• 제목/요약/키워드: Thin Film of (Ti,Cr)N

검색결과 17건 처리시간 0.017초

아크이온플레이팅에 의한 질화 티탄-크롬의 박막특성 평가 (Evaluation for Thin Films Characteristics of Nitride Titanium-Chromium using Arc Ion Plating)

  • 후지타 카즈히사;양영준
    • 한국기계가공학회지
    • /
    • 제10권4호
    • /
    • pp.96-101
    • /
    • 2011
  • The thin films of TiN have been used extensively as wear-resistant materials, for instance, such as tools of high-speed cutting, metal mold forming etc. In these days, because the thin films capable of being used more severe conditions are needed, the technologies of arc ion plating are tried to improve its characteristics. The purpose of this study is to investigate the characteristics of thin films of (Ti,Cr)N compared with those of TiN. The method of arc ion plating, which is known as showing good tight-adherence and productivity, was used. After manufacturing thin films of ($Ti_{1-x}Cr_{x}$)N (x=0~1) with change of Cr in (Ti,Cr) target, atomic concentration, structure, size of crystallite, residual stress and surface roughness of thin films on substrate were investigated. As the results, it was confirmed that Cr atomic concentrations of thin films were proportionally changed with Cr atomic concentrations of target, and thin films of ($Ti_{1-x}Cr_{x}$)N (x=0~1) showed NaCl type and CrN existed as solid solution to TiN.

CrN 박막처리된 Ti-6Al-4V 합금의 기계적 성질과 피로특성 (Mechanical Properties and Fatigue Characteristics of CrN Coated Ti-6Al-4V alloy)

  • 박용권;백창현;위명용
    • 한국재료학회지
    • /
    • 제12권8호
    • /
    • pp.669-675
    • /
    • 2002
  • CrN film coated by AIP method, improved the mechanical properties (Hardness, Roughness, wear and fatigue) of Ti-6Al-4V alloy. The properties were studied using GXRD, XPS, Hardness, Roughness, wear and fatigue testers. CrN thin film thickness was about 7.5$\mu\textrm{m}$ and grew with (111) orientation. Hardness of CrN thin film was very high (Hv 1390) and roughness of the surface layer was greatly improved (Ra=0.063$\mu\textrm{m}$) compared with matrix alloy (Ra=0.321$\mu\textrm{m}$). Such changes of hardness and roughness could be contributed to improving the wear resistance and fatigue life. Striation like pattern with dimples and voids, a typical fatigue fracture mode, was observed throughout the specimen.

Adhesive Behaviors of the Aluminum Alloy-Based CrN and TiN Coating Films for Ocean Plant

  • Murakami, Ri-Ichi;Yahya, Syed Qamma Bin
    • International Journal of Ocean System Engineering
    • /
    • 제2권2호
    • /
    • pp.106-115
    • /
    • 2012
  • In the present study, TiN and CrN films were coated by arc ion plating equipment onto aluminum alloy substrate, A2024. The film thickness was about 4.65 ${\mu}m$. TiN and CrN films were analyzed by X-ray diffraction and energy dispersive X-ray equipments. The Young's modulus and the micro-Vickers hardness of aluminum substrate were modified by the ceramic film coatings. The difference in Young's modulus between substrate and coating film would affect on the wear resistance. The critical load, Lc, was 75.8 N for TiN and 85.5 N for CrN. It indicated from the observation of optical micrographs for TiN and CrN films that lots of cracks widely propagated toward the both sides of scratch track in the early stage of MODE I. TiN film began to delaminate completely at MODE II stage. The substrate was finally glittered at MODE III stage. For CrN film, a few crack can be observed at MODE I stage. The delamination of film was not still occurred at MODE II and then was happened at MODE III. This agrees with critical load measurement which the adhesive strength was greater for CrN film than for TiN film. Consequently, it was difficult for CrN to delaminate because the adhesive strength was excellent against Al substrate. The wear process, which the film adheres and the ball transfers, could be enhanced because of the increase in loading. The wear weight of ball was less for CrN than for TiN. This means that the wear damage of ball was greater for TiN than for CrN film. It is also obvious that it was difficult to delaminate because the CrN coating film has high toughness. The coefficient of friction was less for CrN coating film than for TiN film.

