A Study on the Coated Characteristics of Ceramic Tools (세라믹공구 재료의 피복특성에 관한 연구)

  • Lee, Myeong-Je;Im, Hong-Seop;Yu, Bong-Hwan
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.4 s.175
    • /
    • pp.900-906
    • /
    • 2000
  • Ceramic, PCD and CBN tools are available for the difficult-to-cut-materials such as hardened carbon tool steel, stainless steel, Inconel 718 and etc. Ceramic tools are likely to be chipped and abruptly broken before the appearance of normal wear in turning. Ceramic tools are suitable for continuous in turning, not for intermittent in milling. In this study, TiN/TiCN multi-layer coated ceramic tools were found to restrain the chipping, breaking and early fracture and to increase the critical cutting speed owing to TiN/TiCN multi-layer coating in Arc Ion Plating of PVD method.

Effect of $Mo_2C$ Content on the Microstructure and Properties of Ti(CN)-$Mo_2C$ Ceramics

  • Park, Dong-Soo;Lee, Yang-Doo;Taejoo Jung
    • The Korean Journal of Ceramics
    • /
    • v.5 no.3
    • /
    • pp.230-234
    • /
    • 1999
  • Ti(CN)-0.3mole% $Mo_2C$ ceramics were prepared by pressureless sintering. $Mo_2C$ dissolved in Ti(CN) more easily in a nitrogen environment than in the other environment because nitrogen forced Mo to form a solid solution, (Ti, No)(C, N). A "core-rim" structure developed within the grains. The boundary between the "core" and the rim was delineated by thermal etching in the sample with more than 2 mole% $Mo_2C$. The rim thickness and the grain size decreased as the $Mo_2C$ content increased. The hardness and the flexural strength showed maxima of 18.2 GPa and 1.23 GPa, respectively when the $Mo_2C$ content was 2 mole%. The post-sintering heat treatments improved the properties.oved the properties.

  • PDF

Comparison of Degradation Behaviors for Titanium-based Hard Coatings by Pulsed Laser Thermal Shock

  • Jeon, Seol;Lee, Heesoo
    • Journal of the Korean Ceramic Society
    • /
    • v.50 no.6
    • /
    • pp.523-527
    • /
    • 2013
  • Ti-based coatings following laser ablation were studied to compare degradation behaviors by thermomechanical stress. TiN, TiCN, and TiAlN coatings were degraded by a Nd:YAG pulsed laser with an increase in the laser pulses. A decrease in the hardness was identified as the pulses increased, and the hardness levels were in the order of TiAlN > TiCN > TiN. The TiN showed cracks on the surface, and cracks with pores formed along the cracks were observed in the TiCN. The dominant degradation behavior of the TiAlN was surface pore formation. EDS results revealed that diffusion of substrate atoms to the coating surface occurred in the TiN. Delamination occurred in the TiN and TiCN, while the TiAlN which has higher thermal stability than the TiN and TiCN maintained adhesion to the substrate. It was considered that the decrease in the hardness of the Ti-based hard coatings is attributed to surface cracking and the diffusion of substrate atoms.

The Effects of Deposition Temperature and RF Power on the Plasma Assisted Chemical Vapor Deposition of TiCN Films (증착온도와 RF Power가 TiCN박막의 플라즈마 화학증착에 미치는 영향)

  • 김시범;김광호;김상호;천성순
    • Journal of the Korean Ceramic Society
    • /
    • v.26 no.3
    • /
    • pp.323-330
    • /
    • 1989
  • Wear restance titanium carbonitride (TiCN) films were deposited on the SKH9 tool steels and WC-Co cutting tools by plasma assisted chemical vapor deposition (PACVD) using a gaseous mixture of TiCl4, CH4, N2, H2 and Ar. The effects of the deposition temperature and RF(Radio Frequency) power on the deposition rate, chlorine content and crystallinity of the deposited layer were studied. The experimental results showed that the stable and adherent films could be obtained above the deposition temperature of 47$0^{\circ}C$ and maximum deposition rate was obtained at 485$^{\circ}C$. The deposition rate was much affected by RF power and maximum at 40W. The crystallinity of the deposited layer was improved with increasing the deposition temperature and RF power. The TiCN films deposited by PACVD contained much chlorine. The chlorine content in the TiCN films was affected by deposition conditions and decreased with improving the crystallinity of the deposited layer. The deposited TiCN films deposited at the deposition temperature of 52$0^{\circ}C$ and RF power of 40W had an uniform surface with very fine grains of about 500$\AA$ size. The microhardness of the deposited layer was 2,300Kg/$\textrm{mm}^2$.

