• Title/Summary/Keyword: Thermal-structure Stability

Search Result 650, Processing Time 0.027 seconds

Evaluation of Characteristic for SS400 and STS304 steel by Weld Thermal Cycle Simulation - 1st Report : on the Mechanical Properties and Microstructure (용접열사이클 재현에 의한 SS400강 및 STS304강의 특성 평가 - 제1보 : 기계적 특성 및 조직)

  • Ahn, Seok-Hwan;Jeong, Jeong-Hwan;Nam, Ki-Woo
    • Journal of Ocean Engineering and Technology
    • /
    • v.19 no.6 s.67
    • /
    • pp.64-71
    • /
    • 2005
  • The welding methods have been applied to the most structural products used in the automobile, ship construction, and construction. The structure steel must have sufficient strength of structure; However, the mechanical properties of the welded part changes when it is welded. Therefore, the stability or life of the structure may be affected by the changed mechanical properties. The mechanical properties of the welded part must be examined in order to ensure the safety of structure. In this research, the SS400 steel and the STS304 steel were used to estimate the mechanical properties of the HAZ by weld thermal cycle simulation. In this study, the materials were used to examine the weld thermal cycle simulation characteristic, under two conditions: the drawing with diameter of $\Phi$10 and the residual stress removal treatment. To examine the mechanical properties by the weld thermal cycle simulation, the tensile test was carried out in room temperature. The crosshead speed was lmm/min.

Synthesis and Photocatalytic Properties of Thermally Stable Metal-Oxide Hybrid Nanocatalyst with Ultrathin Oxide Encapsulation

  • Naik, Brundabana;Moon, Song Yi;Kim, Sun Mi;Jung, Chan Ho;Park, Jeong Young
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.08a
    • /
    • pp.317.2-317.2
    • /
    • 2013
  • Ultrathin oxide encapsulated metal-oxide hybrid nanocatalysts have been fabricated by a soft chemical and facile route. First, SiO2 nanoparticles of 25~30 nm size have been synthesized by modified Stobber's method followed by amine functionalization. Metal nanoparticles (Ru, Rh, Pt) capped with polymer/citrate have been deposited on functionalized SiO2 and finally an ultrathin layer of TiO2 coated on surface which prevents sintering and provides high thermal stability while maximizing the metal-oxide interface for higher catalytic activity. TEM studies confirmed that 2.5 nm sized metal nanoparticles are well dispersed and distributed throughout the surface of 25 nm SiO2 nanoparticles with a 3-4 nm TiO2 ultrathin layer. The metal nanoparticles are still well exposed to outer surface, being enabled for surface characterization and catalytic activity. Even after calcination at $600^{\circ}C$, the structure and morphology of hybrid nanocatalysts remain intact confirm the high thermal stability. XPS spectra of hybrid nanocatalyst suggest the metallic states as well as their corresponding oxide states. The catalytic activity has been evaluated for high temperature CO oxidation reaction as well as photocatalytic H2 generation under solar simulation. The design of hybrid structure, high thermal stability, and better exposure of metal active sites are the key parameters for the high catalytic activity. The maximization of metal-TiO2 interface interaction has the great role in photocatalytic H2 production.

  • PDF

A Study on the Combustion Characteristics of Useful Imported Wood for Building Materials - Focusing on the North American species (Douglas-fir, Western Red cedar) and African species(Makore, Padauk, Bubinga) - (국내 유용 건축자재용 수입 목재의 연소특성에 관한 연구 - 북미 산재(Douglas-fir, Western Red cedar)와 아프리카 산재 (Makore, Padauk, Bubinga)를 중심으로 -)

  • Seo, Hyun Jeong;Baek, Jong Kyo;Lee, Min Chul
    • Journal of the Korean Society of Safety
    • /
    • v.32 no.3
    • /
    • pp.8-14
    • /
    • 2017
  • This study examined the combustion and thermal characteristics of imported woods for building materials in Korea. Wooden specimens were confirmed by a cone calorimeter according to the KS F ISO 5660-1 standard. The combustion properties of the wooden specimens were measured in terms of the heat release rate (HRR), total heat released (THR), mass lose rate (MLR), and ignition time (time to ignition; TTI). The optical microscope was used for determine the anatomical characteristics of wood pit and structure. Also, the thermal properties were measured by thermogravimetric analysis (TGA) to determine the thermal stability of wooden specimens. The result of this experiment would be useful for fundamentals of guiding the combustion properties and thermal stability using wood application.

