열간압축성형으로 제조한 Co1-xNixSb3의 열전특성 (Thermoelectric Properties of Co1-xNixSb3 Prepared by Hot Pressing)

  • 김미정;어순철;김일호
    • 한국재료학회지
    • /
    • 제16권6호
    • /
    • pp.382-385
    • /
    • 2006
  • Ni-doped $CoSb_3$ was prepared by the hot pressing, and its doping effects on the thermoelectric properties were investigated. Single phase ${\delta}-CoSb_3$ was successfully obtained by encapsulated induction melting and the subsequent heat treatment at 773 K for 24 hrs, followed by the hot pressing under 60 MPa at 773 K for 2 hrs. Nickel atoms acted as electron donors by substituting cobalt atoms. Thermoelectric properties were remarkably improved by the Ni doping.

Thermoelectric Properties of Ni-doped $CoSb_3$ Prepared by Encapsulated Induction Melting and Hot Pressing

  • Kim, Mi-Jung;Park, Kwan-Ho;Jung, Jae-Yong;You, Sin-Wook;Lee, Jung-Il;Ur, Soon-Chul;Kim, Il-Ho
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.688-689
    • /
    • 2006
  • Ni-doped $CoSb_3$ was prepared by the encapsulated induction melting and hot pressing, and its doping effects on the thermoelectric properties were investigated. Single phase $\delta-CoSb_3$ was successfully obtained by the subsequent heat treatment at 773K for 24 hours. Nickel atoms acted as electron donors by substituting cobalt atoms. Thermoelectric properties were remarkably improved by the appropriate doping.

  • PDF

6H-SiC로부터 제작한 SiC 세라믹스의 열전변환 특성 (Thermoelectric Conversion Characteristics of SiC Ceramics Fabricated from 6H-SiC Powder)

  • 배철훈
    • 한국세라믹학회지
    • /
    • 제27권3호
    • /
    • pp.412-422
    • /
    • 1990
  • Porous SiC ceramics were proposed to be promising materials for high-temperature thermoelectric energy conversion. Throughthe thermoelectric property measurements and microstructure observations on the porous alpha SiC and the mixture of $\alpha$-and $\beta$-SiC, it was experimentally clarified that elimination of stacking faults and twin boundaries by grain growth is effective to increase the seebeck coefficient and increasing content of $\alpha$-SiC gives rise to lower electrical conductivity. Furthermore, the effects of additives on the thermoelectric properties of 6H-SiC ceramics were also studied. The electrical conductivity and the seebeck coefficient were measured at 35$0^{\circ}C$ to 105$0^{\circ}C$ in argon atmospehre. The thermoelectric conversion efficiency of $\alpha$-SiC ceramics was lower than that of $\beta$-SiC ceramics. The phase homogeneity would be needed to improve the seebeck coefficient and electrical conductivity decreased with increasing the content of $\alpha$-phase. In the case of B addition, XRD analysis showed that the phase transformation did not occur during sintering. On the other hand, AlN addiiton enhanced the reverse phase transformation from 6H-SiC to 4H-SiC, and this phenomenon had a great effect upon the electrical conductivity.

  • PDF

고전력 전자소자에서 열전생성기의 생성효율과 열적성능 (Generation Efficiency and Thermal Performance of a Thermoelectric Generator with a High Power Electronic Component)

  • 김경준
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제36권1호
    • /
    • pp.51-56
    • /
    • 2012
  • 본 논문은 고파워 전자소자의 폐열로부터 에너지 수확을 목적으로 하는 열전생성기의 생성효율과 열적 성능에 대하여 논한다. 열경계저항을 포함하는 열전모델이 적용되어 생성효율과 고전력 전자소자의 junction 온도를 예측하였고 그 결과는 실험치로 검증되어진다. 검증결과는 예측치와 계측치의 오차가 작음을 보인다. 검증후 열전모델은 다양한 로드저항과 열원의 열율에서 생성효율, 열전생성기 양면의 온도차, 소자의 junction 온도를 예측한다. 본 연구는 로드저항이 생성효율, 열전생성기 양면의 온도차, junction 온도에 미치는 영향에 대해서도 탐구한다.

