• 제목/요약/키워드: Surface wrinkle

검색결과 66건 처리시간 0.029초

Styrene-Butadiene-Styrene Block Copolymer 위 이온빔 조사를 이용한 주름 구조 생성 메커니즘 연구 (Mechanism of Wrinkle Formation on Styrene-Butadiene-Styrene Block Copolymer via Ion-Beam Irradiation)

  • 이주환;김대현
    • 한국전기전자재료학회논문지
    • /
    • 제34권2호
    • /
    • pp.130-135
    • /
    • 2021
  • Wrinkle patterns were fabricated on styrene-butadiene-styrene (SBS) block copolymer substrates using ion-beam (IB) irradiation with various intensities. The wavelength of the wrinkle pattern increased as the IB intensity was increased from 800 to 1,600 eV. IB irradiation-induced changes in the surface properties that were confirmed via physicochemical surface analyses. X-ray photoelectron spectroscopy analysis revealed chemical surface reformation due to the IB irradiation, resulting in C-O/C=O bonds after IB irradiation that were not reported before. These results indicate that the surface chemical modification caused by IB irradiation is strongly related to the surface modulus, which is important when fabricating wrinkle patterns. Furthermore, a strong IB irradiation induced a strong compressive strain; thus the size of the wrinkle pattern was increased.

저탄소강 선재 압연의 주름성 결함 (Wrinkle Defect of Low Carbon Steel in Wire Rod Rolling)

  • 김학영;권혁철;변상민;박해두;임용택
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 제5회 압연심포지엄 신 시장 개척을 위한 압연기술
    • /
    • pp.307-316
    • /
    • 2004
  • This study examined the cause of the wrinkle defect which is frequently encountered in wire rod rolling of low carbon steel$(C0.08\~0.13wt.\%)$. Even a small defect on the surface of rolled bars can easily develop into fatal cracks during cold heading process of low carbon steel, and it is therefore necessary to minimize inherent defects on the surface of hot rolled bars. Hot rolling process of low carbon steel was analyzed to identify the cause of the wrinkle defect in conjunction with FE analysis. The integrated analysis revealed that the wrinkle defect initiated in the first stage of rolling, and it was at the billet edge where severe deformation and drastic temperature drop were present. To elucidate the micro-mechanical mechanism of the wrinkle defect, hot compression tests were carried out at various temperatures and strain rates using Gleeble-3800. The surface profile of the each other compressed specimens was compared, and rough surface lines were observed at relatively low temperatures. Those surface defects can develop into wrinkles during multi-pass rolling. To control the wrinkle defect in rolling, it is necessary to design an adequate caliber which can minimize the loss of ductility, and thereby prevent flow localization. To use the result of this study fur other steels, the quantitative measure of the wrinkle defect and flow localization parameter should be proposed.

  • PDF

UV/Ozone 처리를 통한 Polydimethylsiloxane(PDMS) 주름 구조의 물리화학적 특성 분석 (Physicochemical Characteristics of UV/Ozone Treated Polydimethylsiloxane(PDMS) Wrinkle Structures)

  • 박홍규;박승엽
    • 한국정보전자통신기술학회논문지
    • /
    • 제15권5호
    • /
    • pp.321-327
    • /
    • 2022
  • 본 논문에서는 UV/Ozone 처리를 통해 Polydimethylsiloxane(PDMS) 표면에 주름 구조를 형성하고, 물리화학적 특성 분석을 통해 줄금 구조 형성 메커니즘을 밝혔다. 30분의 UV/Ozone 처리를 통해 PDMS 표면에 주름 구조를 형성하였으며, 주사전자현미경의 단면 촬영으로 PDMS 표면의 주기적인 주름 형성을 확인할 수 있었다. 또한, XPS 스펙트럼 분석을 통해 PDMS 표면에 SiOx의 실리카 경질 표면이 UV/Ozone에 의해 만들어지는 것을 확인하였고, PDMS 표면의 경질층과 내부의 연질층 사이의 탄성 계수 불일치는 PDMS의 주름 형성의 팽윤 메커니즘을 확인시켜 준다. 본 연구 결과는 UV/Ozone 처리에 의한 PDMS 표면의 주름 구조 형성 메커니즘의 이해도를 향상시킬 뿐만 아니라, 향후 UV/Ozone 조사 조건에 따라 주름 구조의 진폭과 주기를 조정하는데 기초 연구로 쓰일 수 있을 것이다.

마이크로 표면주름 구조에 따른 물방울 동적거동에 관한 실험적 연구 (Experimental Study of Dynamic Behavior of a Water Droplet on Diverse Wrinkling Surfaces)

  • 백대현;;박상후
    • 한국정밀공학회지
    • /
    • 제32권6호
    • /
    • pp.577-585
    • /
    • 2015
  • We fabricated multi-scale such as macro-, micro-, and multi-scale wrinkles by using repetitive volume dividing (RVD) method and thermal curing process. Also wrinkle surface was modified with coating of a self-assembled monolayer (SAM). We measured the contact angle of each wrinkled surface, and observed the behavior of droplets on sloping surface. Through experimental study, we found out that the contact angle was much higher in case of multi-scale and SAM coated wrinkles. And micro-scale wrinkle showed a high contact angle comparing with that of macro-scale wrinkle. Dynamic behaviors of a water droplet like sliding velocity on diverse wrinkled surfaces were dependent on their static contact angles. These results showed that hydro-dynamic characteristics were changed depending on the wrinkle structure and the material forming the wrinkle. These dynamic characteristics can be utilized in bio-chip, microfluidics, and many others in order to control easily chemical reactivity.

