• 제목/요약/키워드: Storage modulus

검색결과 335건 처리시간 0.026초

Effect of temperature on the rheological properties of dental interocclusal recording materials

  • Pae, Ahran;Lee, Ho-Rim;Kim, Hyeong-Seob
    • Korea-Australia Rheology Journal
    • /
    • 제20권4호
    • /
    • pp.221-226
    • /
    • 2008
  • The purpose of this study was to compare rheological properties of six dental interocclusal recording materials and to investigate the effect of temperature on the rheological properties during setting. Five polyvinylsiloxane materials and one polyether material were investigated in this study. The storage modulus (G') and the loss factor ($tan{\delta}$) were measured from 30s after mixing during setting, using the universal dynamic spectrometer. Viscoelastic properties were evaluated by means of G' and $tan{\delta}$ from 5 repeats at $21^{\circ}C$ and $33^{\circ}C$. Individual changes during setting were also evaluated. All data were statistically analyzed using one-way ANOVA and multiple comparison $Scheff{\acute{e}}$ test at the significance level of 0.05. The mean of G was checked at $t_{set}$ (the setting time provided from manufacturer) and $t_{300}$ (the end of experimental time) and the mean of $tan{\delta}$ was checked at to and $t_{set}$. Whereas the increase of the G' value showed generally exponential changes at $21^{\circ}C$, the change of the G' value at $33^{\circ}C$ displayed sigmoidal curves during setting. The change of loss factor $tan{\delta}$ during setting varied. Within the limitations of this study, dental interocclusal recording materials had different viscoelastic properties and most of the materials showed different fluidity at $21^{\circ}C$ and $33^{\circ}C$.

자외선 경화형 점착제의 접착 및 재박리 특성 (Adhesive and Removable Characteristics of UV Curable Adhesive)

  • 김인범;이명천
    • Korean Chemical Engineering Research
    • /
    • 제46권1호
    • /
    • pp.76-81
    • /
    • 2008
  • 아크릴계 점착제를 합성한 후 이관능성 혹은 육관능성 우레탄-아크릴레이트 올리고머를 혼합하여 자외선 경화형 점착제를 제조하였다. 올리고머 종류 및 함량을 변화시켜 그에 따른 접착력 변화와 재박리 특성을 조사하였다. 자외선 경화전에는 올리고머의 함량의 증가에 따라 박리력이 증가하였으나 자외선 경화 후에는 감소하는 경향을 보였다. 저장 탄성률(G')이 낮을수록 박리력은 증가하지만 점착제 내부의 상용성과 손실계수(tan ${\delta}$) 값에 따라 점착제의 박리정도와 접착력에 영향을 주는 것을 확인할 수 있었다.

충격 보강제와 탈크를 이용한 PLLA 얼로이 연구 (Study on PLLA Alloys with Impact Modifier and Talc)

  • 정동석;남병욱;장미옥;홍채환
    • Elastomers and Composites
    • /
    • 제45권2호
    • /
    • pp.129-136
    • /
    • 2010
  • 본 연구는 이축 압출기를 사용하여 생분해성 고분자인 Poly-L-lactic acid(PLLA)와 충격보강제로 Poly (ethylene-co-glycidyl methacrylate)(EGMA)와 Engage를 각각 PLLA에 대해 100/0, 75/25, 50/50, 25/75, 0/100의 조성으로 블렌드를 제조하였고, 3개의 PLLA/EGMA 블렌드에는 탈크를 첨가하였다. 이를 DMA, FESEM, UTM, Izod 충격시험기를 사용하여 PLLA 블렌드의 모폴로지와 점탄성, 기계적 특성을 측정하였다. DMA와 충격시험기의 측정결과 EGMA와 Engage의 함량이 증가함에 따라 상온에서의 저장탄성률이 감소하였고, 충격강도는 증가하였다. 한편 탈크가 첨가되면 저장탄성률은 증가하고 충격강도는 감소하였다. FESEM 분석으로부터, 매트릭스에 도메인이 잘 분산되어 있음을 알 수 있었고, UTM을 통하여 EGMA와 Engage의 함량이 증가하면 굴곡탄성률과 인장강도가 감소되지만, 탈크를 첨가함으로써 이를 보완할 수 있었다.

