• Title/Summary/Keyword: Surface finishing materials

Search Result 212, Processing Time 0.026 seconds

The Effects of Surface Finish and Grain Size on the Strength of Sintered SiC (소결탄화규소의 표면처리 및 비정상 성장입자가 강도에 미치는 영향)

  • 유영혁;김영욱;이준근;김종희
    • Journal of the Korean Ceramic Society
    • /
    • v.21 no.1
    • /
    • pp.27-32
    • /
    • 1984
  • During the last decade there have been many studies on the new ceramics especially engineering ceramics. Sintered silicon carbide is one of the main materials in engineering ceramics. This study shows the effects of surface treatment and microstructure especially the abnormal grain growth on the strength of sintered SiC. Surface of sintered SiC and treated with 400, 800 and 1200 grit diamond wheel. Grain growth is introduced by increasing the sintering times at 205$0^{\circ}C$. The $\beta$longrightarrow$\alpha$ transformation occurs during the sintering of $\beta$-starting materials and is often accompanied by abnormal grain growth. The overall strength distribution are estimated using the Weibull statistics. The results show that the strength of sintered SiC is limited by extrinsic surface flaws in normal-sintered specimens. And it is sound that the finer the surface finishing and the grain size the higher the strength results. But the strength of abnormal sintering specimens is limited by the abnormally-grown large tabular grains. The Weibull modulus increases with the decreasing grain size and the decreasing grit size of grinding.

  • PDF

Change of Stiffness and Impact-Resistance of Flush Door Depending on Core Composition (플러쉬문의 심재구성에 따른 강성도 및 내충격성의 변화)

  • 장상식
    • Journal of the Korea Furniture Society
    • /
    • v.12 no.1
    • /
    • pp.39-45
    • /
    • 2001
  • This study was carried out to evaluate the feasibility of using HDF as surface panels as well as core materials for flush door manufacturing. Several core compositions were developed and applied to manufacture door specimens. Core materials were tested under bending load, door manufacturing process was analysed to find better way of using HDF for door manufacturing, and door specimens were tested under bending, twisting and impact loads. From this study, it was concluded that HDF can be used to manufacture quality flush doors. And it was desirable to use light color HDF as surface panels because dark color HDF caused a problem in manufacturing process by shadow shown through finishing veneer. HDF doors were light, and showed good quality and higher resistance against bending twisting and impact loads.

  • PDF

Improving the Photo-stability of p-aramid Fiber by TiO2 Nanosol (TiO2 sol-gel 합성에 의한 파라 아라미드 섬유의 내광성 증진 연구)

  • Park, Sung-Min;Kwon, Il-Jun;Sim, Ji-Hyun;Lee, Jae-Ho;Kim, Sam-Soo;Lee, Mun-Cheul;Choi, Jong-Seok
    • Textile Coloration and Finishing
    • /
    • v.25 no.2
    • /
    • pp.126-133
    • /
    • 2013
  • Although para-aramid fibers poss higher mechanical properties, they show very low resistance to sunlight exposure. This paper studied on the effect of nano-sol coated $TiO_2$ to improve the photo-stability of p-aramid fibers. Titanium dioxides were prepared by sol-gel method from titanium iso-propoxide at different R ratio ($H_2O$/titanium iso-propoxide). All samples were characterized by XRD, TEM and UV-vis spectrometer. The mechanical properties of p-aramid fabrics by $TiO_2$ nano-sol coating before and after sunlight irradiation were measured with tensile tester. XRD pattern of titanium dioxide particles was observed by mixing phase together with rutile and anatase type. The results showed, after sunlight irradiation, the decreased mechanical properties of the fiber. Furthermore, the sunlight irradiation obviously deteriorated the surface and defected areas of the fiber severely by photo-induced chain scission and end group oxidation in air.

