱;조원승
    • 한국분말재료학회지
    • /
    • 제18권1호
    • /
    • pp.41-48
    • /
    • 2011
  • As a pore precursor, carbon black with different content of 0 to 60 vol% were added to (Ba,Sr)$TiO_3$ powder. Porous (Ba,Sr)$TiO_3$ ceramics were prepared by pressureless sintering at $1350^{\circ}C$ for 1h under air. Effects of carbon black content on the microstructure and PTCR characteristics of porous (Ba,Sr)$TiO_3$ ceramics were investigated. The porosity of porous (Ba,Sr)$TiO_3$ ceramics increased from 6.97% to 18.22% and the grain size slightly decreased from $7.51\;{\mu}m$ to $5.96\;{\mu}m$ with increasing carbon black contents. PTCR jump of the (Ba,Sr)$TiO_3$ ceramics prepared by adding carbon black was more than $10^5$, and slightly increased with increasing carbon black. The PTCR jump in the (Ba,Sr)$TiO_3$ ceramics prepared by adding 40 vol% carbon black showed an excellent value of $9.68{\times}10^5$, which was above two times higher than that in (Ba,Sr)$TiO_3$ ceramics. These results correspond with Heywang model for the explanation of PTCR effect in (Ba,Sr)$TiO_3$ ceramics. It was considered that carbon black is an effective additive for preparing porous $BaTiO_3$ based ceramics. It is believed that newly prepared (Ba,Sr)$TiO_3$ cermics can be used for PTC thermistor.

TiC 분산된 니켈기 합금의 미세조직 및 기계적 특성에 미치는 열처리 영향 (Effect of Heat Treatment on the Microstuctures and Mechanical Properties of TiC Dispersed Ni-base Alloy)

  • 홍성현;황금철;이원혁;진억용
    • 한국분말재료학회지
    • /
    • 제9권6호
    • /
    • pp.455-462
    • /
    • 2002
  • The microstructures and properties of TiC dispersed nickel-base alloy were studied in this work. The alloy prepared by powder metallurgical processing was solution treated, 1st-aged at $880^{\circ}C$ for 16 hours, and then 2nd-aged at $760^{\circ}C$ for 4 hours. Microstucture of sintered specimen showed that TiC particles are uniformly dispersed in Ni base alloy. In the specimen aged at $880^{\circ}C$ for 8 hours, the fine $\gammaNi_3$(Al,Ti) precipitates with round shape are observed and the very fine $\gammaNi_3$(Al,Ti) particles with round shape are precipitated in the specimen aged at $760^{\circ}C$ for 4 hours. The presence of ${\gamma}$precipitates in TiC/Ni base alloy increased the hardness and wear resistance of the specimen. The hardness and wear resistance of the Ni-base with TiC are higher than those of conventional Ni-base superalloy X-750 because of dispersion strengthening of TiC particles. The hardness, transverse rupture strength and resistance of the specimen 2nd-aged at $760^{\circ}C$ for 4 hours are higher than those of 1st-aged specimen due to ultrafine $\gammaNi_3$(Al,Ti) precipitates.

Laser Powder Bed Fusion 공정으로 제조된 Ti-6Al-4V 합금의 형상 차이에 따른 기계적 특성 변화 (Effect of Bulk Shape on Mechanical Properties of Ti-6Al-4V Alloy Manufactured by Laser Powder Bed Fusion)

  • 박하음;김연우;이승연;최중호;유지훈;김정기;박정민
    • 한국분말재료학회지
    • /
    • 제30권2호
    • /
    • pp.140-145
    • /
    • 2023
  • Although the Ti-6Al-4V alloy has been used in the aircraft industry owing to its excellent mechanical properties and low density, the low formability of the alloy hinders broadening its applications. Recently, laser-powder bed fusion (L-PBF) has become a novel process for overcoming the limitations of the alloy (i.e., low formability), owing to the high degree of design freedom for the geometry of products having outstanding performance used in high-tech applications. In this study, to investigate the effect of bulk shape on the microstructure and mechanical properties of L-PBFed Ti-6Al-4V alloys, two types of samples are fabricated using L-PBF: thick and thin samples. The thick sample exhibits lower strength and higher ductility than the thin sample owing to the larger grain size and lower residual dislocation density of the thick sample because of the heat input during the L-PBF process.

레이저 클래딩을 이용한 Ti-6AI-4V의 Zirconia 세라믹 분말 코팅 (Zirconia Ceramic Powder Coating of Ti-6AI-4V by Laser Cladding)

  • 강경호;김재도
    • 한국정밀공학회지
    • /
    • 제28권7호
    • /
    • pp.783-788
    • /
    • 2011
  • The recent development of bio-ceramic material is being studied in various bio-material engineering field. There are lots of technical difficulties because manufacturing or bonding technique are required bio-friendliness, cleanliness and persistence. Zirconia ceramic powder is cladded on Ti-6AI-4V metallurgically by laser cladding processing. Laser cladding system with powder feeding delivery is designed and manufactured for optimum processing condition. Increasing of manufacturing speed and good quality of clad layer are achieved by application of preheating of substrate before laser cladding. The thin dilution and good clad layer on the substrate are obtained for applications of bio-materials such as the dental materials and the articulated joints of human body.