젤라틴의 동적 레올로지 특성 (Dynamic Rheological Properties of Gelatin)

  • 최윤희;임승택;유병승
    • 한국식품과학회지
    • /
    • 제34권5호
    • /
    • pp.830-834
    • /
    • 2002
  • 본 연구는 동적 전단진동(dynamic shear oscillation) 측정방법을 이용하여 농도가 젤라틴의 동적 레올로지 특성에 미치는 영향에 대하여 관찰하였다. $5^{\circ}C$에서의 젤라틴의 저장 탄성률(storage modulus, G#)과 손실 탄성률(loss modulus, G@)은 농도가 증가함에 따라 증가하는 경향을 보였다. 0.9%를 제외한 모든 농도(2.0-4.9%)에서 젤라틴의 G#은 G@보다 매우 높은 값을 나타냈으며, G#과 G@이 ${\omega}$ 의존성이 없는 true 겔과 같은 거동을 나타냈다. 젤라틴의 농도와 K#(G#에 대한 절편)와의 관계에서는 높은 결정계수$(R^2=0.99)$를 보여주면서 좋은 상관관계를 나타냈다. 여러 온도범위$(-5,\;0,\;5,\;10^{\circ}C)$에서 각 온도별로 측정된 K#값은 $-5^{\circ}C(59.5Pa)\;>\;0^{\circ}C(4.09Pa)\;>\;5^{\circ}C(1.41Pa)\;>\;10^{\circ}C(0.35Pa)$의 순으로 가장 낮은 온도에서 K#값이 가장 높은 것으로 나타났다. 또한 냉각과정에서 최종냉각온도인 $5^{\circ}C$에서 측정된 젤라틴의 최대 G#수치는 4.9%(2399Pa)>4.1%(1744Pa)>3.0%(1159Pa)>2.0%(519.3Pa)>0.9%(3.15Pa)의 순으로 높은 농도에서 높게 나타났다. Aging 10시간 동안 젤라틴 겔의 구조형성은 겉보기 first-order kinetics로부터 겉보기 구조형성 속도상수(K)를 결정함으로써 파악될 수 있다. 젤라틴의 농도가 증가함에 따라 K값은 증가하였으며, 농도와 K값과의 관계는 높은 결정계수$(R^2)$를 나타내면서 좋은 상관관계를 보여주었다(Fig. 7). 10시간 aging 후 G#은주파수$({\omega})$ 의존성이 없이 독립적인 것으로 나타났다. 따라서 이들 젤라틴 겔은 aging하는 동안에 탄성이 점점 강해지고 10시간 후에는 가교결합의 밀도가 증가하여 강한 탄성을 가진 고무질 망상구조(rubber network)를 형성했음을 알 수 있다.

Peroxide 개질에 따른 Nylon 12 elastomer의 특성 연구 (Peroxide Modification of Nylon 12 Elastomer)

  • 최명찬;정지연;장영욱
    • Elastomers and Composites
    • /
    • 제48권1호
    • /
    • pp.18-23
    • /
    • 2013
  • 용융상태에서 nylon 12 elastomer에 소량의 dicumyl peroxide (DCP) 와 triallyl cyanuate (TAC)를 첨가하여 nylon 12 elastomer를 부분적으로 가교시켰으며, 이에 따른 nylon 12 elastomer의 기계적, 동적기계적 그리고 유변학적 특성을 tensile test, DMA, small amplitude oscillating rheometer를 이용하여 각각 알아보았다. TAC의 함량이 증가함에 따라 인장탄성률과 영률은 증가하고, 파단신율은 감소하였다. DMA 측정결과, DCP로 부분적으로 가교시킨 nylon 12 elastomer의 PTMG상의 유리전이온도는 순수한 nylon 12 elstomer에 비해 증가하였고, storage modulus는 nylon 12상의 용융온도 이상에서도 거의 일정한 값을 나타내었다. 부분적으로 가교시킴에 따른 유변학적 특성의 변화는 TAC의 함량이 증가함에 따라 solid like behavior와 shear thinning behavior가 점점 뚜렷하게 나타남을 알 수 있었다. 이로부터 nylon 12 elastomer를 용융상태에서 부분적으로 가교시킴으로써 용융가공성을 저하시키지 않으면서, 기계적 물성은 효과적으로 향상시킬 수 있었으며, 특히, nylon 12 elastomer의 사용가능 온도범위를 증가시킬 수 있었다.