  • PDF

Fatigue crack growth properties of ceramic coated 1Cr-1Mo-0.25V steel (세라믹 코팅된 1Cr-1Mo-0.25V강의 피로균열성장 특성)

  • Seo, Chang-Min;Kim, Gyeong-Ryeol
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.21 no.10
    • /
    • pp.1674-1682
    • /
    • 1997
  • Fatigue tests were performed to investigate the effect of ceramic coatings as in TiN and TiCN on fatigue crack growth properties of ceramic coated 1Cr-1Mo-0.25V steel with different coating thickness in laboratory air conditions. The experimental results are described with respect to a Paris equation, da/dN=C(.DELTA.K)$^{m}$ , where the crack growth rate of coated specimens provided as similar growth rate as that of the uncoated specimen regardless of coating thickness. Furthermore, it was observed that the type of coating layer had virtually no effect on crack growth rate in the full region of stress intensity factor range. And it was also appeared that the final crack length of TiCN coated specimens was short compared to that of TiN coated, and the substrate specimens, in which it was inferred due to lowering the toughness of coated material from high hardness of TiCN coating layer itself.

Effect of VC Addition on the Microstructure & Mechanical Properties of Ti(CN)-based Cermet (VC 첨가가 Ti(CN)계 써메트의 미세구조 및 기계적 성질에 미치는 영향)

  • 안성용;강신후
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.12
    • /
    • pp.1316-1322
    • /
    • 1998
  • The amount of VC and C/N ratio in Ti(CN) was varied to investigate the effect of VC addition on the mi-crostructural change in Ti(CN)-Ni system. As the amount of VC addition increases in Ti(C0.7N0.3)-20Ni sys-tem a complete solid solution was observed in Ti(C0.7N0.3)-20Ni-25VC system. It implies that the ratio of the dissolution rates of Ti(C0.7N0.3)to that of VC is nearly 2:1 at the sintering conditions used in this study. It was found from the experiments that the system composed of the Ti(C0.7N0.3) phase exhibits a rimless structure and relatively small amount of solid solution. That is among Ti(C0.7N0.3) phase exhibits a rimless structure and relatively small amount of solid solution. This is among Ti(C1-xNx) phases the dissolution rate of Ti(C0.3N0.7) is the lowest. Also fracture toughness(KIC) of the cermet was measured by indentation method. Attentions were paid to crack propagation path to look for a dominant fracture mode and to cor-relate it with fracture toughness values. The fracture toughness was relatively high with the addition of VC content. But the addition of a large VC content reduced the overall toughness of the cermet. This result is explained with the difference in fracture mode.

  • PDF

A Study on the Coated Characteristics of Ceramic Tools (코팅공구의 절삭성능에 관한 연구)

  • 유봉환
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.9 no.1
    • /
    • pp.96-101
    • /
    • 2000
  • Ceramic, PCD and CBN tools are available for the difficult-to-cut-materials such as hardened carbon tool steel, stainless steel, Inconel 718 and etc.. Ceramic toolsare likely to be chipped and abruptly broken before the appearance of normal wear in turning. Ther2efore ceramic tools are suitable for continuous cut in turning not for intermittent in milling. In this study, TiN/TiCN multi-layer coated ceramic tools were found to restrain the chipping, breaking and early fracture and to increase the critical cutting speed owing to TiN/TiCN multi-layer coating in Arc Ion Plating of PVD method.

  • PDF