Fabrication of Highly Conductive Yarn using Electroless Nickel Plating (무전해 니켈 도금법을 이용한 고성능 도전사의 제조)

  • Hong, So-Ya;Lee, Chang-Hwan;Kim, Joo-Yong
    • Textile Coloration and Finishing
    • /
    • v.22 no.1
    • /
    • pp.77-82
    • /
    • 2010
  • Highly conductive yarn was successfully obtained using electroless nickel plating method with palladium activation. In the presence of palladium seed on surface of fibers as a catalyst, continuos nickel layer produced on surface of fibers by reducing $Ni${2+}$ ion in the electroless plating bath to $Ni^0$. It was found that the Pd-activation using $SnCl_2$ and $PdCl_2$ to deposit palladium seeds on the surface of fibers plays a key role in the subsequent electroless plating of nickel. It also found that electroless nickel plating on the fibers can induce the nickel-plated $ELEX^{(R)}$ fibers to improve the electrical conductivity of the fibers. The thickness of nickel coating layer on the Pd-activated $ELEX^{(R)}$ fibers and specific conductivity of the fiber were increased through electroless plating time. The temperature of nickel plating bath was very effective to enhance the nickel deposition rate.

AN EXPERIMENTAL STUDY ON THE SURFACE POLISHING EFFECTS OF VARIOUS RESTORATIVE MATERIALS (수종(數種) 수복물(修復物)의 표면(表面) 연마효과(硏磨效果)에 관(關)한 실험적(實驗的) 연구(硏究))

  • Park, Young-Ho;Min, Byung-Soon;Choi, Ho-Young;Park, Sang-Jin
    • Restorative Dentistry and Endodontics
    • /
    • v.10 no.1
    • /
    • pp.103-114
    • /
    • 1984
  • The purpose of this study was to compare the polished surfaces of two composite resins (Clearfil F and Durafill) with those of glass ionomer cement (Fuji ionomer cement) and to observe what types of polishing devices are valuable, and then to establish a clinically satisfactory procedures. Studies have been undertaken to determine the effects of glass plate matrix and finishing instruments (Carborundum point, White point and Sof-Lex medium) on the surface finish of three restorative materials. The results were examined with profilometer (Kosaka laboratory LTD. Tokyo, Japan) and scanning electron microscopy (JSM-T20: JEOL). The results were as follows: 1. The most satisfactory surface finishes were produced against glass matrix. 2. Coarser finishes were obtained with use of carborundum point. 3. Generally Fuji ionomer cement were left surfaces with higher roughness values. 4. The smoothest finishes were obtained with Sof-lex medium. 5. Clearfil-F was showed more smoother than the other restorative materials.

  • PDF

Concrete Specification and Mixing Design for the Reduction of Slab Defects in Underground Parking Lot (지하주차장 슬래브 하자 저감을 위한 콘크리트 규격 및 배합설계)

  • Kim, Han-Sic;Ha, Jung-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2023.05a
    • /
    • pp.235-236
    • /
    • 2023
  • Concrete surfaces have weak surface strength due to bleeding and laitance, and problems such as peeling, cracking, and cracking may occur. In particular, underground parking lots can be said to be more vulnerable to peeling, breaking, and cracking if excessive loading of materials and equipment movement are not managed at the initial age after placing of concrete. Cracks, peeling, and cracking problems in slab concrete in underground parking lots of apartments can lead to leakage problems and affect finishing materials constructed on top of topping concrete, reducing the performance required for waterproof materials. Therefore, in this study, the bleeding and surface strength according to the standard of topping concrete and the use of admixture were reviewed to solve the crack, peeling, and cracking problems among the types of defects in underground parking lot slab concrete. As a result, it was derived that the optimal concrete compressive strength is 30MPa or more, and it is a reasonable performance design method to prohibit the substitution of admixtures.

  • PDF

The Optimum Binder Ratio for High-Strength Self-Leveling Material (고강도 Self-Leveling재의 최적 결합재비)

  • 김진만
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2002.11a
    • /
    • pp.67-76
    • /
    • 2002
  • Self-leveling material(SLM) is one of the floor finishing materials which make flat surface like as water level by itself in a short time. So it is possible to increase construction speed and enhance economical efficiency. In this study, author intended to develop SLM for the industrial warehouse and factory loading heavy weight machinery and vehicles. The demanded properties for this type of SLM are above 20mm of flow value and above 300kgf/cm2 of 28-days compressive strength. To possess demended strength and fluidity, SLM have to be composed of many types of binders and chemical additives. So it is difficult to decide suitable mixing proportion of composition materials. In this study, author investigated the weight percentage effect of main composition materials for high-strength self-leveling material, by experimental design such as tables of orthogonal arrays and simplex design, and by statistical analysis such as analysis of variance and analysis of response surface. Variables of experiments were ordinary portland cement(OPC), alumina cement(AC), anhydrous gypsum(AG), lime stone(LS) and sand, and properties of tests were fluidity of fresh state and strength of hardened state. Results of this study are showed that suitable mix proportions of binders for the high strength self-leveling materials are two groups. One is 78~85.5% OPC, 7.5~9.5% AC, 9~12.5% AG and the other is 72.5~78% OPC, 9~12.5% AC, 13~l5% AG.