실란커플링제 처리가 폴리케톤섬유/에폭시 복합재료의 계면접착성 및 물성에 미치는 영향 (Effect of Silane Coupling Agent on the Interfacial Adhesion and Mechanical Properties of Polyketone Fiber Reinforced Epoxy Composites)

  • 조하니;양지우;임현수;오우진;이승구
    • 한국염색가공학회지
    • /
    • 제29권2호
    • /
    • pp.77-85
    • /
    • 2017
  • The interfacial adhesion between fiber and matrix affects the physical properties of fiber reinforced composites. In this study, 3-(Methacryloyloxy)propyltrimethoxy silane(MPS) coupling agent was used to increase the interfacial adhesion between polyketone fiber and epoxy resin. The change of surface chemical composition of polyketone fiber treated with MPS was analyzed using a FTIR-ATR. The interfacial bonding between fiber and resin increased with silane coupling agent largely. Consequently, interfacial shear strength(IFSS) was enhanced with increasing concentration of MPS coupling agent and thus, the physical properties of the composites such as flexural properties and dynamic mechanical properties were changed. Flexural strength and modulus increased when the MPS concentration was higher than 0.5wt%. The dynamic storage modulus of Polyketone/Epoxy composites treated with MPS was higher than that of the untreated one. When the MPS concentration of 3wt%, the highest storage modulus was obtained.

Rheology of concentrated xanthan gum solutions: Oscillatory shear flow behavior

  • Song Ki-Won;Kuk Hoa-Youn;Chang Gap-Shik
    • Korea-Australia Rheology Journal
    • /
    • 제18권2호
    • /
    • pp.67-81
    • /
    • 2006
  • Using a strain-controlled rheometer, the dynamic viscoelastic properties of aqueous xanthan gum solutions with different concentrations were measured over a wide range of strain amplitudes and then the linear viscoelastic behavior in small amplitude oscillatory shear flow fields was investigated over a broad range of angular frequencies. In this article, both the strain amplitude and concentration dependencies of dynamic viscoelastic behavior were reported at full length from the experimental data obtained from strain-sweep tests. In addition, the linear viscoelastic behavior was explained in detail and the effects of angular frequency and concentration on this behavior were discussed using the well-known power-law type equations. Finally, a fractional derivative model originally developed by Ma and Barbosa-Canovas (1996) was employed to make a quantitative description of a linear viscoelastic behavior and then the applicability of this model was examined with a brief comment on its limitations. Main findings obtained from this study can be summarized as follows: (1) At strain amplitude range larger than 10%, the storage modulus shows a nonlinear strain-thinning behavior, indicating a decrease in storage modulus as an increase in strain amplitude. (2) At strain amplitude range larger than 80%, the loss modulus exhibits an exceptional nonlinear strain-overshoot behavior, indicating that the loss modulus is first increased up to a certain strain amplitude(${\gamma}_0{\approx}150%$) beyond which followed by a decrease in loss modulus with an increase in strain amplitude. (3) At sufficiently large strain amplitude range (${\gamma}_0>200%$), a viscous behavior becomes superior to an elastic behavior. (4) An ability to flow without fracture at large strain amplitudes is one of the most important differences between typical strong gel systems and concentrated xanthan gum solutions. (5) The linear viscoelastic behavior of concentrated xanthan gum solutions is dominated by an elastic nature rather than a viscous nature and a gel-like structure is present in these systems. (6) As the polymer concentration is increased, xanthan gum solutions become more elastic and can be characterized by a slower relaxation mechanism. (7) Concentrated xanthan gum solutions do not form a chemically cross-linked stable (strong) gel but exhibit a weak gel-like behavior. (8) A fractional derivative model may be an attractive means for predicting a linear viscoelastic behavior of concentrated xanthan gum solutions but classified as a semi-empirical relationship because there exists no real physical meaning for the model parameters.

유동성 및 응축성 복합레진의 점탄성에 관한 유변학적 연구 (RHEOLOGIC STUDY ON THE VISCOELASTIC PROPERTIES OF FLOWABLE AND CONDENSABLE RESIN COMPOSITES)

