Soil Water Characteristic Curve for Weathered Granite Soils - A Test Method (화강풍화토에 대한 함수특성곡선 - 실험방법에 대한 연구)

  • Lee Sung Jin;Lee Seung Rae
    • Journal of the Korean Geotechnical Society
    • /
    • v.21 no.2
    • /
    • pp.17-26
    • /
    • 2005
  • Soil water characteristic curve (SWCC) is a unique characteristic that should be considered In the analysis of unsaturated soil and prediction of unsaturated properties. However, the volume change of soil specimens that happens in the existing apparatus affects the SWCC, Therefore, In this study, we intended to obtain more appropriate SWCC by measuring the change In the volume of the specimen in the SWCC tests. The measured change of void ratio indicates that the saturation step prior to the test changes the original structure of the soil specimen. Thus we carried out the test far the same specimen omitting the saturation step prior to the test. The change of void ratio by this test procedure is relatively small.

Experimental Testing of Rubber Materials for Finite Element Analysis (유한요소해석을 위한 고무재료시험)

  • Kim, Wan-Doo;Kim, Wan-Soo;Woo, Chang-Soo;Lee, Hak-Ju
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.704-709
    • /
    • 2001
  • Experimental methods to determine non-linear properties of rubber materials for finite element analysis is discussed. In simple tension tests, dumbbell specimens are generally used to obtain states of pure tension strain. It is shown that the strip specimens of which length is over 10 times of the width can be also used. In simple compression tests, the effect of the friction between the test specimen and the platens is investigated. the new test method with the tapered platen is proposed in order to overcome the effect of friction and it is verified by experimental and finite element analysis results. In pure shear tests, it is shown that the width of the specimen must be at least 10 times of the height. The mechanical conditioning is suggested to stabilize the properties of the rubber materials. Also, engine mount for automotive is analyzed and experimented for each cases.

  • PDF

Laser-Ultrasonics Application for Non-Contact and Non-destructive Evaluation of Structure (구조물의 비접촉 비파괴 검사를 위한 레이저 초음파법 적용)

  • Kim Jae-Yeal;Song Kyung-Seok;Yang Dong-Jo
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.14 no.4
    • /
    • pp.49-54
    • /
    • 2005
  • Measuring defects on the inside and on the surface of a steel structure is very important technology in order to predict the life span of the structure. In particular, a place with a high probability that it may contain defects is a welded part and it is very important to check defects in the part, absence/presence of non-uniform substances, its shape, and the location. Many non-destructive tests can be applied, but the ultrasonic flow detection test is widely used with some advantages. The ultrasonic flow detection test, however, cannot be applied when there is a problem by a contact medium between PZT and a specimen, in case of a small and complicated shape or a moving object or when the specimen is hot. In this study, to solve the problems of the contact ultrasonic flow detection test, the non-contact ultrasonic flow detection test for sending/receiving ultrasonic waves using lasers was described. I intended to develop a non-destructive detection system applying the laser application ultrasonic test to a steel structure by detecting the defects inside of and on the surface of the specimen.

Failure Behavior of High Strength Concrete under Uniaxial and Biaxial Compression (고강도 콘크리트의 일축 및 이축 압축하의 파괴거동)

  • Lee, Sang-Kuen;Song, Young-Chul
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.6 no.1
    • /
    • pp.223-231
    • /
    • 2002
  • The pilot tests for the development of biaxial failure envelope of high strength concrete of reactor containments were performed. To apply biaxial loads to concrete, the plate specimens were used. The technical difficulties encountered on the development of a suitable biaxial test setup were discussed. To decide the optimum thickness of plate specimen, the nonlinear finite element analyses using ABAQUS were performed for a 1/8 model of cylindrical specimen(${\Phi}150{\times}300$) and four 1/4 models of plate Specimens ($200{\times}200{\times}T$(=30, 50, 60, 70)mm) under uniaxial compression. Analytical values and test data of relative strength ratio between those specimens with different geometric shapes were also compared. The various test data were obtained under uniaxial compression, uniaxial tension, and biaxial compression and then the stress-strain responses were plotted. The test data indicated that the strength of concrete under biaxial compression, $f_1/f_2=-1/-1$, is 15 percent larger than that under uniaxial compression and the poisson's ratio of concrete is 0.16. Teflon pads employed to eliminate friction between test specimen and loading platens showed an excellent effect under biaxial compression.