마이크로파 수열법에 의한 PbTiO$_3$ PMN 세라믹분말의 합성 (Microwave Hydrothermal Sythesis of PbTiO$_3$ and PMN Ceramic Powders)

  • 배강
    • 한국세라믹학회지
    • /
    • 제35권5호
    • /
    • pp.465-471
    • /
    • 1998
  • Lead titanate(PT) and lead magnesium niobate(PMN) ceramic powders were prepared by microwave hy-drothermal method using teflon bomb. Raw materials were Pb(NO3)2 and TiO2 for lead titanate and Pb(NO3)2 Nb2O5 and Mg(NO)3.6H2O for PMN with NaOH as mineralizer in both cases. in lead titanate synthsis rate of microwave hydrothermal method was faster three times than one f conventional hydrothermal methods In lead magnesium niobate synthsis the mixture of perovskite and pyrochlore phases was obtained by single step technique and the PMN was not obtained by double step technique due to low temperature limitation of teflon bomb.

  • PDF

자체반응열 고온합성법에 의한 질화티타늄 합성에 관한 연구 (A Study on the Synthesis of Titanium Nitride by SHS(Self-propagating High-temperature Synthesis) Method)

  • 하호;김광래;이희철
    • 한국세라믹학회지
    • /
    • 제30권12호
    • /
    • pp.1096-1102
    • /
    • 1993
  • Titanium nitride was synthesized by reacting Ti powder with nitrogen gas using SHS method. In this process, the effects of nitrogen pressure, dilution with TiN, or additiion of titanium hydride(TiH1.924) on the conversion of Ti to TiN were investigated. In particular, much effects were given to solve the problem of the conversion drop due to partial melting and subsequent sintering of Ti parciels, by controlling combustion temperature and combustion wave velocity via mixing Ti powder with TiN or/and TiH1.924. For the diluted titanium powders with TiN, the conversion close to 100% was resulted when the nitrogen pressure was over 8atm and with diluent content of 60wt%, and the self-propagating reaction was not sustained when the diluent content was higher than 60wt%. For samples mixed to be 55wt% in Ti component in the mixture of Ti, TiH1.924, and 45% TiN, the conversion was closed to 100% when the amount of titanium hydride added was over 7wt% and the nitrogen pressure was higher than 5atm. The combustion reaction, however, was not sustained when titanium hydride added was more than 10wt%.

  • PDF

Sol-Gel법에 의한 강유전체 Pb(Zr, Ti)$O_3$의 제조 및 특성에 관한 연구 (Investigation on the property and preparation of ferroelectric Pb(Zr,Ti)$O_3$ by Sol-Gel method)

  • 임정한;김영식;장복기
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제7권6호
    • /
    • pp.496-503
    • /
    • 1994
  • In recent years Sol-Gel processing provides an interesting alternative method for the fabrication of ferroelectric thin layers and powder. PZT powder was prepared from an alkoxide-based solution by a Sol-Gel method. Gelation of synthesized complex solutions, microstructure, thermal analysis and crystallization behaviors of the calcined powder were studied in accordance with a water content and a catalyst. Especially gelation and crystallization behavior were analysed with the change of pH. The gelation time decreased as the pH of the mixed solution increased. For PZT powder with 650.deg. C heat treatment, 100% perovskite phase was formed by using either acidic or basic catalyst. By using either acidic or basic catalyst, we were able to get very fine powders of uniform shape with an average particle size of 0.8-1.mu.m.

  • PDF

하소분체의 입도조절에 따른 $BaTiO_3$ 요업체의 비정상 입성장거동 (Abnormal Grain Growth Behaviors of $BaTiO_3$ Ceramics with Controlling of Particle Size Distributjion of Calcined Powder)

  • 이태헌;김정주;김남경;조상희
    • 한국세라믹학회지
    • /
    • 제32권2호
    • /
    • pp.147-154
    • /
    • 1995
  • Abnormal grain growth behavior of BaTiO3 ceramics with controlling of particle size distribution of calcined powder was investigated. The particle size distribution was controlled by changing the calcining temperature or by using of classification and regrinding process. With broadening of the normallized size distribution in calcined powder, it showeda normal grain growth behavior in sintered body due to an increase of volume fraction of seed grain in the calcined powder. It was supposed that the seed grains could easily contact each other for the rapid grain growth during sintering process and resulted in fast switching-over from abnormal to normal grain growth stage.