Projection of the Climate Change Effects on the Vertical Thermal Structure of Juam Reservoir (기후변화가 주암호 수온성층구조에 미치는 영향 예측)

  • Yoon, Sung Wan;Park, Gwan Yeong;Chung, Se Woong;Kang, Boo Sik
    • Journal of Korean Society on Water Environment
    • /
    • v.30 no.5
    • /
    • pp.491-502
    • /
    • 2014
  • As meteorology is the driving force for lake thermodynamics and mixing processes, the effects of climate change on the physical limnology and associated ecosystem are emerging issues. The potential impacts of climate change on the physical features of a reservoir include the heat budget and thermodynamic balance across the air-water interface, formation and stability of the thermal stratification, and the timing of turn over. In addition, the changed physical processes may result in alteration of materials and energy flow because the biogeochemical processes of a stratified waterbody is strongly associated with the thermal stability. In this study, a novel modeling framework that consists of an artificial neural network (ANN), a watershed model (SWAT), a reservoir operation model(HEC-ResSim) and a hydrodynamic and water quality model (CE-QUAL-W2) is developed for projecting the effects of climate change on the reservoir water temperature and thermal stability. The results showed that increasing air temperature will cause higher epilimnion temperatures, earlier and more persistent thermal stratification, and increased thermal stability in the future. The Schmidt stability index used to evaluate the stratification strength showed tendency to increase, implying that the climate change may have considerable impacts on the water quality and ecosystem through changing the vertical mixing characteristics of the reservoir.

NMR Study on Thermal Stability of the Double Helical Structures of d(CGAATTCG)2, d(CGTATACG)2 and their berenil complexes

  • Kim, Eun-Hee;Hong, Seok-Joo;Huh, Sung-Ho
    • Journal of the Korean Magnetic Resonance Society
    • /
    • v.8 no.2
    • /
    • pp.96-107
    • /
    • 2004
  • We prepared two oligonucleotides containing same base pairing, but different base sequence in the middle region, d(CGAATTCG) and d(CGTATACG). NMR and UV absorbance data represented that such variation in base sequence could cause a significant difference in melting temperature and dynamics between d(CGAATTCG)$_2$ and d(CGTATACG)$_2$ duplexes, which are regarded to be associated with the stacked structure and the width of the minor groove of them. The latter showed poor stability compared to the former, because of poor stacking of bases. And berenil could bind to the minor groove of d(CGAATTCG)$_2$ which is relatively narrow, more strongly than d(CGTATACG)$_2$ and this gave rise to large improvement in thermal stability of the d(CGAATTCG)$_2$ duplex, compared to d(CGTATACG)$_2$.

  • PDF

Numerical Analysis on Thermal-Induced Degradation of n-i-p Structure Perovskite Solar Cells Using SCAPS-1D (SCAPS-1D 시뮬레이션을 이용한 n-i-p 구조 페로브스카이트 태양전지의 열적 열화 원인 분석)

  • Kim, Seongtak;Bae, Soohyun;Jeong, Younghun;Han, Dong-Woon;Kim, Donghwan;Mo, Chan Bin
    • Current Photovoltaic Research
    • /
    • v.10 no.1
    • /
    • pp.16-22
    • /
    • 2022
  • The long-term stability of PSCs against visual and UV light, moisture, electrical bias and high temperature is an important issue for commercialization. In particular, since the operation temperature of solar cell can rise above 85℃, a study on thermal stability is required. In this study, the cause of thermal-induced degradation of PSCs was investigated using the SCAPS-1D simulation tool. First, PSCs of TiO2/CH3NH3PbI3/Spiro-OMeTAD/Au structure were exposed to a constant temperature of 85℃ to observe changes in conversion efficiency and quantum efficiency. Because the EQE reduction above 500 nm was remarkable, we simulated PSCs performance as a function of lifetime, doping density of perovskite and spiro-OMeTAD. Consequently, the main cause of thermal-induced degradation is considered to be the change in the perovskite doping concentration and lifetime due to ion migration of perovskite.

Effect of Microporous Structure of Al2O3/PVdF_HFP Ceramic Coating Layers on Thermal Stability and Electrochemical Performance of Composite Separators for Lithium-Ion Batteries (Al2O3/PVdF_HFP 세라믹코팅층의 미세기공구조가 리튬이차전지용 복합분리막의 열 안정성 및 전기화학특성에 미치는 영향)

  • Jeong, Hyun-Seok;Kim, Kyu-Chul;Lee, Sang-Young
    • Journal of the Korean Electrochemical Society
    • /
    • v.12 no.4
    • /
    • pp.324-328
    • /
    • 2009
  • The internal short-circuit between cathodes and anodes has been known to be a critical concern for the safety failures of lithium-ion batteries, which is strongly influenced by the thermal stability of separators. In this study, to effectively suppress the internal short-circuit failures, we developed a new composite separator with the improved thermal stability compared to conventional polyolefin-based separators. The composite separators were prepared by introducing a ceramic coating layer ($Al_2O_3$/PVdF-HFP) onto both sides of a polyethylene (PE) separator. The microporous structure of ceramic coating layers is determined by controlling the phase inversion of coating solutions and becomes more developed with the increase of nonsolvent (water) content. This structural change of ceramic coating layers was observed to greatly affect the thermal stability as well as the electrochemical performance of composite separators, which was systematically discussed in terms of phase inversion.

