• 제목/요약/키워드: TIG 용접

검색결과 219건 처리시간 0.026초

Ar-He 혼합가스와 hot-wire를 이용한 협개선 TIG 용접에 관한 연구 (Study on Narrow groove TIG welding using Ar-He of shielding gas & hot wire)

  • 최준태;박종련;김대순
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 춘계학술발표대회 개요집
    • /
    • pp.346-348
    • /
    • 2005
  • TIG welding can produce high quality of weld, but has the disadvantage of low productivity and high possibility of lack-of-fusion especially on heavy wall groove welding. In order to overcome such demerits of TIG welding, the hot-wire method which provides pre-heated wire and the use of He-Ar mixture gas as shielding gas were adopted. Through this study, both methods were turned out to be beneficial to the prevention of lack-of-fusion and the increase of productivity and welding speed.

  • PDF

소형펀치 시험법에 의한 초전도 마그넷 구조용강 TIG 용접부의 극저온 파괴특성 평가 (Evaluation of Cryogenic Fracture Characteristics on TIG Weldments of Superconducting Magnets Structural Steel by Small Punch Testing Method)

  • 권일현;;정세희
    • Journal of Welding and Joining
    • /
    • 제14권5호
    • /
    • pp.122-133
    • /
    • 1996
  • In order to evaluate the cryogenic fracture characteristics of structural steels for superconducting magnets of fusion reactor, small punch (SP) testing was performed on austenitic stainless steel (JN1 base metal) and its TIG weldments at 293K, 77K and 4K. The mechanical properties with respect to the extracted location of the weld metal, on the effects of welding heat cycle about base metal near fusion line in TIG weldments were investigated. The mechanical property of the weld metal in TIG weldments depends on distance from welding root, root region of weldments having the lowest mechanical property. The base metal near fusion line showed degradation of mechanical property caused by cyclic heating during the TIG welding. Based on the test results, HAZ was found to be up to 5mm from the fusion line. It is shown that SP testing is a useful tool to evaluate the mechanical properties with respect to the microstructures changes such as HAZ as well as weld metal in TIG weldments at cryogenic temperature.

  • PDF

STS 304 TIG 용접시 발생하는 열응력 해석에 관한 연구 (A Study on the Analysis of the Thermal Stress in Process of STS 304 TIG Welding)

  • 고준빈;최원두;이영호
    • Journal of Welding and Joining
    • /
    • 제19권6호
    • /
    • pp.658-663
    • /
    • 2001
  • Residual stress caused in the weldments with high restraint force are often during welding observed in the weldments of large size nozzles or radial tanks. The reason is that quantitative analysis about thermal stresses during welding is lack for this weldments. To verify FEM theory, the temperature was measured with thermocouple in a real time in this paper. Also analysis of the thermal stress for welding condition is performed by ABAQUS program package on various welding condition in STS butt welding.

  • PDF

용접 후처리에 의한 필렛용접부의 피로강도 향상에 관한 연구 (A Study on the Fatigue Strength Improvement of the Fillet Welded Connections with respect to Post-Weld Treatment)

  • 이승용;경갑수
    • 대한토목학회논문집
    • /
    • 제28권5A호
    • /
    • pp.665-672
    • /
    • 2008
  • 본 연구에서는 교량이나 선박 등의 강구조물에서 널리 사용되고 있는 하중 전달형 십자형 필렛용접 시험편에 대해 피로시험을 실시하여, 용접 후처리 조건에 따른 피로강도를 분석하였다. 용접 후처리 방법으로는 Toe Grinding, TIG Dressing 및 Weld Profiling을 적용하였으며, 피로시험은 일정진폭 반복하중 하에서 실시하였다. 피로시험 결과 하중 전달형 십자형 필렛용접 시험편은 용접 후처리를 실시한 경우와 실시하지 않은 경우 모두에서 BS 피로설계기준의 F등급을 만족하는 결과를 나타내었다. 또한 용접 후처리 방법에 따른 피로강도의 향상 효과는 Toe Grinding, TIG Dressing, Weld Profiling 순서로 증가하는 것을 알 수 있었다.

저주기 피로부하에서 F82H 강 TIG 용접 접합부의 피로손상거동 (Fatigue Damage Behavior in TIG Welded Joint of F82H Steel under Low Cycle Fatigue Loading)

  • 김동현;박기원
    • Journal of Welding and Joining
    • /
    • 제33권6호
    • /
    • pp.42-48
    • /
    • 2015
  • Reduced activation ferritic/martensitic steels are recognized as the primary candidate structural materials for fusion blanket systems. Welding is an inevitable for breeding blanket for pressure tightness and radioisotope confinement. Especially, TIG welding was chosen for sealing because it has the largest gap allowance compared to the other welding methods, and its properties are controllable by feed wire and welding conditions. In this study, the low cycle fatigue test using two-type gage such as extensometer and strain gage was applied to the TIG welded joint of F82H steel, for evaluating fatigue damage accumulation behavior of the HAZs. As the result, the over-tempered HAZ have shown a higher fatigue damage accumulation compared with other materials at all the testing conditions.