  • 이인복;조병훈;손호현;권혁춘;엄정문
    • Restorative Dentistry and Endodontics
    • /
    • 제25권3호
    • /
    • pp.359-370
    • /
    • 2000
  • The purpose of this investigation was to observe the viscoelastic properties of five commercial flowable(Aeliteflo, Flow it, Revolution, Tetric flow, Compoglass flow), three conventional hybrid(Z-100, Z-250, P-60) and two condensable(Synergy compact, SureFil) resin composites. A dynamic oscillatory shear test was done to evaluate the storage shear modulus (G'), loss shear modulus(G"), loss tangent(tan ${\delta}$) and complex viscosity(${\eta}^*$) of the resin composites as a function of frequency - dynamic frequency sweep test from 0.01 to 100 rad/s at $25^{\circ}C$ - by using Advanced Rheometric Expansion System(ARES). To investigate the effect on the viscosity of resin composites of filler volume fraction, the filler weight % and volume % were measured by means of Archimedes' principle using a pyknometer. The results were as follows 1. The complex viscosity ${\eta}^*$ of flowable resins was lower than that of hybrid resins and significant differences were observed between brands. The complex viscosity ${\eta}^*$ of condensable resins was higher than that of hybrid resins. The order of complex viscosity ${\eta}^*$ at ${\omega}$=10 rad/s was as follows, Surefil, Synergy compact, P-60, Z-250, Z-100, Aeliteflo, Tetric flow, Compoglass flow, Flow it, Revolution. The relative complex viscosity of flowable resins compared to Z-100 was 0.04~0.56 but Surefil was 30.4 times higher than that of Z-100. 2. The storage shear modulus G' and the loss shear modulus G" of flowable resins were lower than those of hybrid resins but those of condensable resins were higher. The patterns of the change of loss tangent, tan ${\delta}$, of resin composites with increasing frequency were significantly different between brands. The phase angles, ${\delta}$, ranged from $30.2{\sim}78.1^{\circ}$ at ${\omega}$=10 rad/s. 3. All composite resins represent pseudoplastic nature with increasing shear rate. 4. The complex shear modulus $G^*$ and the phase angle ${\delta}$ was represented by the frequency domain phasor form, $G^*({\omega})=G^*e^{i{\delta}}=G^*{\angle}{\delta}$. The locus of frequency domain phasor plots in a complex plane was a valuable method that represent the viscoelastic properties of composite resins. 5. There was no direct linear correlationship but a weak positive relation was observed between filler volume % or weight % and the viscosity of the resin composites.

  • PDF

Deformation Behaviour of Metamorphic Tuff from Plate Loading Test

  • Lee, Young-Nam;Suh, Young-Ho;Kim, Dae-Young
    • 한국지반공학회지:지반
    • /
    • 제13권3호
    • /
    • pp.87-100
    • /
    • 1997
  • 본 논문에서는 건설 중인 국내의 한 지하 원유비축기지의 기반암인 변성응회암의 변형특성을 파악하고 변형계수를 결정하기 위하여 평판재하시험 및 불연속체 수치해석을 수행하였다. 평판 재하시험에서는 직경 1m의 flat jack을 이용하여 최대 14MPa의 하중을 기반암에 가하고 이에 대한 반력장치로서 록 앵커 시스템을 이용하였다. 본 시험으로부터 얻어진 변형계수 결과치는 실내시험, 이축압축시험, 공내재하시험 등에서 구한 값들과 비교되었다. 그 결과, 평판재하시험에서 구한 변형계수는 신선한 암편 탄성계수의 약 50%정도인 것으로 나타났으며, 현지 기반암의 변형계수는 암반에 분포하는 절리들로 인하여 25-350pa의 범위에 속하는 것으로 판정되었다. 또한 시험 부지내에 분포하는 여러 불연속면들을 고려한 불연속체 해석을 실시하여 평판재 하시험을 모사하고 절리들이 암반의 변형특성에 미치는 영향을 분석하였다.

  • PDF

Effect of Homogenization Pressure and Supplementation with Sucrose Fatty Acid Ester on the Physical Properties of Dairy Cream-based Emulsions

  • Seo, Chan-Won;Kang, Shin-Ho;Shin, Yong-Kook;Yoo, Byoungseung
    • 한국축산식품학회지
    • /
    • 제38권3호
    • /
    • pp.476-486
    • /
    • 2018
  • In this study, the droplet size distribution, rheological properties, and stability of dairy cream-based emulsions homogenized with different sucrose fatty acid ester (SFAE, a non-ionic small-molecule emulsifier) concentrations (0.08%, 0.16%, and 0.24% w/w) at different homogenization pressures (10 MPa and 20 MPa) were examined. Homogenization at a high pressure resulted in a smaller droplet size and narrower droplet size distribution. The D[4,3] (volume-weighted mean) and D[3,2] (surface-weighted mean) values of the emulsions decreased with an increase in the SFAE concentration. The flow properties of the emulsions homogenized with SFAE showed shear-thinning (n=0.21-0.46) behavior. The apparent viscosity (${\eta}_{a,10}$) and consistency index (K) of the homogenized emulsions were lower than those of the control sample that is non-homogenized and without SFAE, and decreased with an increase in SFAE concentration. The storage modulus (G') and loss modulus (G") of all emulsions homogenized with SFAE were also lower than those of the control sample. The stability of all emulsions with SFAE did not show any significant change for 30 d at $5^{\circ}C$. However, the emulsions stored at $40^{\circ}C$ were unstable over the storage period. Therefore, the addition of SFAE enhanced the stability of dairy cream emulsions during storage at refrigeration temperature ($5^{\circ}C$).