z-cut $Ti;LiNbO_3$ Waveguide Optical Properties and lnsertion Loss As a Function of $Ti;LiNbO_3$thickness Fabricated by wet Oxygen Atmosphere (Wet Oxygen 분위기로 제작한 z-cut $Ti;LiNbO_3$도파로 광특성 및 두께에 따른 삽입손실)

  • Kim, Seong-Ku;Yoon, Hyung-Do;Yoon, Dae-Won;Park, Gye-Choon;Chung, Hae-Duck;Lee, JIn
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.11 no.10
    • /
    • pp.903-910
    • /
    • 1998
  • Ti:LiNbO$_3$ optical waveguides have been fabricated by Ti-diffusion in wet oxygen atmosphere. The fabrication conditions of furnace temperature, diffusion time and bubbler temperature were 105$0^{\circ}C$, 8 hours and 9$0^{\circ}C$, respectively and Ti thickness was varied from 700$\AA$ to 1500$\AA$. In this paper, the nearfield patterns, mode sizes (hirizontal/vertical) and insertion loss of waveguides were discussed at wavelength 1550 nm ad function of Ti thickness. With the planar waveguide, the effective index change and diffusion depth were calculated at 632.8nm using the prism coupling method. From these results, the best Ti thickness in our conditions seems like to by 1200$\AA$~1300$\AA$.

  • PDF

Fabrication and Characteristics of z-cut Ti:LiNbO$_3$ Internal Chip for Optical Modulator (z-cut $Ti:LiNbO_3$광변조기 내부칩 제작 및 특성평가)

  • Kim, Seong-Ku;Yoon, Hyung-Do;Lee, Han-Young;Park, Gye-Choon;Lee, Jin;Kang, Sung-Jun
    • Proceedings of the IEEK Conference
    • /
    • 1999.06a
    • /
    • pp.319-322
    • /
    • 1999
  • In this paper, we report characteristics of a internal chip of LiNbO$_3$ modulator with low-driving-voltage at 150nm wavelength. A Ti diffusion method for LiNbO$_3$ optical waveguide and a buffer layer for improving phase velocity mismatch between optical and microwave waves were employed. The traveling-wave coplanar waveguide electrode of 35mm is used for reducing the driving voltage. From this work, wideband modulation of 10㎓ and low-driving voltage of 3.9volts are realized.

  • PDF

Fabrication and Characterization of Ti:LiNbO_3$ Optical Waveguides (확산방식에 의한 Ti:LiNbO_3$ 광도파로의 제작 및 특성측정)

  • 손영성;강원구;갑상영;권영세
    • Journal of the Korean Institute of Telematics and Electronics
    • /
    • v.25 no.3
    • /
    • pp.343-351
    • /
    • 1988
  • Planar optical waveguides are fabricated on a Y-cut LiNbO3 single crystal substrate by Ti indiffusion method. From data measured by the bright M-line spectroscopy, refractive index profiles are reconstructed by WKB approximation method. Then, single strip, X-crossing strip, and Y-brinch strip optical waveguides are fabricated on X-cut LiNbO3 single crystal substrate, with waveguide patterns made by the laser beam direct writing method. And their near-field intensity profiles are observed after coupling the light to the waveguide edges.

  • PDF

Fabrication of a $LiNbO_3$ Single-Mode Optical Waveguide ($LiNbO_3$ 단일모드 광도파관의 제작)

  • 박동철
    • Journal of the Korean Institute of Telematics and Electronics
    • /
    • v.16 no.2
    • /
    • pp.15-18
    • /
    • 1979
  • Deposited film of a transition metal, Ti was diffused into LiNbO3 crystals to form integrated optical waveguides. By suppressing L O out -diffusion, single-mode waveguides could be constructed. Measurements on characteristics were performed by using the prise coupling technique and a He-Ne laser. ( λ = 0.6328 $\mu$m)

  • PDF

2×2 Ti:LiNbO3 optical add/drop multiplexers utilizing tilted film-loaded SAW waveguides (Tilted Film-Leaded SAW 도파로를 이용한 2×2 Ti:LiNbO3 광 삽입/분기 멀티플렉서)

  • 강창민;정흥식
    • Korean Journal of Optics and Photonics
    • /
    • v.14 no.6
    • /
    • pp.657-662
    • /
    • 2003
  • Optimum Hamming apodized acousto-optic 2${\times}$2 add/drop multiplexers, using SiO$_2$ film loaded acoustic waveguide with angular offset to the Ti:LiNbO$_3$ waveguide, were fabricated. The four-port device consists of two input waveguides, a polarization beam splitter (PBS), two polarization conversion/acoustooptic tuning waveguide sections, a second PBS and two output waveguides. Insertion loss <7.1 ㏈ has been obtained and side-lobe of -19 ㏈ for -32 ㎽ RF driving power has been realized. Add/drop performance has been confirmed and a linear tuning rate of 8.1 nm/MHz and a 3 ㏈ spectral width of -1.5 nm were demonstrated.

Fabrication of Electro-Optic Grating Modulator Using $Ti:LiNbO_3$ Optical Waveguide ($Ti:LiNbO_3$ 광도파로를 이용한 전기광학 격자형 변조기 제작)

  • 노대철;이철규;윤태훈;김재창;한정희;이용탁
    • Journal of the Korean Institute of Telematics and Electronics
    • /
    • v.26 no.10
    • /
    • pp.1584-1590
    • /
    • 1989
  • In this study, a planar waveguide has been fabricated on a Y-cut LiNbO3 substrate by the Ti indiffusion technique and its guiding characteristics are measured by bright M-line spectroscopy. Using the photolithography method, an electro-optic grating modulator with interdigital electrodes has been fabricated by depositing Al on the Ti:LiNbO3 planar waveguide. And the beam intensity diffracted by the grating is measured as the applied voltage is increased.

