  • Porous SiC ceramics were proposed to be promising materials for high-temperature thermoelectric energy conversion. Throughthe thermoelectric property measurements and microstructure observations on the porous alpha SiC and the mixture of $\alpha$-and $\beta$-SiC, it was experimentally clarified that elimination of stacking faults and twin boundaries by grain growth is effective to increase the seebeck coefficient and increasing content of $\alpha$-SiC gives rise to lower electrical conductivity. Furthermore, the effects of additives on the thermoelectric properties of 6H-SiC ceramics were also studied. The electrical conductivity and the seebeck coefficient were measured at 35$0^{\circ}C$ to 105$0^{\circ}C$ in argon atmospehre. The thermoelectric conversion efficiency of $\alpha$-SiC ceramics was lower than that of $\beta$-SiC ceramics. The phase homogeneity would be needed to improve the seebeck coefficient and electrical conductivity decreased with increasing the content of $\alpha$-phase. In the case of B addition, XRD analysis showed that the phase transformation did not occur during sintering. On the other hand, AlN addiiton enhanced the reverse phase transformation from 6H-SiC to 4H-SiC, and this phenomenon had a great effect upon the electrical conductivity.

  • PDF

Thickness and Annealing Effects on the Thermoelectric Properties of P-type Bi0.5Sb1.5Te3 Thin Films (P형 Bi0.5Sb1.5Te3 박막의 열전 특성에 미치는 두께 및 어닐링 효과)

  • Kim Il-Ho;Jang Kyug-Wook
    • Korean Journal of Materials Research
    • /
    • v.14 no.1
    • /
    • pp.41-45
    • /
    • 2004
  • P-type $Bi_{0.5}$$Sb_{1.5}$ $Te_3$ thin films were deposited by the flash evaporation technique, and their thermoelectric properties and electronic transport parameters were investigated. The effective mean free path model was adopted to examine the thickness effect on the thermoelectric properties. Annealing effects on the carrier concentration and mobility were also studied, and their variations were analyzed in conjunction with the antisite defects. Seebeck coefficient and electrical resistivity versus inverse thickness showed a linear relationship, and the effective mean free path was found to be 3150$\AA$. No phase transformation and composition change were observed after annealing treatment, but carrier mobility increased due to grain growth. Carrier concentration decreased considerably due to reduction of the antisite defects, so that electrical conductivity decreased and Seebeck coefficient increased. When annealed at 473 K for 1 hr, Seebeck coefficient and electrical conductivity were $160\mu$V/K and 610 $W^{-1}$ $cm^{ -1}$, respectively. Therefore, the thermoelectric quality factor were also enhanced to be $16\mu$W/cm $K^2$.>.

Thermoelectric Properties of AlN-doped SiC Ceramics (AlN 첨가 SiC 세라믹스의 열전변환특성)

  • Pai, Chul-Hoon
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.11
    • /
    • pp.839-845
    • /
    • 2012
  • The effect of an AlN additive on the thermoelectric properties of SiC ceramics was studied. Porous SiC ceramics with 48-54% relative density were fabricated by sintering the pressed ${\alpha}-SiC$ powder compacts with AlN at $2100-2200^{\circ}C$ for 3 h in an Ar atmosphere. In the undoped specimens, the Seebeck coefficients were positive (p-type semiconducting) possibly due to a dominant effect of the acceptor impurities (Al, Fe) contained in the starting powder. With AlN addition, the reverse phase transformation of 6H-SiC to 4H-SiC was observed during the sintering process. The electrical conductivity of the AlN doped specimen was larger than that of the undoped specimen under the same conditions, which might be due to a reverse phase trans-formation. The Seebeck coefficient of the AlN doped specimen was also larger than that of the undoped specimen. The density of specimen and the amount of addition had significant effects on the thermoelectric properties.

Thermoelectric Properties of Al4C3-doped α-SiC (Al4C3 첨가 α-SiC의 열전변환특성)

  • 박영석;배철훈
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.10
    • /
    • pp.991-997
    • /
    • 2003
  • The effect of A1$_4$C$_3$ additive on the thermoelectric properties of SiC ceramics were studied. Porous SiC ceramics with 47∼59% relative density were fabricated by sintering the pressed $\alpha$-SiC powder compacts with A1$_4$C$_3$at 2100∼220$0^{\circ}C$ for 3 h in Ar atmosphere. Crystalline phases of the sintered bodies were identified by powder X-Ray Diffraction (XRD) and their microstructures were observed with a Scanning Electron Microscope (SEM). In the case of A1$_4$C$_3$ addition, the phase transformation of 6H-SiC to 4H-SiC could be observed during sintering. The Seebeck coefficient and electrical conductivity were measured at 550∼95$0^{\circ}C$ in Ar atmosphere. In the case of undoped specimens, the Seebeck coefficients were positive (p-type semiconducting) possibly due to a dominant effect of the acceptor impurities (Al, Fe) contained in the starting powder and electrical conductivity increased as increasing sintering temperature. Electrical conductivity of A1$_4$C$_3$doped specimen is larger than that of undoped specimen under the same condition, which might be due to the reverse phase transformation and increasing of carrier density. And the Seebeck coefficient of A1$_4$C$_3$ doped specimen is also larger than that of undoped specimen. The density of specimen, the amount of addition and sintering atmosphere had significant effects on the thermoelectric property.

The Effect of Powder Oxidation on the Thermoelectric Properties of β-FeSi2 (β-FeSi2의 열전변환특성에 미치는 분말산화의 영향)

  • ;Kunihito Koumoto
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.11
    • /
    • pp.1106-1112
    • /
    • 2003
  • For the purpose of making clear the role of oxygen in the thermoelectric properties of FeSi$_2$, thermoelectric measurements and spectroscopic characterization were conducted for the oxidized specimens fabricated from ($\alpha$+$\varepsilon$)-phases and/or $\beta$-phase. Addition of oxygen to FeSi$_2$ prevented both densification during sintering and transformation from metallic phases to semiconducting phase during annealing treatment. In an specimens, electrical conductivity and thermal conductivity decreased with oxidation time. The Seebeck coefficient was positive and small for pure FeSi$_2$. And/or the oxidized specimens fabricated from ($\alpha$+$\varepsilon$)-phases. However, it was negative and showed a maximum peak at about 500 K for the oxidized FeSi$_2$ fabricated from $\beta$-phase. The value of maximum peak increased with oxidation time.

Experimental Study of Thermo-electric material using Lithium-Ammonia$(Li(NH_3)_n)$ Solution (리튬-암모니아 $(Li(NH_3)_n)$ 용액을 이용한 열전기적 특성 실험)

  • Park, Han-Woo;Kim, Ji-Beom;Jeon, Joon-Hyeon
    • Korean Chemical Engineering Research
    • /
    • v.49 no.2
    • /
    • pp.263-270
    • /
    • 2011
  • The aim of this paper is, through the experiment of Lithium-Ammonia solutions $(Li(NH_3)_n)$, to analyze and verify a thermoelectric-conversion property at near Ammonia-boiling point ($-40^{\circ}C$). The experiment results show that the solutions with 0.58 MPM~1.87 MPM generate thermoelectric power at temperature difference $({\Delta}T=0{\sim}15^{\circ}C)$ where Current is constantly proportional to Voltage. This paper provides a new insight into the development of a thermoelectric material.