반복 접촉-분리 방식을 이용한 마이크로 표면주름 구조 제작 (Investigation into the Fabrication of Micro-scale Winkles using Repetitive Contact-and-open Method)

  • 김성진;박상후
    • 한국정밀공학회지
    • /
    • 제29권8호
    • /
    • pp.920-926
    • /
    • 2012
  • Wrinkling is a common phenomenon in nature and the shape of a wrinkle can be defined using characteristic dimensions such as pitch, length, amplitude, and density etc. Wrinkle structure can be utilized in various research fields, and especially it has special characteristics when it used in applications of heat transfer; a wrinkly surface has the effect to promote turbulent flow and increasing surface area. However, the generation of wrinkle structures in somewhat regular is not easy. Till now, there are some research works focused on realization of wrinkles in micro scale. However, most of the processes generally requires high precision equipments and high costs, and also there is a limitation to generate the wrinkles in a large area. In this study, we propose a novel method named as a RCO (repetitive contact-and-open) process to fabricate wrinkle structure with low cost and relative easy way. Using the RCO, we fabricated micro-corrugate structures successfully. From the experimental results, we found out the process parameters of RCO, and showed the possibility of RCO to be used in real applications.

Improving Wrinkle Resistance of Cotton Fabric by Montmorillonite

  • Yuen C.W.M.;Kan C.W.;Lee H.L.
    • Fibers and Polymers
    • /
    • 제7권2호
    • /
    • pp.139-145
    • /
    • 2006
  • Cotton fabric was treated with montmorillonite (MMT) so as to evaluate its effectiveness on improving its wrinkle resistance. The MMT in emulsion form was applied to cotton fabric by padding and finally the wrinkle resistance of the MMT-treated cotton fabric was improved. Furthermore, instrumental methods were used for studying the presence of MMT particles on the cotton fabric surface. It was noted that nano-scale MMT particles adhered on the fiber surface and the particle size played an important role in influencing the wrinkle resistance of the cotton fabric. The experimental results are discussed thoroughly in this paper.

세포 표면 특성을 이용한 사과 신선도 평가 (Evaluation of Apple Freshness by Characterizing Surface Texture of Cells)

  • 조용진
    • Journal of Biosystems Engineering
    • /
    • 제22권4호
    • /
    • pp.433-438
    • /
    • 1997
  • The freshness of apple was evaluated by characterizing the surface texture of flesh cells. The freshness index which was related to the amount of wrinkles on the cell surface was defined to quantify the freshness. Four parameters relevant to the amount of the cell wrinkles were selected and measured using image analysis including wrinkle extraction procedure and Fast Fourier Transform of a wrinkle-extracted image. Out of 4 parameters, three parameters had highly significant correlations with the time elapsed after harvest. But it was concluded that two parameters out of such 3 parameters could be used for description of freshness index.

  • PDF

약한 광중합과 열경화를 이용한 곡면 미세 표면주름 제작 (Fabrication of Microscale Wrinkles on a Curved Surface Using Weak-Polymerization and Thermal Curing Process)

  • 양정호;조지준;박상후
    • 한국정밀공학회지
    • /
    • 제33권10호
    • /
    • pp.875-880
    • /
    • 2016
  • In this study, we proposed an effective and simple way to directly generate wrinkle patterns on a curved surface. A curved surface was prepared using a 3D printer and an UV (Ultraviolet)-lighting system was utilized to weakly polymerize the UV-curable thin resin layer coated on the surface, resulting in a gradient of material properties in the layer thickness. Subsequently, a thermal curing process was conducted to generate microscale wrinkles by compressive forces that were generated during complete curing. Wrinkle shapes from 5, 15, 25 sec of UV-light exposure were compared. With increasing UV-exposure, the line-width of wrinkles became thicker due to much higher strength of skin zone. The results indicated that the proposed fabrication process could be utilized for surface modification in diverse research fields.

수지처리가 환편 니트 소재의 물성에 미치는 영향 (Effect of Resin Finishing on the Physical Properties of the Knitted Fabrics)

  • 권영아;박종식
    • 한국염색가공학회지
    • /
    • 제18권3호
    • /
    • pp.23-30
    • /
    • 2006
  • The bending properties, wrinkle resistance, and fabric retention behaviors of cotton knitted fabrics in the wale and course directions were studied for their dependence upon resin finishing, knit structure, and washing cycles. Stiffness, wrinkle recovery angles, and dimensional stability were investigated before and after resin finishing and laundering. It has been found that any change in the physical properties of the knitted fabrics with respect to knit structure and fabric directions are related to accompanying modifications to the state of the fiber properties. The decrease of fabric shrinkage rates and wrinkle recovery properties from increasing laundering cycles is related with resin incorporated on the fiber surface. This study shows that resin finishing on knitted fabrics can be performed only to improve fabric retention properties with reduced wrinkle recovery properties.

삼각형 태양돛의 주름저감 설계방안 (Wrinkle Reduction Design Method of Triangular Solar Sail)

  • 배홍수;우경식
    • 한국항공우주학회지
    • /
    • 제41권12호
    • /
    • pp.940-949
    • /
    • 2013
  • 본 논문에서는 삼각형 태양돛의 주름저감설계 방안에 대한 연구를 수행하였다. 태양돛 멤브레인에 부분적으로 발생하는 주름으로 인하여 구조물의 추력성능과 제어성능에 영향을 받을 수 있으므로 멤브레인에 발생하는 주름을 감소시키거나 제거하는 것은 매우 중요하다. 주름을 저감하는 방법으로 태양돛 멤브레인과 붐을 연결하는 케이블의 하중의 각도를 조정하는 방식, 현수선 방식 및 현수선-와이어 방식을 고려하였으며 매개변수 연구를 통하여 주름저감효과에 대해 체계적으로 조사하였다.