치과 임플란트 스크루 풀림토크 개선용 DLC 박막 코팅에 관한 연구 (A Study on the DLC Film Coating for Improving Loosening Torque of Dental Implant Screw)

  • 정운조;조재철
    • 전기학회논문지
    • /
    • 제67권10호
    • /
    • pp.1375-1381
    • /
    • 2018
  • In this paper, we studied coatings of the DLC thin film for improving loosening torque of dental implant screw. We used a filtered arc ion plating process which can realize the most dense DLC layer by coating the DLC thin film on the surface of the dental abutment screw. It showed both hardness comparable to diamond and low friction coefficient similar to graphite, and to improve the loosening phenomenon by increasing the screw tightening force Cr/CrN, Ti/TiN or Ti/TiN/Cr/CrN buffer layers were deposited for 5 to 10 minutes to improve the adhesion of the DLC thin film to the surface of the Ti (Gr.5), and then the DLC thin film was coated for about 15 minutes. As a result, the Cr/CrN buffer layer exhibited the highest hardness of 29.7 GPa, the adhesion of 18.62N on average, and a very low coefficient of friction of less than 0.2 as a whole. And we measured loosening torque after one million times with masticatory movement simulator. As a result, the values of the coated screw loosening torque were clearly higher than those of the uncoated screw. From this, it was found that the DLC coating was effective methods improving the loosening torque. In addition, it was confirmed that the cytotoxicity test and cell adhesion test showed high biocompatibility.

$TaN/Al_{2}O_{3}$ 박막 저항소자 개발에 관한 연구 (A study on TCR characteristic of $TaN/Al_{2}O_{3}$ thin film resistors)

  • 김인성;조영란;민복기;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 센서 박막재료 반도체재료 기술교육
    • /
    • pp.82-85
    • /
    • 2002
  • In recent years, the tantalum nitride(TaN) thin-film has been developed for the electronic resistor and capacitor. In this papers, this study presents the surface profile and sheet-resistance property relationship of reactive-sputtered TaN thin film resistor processed by buffer of Ti and Cr on alumina substrate. The TCR properties of the TaN films were discussed in terms of reactive gas ratio, ratio of nitrogen, crystallization and thin films surface morphology due to annealing temperature. It is clear that the TaN thin-films resistor electrical properties are low TCR related with it's buffer layer condition. Ti buffer layer thin film resistor having a good thermal stability and lower TCR properties then Cr buffer expected for the application to the dielectric material of passive component.

  • PDF

AIP 와 스퍼터링으로 복합증착된 420 스테인리스강의 TiN과 CrN 박막에 미치는 중간층의 영향 (Effect of Interlayer on TiN and CrN Thin Films of STS 420 Hybrid-Deposited by AlP and DC Magnetron Sputtering)

  • 최웅섭;김현승;박범수;이경구;이도재;이광민
    • 한국재료학회지
    • /
    • 제17권5호
    • /
    • pp.256-262
    • /
    • 2007
  • Effects of interlayer and the combination of different coating methods on the mechanical and corrosion behaviors of TiN and CrN coated on 420 stainless steel have been studied. STS 420 specimen were tempered at $300^{\circ}C$ for 1 hr in vacuum furnace. The TiN and CrN thin film with 2 ${\mu}m$ thickness were coated by arc ion plating and DC magnetron sputtering following the formation of interlayer for pure titanium and chromium with 0.2 ${\mu}m$ thickness. The microstructure and surface analysis of the specimen were conducted by using SEM, XRD and roughness tester. Mechanical properties such as hardness and adhesion also were examined. XRD patterns of TiN thin films showed that preferred TiN (111) orientation was observed. The peaks of CrN (111) and $Cr_2N$ (300) were only observed in CrN thin films deposited by arc ion plating. Both TiN and CrN deposited by arc ion plating had the higher adhesion and hardness compared to those formed by magnetron sputtering. The specimen of TiN and CrN on which interlayer deposited by magnetron sputtering and thin film deposited by arc ion plating had the highest adhesion with 22.2 N and 19.2 N. respectively. TiN and CrN samples shown the most noble corrosion potentials when the interlayers were deposited by using magnetron sputtering and the metal nitrides were deposited by using arc ion plating. The most noble corrosion potentials of TiN and CrN were found to be approximately -170 and -70 mV, respectively.

Adhesion of Human Osteoblasts Cell on CrN Thin Film Deposited by Cathodic Arc Plasma Deposition

  • Pham, Vuong-Hung;Kim, Sun-Kyu
    • 한국표면공학회지
    • /
    • 제42권5호
    • /
    • pp.203-207
    • /
    • 2009
  • Interaction between human osteoblast (hFOB 1.19) and CrN films was conducted in vitro. CrN films were produced by cathodic arc plasma deposition. The surface was characterized by atomic force microscopy (AFM). CrN films, glass substrates and TiN films were cultured with human osteoblasts for 48 and 72 hours. Actin stress fiber patterns and cell adhesion of osteoblasts were found less organized and weak on CrN films compared to those on the glass substrates and the TiN films. Human osteoblasts also showed less proliferation and less distributed microtubule on CrN films compared to those on glass substrates and TiN films. Focal contact adhesion was not observed in the cells cultured on CrN films, whereas focal contact adhesion was observed well in the cells cultured on glass substrates and TiN films. As a result, the CrN film is a potential candidate as a surface coating to be used for implantable devices which requires minimal cellular adhesion.

