A study of the damage evolution laws for ductile materials was carried out to predict the ductile fracture behavior of a marine structural steel (EH36). We conducted proportional and non-proportional stress tests in the experiments. The existing 3-D fracture strain surface was newly calibrated using two fracture parameters: the average stress triaxiality and average normalized load angle taken from the proportional tests. Linear and non-linear damage evolution models were taken into account in this study. A damage exponent of 3.0 for the non-linear damage model was determined based on a simple optimization technique, for which proportional and non-proportional stress tests were simultaneously used. We verified the validity of the three fracture models: the newly calibrated fracture strain model, linear damage evolution model, and non-linear damage evolution model for the tensile tests of the asymmetric notch specimens. Because the stress evolution pattern for the verification tests remained at mode I in terms of the linear elastic fracture mechanics, the three models did not show significant differences in their fracture initiation predictions.
Standard compression tests of steel fiber reinforced concrete (SFRC) cylinders are conducted to formulate compressive stress versus compressive strain relationship of SFRC. Axial pullout tests of SFRC specimens are also conducted to explore its tensile stress strain relationship. Cover concrete spalling and reinforcement buckling models developed originally for normal reinforced concrete are modified to extend their application to SFRC. Thus obtained monotonic material models of concrete and reinforcing bars in SFRC members are combined with unloading/reloading loops used in the cyclic models of concrete and reinforcing bars in normal reinforced concrete. The resulting path-dependent cyclic material models are then incorporated in a finite-element based fiber analysis program. The applicability of these models at member level is verified by simulating cyclic lateral loading tests of SFRC columns under constant axial compression. The analysis using the proposed SFRC models yield results that are much closer to the experimental results than the analytical results obtained using the normal reinforced concrete models are.
실내시험은 다양한 응력조건과 배수조건의 모사가 가능하므로 상용 유한요소 해석프로그램의 입력변수 산정에 필수적인 요소가 되나 시료의 운송, 시료추출, 트리밍, 함수비 손실, 응력이완으로 인한 교란과 채취가 관입시의 교란으로 양질의 시료를 얻는데 한계가 있다. 이러한 한계를 극복하기 위하여 교란에 따른 시료의 변화를 이해하고 이를 실내 시험 결과로부터 입력변수 산정에 적용할 수 있는 방법을 찾아내는 것이 필요하다. 따라서 본 연구에서는 정확한 입력정수의 산정이 필수적인 연약점성토의 교란에 대한 영향을 파악하고자 정규압밀 점성토의 교란에 따른 강도 및 강성의 변화를 삽축시험기를 이용한 응력경로시험을 통하여 파악하였다. 그 결과, 교란의 정도가 강도에 미치는 영향은 크지 않았으나, 전단강성계수와 커플링강성계수의 변형률에 따른 감쇠 경향에는 큰 영향을 미치는 것으로 나타났다.
In the present investigation, it was attempted to design the rolling pass schedule fur a clean steel of 0.1C-1.5Mn-0.25Si with the objective of the austenite grain refinement. As the method of approach, a coupled mathematical modeling technique was proposed which consists of a recrystallization model and a flow stress modes. The validity of the coupled model was examined through comparison with results of continuous and discontinuous compression tests at various temperatures, strains and strain rates. The coupled model was incorporated with the finite element method to set up a systematic design methodology far the rolling path schedule for austenite grain refinement. Two path schedules were obtained and discussed in the paper with regard to rolling path time, average grain size, grain size deviation in thickness, etc.
주응력회전시 모래의 강도특성을 연구하기 위하여 일련의 응력경로에 대해 시험을 실시하였다. 이들 결과는 공시체의 높이에 따라 25cm와 40cm로 분류할 수 있으며 공시체에 작용된 토르 크(Torque)는 시계방향으로만 작용시켰다. 본 연구에서는 비 틀림전단시험시 주응력비에 대한 모래의 강도특성이 조사되었고 그 결과를 Lade의 파괴규준과 비교하여 보았다. 그리고 공시체높 이에 대한 영향을 고려하였다. 이들 시험결과로 부터 모래의 내부마찰각은 축차주응력비 $b:(\sigma_2 -\sigma_s)/(\sigma_2,-\sigma_3)$에 많은 영향을 받는 것으로 나타났다. 모래의 파괴강도는 응력경로에 영향을 받지 않고 현재의 응력상태에 의해 결정 되어지며 25cm와 40cm 높이의 공시체에 대한 비교로부터 단부구속의 영향은 발견할 수 없었다. 그리고 신장력이 작용된 b=0.5 이상인 시험에서는 변형을 국부현상에 의한 Necking현상이 발견되었다.