Bi2Te3계 열전박막의 열전 출력인자에 미치는 첨가제의 영향 (Doping Effects to the Thermoelectric Power Factor of Bi2Te3 Thin Films)

  • 배상현;최순목
    • 한국전기전자재료학회논문지
    • /
    • 제33권2호
    • /
    • pp.141-146
    • /
    • 2020
  • Thermoelectric Bi2Te3 thin films were synthesized by a co-sputtering method at 300℃. A Fe dopant was considered to enhance the thermoelectric properties of the system. The Seebeck coefficient of the Fe-doped films increased whereas the electrical conductivity decreased. As a result, the power factor of the system increased owing to the enhanced Seebeck coefficient. Grain growth inhibition was detected in the Fe-doped system, which produced more grain boundaries in the Fe-doped films than in the undoped system. The increased grain boundary scattering was deemed to be effective for a reduced thermal conductivity. This is advantageous for the preparation of high-performance thermoelectric films.

Influence of Annealing Temperature on Structural and Thermoelectrical Properties of Bismuth-Telluride-Selenide Ternary Compound Thin Film

  • Kim, Youngmoon;Choi, Hyejin;Kim, Taehyeon;Cho, Mann-Ho
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2014년도 제46회 동계 정기학술대회 초록집
    • /
    • pp.304.2-304.2
    • /
    • 2014
  • Chalcogenides (Te,Se) and pnictogens(Bi,Sb) materials have been widely investigated as thermoelectric materials. Especially, Bi2Te3 (Bismuth telluride) compound thermoelectric materials in thin film and nanowires are known to have the highest thermoelectric figure of merit ZT at room temperature. Currently, the thermoelectric material research is mostly driven in two directions: (1) enhancing the Seebeck coefficient, electrical conductivity using quantum confinement effects and (2) decreasing thermal conductivity using phonon scattering effect. Herein we demonstrated influence of annealing temperature on structural and thermoelectrical properties of Bismuth-telluride-selenide ternary compound thin film. Te-rich Bismuth-telluride-selenide ternary compound thin film prepared co-deposited by thermal evaporation techniques. After annealing treatment, co-deposited thin film was transformed amorphous phase to Bi2Te3-Bi2Te2Se1 polycrystalline thin film. In the experiment, to investigate the structural and thermoelectric characteristics of Bi2Te3-i2Te2Se1 films, we measured Rutherford Backscattering spectrometry (RBS), X-ray diffraction (XRD), Raman spectroscopy, Scanning eletron microscopy (SEM), Transmission electron microscopy (TEM), Seebeck coefficient measurement and Hall measurement. After annealing treatment, electrical conductivity and Seebeck coefficient was increased by defect states dominated by selenium vacant sites. These charged selenium vacancies behave as electron donors, resulting in carrier concentration was increased. Moreover, Thermal conductivity was significantly decreased because phonon scattering was enhanced through the grain boundary in Bi2Te3-Bi2Te2Se1 polycrystalline compound. As a result, The enhancement of thermoelectric figure-of-merit could be obtained by optimal annealing treatment.

  • PDF

열간등방가압 공정을 통한 P형 Bi0.5Sb1.5Te3.0 소결체의 격자 열전도도 감소 및 열전 특성 향상 (Enhancement of Thermoelectric Performance in Spark Plasma Sintered p-Type Bi0.5Sb1.5Te3.0 Compound via Hot Isostatic Pressing (HIP) Induced Reduction of Lattice Thermal Conductivity)

  • 정수호;우예진;김경태;조승기
    • 한국분말재료학회지
    • /
    • 제30권2호
    • /
    • pp.123-129
    • /
    • 2023
  • High-temperature and high-pressure post-processing applied to sintered thermoelectric materials can create nanoscale defects, thereby enhancing their thermoelectric performance. Here, we investigate the effect of hot isostatic pressing (HIP) as a post-processing treatment on the thermoelectric properties of p-type Bi0.5Sb1.5Te3.0 compounds sintered via spark plasma sintering. The sample post-processed via HIP maintains its electronic transport properties despite the reduced microstructural texturing. Moreover, lattice thermal conductivity is significantly reduced owing to activated phonon scattering, which can be attributed to the nanoscale defects created during HIP, resulting in an ~18% increase in peak zT value, which reaches ~1.43 at 100℃. This study validates that HIP enhances the thermoelectric performance by controlling the thermal transport without having any detrimental effects on the electronic transport properties of thermoelectric materials.

