• Title/Summary/Keyword: Thermal damage

Search Result 918, Processing Time 0.026 seconds

Measurements of Temperature Rise and Temperature Distribution of Samples by Infrared Radiation (적외선 복사에 의한 시료의 온도상승과 온도분포 측정)

  • Han, Jong-Sung;Kim, Ki-Hoon;Kim, Hoon
    • Proceedings of the Korean Institute of IIIuminating and Electrical Installation Engineers Conference
    • /
    • 2003.11a
    • /
    • pp.133-137
    • /
    • 2003
  • When a light is projected upon a material, part of its radiation energy is absorbed and the rest is reflected or transmitted according to the nature of the material. The molecules of the substance absorbing a light obtains the radiation energy to the wavelength of the light to make photochemical degradation by ultraviolet ray or thermal reactions like physical damage by infrared ray. The degree of damage by radiation energy varies to the substances of materials, the spectral power distribution of the light source and the duration of irradiation. Because the damage brings about a devaluation of material and once damaged, it is irretrievable, it is necessary to minimize the damage and conserve the native quality of a material by a protective lighting system. A measuring system was set up to measure the temperature rise of each sample by infrared radiation from light sources. And the temperature rise and temperature distribution by various infrared lamps were measured with varying time.

  • PDF

IRRADIATION EFFECTS OF HT-9 MARTENSITIC STEEL

  • Chen, Yiren
    • Nuclear Engineering and Technology
    • /
    • v.45 no.3
    • /
    • pp.311-322
    • /
    • 2013
  • High-Cr martensitic steel HT-9 is one of the candidate materials for advanced nuclear energy systems. Thanks to its excellent thermal conductivity and irradiation resistance, ferritic/martensitic steels such as HT-9 are considered for in-core applications of advanced nuclear reactors. The harsh neutron irradiation environments at the reactor core region pose a unique challenge for structural and cladding materials. Microstructural and microchemical changes resulting from displacement damage are anticipated for structural materials after prolonged neutron exposure. Consequently, various irradiation effects on the service performance of in-core materials need to be understood. In this work, the fundamentals of radiation damage and irradiation effects of the HT-9 martensitic steel are reviewed. The objective of this paper is to provide a background introduction of displacement damage, microstructural evolution, and subsequent effects on mechanical properties of the HT-9 martensitic steel under neutron irradiations. Mechanical test results of the irradiated HT-9 steel obtained from previous fast reactor and fusion programs are summarized along with the information of irradiated microstructure. This review can serve as a starting point for additional investigations on the in-core applications of ferritic/martensitic steels in advanced nuclear reactors.

Numerical Analysis of Frost Depth behind the Lining of Road Tunnel in Gangwon Province (수치해석을 통한 강원지역 도로터널 라이닝 배면지반의 동결깊이 분석)

  • Son, Hee-Su;Jun, Kyoung-Jea;Yune, Chan-Young
    • Journal of the Korean GEO-environmental Society
    • /
    • v.18 no.3
    • /
    • pp.15-23
    • /
    • 2017
  • Gangwon Province, located in the northeastern part of South Korea, is the coldest area in South Korea with 90% of the total area as mountainous. Therefore, tunnel damage has been reported continuously in winter. But there has been lack of researches on frost heave occurring behind tunnel lining. In this study, numerical analysis was conducted to investigate the frost depth in road tunnel constructed in Gangwon province. Based on the database on road tunnel and weather in Gangwon province, a standard tunnel shape and geotechnical properties of ground was determined. And then thermal analysis for the frost depth according to the temperature change and ground conditions were conducted. Analysis result showed that the sensitivity to frost heave of metamorphic rock and sedimentary rock is higher than sand. Lower initial ground temperature leads to deeper frost depth and consequently increases frost damage. In addition, lining thickness, specific heat capacity, and thermal conductivity also affect greatly on the variation of frost depth.