  • PDF

A Study on the Fabrication LiNbO3 Optical Waveguide (LiNbO3 광도파로 제작에 관한 연구)

  • Kim, Sun-Yeob
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.16 no.9
    • /
    • pp.6221-6226
    • /
    • 2015
  • In this paper, waveguide analysis was interpreted as an optical waveguide using the feedback perturbation method simple and easy to apply compared to the analysis method, while the other almost identical to the numerical calculation method. In addition, efficient coupling with an optical transmission line of optical fiber and the waveguide form the thin film of different functional elements is required in order to achieve the full optical communication system. However, problems arise, such as the light field (field) and the decrease of the access efficiency due to inconsistency in the distribution characteristics of the connection surface by the difference in size of the cross section thereof when connecting the optical fiber and the waveguide directly to the combination of a thin film. Therefore propose a new type of connector structure to increase the efficiency of the connection when connecting the optical fiber waveguide and the thin film was analyzed by applying a coupled mode theory, the binding efficiency of the modified contactor. And by diffusing Ti on the $LiNbO_3$ substrate and a wide range of applications in the manufacture of integrated optical material made of a current low-loss Ti: $LiNbO_3$ optical waveguide and making the Y-branch waveguide, and the properties were confirmed.

The Pigrailing and The Loss Analysis of low loss LiNbO$_3$ Optical Waveguide with Fiber-to-fiber Insetion Loss<6dB (Total Fiber-to-fiber Insertion Loss가 <6dB 인 Ti:$LiNbO_3$ 과도파로 Pigtailing 및 손실분석)

  • 김성구;박계춘;조재철
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.11 no.7
    • /
    • pp.557-564
    • /
    • 1998
  • A low loss x-cut $LiNbO_3$optical waveguide was fabricated by Yi in-diffusion, and the properties of guided-mode and the total insertion loss of the pigtailed waveguide with polarization maintaining fiber(PMF) were measured at optical wavelength 1550nm. for forming the waveguides, the parameters of diffusion, Ti thickness, waveguide line-width, length, diffusion temperature, time and atmosphere were set $1400{\AA}$, $8{\mu}m$, 3.3cm, $1050^{\circ}C$, 8 hours and wet bubbled oxygen, respectively. And then after the polishing and piatailing, it showed that the total insertion loss was -4.1dB for TM mode, -5.5dB for TE mode, and mode size, that is, the horizontal/ vertical size were $13.8{\mu}m/18{\mu}m$ for TM mode, $9.6{\mu}m/6.5{\mu}m$ for TE mode.

  • PDF

Optical Characterizations of $LiNbO_{3}$ Single Crystals Doped with $MgO/TiO_{2}$

  • You-song Kim
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.1 no.1
    • /
    • pp.1-4
    • /
    • 1991
  • The applicability of $LiNbO_{3}$ as a substrate for fabrication of Ti-indiffused waveguide electro-optic devices is limited. Ti diffuses comparatively in congruently melting $LiNbO_{3}$; the Curie temperature of this material is too low to permit diffusion temperatures much above $1100^{\circ}C$ without the necessity of re-poling the crystal. Both of hese difficulties could be eliminated by incorporating certain dopants in $LiNbO_{3}$. Crystals of $LiNbO_{3}$ doped with Ti and Mg were grown and evaluated. The electroptic coefficients and birefringence of $LiNbO_{3}$ doped crystals were measured at ${\lambda}=.6328$ and $1.32\;$\mu{m}$. Curie temperatures were measured. The Curie temperature of both undoped and Ti-doped $LiNbO_{3}$ was $1130^{\circ}C$; that for Mg-doped $LiNbO_{3}$ was $30^{\circ}$ higher. From these data, a composition for the crystals was estimated. Thermogravimetric data confirmed this estimate and showed that the composition of Mg : $LiNbO_{3}$ was $49.3{\pm}0.2mole%\;Li_{2}O$ ; the composition of the undoped and Ti : $LiNbO_{3}$ samples was $48.6{\pm}0.2mole%$. Diffusion of Ti into both Mg-doped and Ti-doped $LiNbO_{3}$ crystals was studied as a function of $Li/NbO_{3}$ ratio and temperature.

  • PDF

Fabrication of High Speed Optical Matrix Wwitch by Ti:Ti:LiNbO3 (Ti:Ti:LiNbO3를 이용한 초고속 광 매트릭스 스위치 제조)

  • Yang, U-Seok;Kwak, Yong-Seok;Kim, Je-Min;Yoon, Hyeong-Do;Lee, Han-Yeong;Yoon, Dae-Ho
    • Korean Journal of Materials Research
    • /
    • v.12 no.4
    • /
    • pp.254-258
    • /
    • 2002
  • To realize channel cross-connecting in optical communications systems, a high speed optical matrix switch was fabricated using z-cut $LiNbO_3$. For switch fabrication was design bending structure and coupling length and four $2{\times}2$ directional couplers were integrated on one substrate far construction of a $4{\times}4$ switch. Single-mode optical waveguides were formed by Ti-diffusion at a wet $O_2$ atmosphere. Ti-diffusion profile, refractive index variation and waveguide morphology were analyzed by Prism coupler and optical microscopy, respectively.