Bi-Te계 n형 열전분말의 열전특성에 미치는 Cu 도핑의 영향 (Thermoelectric Properties in the Cu Doping Effects of the n-type Bi-Te Powders)

  • 박민수;구혜영;하국현;박용호
    • 한국분말재료학회지
    • /
    • 제22권4호
    • /
    • pp.254-259
    • /
    • 2015
  • $Bi_2Te_3$ related compounds show the best thermoelectric properties at room temperature. However, n-type $Bi_2Te_{2.7}Se_{0.3}$ showed no improvement on ZT values. To improve the thermolectric propterties of n-type $Bi_2Te_{2.7}Se_{0.3}$, this research has Cu-doped n-type powder. This study focused on effects of Cu-doping method on the thermoelectric properties of n-type materials, and evaluated the comparison between the Cu chemical and mechanical doping. The synthesized powder was manufactured by the spark plasma sintering(SPS). The thermoelectric properties of the sintered body were evaluated by measuring their Seebeck coefficient, electrical resistivity, thermal conductivity, and hall coefficient. An introduction of a small amount of Cu reduced the thermal conductivity and improved the electrical properties with Seebeck coefficient. The authors provided the optimal concentration of $Cu_{0.1}Bi_{1.99}Se_{0.3}Te_{2.7}$. A figure of merit (ZT) value of 1.22 was obtained for $Cu_{0.1}Bi_{1.9}Se_{0.3}Te_{2.7}$ at 373K by Cu chemical doping, which was obviously higher than those of $Cu_{0.1}Bi_{1.9}Se_{0.3}Te_{2.7}$ at 373K by Cu mechanical doping (ZT=0.56) and Cu-free $Bi_2Se_{0.3}Te_{2.7}$ (ZT=0.51).

Thermal conductivity of individual single-crystalline Bi nanowires grown by stress-induced recrystallization

  • Roh, Jong-Wook;Chen, Ren-Kun;Lee, Jun-Min;Ham, Jin-Hee;Lee, Seung-Hyn;Hochbaum, Allon;Hippalgaonkar, Kedar;Yang, Pei-Dong;Majumdar, Arun;Kim, Woo-Chul;Lee, Woo-Young
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 춘계학술대회 논문집
    • /
    • pp.23-23
    • /
    • 2009
  • It has been challenging to increase the thermoelectric figure of merit ($ZT=S^2{\sigma}T/\kappa$) of materials, which determine the efficiency of thermoelectric devices, because the three parameters Seebeck coefficient (S), electrical conductivity ($\sigma$), and thermal conductivity ($\kappa$) of bulk materials are inter-dependent. With the development of nanotechnology, ZT values of nanostructured materials are predicted to be enhanced by classical size effects and quantum confinement effects. In particular, Bi nanowires were suggested as one of ideal thermoelectric materials due to the expected quantum confinement effects for the simultaneous increase in Sand. In this work, we have investigated the thermal conductivity of individual single crystalline Bi nanowires with d = 98 nm and d = 327 nm in the temperature range 40 - 300 K using MEMS devices. The for the Bi nanowire with d = 98 nm was observed to be ~ 1.6 W/m-K at 300 K, which is much lower than that of Bi bulk (8 W/m-K at 300 K). This indicates that the thermal conductivity of the Bi suppressed due to enhanced surface boundary scattering in one-dimensional structures. Our results suggest that Bi nanowires grown by stress-induced method can be used for high-efficiency thermoelectric devices.

  • PDF

밀폐유도용해로 제조한 Co1-xNixSb3의 열전특성 (Thermoelectric Properties of Co1-xNixSb3 Prepared by Encapsulated Induction Melting)

  • 김미정;최현모;어순철;김일호
    • 한국재료학회지
    • /
    • 제16권6호
    • /
    • pp.377-381
    • /
    • 2006
  • Skutterudite $CoSb_3$ doped with nickel was prepared by encapsulated induction melting, and its doping effects on thermoelectric properties were investigated. Single phase ${\delta}-CoSb_3$ was successfully obtained by encapsulated induction melting and subsequent heat treatment at 773 K for 24 h. Nickel atoms acted as electron donors by substituting cobalt atoms. Thermoelectric properties were remarkably improved by appropriate heat treatment and doping, and they were closely related to phase transitions and dopant activation. The maximum ZT(dimensionless figure of merit) was achieved as 0.2 at 600 K for the $Co_{0.93}Ni_{0.07}Sb_3$ specimen.