An Application of the Water Mist System for Underground Utility Tunnel (지하구 미분무수 소화설비 적용에 관한 연구)

  • 김운형;김종훈;박승민;김태수;민인홍;전동일;김상욱
    • Fire Science and Engineering
    • /
    • v.16 no.1
    • /
    • pp.66-76
    • /
    • 2002
  • This paper includes new nozzle design, basic design factors of water mist system that minimize a thermal damage of cable causing business interruption and applying underground utility tunnel. A underground concrete structure (2.5 m(H)$\times$2.5 m(W)$\times$25 m(D)) is constructed in order to test a nozzle performance. Under the designing fire scenario, critical thermal damage of cable sheath ($400^{\circ}c$) reached within a 2 minutes with unsuppressed fire, but type 1 nozzle (SMD 470 $\mu{m}$) and type 2 nozzle (SMD 650 $\mu{m}$) control cable temperature below $400^{\circ}c$. A system performance and fundamental design factors; K factor, flow rate, spray angle, size distribution, nozzle pressure, spray density are analyzed and proposed for system optimization.

Thermal-Structure Interaction Parallel Fire Analysis for Steel-Concrete Composite Structures under Bridge Exposed to Fire Loading (화재에 노출된 교량하부 강합성 구조물에 대한 열-구조 연성 병렬화재해석)

  • Yun, Sung-Hwan;Gil, Heungbae;Lee, Ilkeun;Kim, Wooseok;Park, Taehyo
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.26 no.4
    • /
    • pp.283-292
    • /
    • 2013
  • The objective of this research is to evaluate of global and local damage for steel-concrete composite structures under highway bridge exposed to fire loading. To enhance the accuracy and efficiency of the numerical analysis, the proposed transient nonlinear thermal structure interaction(TSI) parallel fire analysis method is implemented in ANSYS. To validate the TSI parallel fire analysis method, a comparison is made with the standard fire test results. The proposed TSI parallel fire analysis method is applied to fire damage analysis and performance evaluation for Buchen highway bridge. The result of analysis, temperature of low flange and web are exceed the critical temperature. The deflection and deformation state show good agreement with the fire accident of buchen highway bridge.

The Effect of Multilayer Passivation Film on Life Time Characteristics of OLED Device (OLED소자의 수명에 미치는 다층 보호막의 영향)

  • Ju, Sung-Hoo;Yang, Jae-Woong
    • Journal of the Korean institute of surface engineering
    • /
    • v.45 no.1
    • /
    • pp.20-24
    • /
    • 2012
  • Multilayer passivation film on OLED with organic/inorganic hybrid structure as to diminish the thermal stress and expansion was researched to protect device from the direct damage of $O_2$ and $H_2O$ and improve life time characteristics. Red OLED doped with 1 vol.% Rubrene in $Alq_3$ was used as a basic device. The films consist of ITO(150 nm)/ELM200_HIL(50 nm)/ELM002_HTL(30 nm)/$Alq_3$: 1 vol.% Rubrene(30 nm)/$Alq_3$(30 nm) and LiF(0.7 nm)/Al(100 nm) which were formed in that order. Using LiF/$SiN_x$ as a buffer layer was determined because it significantly improved life time characteristics without suffering damage in the process of forming passivation film. Multilayer passivation film on buffer layer didn't produce much change in current efficiency, while the half life time at 1,000 $cd/m^2$ of OLED/LiF/$SiN_x$/E1/$SiN_x$ was 710 hours which showed about 1.5 times longer than OLED/LiF/$SiN_x$/E1 with 498 hours. futhermore, OLED/LiF/$SiN_x$/E1/$SiN_x$/E1/$SiN_x$ with 1301 hours showed about twice than OLED/LiF/$SiN_x$/E1/$SiN_x$ which demonstrated that superior characteristics of life time was obtained in multilayer passivation film. Through the above result, it was suggested using LiF/$SiN_x$ as a buffer layer could reduce the damage from the difference of thermal expansion coefficient in OLED with protective films, and epoxy layer in multilayer passivation film could function like a buffer between $SiN_x$ inorganic layers with relatively large thermal stress.

