Nanotube Morphology Change of Ti-Ta-Zr Alloy as Zr Content

  • Kim, Won-Gi;Choe, Han-Cheol;Ko, Yeong-Mu
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2008년도 추계학술대회 초록집
    • /
    • pp.105-106
    • /
    • 2008
  • Nanotube morphology change of Ti-Ta-Zr alloy as Zr content increase has been researched using various experimental methods. Ti-Ta-Zr(3, 7 and 15 wt%) alloys were prepared by arc melting and nano-structure controlled for 24 hr at $1000^{\circ}C$ in argon atmosphere. Formation of oxide nanotubes are conducted by anodizing a Ti-Ta-Zr alloy in $H_3PO_4$ electrolytes with small amounts of fluoride ions at room temperature. Electrochemical experiments were carried out with conventional three-electrode configuration with a platinum counter electrode and a saturated calomel reference electrode. The samples were embedded with epoxy resin, leaving a square surface area of $10mm^2$ exposed to the anodizing electrolyte, 1.0M $H_3PO_4$ containing 0.8wt% NaF.

  • PDF

Corrosion Characteristics of Cell-Covered Ternary Ti-Nb-Ta Alloy for Biomaterials

  • Kim, W.G.;Yu, J.W.;Choe, H.C.;Ko, Y.M.;Park, G.H.
    • Corrosion Science and Technology
    • /
    • 제8권2호
    • /
    • pp.62-67
    • /
    • 2009
  • Ti and Ti-alloys have good biocompatibility, appropriate mechanical properties and excellent corrosion resistance. However, the widely used Ti-6Al-4V is found to release toxic ions (Al and V) into the body, leading to undesirable long-term effects. Ti-6Al-4V has much higher elastic modulus (100 GPa) than cortical bone (20 GPa). Therefore, titanium alloys with low elastic modulus have been developed as biomaterials to minimize stress shielding. The electrochemical behavior of surface-modified and MC3T3-E1 cell-cultured Ti-30(Nb,Ta) alloys with low elastic modulus have been investigated using various electrochemical methods. Surfaces of test samples were treated as follows: $0.3{\mu}m$ polished; $25{\mu}m$, $50{\mu}m$ and $125{\mu}m$ sandblasted. Specimen surfaces were cultured with MC3T3-E1 cells for 2 days. Average surface roughness ($R_a$) and morphology of specimens were determined using a surface profilometer, OM, and FE-SEM. Corrosion behavior was investigated using a potentiostat(EG&G PARSTAT 2273), and electrochemical impedance spectroscopy was performed (10 mHz to 100 kHz) in 0.9% NaCl solution at $36.5{\pm}1^{\circ}C$. The microstructures of the Ti-30(Ta,Nb) alloys had a needle-like appearance. The $R_a$ of polished Ti-30Ta and Ti-30Nb alloys was lower than that of the sandblasted Ti alloy. Cultured cells displayed round shapes. For polished alloy samples, cells were well-cultured on all surfaces compared to sandblasted alloy samples. In sandblasted and cell-cultured Ti-30(Nb,Ta) alloy, the pitting potential decreased and passive current density increased as $R_a$ increased. Anodic polarization curves of cell-cultured Ti alloys showed unstable behavior in the passive region compared to non-cell-cultured alloys. From impedance tests of sandblasted and cell-cultured alloys, the polarization resistance decreased as $R_a$ increased, whereas, $R_a$ for cell-cultured Ti alloys increased compared to non-cell-cultured Ti alloys.

High density plasma etching of novel dielectric thin films: $Ta_{2}O_{5}$ and $(Ba,Sr)TiO_{3}$

  • Cho, Hyun
    • 한국결정성장학회지
    • /
    • 제11권5호
    • /
    • pp.231-237
    • /
    • 2001
  • Etch rates up to 120 nm/min for $Ta_{2}O_{5}$ were achieved in both $SF_{6}/Ar$ and $Cl_{2}/Ar$ discharges. The effect of ultraviolet (UV) light illumination during ICP etching on $Ta_{2}O_{5}$ etch rate in those plasma chemistries was examined and UV illumination was found to produce significant enhancements in $Ta_{2}O_{5}$ etch rates most likely due to photoassisted desorption of the etch products. The effects of ion flux, ion energy, and plasma composition on (Ba, Sr)$TiO_3$ etch rate were examined and maximum etch rate ~90 nm/min was achieved in $Cl_{2}/Ar$ ICP discharges while $CH_{4}/H_{2}/Ar$ chemistry produced extremely low etch rates (${\leq}10\;nm/min$) under all conditions.

  • PDF

Zn-Vapor확산에 의한 Ti:LiTaO$_{3}$ 광도파로의 굴절률 증가에 관한 연구 (A study on the enhancement of refractive index in Ti:LiTaO$_{3}$ optical waveguides by Zn-vapor diffusion)

  • 정홍식;정영식
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제9권3호
    • /
    • pp.298-303
    • /
    • 1996
  • A double diffusion technique is developed to enhance the effective mode index of optical waveguides in $LiTaO_3$. It consists of Zn diffusion from the vapor phase at relatively low temperatures (750->$800^{\circ}C$), into waveguides initially produced by Ti indiffusion at higher temperature (1150->$1200^{\circ}C$). Both X- and Z-cut substrates are investigated. A model that combines profiles of both diffusion is formulated to calculate the expected effective index values for planar waveguides. Good agreement is found between experimental results and model predictions which assume that the initial Ti profile is not affected by the lower temperature Zn diffusion. Effective index enhancements as high as 0.005 and 0.003 are obtained by this method for the fundamental extraordinary and ordinary modes, respectively.

  • PDF

Ti 합금의 기계가공 방법에 따른 경도 변화에 관한 연구 (Hardness of Ti alloys by mechanical processing methods)

  • 반재삼;김규하;정상원;기강호;조규종
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 추계학술대회 논문집
    • /
    • pp.792-795
    • /
    • 2002
  • In previous researches, it is reported that Ti-10Ta-10Nb is robuster than Ti-6A1-4V which is used as a biomaterial in a experiment of cytotoxicity. Ti-10Ta-10Nb has enough hardness to be required as a biomaterial because the change of its hardness can be controlled more than 100% according to heat treatment condition and manufacturing condition. There are many hardness changing condition including Cast Homogenization, Solution treatment. Forging, Rolling in this research. The changing form and amount of new Ti-10Ta-10Nb to be developed in this researches, are measured as quantitative. Specially, the changing hardness amount of the specimen that is manufactured in single phase temperature, i.e. 80$0^{\circ}C$, are measured in case of high temperature rolling and high temperature cast condition.