Mechanical Properties of Laser-Welded Multi-Material Tailor-Welded Blanks (레이저 TWB된 이종접합강의 기계적 특성)

  • Nam, Ki-Woo;Park, Sang-Hyun;Lee, Kyu-Hyun;Lee, Mun-Yong
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.36 no.8
    • /
    • pp.857-863
    • /
    • 2012
  • In this study, tailor-welded blanks(TWB) were formed between high-strength steel(SABC1470) and cold rolled steels(SPFH590 and SPFC980) to improve passenger safety and reduce the weight of cars. Multi-material TWB specimens were highly strengthened through the heat treatment of SABC1470. The change in tensile strength caused by the stand-by time until water cooling after stamping and the deformation behavior of high-speed bending in a statically indeterminate condition such as in the center-pillar were evaluated. Multi-material TWB specimens that were heat-treated at the same temperature tended to show a decrease in tensile and yield strength, depending on the stand-by time until water cooling. On the other hand, Multi-material TWB specimens(SABC1470+SPFH590) that were heat treated at $850^{\circ}C$ showed good properties that were suitable for ensuring passenger safety in car accidents. From the viewpoint of passenger safety, it is best to use SABC1470 and SPFH590 in the upper and lower area of the center-pillar, respectively.

Mechanical characteristics and bead geometry according to laser welding parameters for tailor-welded-branks of hot press forming steel (레이저용접을 이용한 핫프레스포밍강의 맞춤식 재단 용접강판에서 용접공정변수에 따른 기계적 특성 및 비드형상)

  • Kang, Minjung;Kim, Cheolhee;Seo, Jong Dock;Lim, Chang Young
    • Laser Solutions
    • /
    • v.18 no.2
    • /
    • pp.5-10
    • /
    • 2015
  • A tailor welded blank (TWB) is a welded blank comprised of two or more sheets with different properties - thickness, strengths or formabilities. TWBs are applied to the body panels to reduce weight and cost of the part. In this research, ultra high strength steel and high ductility steel were joined and laser tailor welded blanks were implemented. Yb:YAG laser welding tests were conducted with various welding conditions, and mechanical and geometrical characteristics of weldments were evaluated.

Development of Reinforcement Side Outer Using TWB Hot Stamping Process (TWB 핫스탬핑 공법 적용을 통한 일체형 사이드아우터 부품 개발)

  • Kim, Soyoun;Kong, Hoyoung
    • Journal of Welding and Joining
    • /
    • v.33 no.6
    • /
    • pp.36-41
    • /
    • 2015
  • In the automotive industry, TWB hot stamping process is broadly adapted to reduce weight of the car and improve fuel efficiency. However, the process faces a problem of weakened strength of the welded zone after hot stamping process, due to the fact that Al-Si elements of the coating layer penetrating the welded zone. In this study, filler wires with high percentages of carbon and manganese is adapted during laser welding process to secure the strength of the fusion zone. In addition, wire feeding speed and laser welding speed are optimized by sample test.

Flow Behavior of Laser Welded Boron Steel Sheet in Uniaxial Tension at Elevated Temperature (레이저 용접된 보론강판의 고온 인장 특성 평가)

  • Kim, D.;Kim, J.H.;Yoo, D.H.;Chung, K.;Kim, Y.;Lee, M.Y.
    • Transactions of Materials Processing
    • /
    • v.20 no.5
    • /
    • pp.362-368
    • /
    • 2011
  • For the purpose of improving crashworthiness qualities and maximizing weight saving efficiency, TWB's(tailor welded blanks) of quench-hardenable boron steel sheet formed by hot stamping processes has been used for automotive BIW (body in white) applications. In this work, the flow behaviors of TWB of quench-hardenable boron steel sheet were investigated in uniaxial tension tests at elevated temperature. TWB's having a uniform thickness of 1.4mm were fabricated by laser welding. Specimens with two weld line directions were used to test the mechanical property and reliability of the weld zone. After heating at $950^{\circ}C$ for 5min, the specimens were subjected to tension test at 650, 700 and $800^{\circ}C$ with a strain rate of 0.01 /s and at $700^{\circ}C$ with strain rates of 0.01, 0.1 and 1/s. The ultimate strength of the weld zones was higher than that of the base materials at 650 and $700^{\circ}C$, but was similar to the base metal at $800^{\circ}C$. Fracture occurred at the base material at 650 and $700^{\circ}C$, but at the weld zone at $800^{\circ}C$.

Study on the Failure Criterion for Finite Element Analysis of Precise Shearing (정밀전단시의 유한요소 해석을 위한 파단기준 연구)

  • 강대철
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.9 no.5
    • /
    • pp.80-86
    • /
    • 2000
  • The Tailor Welded Blanks(TWB) are using various materials (different thickness, strength and different materials) can be welded together prior to the forming process. Therefore, TWB applications have become little by little important in automobile industries, because it has more light weight and process reduction. A burnish area is very important for TWB using laser welding. In this paper, evaluated failure criterion, effect of clearance and distance of between pad and punch by computer simulation. We used element separation method for fracture. And applied a plastic strain to failure criterion. According to the analysis results, we obtain failure criterion, when plastic strain is 2.0. The burnish area and clearance were inverse proportional.