Evaluation on Thermal Shock Damage of Smart Composite using Nondestructive Technique (비파괴 기법을 이용한 스마트 복합재료의 열충격손상평가)

  • Lee, Jin-Kyung;Park, Young-Chul;Lee, Kyu-Chang;Lee, Joon-Hyun
    • Composites Research
    • /
    • v.20 no.3
    • /
    • pp.37-42
    • /
    • 2007
  • Tensile residual stress is occurred by difference of coefficients of thermal expansion between fiber and matrix is one of the serious problems in metal matrix composite(MMC). TiNi alloy fiber was used to solve the problem of the tensile residual stress as the reinforced material. TiNi alloy fiber improves the tensile strength of composite with occurring of compressive residual stress in the matrix by its shape memory effect. A hot press method was used to create the optimal fabrication condition for a Shape Memory Alloy(SMA) composite. The bonding effect of the matrix and the reinforcement within the SMA composite by the hot press method was strengthened by cold rolling. In addition, acoustic emission technique was used to quantify the microscopic damage behavior of cold rolled TiNi/A16061 shape memory alloy composite at low temperature. The damage degree for the specimen that underwent thermal shock cycles was also discussed.

Degradation and Preservation of wood (목재문화재의 열화에 대한 고찰)

  • Kim, Ik-Ju
    • 보존과학연구
    • /
    • s.7
    • /
    • pp.265-277
    • /
    • 1986
  • The degradation of wood is maimly caused by biological and thermal factor. In general, the field of wood preservation can be divided into two broadcategories; namely the deterioration, protection of wood, and the teatment of wood with preservatives. Wood in sea or brackish water incurs marine borer damage, consisting of attack by marine animal and also wood on land suffers severely from insect damage. But the largest wood degradation is caused by microorganism. Animals that attack wood in a marine environment are especially destructive in warm water-regions, little was achieved in their control recently. Therefore this manuscript only introduce the importance of wood deterioration caused by marine animal.

  • PDF

Effect of Microstructure on Alternating Current-induced Damage in Cu Lines

  • Park Young-Bae
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.12 no.1 s.34
    • /
    • pp.27-33
    • /
    • 2005
  • The effect of microstructure on alternating current-induced damage in 200 and 300 nm thick polycrystalline sputtered Cu lines on Si substrates has been investigated. Alternating currents were used to generate temperature cycles (with ranges from 100 to $300^{\circ}C$) and thermal strains (with ranges from 0.14 to $0.42\%$) in the Cu lines at a frequency of 10 kHz. Fatigue loading caused the development of severe surface roughness that was localized within individual grains which depends severely on grain orientations.

  • PDF

Multi-phase Accelerating Test Method of Thermal Aging Considering Heat Generation of Electric Equipment (전기기기의 발열을 고려한 다단계 가속열노화 방법)

  • Lim, Byung-Ju;Park, Chang-Dae;Chung, Kyung-Yul
    • The KSFM Journal of Fluid Machinery
    • /
    • v.16 no.5
    • /
    • pp.18-23
    • /
    • 2013
  • Thermal aging test is performed to qualify the life time of equipment in thermally aged condition. Due to long life time more than 10 years like as in power plant, the equipment is subjected to the accelerated thermal aging condition which is able to shorten the long aging test period by increasing aging temperature. Normally, conservatism of thermal aging test causes to impose unbalanced and excessive thermal load on components of the equipment, and deformation and damage problems of the components. Additionally, temperature rise of each component through heat generation of the electric equipment leads to long-term problem of the test period. Multi-phase accelerating aging test is to perform thermal aging test in multiple aging conditions after dividing into groups with various components of equipment. The groups might be classified considering various factors such as activation energy, temperature rise, glass transition temperature and melting temperature. In this study, we verify that the multi-phase accelerating aging test method can reduce and equalize the thermal over load of the components and shorten aging test time.