The Influence of Hydrotalcite Intercalated with Benzoate on UV Stability of Acrylic Coating

  • Nguyen, Thuy Duong;Nguyen, Anh Son;Thai, Thu Thuy;Pham, Gia Vu;To, Thi Xuan Hang;Olivier, Marie-Georges
    • Corrosion Science and Technology
    • /
    • v.19 no.1
    • /
    • pp.16-22
    • /
    • 2020
  • It is important to realize that benzoate was intercalated into hydrotalcite (HTC-Bz) by the co-precipitation method. In this case, acrylic coating with 0.5 wt% HTC-Bz was deposited on carbon steel using the spin coating method. Next, the HTC-Bz structure was characterized by Field emission scanning electron microscopy (FESEM), X-ray diffraction (XRD), and Fourier transform infrared spectroscopy (FT-IR). In fact, an ultraviolet vision spectroscopy (UV-Vis) was used to determine the benzoate content in HTC-Bz, and the UV absorption ability of HTC-Bz. Using electrochemical techniques, water contact angle measurement, and thermal-gravimetric analysis, we compared the protective properties before and after QUV test, hydrophobicity and the thermal stability of acrylic coating containing HTC-Bz. The obtained results showed that HTC-Bz with a plate-like structure was successfully synthesized; benzoate was intercalated into the interlayer of hydrotalcite with a concentration of 28 wt%. Additionally, it was noted that HTC-Bz has an UV absorption peak at 225 nm. In conclusion, the addition of HTC-Bz enhanced the UV stability, hydrophobicity and the thermal stability of acrylic coating.

Tensile Properties and Thermal Stability of Cellulose Nanofibril/Clay Nanocomposites

  • Park, Byung-Dae;Singh, Adya P.;Um, In Chul
    • Current Research on Agriculture and Life Sciences
    • /
    • v.31 no.1
    • /
    • pp.18-24
    • /
    • 2013
  • This work attempted to fabricate organic/inorganic nanocomposite by combining organic cellulose nanofibrils (CNFs), isolated by 2,2,6,6-tetramethylpiperidine-1-oxy radical (TEMPO)-mediated oxidation of native cellulose with inorganic nanoclay. The morphology and dimension of CNFs, and tensile properties and thermal stability of CNF/clay nanocomposites were characterized by transmission electron microscope (TEM), tensile test, and thermogravimetry (TG), respectively. TEM observation showed that CNFs were fibrillated structure with a diameter of about $4.86{\pm}1.341nm$. Tensile strength and modulus of the hybrid nanocomposite decreased as the clay content of the nanocomposite increased, indicating a poor dispersion of CNFs or inefficient stress transfer between the CNFs and clay. The elongation at break increased at 1% clay level and then continuously decreased as the clay content increased, suggesting increased brittleness. Analysis of TG and derivative thermogravimetry (DTG) curves of the nanocomposites identified two thermal degradation peak temperatures ($T_{p1}$ and $T_{p2}$), which suggested thermal decomposition of the nanocomposites to be a two steps-process. We think that $T_{p1}$ values from $219.6^{\circ}C$ to $235^{\circ}C$ resulted from the sodium carboxylate groups in the CNFs, and that $T_{p2}$ values from $267^{\circ}C$ to $273.5^{\circ}C$ were mainly responsible for the thermal decomposition of crystalline cellulose in the nanocomposite. An increase in the clay level of the CNF/clay nanocomposite predominately affected $T_{p2}$ values, which continuously increased as the clay content increased. These results indicate that the addition of clay improved thermal stability of the CNF/clay nanocomposite but at the expense of nanocomposite's tensile properties.

  • PDF

Analysis of Temperature of Molten Aluminium Holding Furnace and Stress of Substructure Frame (알루미늄 용탕 보온로의 열해석 및 하부 구조물의 강도해석)

  • Park, Sang-Soo;Kang, Chung-Gil;Kim, Byung-Min
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.22 no.10 s.175
    • /
    • pp.129-136
    • /
    • 2005
  • The demand on thermos furnace of Al molten metal has recently been getting higher and higher according to the increase in use of Al and Al alloys. This study considers the estimation of the thermal and mechanical stability in the thermos furnace for Al casting. It is executed through the analysis of heat transfer on the refractory material and heat stress on each steel shell. Also, the estimation of structural stability was appraised through the strength analysis of the lower structure. In result, the temperature of steel shell rose to 320.15K and its elastic deformation was about 1.5mm. The elastic deformation of the lower structure was about 0.66mm. As a result of it, the data obtain from the analysis in this study are regarded as stable value on considering that the size of the furnace is 2500mm.