플라즈마 침탄 및 CrN 코팅된 Ti-6Al-4V 합금의 구조 및 Creep특성 (Creep Properties of Plasma Carburized and CrN Coated Ti-6Al-4V Alloy)

  • 위명용;박용권
    • 한국재료학회지
    • /
    • 제14권8호
    • /
    • pp.558-564
    • /
    • 2004
  • In order to improve the low hardness and low wear resistance of Ti-6Al-4V alloy, plasma carburization treatment and CrN film coating were carried out. Effects of the plasma carburization and CrN coating were analyzed and compared with the non-treated alloy by mechanical and creep tests. After plasma carburization and CrN coating treatments, the carburized layer was about 150 ${\mu}m$ in depth and CrN coated layer was about 7.5 ${\mu}m$ in thickness. Hardness value of about $H_{v}$ 402 of the non-treated alloy was improved to $H_{v}$ 1600 and 1390 by plasma carburization and CrN thin film coating, respectively. Stress exponent(n) was decreased from 9.10 in CrN coating specimen to 8.95 in carburized specimen. However, the activation energy(Q) was increased from 242 to 250 kJ/mol. It can be concluded that the static creep deformation for Ti-6Al-4V alloy is controlled by the dislocation climb over the ranges of the experimental conditions.

TiZrN 박막의 조성이 구조적 특성 및 열적 특성에 미치는 영향 (Effect of composition on the structural and thermal properties of TiZrN thin film)

  • 최병수;엄지훈;석민준;이병우;김진곤;조현
    • 한국결정성장학회지
    • /
    • 제31권1호
    • /
    • pp.37-42
    • /
    • 2021
  • 화학적 조성이 TiZrN 박막의 구조적 특성 및 열적 특성에 미치는 영향을 조사하였다. 증착된 TixZr1-xN(x = 0.87, 0.82, 0.7, 0.6, 0.28) 박막에서 Zr 분율이 증가함에 따라 결정립 크기가 감소하고 주상 구조에서 입계상 구조로 점진적으로 변화하는 미세구조 변화가 관찰되었다. 또한 XRD 분석을 통해 Zr 분율이 0.4까지 증가할 때 TiN 상에서 TiZrN 상으로의 점진적인 결정상 전이가 일어났음을 확인하였다. 900℃ 온도에서의 열처리 이후 Ti0.82Zr0.18N과 Ti0.7Zr0.3N 박막은 rutile 상 TiO2와 TiZrO4 산화물이 공존하는 형태로 전환된 반면에 Ti0.6Zr0.4N 박막은 TiZrO4 산화물로 변화함을 확인하였다. 다섯 가지 조성의 TiZrN 박막 중에서 Ti0.6Zr0.4N 박막이 가장 우수한 고온 안정성을 나타내었고, Inconel 617 기판의 열산화에 의해 발생하는 Cr의 표면 확산을 억제하는 열산화 저항성 향상 효과가 가장 우수함을 확인하였다.

이온주입 제어에 의한 재료특성 개선에 관한 연구 (A Study on Improvement of Material Characteristics by Control of Ion Implantation)

  • 양영준;이치우;후지타 카즈히사
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제32권8호
    • /
    • pp.1178-1184
    • /
    • 2008
  • In this study, techniques of ion implantation were used in order to improve the characteristics of metal materials such as the oxidation and wear resistant. In particular it is necessary to develope their oxidation and wear resistant that could be used in severe environmental conditions. There are mainly two elementary technologies including ion implantation and/or thin film coating. Ion implantation method was performed for surface modification. As a result, it was found that some ion implantations methods such as Nb, high-temperature Nb ion implantation and Nb+C combined implantation are somewhat effective for improving the oxidation resistance of TiAl alloy. Furthermore, the fluorine PBII treatment is more effective for improving the oxidation resistance of the TiAl alloy with three-dimensional shapes. The implantation of boron ion into thin film of TiN was also effective for improving the properties of materials like high temperature wear resistance. TiCrN film was applied to the actual seal ring for steam turbines, and it was observed that its sliding property showed a successfully good performance.