Basic Experimental Study for Ice-Concrete Friction Behavior (빙-콘크리트 마찰 특성 평가를 위한 실험적 기초 연구)

  • Do, Youngjun;Kim, Yooil
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.57 no.6
    • /
    • pp.365-372
    • /
    • 2020
  • Ice induced abrasion is known as a critical problem in concrete gravity based offshore structures, which are mainly used in the arctic regions. Although many researches on ice abrasion have been conducted for the last several decades, there still are some difficulties in designing concrete gravity based offshore structures against abrasion problem because there is no standardized method yet due to the uncertain physics involved in. This paper presents an experimental study for the evaluation of concrete abrasion characteristics due to ice friction on concrete surface. For the test, a testing machine capable of abrasion and friction was designed and produced, and standardized procedure was proposed to produce ice specimen used for abrasion test. For the experiment, compressive strength of the ice specimen were explored through a static compression test. Then the friction test between ice specimen and concrete surface was performed and friction coefficients were derived using measured vertical and horizontal forces. Dependency of friction coefficients on some test parameters were studied and discussed as well.

An Experimental Study on the Characteristics of Fiber-Reinforced Concrete Beam Without Shear Reinforcement (전단보강근이 없는 섬유보강 철근콘크리트 보의 특성에 관한 실험적 연구)

  • Kim, Jeong-Sup;Go, Song-Kyoon;Choi, Jin-Seok
    • Journal of the Korea Institute of Building Construction
    • /
    • v.3 no.3
    • /
    • pp.83-90
    • /
    • 2003
  • This study examines the material characteristics of fibers and their influences on reinforced concrete through the tests of reinforced concrete by the types of fibers including non-reinforced, steel, polypropylene and cellulose fibers and the test of compressive strength and reinforced concrete beam without shear reinforcement and consequently it obtains the following conclusions. As a result of conducting compressive strength by the types of specimens, fiber reinforced specimen with the highest compressive strength value at 28 days of age was cellulose fiber reinforced specimen as 280.4kgf/$\textrm{cm}^2$ and steel fiber specimen had the highest compressive strength of 250.7kgf/$\textrm{cm}^2$ at 180 days of age. In case of non-reinforced specimen, its compressive strength was 277.4kgf/$\textrm{cm}^2$ at 28 days of age and 273.1kgf/$\textrm{cm}^2$ at 180 days of age. Comparing the compressive strength of non-reinforced specimen to that fiber reinforced specimen showed that the compressive strength of fiber reinforced specimen was lower in the passage of age and the results of this experiment showed no effects of fiber reinforcement. As a result of testing reinforced concrete beam without shear reinforcement, ductility factors of specimens were 4.67 for non-reinforced specimen, 8.18 for steel fiber reinforced specimen, 6.20 for polypropylene fiber reinforced specimen and 5.49 for cellulose reinforced specimen, and it is found that steel fiber reinforced specimen was highest. When non-reinforced specimen and steel fiber reinforced specimen were compared, steel fiber reinforced specimen had higher ductility factor of about 75.2% than that of non-reinforced specimen.

Efforts of Specimen Sizes on Crack Opening Displacement (COD) for Submerged Arc Weldments of Fine Grained Steel (미세립강 잠호 용접부의 COD에 미치는 시편 크기의 영향)

  • 윤중근;김대훈;김문일
    • Journal of Welding and Joining
    • /
    • v.1 no.2
    • /
    • pp.53-60
    • /
    • 1983
  • COD test based on fracture mechanics concept was used in this study to evaluate the fracture toughness quantitatively. Effects of specimen sizes on critical COD value for ABS EH 36 steel and its submerged arc weldments, and the variation of critical COD value depending on metallurgical/mechanical heterogeneities caused by weld thermal cycles were investigated. Experiment was performed by using specimens made from base metal and submerged arc weldments according to BS 5762. Obtained results are summarized as follows; 1) Critical COD value for base metal decreases with increasing thickness of specimen. On hand, as the reduction ratio of critical COD decreases with increasing specimen thickness, critical COD value becomes constant above a thickness of specimen. 2) Critical COD value for weldment decreases with increasing thickness of specimen and was also affected by metallurgical states of base metal. 3) Size effects for weldment was greater at the hardened region. 4) Critical COD value was affected by microstructural change due to weld thermal cycles in weldments; that is, accicular ferrite formation is favorable for increasing of COD value.