본 연구에서는 포화 점성토지반 침하량의 합리적인 평가를 위한 새로운 개념의 응력경로법 적용방법을 제안하였다. 제안된 적용방법은 특정 점성토지반에 대해 구조물 침하와 관련하여 현장에서 나타날 수 있는 모든 응력변화 조건을 포괄하는 특성변형거동을 실험적으로 선행하여 평가한 다음, 이를 이용하여 일체의 추가적인 시험없이 발생가능한 다양한 현장조건에 대해 손쉽게 침하량을 평가하는 방법이다. 본 연구의 Part I에서는 이러한 새로운 침하량 평가개념의 실용화와 관련하여 포화 점성토지반의 침하관련 특성변형거동을 최소한의 시험만으로 효율적으로 평가하고 이를 바탕으로 임의의 응력변화 조건에 대해 손쉽게 변형거동을 예측하는 구체적인 방법을 개발하였으며, 그 적용성을 실제 사례를 통해 명확히 확인하였다.
저토피 구간에서 기존터널 하부에 새로운 터널을 교차하여 신설할 때에 하부 터널굴착으로 인하여 발생하는 교차부 주변지반의 거동을 대형모형실험과 수치해석을 통하여 연구하였다. 모형실험결과 교차 전 후의 하부터널 굴착에 따른 종방향 응력전이가 상부터널에 의하여 차단됨을 알 수 있었다. 수치해석결과에 의하면 측압계수 K = 0.38인 경우에 응력그림자 현상으로 단일터널 천단부에서의 최소주응력 감소는 상하교차터널의 천단에서보다 크게 발생한다. 직각교차터널에서는 기존상부터널의 영향으로 응력그림자 현상이 나타나 단일터널에 비하여 작은 응력감소를 보인다.
풍화토의 다짐성형 시료에 대한 삼축시험의 $K_0$ 압밀 결과를 바탕으로 불포화토에 대한 유효응력 가설을 검증하였다. 흡수응력 특성곡선은 함수특성에 관한 불포화토 거동을 기술하며, 전단강도나 함수특성곡선으로부터 구할 수 있다. 본 연구에서는 K0 압밀 경로도 흡수응력 특성곡선을 정의할 수 있음을 밝혔다. 그리고 흡수응력에 근거하여 유효응력을 정의할 수 있었다. 다양한 모관흡수력 하에서 $K_0$ 경로는 유효응력에 의하여 유일한 직선으로 기술될 수 있었다. 또한 측정된 $K_0$ 값은 유효응력에 의하여 임의의 모관흡수력에 대하여 일정한 값으로 분석되었다. $K_0$ 압밀경로로부터 구한 흡수응력 특성곡선은 파괴규준으로부터 구한 것과 일치한다. 특히 함수특성곡선으로부터 구한 흡수응력 특성곡선이 $K_0$ 압밀 경로 및 파괴시 응력에서 나타나는 유효응력 거동을 모두 일관되게 기술할 수 있었다. 흡수응력 특성곡선에 기반한 유효응력은 압밀에서 파괴에 이르는 불포화토의 전 거동을 기술할 수 있다.
Fatigue crack propagation tests for the brake disc cast iron were conducted for investigating fatigue crack propagation rate(da/dN), crack propagation path and fracture toughness($K_c$) of the material. The threshold stress intensity factor range, ${\Delta}K_{th}$, was found to be about $6MPa{\sqrt{m}}$ at the stress ratio of R = 0.1. Also, fracture toughness value was determined to be $24.7MPa{\sqrt{m}}$. Irregular fatigue fracture surfaces were observed, indicating that fatigue crack growth occurred at the interface between randomly scattered flak graphite and ferrite, where the interfacial strength was relatively weak.
대응력반전시 모래의 거동을 연구하기 위하여 여러 가지 응력경로에 따른 비틀림전단시험이 수행되었다. 응력경로는 토르크의 작용방향에 따라 시계방향과 반시계방향으로 구분할 수 있으며 대응력반전을 포함하는 응력경로에 대한 소성변형률증분의 방향이 응력상태 및 응력증분의 방향과 비교된다. 이들 시험 결과로부터, St, Venant의 원리를 이용한 등방경화이론은 최초재하와 파괴점 부근에서 소성변형률증분의 방향이 응력의 방향과 일치하는 좋은 결과를 나타내었으나 응력반전에 의한 감하과 재재하 부분에서는 차이가 있는 것으로 나타났다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.