  • PDF

Experimental Formability Investigation for FSW Sheets with Respect to Base Material's Directional Combination (모재의 방향성에 따른 마찰교반용접 판재의 성형성에 관한 실험적 연구)

  • Kim, Dae-Yong;Lee, Won-Oh;Kim, June-Hyung;Kim, Chong-Min;Chung, Kwan-Soo
    • Transactions of Materials Processing
    • /
    • v.18 no.1
    • /
    • pp.73-79
    • /
    • 2009
  • In order to investigate the formability of friction stir welded(FSW) tailor welded blanks(TWB) with respect to the base material's directional combination, aluminum alloy AA6111-T4 sheets were welded with three different conjoining types: RD-RD, TD-RD and TD-TD. Here, RD and TD represent rolling and transverse directions, respectively. For experimental formability study, three tests with gradual complexity were performed: the simple tension test with various weld line directions for uni-axial elongation, the hemisphere dome stretching test for biaxial stretching and the cylindrical cup deep drawing test. As a result, all three forming tests showed that RD-RD type samples exhibited the best formability, while TD-TD type sheets showed the least formability performance.

Weldline Movement Characteristics for the Warm Deep Drawing of Tailor Welded Blanks (용접 판재의 온간 성형에서의 용접선 이동 특성)

  • Yoo J. S.;Heo Y. M.;Lee S. M.;Seo D. G.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2001.05a
    • /
    • pp.151-155
    • /
    • 2001
  • The purpose of this study is to investigate the weldline movement of the laser welded sheets during the warm deep drawing process. For this investigation, Five steps of temperature ranges, from room temperature to $200^{\circ}C$, and two kinds of thickness combination, 0.8 mm${\times}$1.2 mm and 0.8 mm${\times}$1.6 mm SCP1 material sheets, were adopted. Also, the numerical analysis using the PAM-STAMP has been carried out with the same models as the specimens. As a result the higher temperature was adopted, the less weld-line movement was observed.

  • PDF

Development of Shearing Mechanism for Without Burr (Burr 없는 전단을 위한 전단기구 개발)

  • 강대철
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 2000.04a
    • /
    • pp.573-578
    • /
    • 2000
  • Recently, Tailor Welded Blanks(TWB) is widely used in automotive industry since the transformation characteristics of its material can be changed. However, clearance between welding surface becomes the important factor which affect the quality of the laser weld, causing difficulties in preparing the sheet. The objective of this paper is to systematically evaluate the effects of previously presented fracture criterion and shearing condition on precise mechanical shearing simulation result. Also predict the optimum shearing condition, effect of shearing condition such as clearance and punch radius on the shear plane shape was evaluated.

  • PDF

The Effect of Mechanical Property of Tailor Welding Blank and Hot Press Forming Process by the Different Anti-oxidation Coating Treatment on Boron-steel Sheet (핫프레스포밍 공정에서 내산화 코팅처리가 TWB 용접부 특성에 미치는 영향)

  • Kim, Sang-Gweon;Lim, Ok-Dong;Lee, Jae-Hoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.25 no.6
    • /
    • pp.283-291
    • /
    • 2012
  • In order to increase the anti-oxidation property during the tailor welding blanked hot press forming process for a high strength boron steel sheet, we performed a different coating method on the boron-steel sheet such as 87% Al - 13% Si and Fe - 8.87 Zn dipping plating procedure. However, during laser welding process, the Al-Si coated steel sheet has showed a low tensile strength and about half value of elongation than the original boron-steel sheet. Aluminum and silicon, elements of coating layer were diffused into the boron-steel matrix and have shown a low strength result than non-coated specimen. On the other hand, Zinc-coated boron-steel has expectedly showed a excellent tensile strength and micro-harness value in the welded area like original boron-steel.

Analysis of Impact Characteristics of Bonded Dissimilar Materials for Center Pillar (센터필라 적용을 위한 이종 접합강의 충격 특성 해석에 관한 연구)

  • Nam, Ki-Woo;Park, Sang-Hyun;Yoo, Jung-Su;Lee, Sang-Mun
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.36 no.8
    • /
    • pp.929-934
    • /
    • 2012
  • This study was carried out to analyze the dynamic characteristics of laser tailor-welded blanks (TWBs) made of dissimilar materials. The analysis was performed using Hyper Works 10.0 with Solver LS-DYNA v.971. 2D-Shell was used as the modeling element, and the number of elements and nodes was 35,641 and 36,561, respectively. The impact speed was 10 km/h. To analyze the impact characteristics according to the height of the weld line for the upper and lower parts of the center pillar, the length of the lower part was set as 300 and 400 mm. When the lower part was made of SPFC980 steel with a length of 300 mm, the deformation was the smallest and the absorbed energy of the impact force was the largest. On based the lower part of center pillar, the position of TWB shows the shorter and the better value. In other words, the performance depended on the proportion of the upper part made of high-strength SABC1470 steel. A lower part made of SPFH590 steel showed large deformation. In contrast, a lower part made of SPFC980 steel showed significantly lesser deformation. Therefore, the impact performance of a lower part made of SPFC980 steel with a length of 300 mm showed the best analysis result.