  • PDF

Attachment Rate Analysis of Airborne Chlorides by Construction Finish Material to Measure the Amount of Chlorides on the Surface (표면염화물량 산정을 위한 건축마감재별 비래염분 부착율 분석)

  • Cho, Gyu-Hwan;Ji, Dong-Hun;Jung, Jae-Min;Park, Dong-Cheon
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2014.11a
    • /
    • pp.57-58
    • /
    • 2014
  • For durability design to protect against chloride-induced corrosion, it is important to estimate the amount of chlorides on the surface. However, it is difficult to estimate the airborne chlorides, a boundary condition, due to the difference between the amount of chlorides attached to a surface of an actual structure and that in the air. Therefore, in this study the attachment rate analysis of airborne chlorides was evaluated for 13 types of finish materials. As a result, despite differences in the amount of airborne chlorides according to the finishing type, it was found that 60 percent of airborne chlorides were attached to mortar, 30 percent were attached to steel, and 25 percent were attached to tiles compared with the amount of chlorides in the air.

  • PDF

Effect of sintering programs and surface treatments on monolithic zirconia

  • Seren Nur Dokuzlu ;Meryem Gulce Subasi
    • The Journal of Advanced Prosthodontics
    • /
    • v.16 no.1
    • /
    • pp.25-37
    • /
    • 2024
  • PURPOSE. To investigate the effect of sintering programs and surface treatments on surface properties, phase transformation and flexural strength of monolithic zirconia. MATERIALS AND METHODS. Zirconia specimens were sintered using three distinct sintering programs [classic (C), speed (S), and superspeed (SS)] (n = 56, each). One sample from each group underwent scanning electron microscopy (SEM) and grain size analysis following sintering. Remaining samples were divided into five subgroups (n = 11) based on the surface treatments: control (CL), polish (P), glaze (G), grind + polish (GP), and grind + glaze (GG). One sample from each subgroup underwent SEM analysis. Remaining samples were thermally aged. Monoclinic phase volume, surface roughness, and three-point flexural strength were measured. Monoclinic phase volume and surface roughness were analyzed by Kruskal-Wallis and Dunn tests. Flexural strength was analyzed by two-way ANOVA and Weibull analysis. The relationships among the groups were analyzed using Spearman's correlation analysis. RESULTS. Sintering program, surface treatment, and sintering × surface treatment (P ≤ .010) affected the monoclinic phase volume, whereas the type of surface treatment and sintering × surface treatment affected the surface roughness (P < .001). Type of sintering program or surface treatment did not affect the flexural strength. Weibull analysis revealed no significant differences between the m and σo values. Monoclinic phase volume was positively correlated with surface roughness in the SGG and SSP groups. CONCLUSION. After sintering monolithic zirconia in each of the three sintering programs, each of the surface treatments can be used. However, for surface quality and aging resistance, G or GG can be recommended as a surface finishing method.

Effects of Water-Repellent on the Physical Properties of Water Paint (발수제가 수성페인트의 물리적 성능에 미치는 영향)

  • Lee, Soo-Yong;Nam, Gee-Yung;Kim, Ji-Hyun
    • Journal of the Korea Institute of Building Construction
    • /
    • v.14 no.3
    • /
    • pp.259-265
    • /
    • 2014
  • This study is to analyze durability of water-repellent paints mixed with water-repellents as outer surface finishing materials, and evaluate its feasibility. General functions and water-repelling effects were tested, and the feasibility was evaluated based on the test results. The experimental results of heat conduction durability, air permeability, absorption, and bond strength suggested that water-repellent paints mixed with water-repellents were suitable for finishing materials. Considering overall general durability performances, stable mixing ratios were 2, 5, and 8%.