선박엔진 부품의 고능률 보수용접기술 (High-efficiency repair welding technology for marine engine components)

  • 김영식;길상철
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제41권1호
    • /
    • pp.21-30
    • /
    • 2017
  • 현재 국내에서 공장 보수용접이 가장 많이 이루어지고 있는 선박 엔진 부품은 피스톤 크라운과 배기밸브이다. 또한 선박 엔진 밸브와 크랭크 축 등의 경우에는 신규 부품에서도 성능향상을 위해 표면개질방법으로 오버레이 용접이 시공되고 있다. 용착률을 높이는 고능률 오버레이 용접 공정으로 Hot Wire GTAW, Cold Tandem GMAW, Band Arc SAW, Tandem SAW법이 개발되어 있고, 용사방법으로 PTA공정이 현장에서 많이 시공되고 있다. 입열량 제어가 용이한 공정으로 GMAW-Pulse, CMT 용접공정이 있다. 엔진 배기밸브의 보수를 위한 오버레이공정에서 열영향부에 가까운 모재 내에 액화균열이 발생하는 경우가 있어 주의를 요한다. GMAW-Pulse 공정과 CMT공정에서는 입열량 제어가 용이하여 높은 용착속도를 유지하면서도 액화균열의 발생 없이 엔진 밸브의 보수 또는 표면 개질 목적으로 시공이 가능하다. 최근에 국내에서 고능률 용접 공정으로 선박엔진의 보수 또는 표면 개질 목적으로 사용 가능한 Super-TIG 용접공정이 개발되어 있다. 이 공정은 아크를 플라즈마 스트림이라고 보고 전류증가에 따라 커지는 아크압력을 막으면서도 용가재의 용융 효율이 극대화 되도록 폭이 큰 C형의 오목한 용가재를 발명하여 용착률을 획기적으로 향상시킨 용접공정이다.

대전류 고속 TIG 용접 특성에 미치는 He 혼합비의 영향 (Effect of Be Mixing Ratio on the Characteristics of TIG Welding with High Current and High Speed)

  • 오동수;김영식;조상명
    • Journal of Welding and Joining
    • /
    • 제23권3호
    • /
    • pp.54-60
    • /
    • 2005
  • Tungsten Inert Gas(TIG) welding is today one of the most popular arc welding process because of its high quality welds and low equipment costs. Even if welding productivity increases with welding speed and current, this strategy is limited by the appearance of defects such as undercut and humping bead due to the depressed molten metal. The purpose of this study investigates the effect of He mixing ratio on the characteristics with high current and speed in TIG welding. The conclusions obtained permit to explain the arc start characteristics quantitatively and the maximum welding speed on stable bead formation with He mixing ratio for high current and speed TIG welding observed in experiments. Also through the relation of the maximum arc pressure and surface depression depth at high current and speed TIG welding, it made clear the mechanism of unstable bead formation.

TIG 용접한 저방사화 페라이트강 (JLF-1)의 고온강도 및 피로수명특성 (High Temperature Tensile Strength and Fatigue Life Characteristics for Reduced Activation Ferritic Steel (JLF-1) by TIG Welding)

  • 윤한기;이상필;김사웅
    • 대한기계학회논문집A
    • /
    • 제27권9호
    • /
    • pp.1444-1450
    • /
    • 2003
  • The fatigue life and tensile strength of JLF-1 steel (Fe-9Cr-2W-V-Ta) and its TIG weldment were investigated at the room temperature and $400^{\circ}C$. Four kinds of test specimens, which associated with the rolling direction and the TIG welding direction were machined. The base metal of JLF-1 steel represented almost anisotropy in the tensile properties for the rolling direction. And the base metal of JLF-1 steel showed lower strength than that of TIG weldment. Also, the strength of all materials entirely decreased in accordance with elevating test temperature. Moreover, the fatigue limit of weld metal was largely increase than that of base metal at both temperatures. The fatigue limit of JLF-1 steel decreased in accordance with elevating test temperature. The fatigue limit of JLF-1 steel decreased in accordance with elevating test temperature. The SEM fractography of tensile test specimen showed conspicuous cleavage fracture of a radial shape. In case of fatigue life test specimen, there were so many striations at crack initiation region, and dimple was observed at final fracture region as a ductile fracture mode.