  • PDF

Normalization of DBTT Size Effect far Aged 1Cr-lMo-0.25V Steel (열화된 1Cr-1Mo-0.25V강의 DBTT 크기효과 보정에 관한 연구)

  • Nam, Seung-Hun;Kim, Eom-Gi;Lee, Dae-Yeol
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.25 no.12
    • /
    • pp.2109-2115
    • /
    • 2001
  • Miniaturized specimen technology is useful to characterize the mechanical behavior when it is difficult to sample the material enough for the test. In this study, two kinds of miniaturized Charpy impact specimens(i.e., miniaturized specimen with side groove and without side groove) of aged 1Cr- lMo-0.25V steel were prepared and tested. The relationship between the extent of degradation in terms of ductile brittle transition temperature(DBTT) and the fracture stress of 1Cr-1Mo-0.25V steel was established. The fracture stress obtained from miniaturized specimen without side groove turned out to be linearly related with the DBTT of standard specimen. Therefore the fracture toughness of aged turbine rotor steel might be evaluated by the fracture stress. In addition, the correlation between DBTT of standard specimen and that of miniaturized specimen was investigated. As the results of normalizing DBTT by maximum elastic tensile stress, the normalized DBTT of miniaturized specimen without side groove allows one to estimate that of standard specimen.

Effect of Specimen Thickness on Fatigue Crack Growth (피로균열진전에 미치는 시편 두께의 영향)

  • 김재훈;김영균;윤인수
    • Journal of the Korean Society of Safety
    • /
    • v.13 no.4
    • /
    • pp.79-86
    • /
    • 1998
  • The effect of specimen thickness on fatigue crack growth behavior has been carried out by compact tension specimens of thickness of 3mm, 10mm and 25mm for maraging steel and Al 7075-T6. The closure points were determined during the test by means of a clip-gage situated at the notch mouth. Specimen thickness have no apparent influence on the fatigue crack growth rate of maraging steel, but the crack growth rate of 25mm thickness specimen for Al 7075-T6 is faster than that of 3 and 10mm specimens. The difference of crack growth rates can be successfully explained by considering the different stress state of plane strain and plain stress due to the variation of specimen thickness. Also the crack opening ratio of 25mm specimen is greater than those of 3 and 10mm specimens. When a side groove is introduced in a 10mm specimen, the crack growth rate is approximately similar to that of 25mm specimen. The effective thickness expression of $B_e=B_o-(B_o-B_N)^2B_o$ is the most appropriate to evaluate the crack growth rate of side-grooved specimen. Fatigue crack growth rates can be well described by $\Delta K_{eff}$ of the crack closure points in regardless of all thickness and side-grooved specimens.

  • PDF

Concrete Compressive Strength Prediction from Deteriorating Apartment Site (노후아파트 현장에서의 콘크리트 압축강도 추정)

  • Lee Kyu-Dong;Rhim Hong-Chul;Rhim Byeong-Ho
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2006.05a
    • /
    • pp.155-158
    • /
    • 2006
  • Deduction of compressive strength in concrete members is very important to decide stability of structures. In this study, we compare the compressive strength of concrete between nondestructive test done to the building which was to be demolished at residential reconstruction site and destructive test of core specimen from the site. The result is more reliable because ore can compare the measurement of nondestructive tell with the result from destructive test using drilled cores. Compressive strength of each material was calculated with the result of rebound number test. In addition, we performed ultrasonic test for another result of compressive strength. And we made a comparative study of compressive strength of concrete drawn from both nondestructive and destructive tests.