• Title/Summary/Keyword: Stored granular materials

Search Result 5, Processing Time 0.065 seconds

Effect of Storage Conditions on the Setting Properties of Brushite Bone Cement Containing Granular β-Tricalcium Phosphate (과립형 β-삼인산칼슘을 사용한 Brushite계 골시멘트의 보관 조건에 따른 경화 특성)

  • Lee, Sun-Ae;Chung, Tai-Joo;Oh, Kyung-Sik
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.10
    • /
    • pp.625-630
    • /
    • 2008
  • In the bone cement composed of dense granules of $\beta-Ca_3(PO_4){_2}(\beta-TCP)$ and $Ca(H_2PO_4){_2}H_2O$, the compressive strength, setting time and temperature rise were measured to observe the degradation of cement with respect to the stored days before setting. Decreases of compressive strength and temperature rise were observed, while setting time increased with respect to the stored days. The similar trends were repeated with the increase of temperature of storage. Such a change virtually meant the fading of the character of cement and it took place only when the two starting materials were mixed during storage. The degradation could be mitigated taking advantage of granular $\beta$-TCP instead of powdery one. The formation of $CaHPO_4$, which resulted from reaction with ambient humidity, was attributed to the degradation observed during storage. Dependence of the degradation behavior on mixing and temperature during storage was discussed in terms of the driving force for reaction of cement.

Experiments on granular flow in a hexagonal silo: a design that minimizes dynamic stresses

  • Hernandez-Cordero, Juan;Zenit, R.;Geffroy, E.;Mena, B.;Huilgol, R.R.
    • Korea-Australia Rheology Journal
    • /
    • v.12 no.1
    • /
    • pp.55-67
    • /
    • 2000
  • In this paper, an experimental study of the rheological behavior of granular flow in a new type of storage silo is presented. The main characteristic of the new design is a hexagonal shape chosen with the objective of minimizing the stresses applied to the stored grains, and to reduce grain damage during the filling and emptying processes. Measurements of stress distribution and flow patterns are shown for a variety of granular materials. Because of the design of the silo, the granular material adopts its natural rest angle at all times eliminating collisional stresses and impacts between grains. A homogeneous, low friction flow is naturally achieved which provides a controlled stress distribution throughout the silo during filling and emptying. Secondary dynamic stresses, which are responsible for wall failure in conventional silos of the vertical type, are completely eliminated. A comparison between the two geometries is presented with data obtained for these silos and a number of granular materials. The discharge pattern inhibits powder formation in the silo and the filling system virtually eliminates unwanted material packing. Finally, notwithstanding the rheological advantages of this new design, the hexagonal cells that constitute the silo have many other advantages, such as the possible use of solar energy to control the humidity inside them. The cell type design allows for versatile storage capabilities and the elevation above the ground provides unlimited transportation facilities during emptying.

  • PDF

Microstructure and Mechanical Properties of High Strength and Stretch-Flangeability Hot-Rolled Steels (고강도-신장플랜지성 열연강의 미세조직 및 기계적 성질)

  • Chun, Eun-Joon;Lee, Ju-Seung;Do, Hyeong-Hyeop;Kim, Seong-Ju;Park, Yong-Ho;Kang, Nam-Hyun
    • Korean Journal of Materials Research
    • /
    • v.22 no.1
    • /
    • pp.16-23
    • /
    • 2012
  • Research into the development of high strength (1 GPa) and superior formability, such as total elongation (10%), and stretch-flangeability (50%) in hot-rolled steel was conducted with a thermomechanically controlled hot-rolling process. To improve the overall mechanical properties simultaneously, low-carbon steel using precipitation hardening of Ti-Nb-V multimicroalloying elements was employed. And, ideal microstructural characteristics for the realization of balanced mechanical properties were determined using SEM, EBSD, and TEM analyses. The developed steel, 0.06C-2.0Mn-0.5Cr-0.2(Ti + Nb + V), consisted of ferrite as the matrix phase and second phase of granular bainite with fine carbides (20-50 nm) in both phases. The significant factor of the microstructural characteristics that affect stretch-flangeability was found to be the microstructural homogeneity. The microstructural homogeneity, manifest in such characteristics as low localization of plastic strain and internally stored energy, was identified by grain average misorientation method, analyzed by electron backscattered diffraction (EBSD) and hardness deviation between the phases. In summar, a hot-rolled steel having a composition 0.06C-2.0Mn-0.5Cr-0.2(Ti + Nb + V) demonstrated a tensile strength of 998 MPa, a total elongation of 19%, and a hole expansion ratio of 65%. The most important factors to satisfy the mechanical property were the presence of fine carbides and the microstructural homogeneity, which provided low hardness deviation between the phases.

Proposed Design Guidelines for Optimum Economic Silo (사일로의 경제적인 설계 기준 제시)

  • Ko, Hune-Bum
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.17 no.1
    • /
    • pp.389-398
    • /
    • 2016
  • Previous domestic studies on silos have been carried out in many ways in various fields. On the other hand, research on the design and construction of the silo itself have not be conducted actively and an economical approach is rare. The present study provides basic information to determine the scale of the most economical silo, while satisfying the necessary conditions required by construction companies or design firms. The analysis was carried out with various parameters for reinforced concrete structures, including four kinds of storage material (flour, granulated quicklime, sand, and iron ore), five capacity sizes (10,000, 30,000, 50,000, 70,000, 90,000 ton), eight variants of H/D (0.5~4), and three types of concrete compressive strengths (30, 35, 40 MPa). The findings established a general rule in that a silo designed between 1 and 3 H/D with a greater concrete strength (40MPa and over) depending on the type of storage material would be the most cost-effective (more than 50% of quantity and labor savings).

Study for the Conservation Treatment of the Stele for National Preceptor Hongbeop from the Jeongtosa Temple Site in Chungju (충주 정토사지 홍법국사탑비의 보존과학적 연구)

  • Chae, Woomin;Hwang, Hyunsung
    • Conservation Science in Museum
    • /
    • v.19
    • /
    • pp.1-18
    • /
    • 2018
  • The Stele for National Preceptor Hongbeop from the Jeongtosa Temple site in Chungju is one of the most important stone cultural heritage items for exemplifying the style of the Goryeo era. Despite its obvious value, this relic has been stored in a weathered condition at the National Museum of Korea. It had suffered various dismantling and displacements during the Japanese colonial period and had long been exposed in the open air. The stele was selected as a subject for the Stone Monuments Restoration Project launched by the National Museum of Korea in 2015. In preparation for its outdoor exhibition as part of the restoration project, this study investigated the characteristics of its materials, produced a map of its deterioration from weathering, and carried out ultrasonic analysis of the materials to provide findings useful for conservation treatment. The materials analysis revealed that the turtle-shaped pedestal of the stele was made from two-mica granite consisting of medium-grained quartz, plagioclase, alkali feldspar, biotite, and muscovite. Its body stone is crystalline marble, the rock-forming mineral in which is medium-grained calcite in a rose-pink color with dark grey spots. The dragon top of the stele is made of crystalline marble, the major component of which is medium-grained calcite of a light-grey color. The deterioration consists of 21.5% abrasion on the stone body, with its south face most damaged, and 18.6% granular disintegration, with the north face most damaged. The ultrasonic material characterization conducted for mapping the general condition of weathering shows low values on the parts-assembly area of the turtle-shaped pedestal and on the upper portion of the stone body. It is considered that there is dislocation due to partial blistering and fracturing as well as to the differences in surface treatment. Prior to the outdoor exhibition of the stele, the surface was cleaned of contaminants and was consolidated based on the scientific investigation in order to prevent weathering from the external environment.